본 실험에서는, 양극산화 처리된 탄소섬유의 표면변화가 탄소섬유강화 복합재료의 기계적 계면특성을 통하여 살펴보았다. 양극산화 처리된 탄소섬유의 표면특성은 FTIR, XPS, 그리고 SEM을 통하여 알아보았다. 복합재료의 기계적 계면특성은 층간전단강도(interlarminar shear strength; ILSS)와 임계세기인자(critical stress intensity factor; $K_{IC}$) 그리고 임계변형속도에너지(critical strain energy release rate; $G_{IC}$)를 통하여 고찰하였다. 실험결과 양극산화에 의한 각각의 표면 처리된 탄소섬유는 표면특성의 변화를 가져오며, 복합재료의 ILSS, $K_{IC}$, 그리고 $G_{IC}$같은 기계적 계면특성은 탄소섬유의 양극산화를 통하여 향상되어진다. 전해질이 20% 황산/질산(3/1)일 때 다른 전해질보다 기계적 물성의 가장 큰 향상을 보였다. 이는 양극산화로 탄소섬유와 매트릭스 사이의 계면결합력의 향상때문이라 판단된다.
In this study, it was attempted to obtain the fundamental data for the formation and oxidation of soot from a diesel engine. Combustion of spray injected into a cylinder is complex phenomenon having physical and chemical processes, and these processes affect each other. There are many factors in the mechanism of the formation and oxidization of soot and it is necessary to observe spray combustion microscopically. In order to observe with that view, free fuel droplet array was used as an experimental object and the droplet array was injected into an atmospheric combustion chamber with high temperature. Ambient temperature of the combustion chamber, interdroplet spacing, and droplet diameter were selected as parameters, which affect the formation and oxidation of soot. In this study, it was found that the parameters also affect ignition delay of droplet. The ambient temperature especially affected the ignition delay of droplet as well as the flame temperature after self-ignition. As the interdroplet spacing that means the local equivalence ratio in a combustion chamber was narrow, formation of soot was increased. As diameter of droplet was large, surface area of the droplet was also broad, and hence evaporation of the droplet was more active than that of a droplet with relative small diameter.
An ex vivo assay determining the flavin-containing monooxygenase (FMO) activity in perfused rat liver has been developed by assessing the rate of thiobenzamide S-oxide (TBSO) formation from the infused thiobenzamide (TB). The hepatotoxicity by TB or TBSO was not a critical factor for maintaining the FMO activity for up to 50 min. The FMO activity expressed in nmoles TBSO produced/g liver/min was the same for the recycling and non-recycling perfusion. This implies that reduction of the oxidized TBSO back to the parent compound (TB) is negligible. Hydrolysis of the collected perfusates with either ${\beta}-glucuronidase$ or arylsulfatase did not increase the TBSO level and thus, TBSO does not appear to undergo conjugation either to glucuronide or sulfate esters. Thus, measuring the rate of TB S-oxidation in the isolated perfused liver with 1 mM TB for 50 min provides a useful tool for evaluation of the hepatic FMO activity in the absence of hepatic necrosis and without the interferences caused by further conjugation or back reduction of the TBSO to the parent TB.
A sliding friction and wear test for silicon nitride (Si,N4) was conducted using a ball-on-disk specimen configuration. The material used in this study was HIPed silicon nitride. The tests were carried out from room temperature to 1000$^{\circ}C$ using self-mated silicon nitride couples in laboratory air. The worn surfaces were observed by SEM and the debris particles from the worn surfaces were analyzed for oxidation by XPS. The normal load was found to have a more significant influence on the friction coefficient of the silicon nitride than an elevated temperature. The specific wear rate was found to decrease along with the sliding distance. The specific wear rate at 29.4 N and 1000$^{\circ}C$ was 292 times larger than that at room temperature. The main wear mechanism from room temperature to 750$^{\circ}C$ was caused by brittle fracture whereas from 750$^{\circ}C$ to 1000$^{\circ}C$ the wear mechanism was mainly influenced by the oxidation of silicon nitride due to the increased temperature. The oxidation of silicon nitride at a high temperature was a significant factor in the wear increase.
Finned segment, with which are lined inner wall of the turbine combustors, are subject to severe degradation when they are exposed to a hostile environmment at elevated temperature. To protect the finned segment from this environment and to maintain good mechanical properties of components at high temperature, they are preferred to be coated. The most governing factor for the durability of coatings used in the high temperature is the microstructure of coatings; these are splat from, distibution of microcacks, size and distribution of pores, thickness of coating layer, adhesion between coating layer, and oxidation of band coating. In this study, based on the evaluation of the imported finned segment, new finned segment segment was manufactured with optimum plasma spraying parameters, and their properties were examined. Using $ZrO_2(8wt$Y_2O_3)$,/TEX> powder for ceramic coating and 67Ni-22Cr-10Al-0.5Y mixing powder for bond coating, thickness of ceramic and bond coating layer were varied in order to find optimum condition, the results showed that B2T4(bond coating : 100~250$\mu\textrm{m}$, ceramic coating : 250~300$\mu\textrm{m}$) was the best among the specimens tested. Compared to the imported finned segment, B2T4 has better bond strength, hardness, and isothermal and cyclic oxidation resistance.
The peroxisome proliferator-activated receptor ${\alpha}$ ($PPAR{\alpha}$) is a nuclear transcription factor that plays a central role in lipid and lipoprotein metabolism. To investigate whether swim training improves obesity and lipid metabolism through $PPAR{\alpha}$ activation in female sham-operated (Sham) and ovariectomized (OVX) mice, we measured body weight, visceral adipose tissue mass, serum free fatty acid at 6 weeks as well as the expression of hepatic $PPAR{\alpha}$ target genes involved in fatty acid oxidation. Swim-trained mice had decreased body weight, visceral adipose tissue mass and serum free fatty acid levels compared to high fat diet fed control mice in both female Sham and OVX mice. These reductions were more prominent in OVX than in Sham mice. Swim training significantly increased hepatic mRNA levels of $PPAR{\alpha}$ target genes responsible for mitochondrial fatty acid ${\beta}$-oxidation, such as carnitine palmitoyltransgerase-1 (CPT-1), very long chain acyl-CoA dehydrogenase (VLCAD), and medium chain acyl-CoA dehydrogenase (MCAD) in OVX mice. However, swim trained female Sham mice did not increase hepatic mRNA levels of $PPAR{\alpha}$ target genes responsible for mitochondrial fatty acid ${\beta}$-oxidation compared to Sham control mice. These results indicate that swim training differentially regulates body weight and adipose tissue mass between OVX and Sham mice, at least in part due to differences in liver $PPAR{\alpha}$ activation.
During the growth of macroscopically dislocation-free Czochralski silicon crystal, micro precipitates causing stacking faults in the silicon wafer during the oxidation are formed Thermal history the cryscausing acquire during the growth process is known to be a key factor determining the nucleation of this micro precipitates. In this article, various mechanisms suggested on the formation of microdefects in the silicon crystal are reviewed to secure the nucleation mechanism of the micro precipitates causing OSF whose pattern is normally ring or annular in CZ silicon crytal. B-defects which are known as vacancy clustering are considered to be the heterogeneous nucleation sites for the micro precipitates causing OSF in the CZ silicon crystals.
In this study, the generation of oxygen-free gas using catalytic combustion for industrial applications is explained ; heat treatment and copper annealing. For the experiment, Pd catalysts were determined by testing their catalytic activities over LPG in a micro-reactor. Combustion characteristics for the generation of oxygen-free atmospheric gas and the effect of flue gas upon surface oxidation were estimated form this experiment. As a result of the experimental investigation, we can state that the catalytic combustion could generate oxygen-free atmospheric gas suitable for industrial applications, but vapor produced by combustion process must be carefully considered as a new factor of surface oxidation.
Fibers with a high degree of axial preferred orientation can be obtained from mesophase pitch. Prior to cabonization, the pitch fibers must be rendered in fusible so that their orientation is preserved. The stabilization of the pitch fibers was heated at temperature between $250^{circ}C$ and $300^{circ}C$ and a treatment time 5 to 80minutes. Oxidized fibers heated $1800^{circ}C$without stretching. Pitch based carbon fiber have a young's modulus as high as 304GN/$m^2$. The structure of the pitch cased carbon fiber is determining factor for the mechanical properties of the produced fibers. The structure depending on the pitch precursor as well as on the oxidation time.
The structure and composition of anodic films, formed on 6063 commercial aluminium alloy at constant current density of $1.5A/^dm2$ with various superimposed cathodic current ratio, in the range 0~33%, in the 11% $H_2SO_4$ with various concentration of $CuSO_4{\cdot}5H_2O$, in the range 0~75 g/l, without cathodic current are generally porous-type and no sign of Cu co-deposition appearance, suggesting that cathodic current is an important factor in the Cu co-deposition. Comparison with the anodic film thickness measurement results obtained from anodic film formed by direct anodic current and anodic film formed by superimposed various portion of cathodic current, the portion of cathodic current of input current increases with decrease of anodic film thickness and increases with increase of concentration of $Cu_2S{\;}and{\;}Cu_2O$ in the anodic film.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.