• Title/Summary/Keyword: Pb content

Search Result 831, Processing Time 0.026 seconds

Study of properties of $YBa_2Cu_3O_x$ with PbO and $BapbO_3$ additives

  • Soh, Dae-Wha;Fan, Zhanguo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07a
    • /
    • pp.543-546
    • /
    • 2004
  • The melting temperature and critical temperature(Tc) of $YBa_2Cu_3O_x$ with deferent content impurities of PbO and $BaPbO_3$ were studied. When the PbO was used as addition in $YBa_2Cu_3O_x$, although the melting point could be reduced, the superconductivity(the transition width, ${\Delta}T_c$) became poor. From the XRD pattern of the sintered mixture of $YBa_2Cu_3O_x$ and PbO it was known that there is a reaction between $YBa_2Cu_3O_x$ and PbO, and the product is $BaPbO_3$. In the process of the reaction the superconducting phase of $YBa_2Cu_3O_x$ was decreased and in the sample $BaPbO_3$ became the main phase. Therefore the superconductivity was reduced. $BaPbO_3$ was chosen as the impurity for the comparative study. The single phase BaPbO3 was synthesized by the simple way from both mixtures of $BaPbO_3$ and PbO, $BaPbO_3\;and\;PbO_2$. Deferent contents of $BaPbO_3$(10%, 20%, 30%) were added in the $YBa_2Cu_3O_x$. By the phase analysis in the XRD patterns it was proved that there werenot reactions between $YBa_2Cu_3O_x$ and $BaPbO_3$. When $BaPbO_3$ was used as impurity in $YBa_2Cu_3O_x$ the superconductivity was much better than PbO as impurity in $YBa_2Cu_3O_x$. But the melting point of $YBa_2Cu_3O_x$ with $BaPbO_3$ could not be found when the temperature was lower than $1000^{\circ}C$ in the DTA measurement.

  • PDF

Characteristics of $(Pb_{1-x}La_x)(Zr_{0.5}Ti_{0.5})O_3$ thin films as a function of La content ($(Pb_{1-x}La_x)(Zr_{0.5}Ti_{0.5})O_3$ 박막의 La 치환량에 따른 특성)

  • Jang, Nak-Won;Lee, Seong-Hwan;Yi, Dong-Young;Kim, Dong-Hun
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.30 no.8
    • /
    • pp.894-900
    • /
    • 2006
  • The electrical characteristics associated with crystal structure changes as a function of La content for $(Pb_{1-x}La_x)(Zr_{0.5}Ti_{0.5})O_3$ thin films were investigated for applications in memory capacitors. Tetragonality of PLZT films decreased with increasing La content. Thin films with La $\geq$ 20 mol% were found to be cubic. Films with La $\geq$ 12 mol% exhibited broader dielectric peaks compared to those of bulk ceramics and behaved as relaxer ferroelectrics. Tetragonal PLZT film with 12 mol% La had a dielectric constant maximum of 1330 at room temperature and a charge storage density of ${\sim}18{\mu}C/cm^2$ at 5 V. Decrease in coercive field and remnant polarization with increase in La content were resulting from less dipolar response caused by the decreased crystal anisotropy. The leakage current densities $<10^{-8}A/cm^2$ up to 5 V bias voltage were observed for the films with La $\geq$ 14 mol%.

Chemical Properties in the Soils of Reclaimed and Natural Tidelands of Southwest Coastal Area of Korea (I) - Distribution of Heavy Metal Fractions - (우리나라 서남해안 간척지 및 간석지 토양의 화학적 특성 (I) - 중금속 오염물질의 형태별 함량 분포 -)

  • Cho, Jae-Young;Koo, Ja-Woong;Son, Jae-Gwon
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.48 no.1
    • /
    • pp.3-10
    • /
    • 2006
  • The chemical fractions of heavy metals were investigated in the soils of reclaimed and natural tidelands of southwest coastal area of Korea. The distribution pattern of each heavy metal in different fractions was in the order: 1) Cu : organic bound > organic complex > residual > exchangeable = water soluble. 2) Cr : residual > organic bound > organic complex > water soluble > exchangeable. 3) Pb : organic bound > residual > organic complex > water soluble > exchangeable. 4) Cd residual > organic bound > organic complex > water soluble = exchangeable. 5) Zn : organic bound > residual > organic complex > water soluble > exchangeable. The content of residual Zn showed positive correlation with organic matter content but organic bound Zn showed negative correlation with CEC. The content of residual and exchangeable Cd showed highly positive correlation with organic matter content but residual, organic bound, and exchangeable Cd showed negative correlations with CEC. Water soluble Pb showed positive correlation with CEC but organic bound Pb showed negative correlation with CEC.

Properties of $YBa_2Cu_3O_x$ with PbO and $BaPbO_3$ additives

  • Fan, Zhanguo;Soh, Daewha;Cho, Yongjoon
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • 2004.05a
    • /
    • pp.57-59
    • /
    • 2004
  • The melting temperature and critical temperature (Tc) of YBa$_2$Cu$_3$Ox with deferent content impurities of PbO and BaPbO$_3$ were studied. When the PbO was used as addition in YBa$_2$Cu$_3$Ox, although the melting point could be reduced, the superconductivity (the transition wide, ΔTc) became poor. From the XRD pattern of the sintered mixture of YBa$_2$Cu$_3$Ox and PbO it was known that there is a reaction between YBa$_2$Cu$_3$Ox and PbO, and the product is BaPbO$_3$. In the process of the reaction the superconducting phase of YBa$_2$Cu$_3$Ox was decreased and in the sample BaPbO$_3$became the main phase. Therefore the superconductivity was reduced. BaPbO$_3$was chosen as the impurity for the comparative study. The single phase BaPbO$_3$was synthesized by the simple way from both mixtures of BaPbO$_3$and PbO, BaPbO$_3$and PbO$_2$. Deferent contents of BaPbO$_3$(10%, 20%, 30%) were added in the YBa$_2$Cu$_3$Ox. By the phase analysis in the XRD patterns it was proved that there were not reactions between YBa$_2$Cu$_3$Ox and BaPbO$_3$. When BaPbO$_3$was used as impurity in YBa$_2$Cu$_3$Ox the superconductivity was much better than PbO as impurity in YBa$_2$Cu$_3$Ox But the melting point of YBa$_2$Cu$_3$Ox with BaPbO$_3$could not be found when the temperature was lower than 1000 $^{\circ}C$ in the DTA measurement.

  • PDF

Metabolism Changes in Growing Rats Fed Diets with Different Levels of Lead and Protein (납(Pb)과 단백질 수준을 달리한 식이로 사육한 성장기 흰쥐의 체내대사 변화)

  • 김미경
    • Journal of Nutrition and Health
    • /
    • v.19 no.5
    • /
    • pp.323-332
    • /
    • 1986
  • This study was performed to see the effects of lead poisoning and dietary protein levels(6, 15 and 40 % casein diets) on growth, protein and lipid metabolisms in growing rats. It was also investigated whether the high protein intake would alleviate lead toxicity by decreasing Pb absorption and/or increasing Pb excretion. The results obtained were summarized as follows ; 1) Weight gain, F.E.R liver weight, weight and length of bone in Pb-administered groups were lower than in Pb-free groups. However, these values in the 40% casein diet group with Pb were increased to the level in 15% casein diet group without Pb. 2) Hematocrt and hemoglobin content in blood were lower in Pb -adminstered groups than in Pb free groups. Especially, these levels were lower in 6% casein diet group with Pb than in any other group. 3) Plasma protein level in th e 40% casein casein diet group was the highest of all groups and those of Pb-administered groups tended to be lower than those of Pb-free groups. Plasma lipid and cholesterol levels were increased with decreasing dietary protein level, and these levels were higher in the animals exposed to Pb than in free groups.4) Total liver protein, lipid and cholesterol contents were increased with increasing dietary protein level, and these contents were lower in Pb-administered groups than in Pb free groups. 5) Fecal Pb excretion was not different between 6 and 40% casein diet groups. However, urinary Pb excretion was higher in the 40% casein diet group than in the 6% casein diet group. Above results suggest that, in exposing to the Pb pollution, sufficient protien intake must be recommended. High protein intake seemed to alleviate lead toxicity by increasing urinary Pb excretion.

  • PDF

Preparation of YBCO with additives of PbO, $BaPbO_3$ and its Superconducting Properties

  • Zhanguo, Fan;Soh, Dae-Wha
    • Journal of the Speleological Society of Korea
    • /
    • no.78
    • /
    • pp.17-22
    • /
    • 2007
  • The melting temperature and critical temperature (Tc) of $YBa_2Cu_3O_x$ with deferent content impurities of PbO and $BaPbO_3$ were studied. When the PbO was used as addition in $YBa_2Cu_3O_x$, although the melting point could be reduced, the superconductivity (the transition wide, ${\Delta}T_c$) became poor. From the XRD pattern of the sintered mixture of $YBa_2Cu_3O_x$ and PbO it was known that there is a reaction between $YBa_2Cu_3O_x$ and PbO, and the product is $BaPbO_3$. In the process of the reaction the superconducting phase of $YBa_2Cu_3O_x$ was decreased and in the sample $BaPbO_3$ became the main phase. Therefore the superconductivity was reduced. $BaPbO_3$ was chosen as the impurity for the comparative study. The single phase $BaPbO_3$ was synthesized by the simple way from both mixtures of $BaCO_3$ and PbO, $BaCO_3$ and $PbO_2$. Deferent contents of $BaPbO_3$ (10%, 20%, 30%) were added in the $YBa_2Cu_3O_x$. By the phase analysis in the XRD patterns it was proved that there were not reactions between $YBa_2Cu_3O_x$ and $BaPbO_3$. When $BaPbO_3$ was used as impurity in $YBa_2Cu_3O_x$ the superconductivity was much better than PbO as impurity in $YBa_2Cu_3O_x$. But the melting point of $YBa_2Cu_3O_x$ with $BaPbO_3$ could not be found when the temperature was lower than $1000^{\circ}C$ in the DTA measurement.

Dielectric and Field-induced Strain Behaviors due to Excess PbO in Lead Yttrium Zirconate Stannate Titanate Ceramics (과잉 PbO에 의한 (Pb,Y) $(Zr,Sn,Ti)O_3$세라믹스의 유전 및 전기장유기변형 특성)

  • Yun, Gi-Hyeon;Kim, Jeong-Hui;Gang, Dong-Heon
    • Korean Journal of Materials Research
    • /
    • v.10 no.1
    • /
    • pp.34-40
    • /
    • 2000
  • The $Pb_{0.94}Y_{0.04}[(Zr_{0.6}Sn_{0.4})_{0.915}Ti_{0.085}]O_3$ ceramics which corresponded to the antiferroelectric-ferroelectric phase boundary composition were prepared for digital-type-piezoelectric/electrostrictive device application. Their dielectric, field-induced polarization (P) and strain (X) behaviors were studied with variations in sintering condition and excess PbO content. The orthorhombic structure of specimens was hardly affected either by excess PbO addition or sintering temperature. With increasing excess PbO content, grains tended to be smaller and rounded ones, and the optimum sintering temperature was lowered. Excess PbO addition stabilized the antiferroelectric phase of the specimen effectively, which was confirmed by P-E and X-E analyses. Also the digital-type-strain character was found to be enhanced despite of slight increase in phase transition (AFE-FE) field and electrical resistivity, and decrease in maximum strain. These results were explained in terms of possible lattice defects and domain wall motion.

  • PDF

The Dielectric and Piezoelectric Properties of (Pb1-1.5xLax)(Ti1-yMny) System ((Pb1-1.5xLax)(Ti1-yMny)O3계의 유전 및 압전성질)

  • 맹성재;정형진
    • Journal of the Korean Ceramic Society
    • /
    • v.25 no.4
    • /
    • pp.321-328
    • /
    • 1988
  • The sintering phenomena, electrical resistivity, dielectric and piezoelectric properties of lead titanate ceramics modified by the partial substitution of La for Pb and Mn for Ti, (Pb1-1.5xLax)(Ti1-yMny)O3 ceramics, have been investigated. In (Pb1-1.5xLax)(Ti1-yMny)O3 system, with increasing lanthanum content, the realtive bulk density increased, but the Curie point and tetragonality (c/a) decreased. The tetragonal-to-cubic phase transition boundary existed in the range of 0.20

  • PDF

Effects of Deposition Parameters on Sputter Deposition of Lead Titanate Thin Films (스퍼터링 증착에 의한 $PbTiO_3$ 박막제조시 증착변수의 영향)

  • 김상섭;강영민;백성기
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.7
    • /
    • pp.578-588
    • /
    • 1993
  • Highly c-axis oriented ferroelectric PbTiO3 thin films were deposited on MgO single crystal substrates by RF magnetron sputtering. We have studied the effects of substrate temperature, RF input power, gas comosition, gas pressure and deposition rate on the chemical and structural characteristics of PbTiO3 thin films. The epitaxy relationship of c-axis oriented films was found to be PbTiO3{100}//MgO(100) and their microstructures were highly mosaic. It was found that the most important parameter to achieve epitaxial PbTiO3 films was the substrate temperature. The activation energy for the epitaxy formation was about 0.92eV. Lower gas pressure and RF input power were favorable for the formation of epitaxial c-axis orientation. It was also found that the optimum oxygen content in Ar gas was 10% to obtain the stoichiometric PbTiO3 composition.

  • PDF

A Study on the Piezoelectric Properties of the Pb($Zn_{1/3}Nb_{2/3})O_3-Ba(Zn_{1/3}Nb_{2/3})O_3-PbTiO_3$ (Pb($Zn_{1/3}Nb_{2/3})O_3-Ba(Zn_{1/3}Nb_{2/3})O_3-PbTiO_3$ 세라믹의 압전특성에 관한 연구)

  • 박혜옥;박인길;이성갑;이영희
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1989.06a
    • /
    • pp.70-73
    • /
    • 1989
  • (1-x-y)Pb($Zn_{1/3}Nb_{2/3})O_3-Ba(Zn_{1/3}Nb_{2/3})O_3-PbTiO_3(0.12{\leq}x{\leq}0.21, 0.24{\leq}y{\leq}0.33$) ternary compound ceramics were fabricated by the mixed oxide method. The sintering temperature and time were 1050 [$^{\circ}C$], 2[hr]. Morphotropic phase boundary region was chosen for the composition. 0.55 PZN-0.21 BZN-0.24 PT specimen had the highest value of relative dielectric constants, 5353. The curie temperature of specimens were increased linearly with PT content. Near the morphotropic phase boundary, electro-mechanical coupoling factor and mechanical quality factor of the specimens had the highest values.

  • PDF