압전변압기용 PT-PZ-PNN 세라믹스의 그레인 크기에 따른 압전특성 (The Piezoelectric Characteristics Depending on the GrainSize of the PT-PZ-PNN Ceramics)

  • 박정호;김철수;김성곤;이상렬
    • 한국전기전자재료학회논문지
    • /
    • 제14권10호
    • /
    • pp.815-820
    • /
    • 2001
  • The piezoelectric properties of the PT-PZ-PNN system ceramics were investigated depending on the variati on of the grain size. The grain size was varied by sintering temperature, and additive. The effect of the grain size on the electrical, dielectric, and piezoelectric properties was studied with respect to the feasibility of the application for the piezoelectric transformer. Grain size increased as the PMW contents increased. The smaller the particle size used, the smaller the grain size obtained. Specimens are densily sintered. Dielectric and piezoelectric properties are not always improved in proportion to the grain sizes. When he particle size are fine and the grain size are increased properly with the optimum additives, the piezoelectric preperties have good values. the specimen sintered at 1200$\^{C}$ with PMW 2 mol% and MnO$\_$2/ 0.5wt% contents exhibited good piezoelectric properties for a piezoelectric transformer.

  • PDF

CuO첨가에 따른 $(K_{0.5}Na_{0.5})_{0.97}(Nb_{0.96}Sb_{0.04})O_3$세라믹스의 유전 및 압전 특성 (Dielectric and piezoelectric properties of CuO added $(K_{0.5}Na_{0.5})_{0.97}(Nb_{0.96}Sb_{0.04})O_3$ ceramics)

  • 이유형;박민호;노정래;류주현;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.160-161
    • /
    • 2009
  • In this study, in order to develop the lead free piezoelectric ceramics with excellent piezoelectric properties, (Na,K)$NbO_3$ ceramics according to the amount CuO addition were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated. At the 0.8mol% CuO added composition, density, electromechanical coupling factor(kp), echanical quality factor(Qm), dielectric constant$(\varepsilon_r$) and piezoelectric constant($d_{33}$) showed the optimum value of $4.459g/cm^3$, 0.469, 540, 410, 69.57pC/N, respectively.

  • PDF

소결시간변화에 따른 (Na,K)NbO3계 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Characteristics of (Na,K)NbO3 Ceramics System According to Sintering Time)

  • 김도형;류주현;김인성;송재성
    • 한국전기전자재료학회논문지
    • /
    • 제21권10호
    • /
    • pp.901-905
    • /
    • 2008
  • In this study, $0.95(K_{0.5}Na_{0.5})NbO_{3}-0.05Li(Sb_{0.8}Nb_{0.2})O_{3}+0.2\;wt%Ag_{2}O$ were investigated as a variations of sintering times in order to improve dielectric and piezoelectric properties of lead-free piezoelectric ceramics. $Ag_{2}O$ were used as sintering aids and the specimens were sintered during 3, 5, 7, 9 and 11 hours, respectively. At the specimen sintered during 7 hour, Electromechanical coupling factor ($k_p$), density, dielectric constant (${\epsilon}_{\gamma}$), piezoelectric constant ($d_{33}$) and curie temperature ($T_c$) of composition ceramics showed the optimal value of 0.450, 4.274 $[g/cm^3]$, 1007, 257 [pC/N] and $396^{\circ}C$, respectively.

저온소결 압전변압기용 PMW-PMN-PZT 의 압전특성 (Piezoelectric Characteristics of Low temperature sintering PMW-PMN-PZT Ceramics for Piezoelecric Transformer)

  • 이현석;정광현;류주현;박창엽;류성림;정영호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.214-215
    • /
    • 2005
  • In this paper, in order to develop low temperature sintering piezoelectric ceramics for piezoelectric transformer, PMW-PMN-PZT ceramics using 0.25wt%$CaCO_3$ and 0.2wt%$Li_2CO_3$ as sintering aids were fabricated according to the variation of amount of PMW and Zr/Ti ratio. Specimens could be sintered at 900$^{\circ}C$ by adding sintering aids. As Zr/Ti ratio was increased, kp was increased and Qm was decreased by approaching MPB region, and kp showed the largest value of 0.58 at Zr/Ti:50/50. The variation of amount of PMN substitution affected the liquid phase sintering of the ceramics using sintering aids, and decreased piezoelectric properties.

  • PDF

ZnO가 첨가된 (Na,K)NbO3계 세라믹스의 압전 특성 (Piezoelectric Properties in ZnO Dopped (Na,K)NbO3 Ceramics)

  • 류성림;권순용;어순철;김시철;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제19권8호
    • /
    • pp.707-711
    • /
    • 2006
  • ZnO was doped up to 0.3 wt% for improving the electrical properties of lead-free $[Li_{0.04}(Na_{0.44}Ko_{0.52})-(Nb_{0.86}\;Ta_{0.10}\;Sb_{0.04})]O_3$ piezoelectric ceramics. The ceramics were fabricated with the conventional sintering processes. Crystal structure of the samples was tetragonal phase regardless of ZnO amount. However, the piezoelectric properties were varied with the ZnO amount. The electro-mechanical coupling factor $(k_p)$ was with the ZnO amount up to 0.2 wt% but decreased with the further addition. the maximum value of $k_p$ was 0.475. Density, piezoelectric charge constant and relative dielectric constant was also showed maximum value at 0.2 wt%. The maximum values are $4.75g/cm^3$, 275 pC/N, 1403, respectively. In contrast, the mechanical quality factor $(Q_m)$ was not varied with increasing the ZnO addition up to 0.2 wt% but rapidly increased at 0.3 wt%.

CuO가 PSN-PZT세라믹스의 저온소결 특성에 미치는 영향 (Effects of CuO on Low-temperature Sintering Characteristics of PSN-PZT System Ceramics)

  • 류주현;우원희;오동언;정영호;정광현;정문영;정회승
    • 한국전기전자재료학회논문지
    • /
    • 제16권12S호
    • /
    • pp.1200-1204
    • /
    • 2003
  • In this study, in order to develop the low temperature sintering ceramics for multi-layer piezoelectric transformer, PSN-PZT system ceramics were manufactured as a function of CuO addition and their dielectric and piezoelectric characteristics were Investigated. CuO addition facilitated densification at low temperature due to the effect of Cu$_2$O-PbO liquid phase. Through the X-ray diffraction pattern study, absence of second phase unwanted was confirmed. Among the specimen to which CuO was added, the 0.6wt% CuO added specimen sintered at 900$^{\circ}C$ and 920$^{\circ}C$ showed the most excellent mechanical quality factor and electromechanical coupling factor, respectively. Besides the densification accelerator, CuO acted as a accepter and increased mechanical quality. Compared with the specimen with no addition sintered at 1150$^{\circ}C$ , the 0.6wt% CuO added specimen sintered at 920$^{\circ}C$ showed the appropriate dielectric and piezoelectric characteristics for multi-layer piezoelectric transformer.

PZT-PSN 세라믹스의 WO3의 첨가량에 따른 압전 특성 (Piezoelectric Characteristics of PZT-PSN Ceramics Depending on WO3Addition)

  • 배숙희;김성곤;김철수;이경화;이상렬
    • 한국전기전자재료학회논문지
    • /
    • 제15권9호
    • /
    • pp.794-797
    • /
    • 2002
  • Piezoelectric properties of PZT-PSN ceramics were investigated as a function of WO$_3$ addition from 0 wt% to 6.0 wt%. The dielectric and piezoelectric characteristics of PZT-PSN ceramics have been investigated at different calcination (80$0^{\circ}C$~90$0^{\circ}C$) and sintering (110$0^{\circ}C$~130$0^{\circ}C$) temperatures. The grain size was increased with the addition of WO$_3$and the sintering temperatures. Anisotropic properties of electromechanical coupling coefficient and piezoelectric coefficient are proven to be dependent on processing temperatures and amount of addition. At the specimen with 0.6 wt% WO$_3$ addition, using calcination temperature of 80$0^{\circ}C$ and sintering temperature of 110$0^{\circ}C$ , mechanical quality factor(Q$_{m}$) and electromechanical coupling coefficient(k$_{p}$) showed the excellent results of 1560 and 0.48, respectively Experimental results indicated that the PZT-PSN system ceramics with WO$_3$impurity could be effectively used for the microtransformer and actuator applications, etc.etc.

$(Na_xK_{0.94-x}Li_{0.06})NbO_3$ 세라믹스의 압전 및 유전 특성 (Piezoelectric Properties of Lead-Free $(Na_xK_{0.94-x}Li_{0.06})NbO_3$ Ceramics)

  • 전소현;김민수;박정주;전순종;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.276-276
    • /
    • 2007
  • As a candidate for lead-free piezoelectric materials, dense $(Na_xK_{0.94-x}Li_{0.06})NbO_3$ ceramics were developed by conventional sintering process. Sintering temperature was lowered by adding 1 mol% $Li_2O$ as a sintering aid. The electrical properties of $(Na_xK_{0.94-x}Li_{0.06})NbO_3$ ceramics were investigated as a function of Na/K ratio. When the sample sintered at $950^{\circ}C$ for 4 h with the compositions of morphotropic phase boundary, 0.47 < x < 0.51, electro-mechanical coupling factor ($k_p$) and piezoelectric coefficient ($d_{33}$) were found to reach the highest values of 0.42 and 190 pC/N, respectively. These excellent piezoelectric and electro-mechanical properties indicate that this system is potentially good candidate for lead-free material for a wide range of electro-mechanical transducer applications.

  • PDF

하소온도변화에 따른 (Na,K)NbO3계 무연 압전세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Characteristics of Lead-free (Na,K)NbO3 Piezoelectric Ceramic System according to Calcination Temperature)

  • 류성림;정광현;류주현;이병률;정영호
    • 한국전기전자재료학회논문지
    • /
    • 제18권9호
    • /
    • pp.821-826
    • /
    • 2005
  • In this paper, in order to develop lead-free piezoelectric ceramics, $(Li_{0.04}Na_{0.44}K_{0.52)(Nb_{0.86}Ta_{0.10}Sb_{0.04})O_3$ ceramics were fabricated with the variation of calcination temperature and sintering temperature. The ceramics couldn't be sintered at temperature less than $1110^{\circ}C$ and showed the highest density at calcination temperature of $800^{\circ}C$. Crystal structure of the ceramics showed pseudo-tetragonal phase. At the calcination temperature of $800^{\circ}C$ and sintering temperature of $1110^{\circ}C$, the optimal values of $density=4.64g/cm^3,\;kp=0.45,\;{\varepsilon}r=1336,\;d_{33}=254pC/N\;and\;Tc=335^{\circ}C$ were obtained.

$Bi_2O_3$ 첨가에 따른 (Na,K,Li)$NbO_3$계 무연 압전 세라믹스의 압전특성 (The Piezoelectrc properties of (Na,K)$NbO_3$-system Pb-free Piezoelectric Ceramics with $Bi_2O_3$ Addition)

  • 류성림;이호일;배세환;김주현;김용주;서상현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.216-217
    • /
    • 2005
  • In this paper, in order to develop Pb-free piezoelectric ceramics, $(Li_{0.05}Na_{0.57}K_{0.38})NbO_3$ ceramic was fabricated with the variation of $Bi_2O_3$ addition. Piezoelectric properties of the ceramic were varied with the amount of $Bi_2O_3$ addition and showed the maximum kp value at.0.2 wt% $Bi_2O_3$ addition. Qm of $Bi_2O_3$ added ceramics showed lower values than the non-added ceramics, however, the kp was increased by the addition of $Bi_2O_3$ up to 0.2 wt%. At the sintering temperature of 1110$^{\circ}C$ and the calcination temperature of 850$^{\circ}C$, the optimal values of density=4.52g/$cm^3$, kp=0.47, $\varepsilon_r$=400 were obtained.

  • PDF