• 제목/요약/키워드: Pb Substitution

검색결과 112건 처리시간 0.026초

CLN-PZT 세라믹스의 전기, 광학 특성에 관한 연구 (A Study on the Electrical and Optical Characteristics of CLN-PZT Ceramics)

  • 강원구
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1988년도 전기.전자공학 학술대회 논문집
    • /
    • pp.799-801
    • /
    • 1988
  • This paper was studied on the effects of Ca-La-Nb substitution and Zr/Ti ratio variation to Pb(Zr, Ti)$O_3$ system on structural, electrical, optical and sound level characteristics in order to develope the piezoelectric and electrooptic ceramic devices. Also the specimens were prepared by the two stage sintering technique. The molecular formular was X($CaO{\cdot}1/4La_{2}O_{3}{\cdot}1/4Nb_{2}O_{5}){\cdot}(1-X)Pb(Zr_{Y}Ti_{1-Y})O_{3}$(x=100X, y=100Y), and the variation of x was $6{\sim}12$, y was 60${\sim}$49 and second stage sintering time was 20${\sim}$40 hours. The experimental results obtained from this study are as follows : 1. The density was decreased, the grain size was increased according to increase of Ca-La-Nb substitution. 2. The crystal structure was rhombohedral in composition 6/60/40, and the crystal structure was tetragonal and cubic according to increase of Ca-La-Nb substitution. 3. The Ca substitution of PZT system enhanced the sintering property. The Pb site vacancy resulting from the substitution of La-Nb increased the dielectrical constant, the piezoelectric charge constant, the dielectric loss and decreased the coercive field. 4. The resistivity of PZT system which has the P type conduction mechanism increased according to substitution of La-Nb because of the substituent acting as donor. 5. The PZT ceramics varied from ferroelectric substance according to increase of Ca-La-Nb substituent. The coercive field and saturation remanent polarization decreased, and at last straight line according to increase of La-Nb substitution. 6. The amount of Ca-La-Nb substitution to improve the light transmittance of speciment was 10 mol%, the Zr/Ti ratio was 49/51, and the second stage sintering time was 40 hours. 7. According to Ca-La-Nb substitution, the specimens was to be transparent. The 7.5/51/49 specimen was suitable for transparent sound vibrator because it had 58% light transmittance (thick 0.2[mm], wave length 700[mm]) and 48% electromechanical coupling factor.

  • PDF

$(Pb, Nd)(Ti, Mn)O_3$ 세라믹의 유전 및 압전특성 (Dielectric and Piezoelectric Properties of $(Pb, Nd)(Ti, Mn)O_3$ Ceramics)

  • 임주수;신혁재;오태희;김종희;송병무;이재신
    • 한국세라믹학회지
    • /
    • 제34권5호
    • /
    • pp.461-466
    • /
    • 1997
  • Dielectric and piezoelectric properties of (Pb1-1.5xLnx)(Ti0.98Mn0.02)O3 ceramics with x=0~0.2 have been investigated. Pb(Ti0.98Mn0.02)O3 showed poor sinterability and cracking on cooling, but the substitution of Nd3+ ions into Pb2+ sites resulted in dense microstructures without cracking through reducing crystallographic anisotropy. The Nd3+ substitution, however, deteriorated the temperature stability of the piezoelectric properties because of lowering the Curie point. Electromechanical anisotropy(Kt/Kp) indicated a maximum value of 10 when x=0.1. This result might be attributed to the counteracting effects that with increasing x, the lattice anisotropy decreases while the poling becomes easier due to the increase in O2- vacancy concentration. Thickness-shear mode resonators with (Pb0.85Nd0.1)(Ti0.98Mn0.02)O3 composition showed good resonant characteristics around 4.5 MHz.

  • PDF

고주파 필터용 PSN-PMN-PZT 세라믹스의 Sr 치환효과 (Effects of Sr Substitution on the PSN-PMN-PZT Ceramics for High Frequency)

  • 오동언;민석규;류주현;박창엽;김종선;윤현상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 추계학술대회 논문집
    • /
    • pp.229-233
    • /
    • 2000
  • In this study, the temperature coefficient of resonant frequency($TCF_r$), dielectric and piezoelectric properties of $Pb_{1-x}Sr_x[(Sb_{1/2}Nb_{1/2})_{0.035}(Mn_{1/3}Nb_{2/3})_{0.065}(Zr_{0.49},Ti_{0.51})_{0.90}]O_3$ ceramics were investigated with the Sr substitution to Pb site. The dielectric constant was increased according to the increase of Sr substitution and electromechanical coupling factor($k_t$) also showed the highest values of 0.485 when the Sr substitution was 5 mol%. Moreover, the mechanical quality factor($Q_{mt}$) showed the highest value of 233 when the Sr substitution was 2 mol%.

  • PDF

Effects of Cd substitution on the superconducting properties of (Pb0.5Cu0.5-xCdx)Sr2(Ca0.7Y0.3)Cu2Oz

  • Lee, Ho Keun;Kim, Jin
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제20권2호
    • /
    • pp.24-28
    • /
    • 2018
  • To understand the effects of Cd substitution for Cu, $(Pb_{0.5}Cu_{0.5-x}Cd_x)Sr_2(Ca_{0.7}Y_{0.3})Cu_2O_z$ (x = 0 ~ 0.5) compounds were synthesized and the structural and superconducting properties of the compounds were characterized. Resistivity data revealed that superconducting transition temperature rises initially up to x = 0.25 and then decreases as the Cd doping content increases. Room-temperature thermoelectric power decreases at first up to x = 0.25 and then increases with higher Cd doping content, indicating that the change in $T_c$ is mainly caused by the change in the hole concentration on the superconducting planes by the Cd doping. The non-monotonic dependence of the lattice parameters and the transition temperature with Cd doping content is discussed in connection with the possible formation of $Pb^{+2}$ ions and the removal of excess oxygen caused by Cd substitution in the charge reservoir layer. A correlation between transition temperature and c/a lattice parameter ratio was observed for the $(Pb_{0.5}Cu_{0.5-x}Cd_x)Sr_2(Ca_{0.7}Y_{0.3})Cu_2O_z$ system.

다이아몬드 엔빌 셀을 이용한 Donor doped Pb(Zr0.52Ti0.48)O3 세라믹스의 상전이 압력 연구 (The Study on Phase Transition Pressure of Donor doped Pb(Zr0.52Ti0.48)O3 Ceramics with Diamond Anvil Cell)

  • 조경호;고영호;서창의;김광주
    • 한국세라믹학회지
    • /
    • 제48권5호
    • /
    • pp.471-478
    • /
    • 2011
  • Investigations of crystal structure and phase transition of $Pb(Zr_{0.52}Ti_{0.48})O_3$ ceramics doped with A-site substitution impurity (La, Nd) or B-site substitution impurity (Sb, Nb) at 2 mol% concentration were carried out. X-ray diffraction patterns of impurities doped $Pb(Zr_{0.52}Ti_{0.48})O_3$ ceramics have been measured at pressures up to ~5 GPa with diamond anvil cell and synchrotron radiation. The patterns were obtained at room temperature using methanol-ethanol mixture as pressure-transmitting media. In order to refine the crystal structure, Rietveld analysis has been performed. The structures of impurities doped $Pb(Zr_{0.52}Ti_{0.48})O_3$ ceramics are tetragonal in space group P4mm at ambient pressure and are transformed into a cubic phase in space group Pm$\bar{3}$m as the pressure increases. In this study, when A-site substitution donor $La^{3+}$ or $Nd^{3+}$ ion was added to $Pb(Zr_{0.52}Ti_{0.48})O_3$ ceramics, the phase transition phenomena showed up at the pressure of 2.5~4.6 GPa, but when B-site substitution donor $Nb^{5+}$ or $Sb^{5+}$ ion was added to it, the phase transition appeared at relatively lower pressure of 1.7~2.6 GPa.

La치환된 PMN계 세라믹스의 유전특성에 관한 연구 (A study on Dielectric Properties using PMN Ceramics with La substitution)

  • 지승한;이능헌;김용혁;김진수;이덕출
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1995년도 하계학술대회 논문집 C
    • /
    • pp.1242-1244
    • /
    • 1995
  • The dielectric and polarizable properties of $0.9Pb_{1-x}La_x({Mg}_{1/3}Nb_{2/3})O_3-0.1PbTiO_3$ (x=0,1,2,3,4,5) have been investigated. The temperature-dependant electrostictive characteristics of 0.9PMN-0.1PT relaxor ferroelectric system were improved by enhencing the extent of the diffuse phase transition(DPT). This was achieved using PMN-PTceramics by the partial substitution of La at the Pb site. The curie temperature and the maximum dielectric permittivity decreased by substituting La and the electric field-related hysteresis phenomena decreased with increasing La substitution amount.

  • PDF

PNN 변화에 따른 저온소결 PMN-PNN-PZT 세라믹스의 유전 및 압전특성 (Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMN-PNN-PZT Ceramics with the amount of PNN substitution)

  • 김국진;이갑수;김도형;류주현
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2007년도 제38회 하계학술대회
    • /
    • pp.1337-1338
    • /
    • 2007
  • In this study, in order to develop low temperature sintering ceramics for multilayer piezoelectric actuator, 0.07Pb$(Mn_{1/3}Nb_{2/3})O_{3}-xPb(Ni_{1/3}Nb_{2/3})O_{3}-(0.93-x)Pb(Zr,Ti)O_{3}$ ceramics system were fabricated using $Li_{2}CO_{3}-Bi_{2}O_{3}$-CuO sintering aids and the specimens were sintered at $930^{\circ}C$. Thereafter their piezoelectric and dielectric characteristics were investigated with the amount of PNN substitution. At 9[mol%] PNN substitution, electromechanical coupling factor (kp), mechanical quality factor (Qm) and piezoelectric constant ($d_{33}$) showed the optimum value of 0.60, 1323 and 387pC/N, respectively.

  • PDF

PNN 치환량에 따른 저손실 저온소결 PMN-PNN-PZT 세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Characteristics of Low Loss Low Temperature Sintering PMN-PNN-PZT Ceramics with the amount of PNN Substitution)

  • 류주현;김국진;정영호;이수호
    • 한국전기전자재료학회논문지
    • /
    • 제20권9호
    • /
    • pp.766-770
    • /
    • 2007
  • In this study, in order to develop low temperature sintering ceramics for multilayer piezoelectric actuator, $0.07Pb(Mn_{1/3}Nb_{2/3})O_3-xPb(Ni_{1/3}Nb_{2/3})O_3-(0.93-x)Pb(Zr,Ti)O_3$ ceramics system were fabricated using $Li_2CO_3-Bi_2O_3-CuO$ sintering aids and the specimens were sintered at $930^{\circ}C$. Thereafter, their piezoelectric and dielectric characteristics were investigated according to the amount of PNN substitution. At 9 mol% PNN substitution, density, electromechanical coupling factor ($k_p$), dielectric constant, mechanical quality factor ($Q_m$) and piezoelectric constant ($d_{33}$) showed the optimum value of $7.86g/cm^3$, 0.60, 1640, 1323 and 387 pC/N, respectively. It is considered that these values are suitable for piezoelectric divece application such ad multilayer piezoelectric actuator and ultrasonic vibrator with pure Ag internal electrode.