The effect of the alloy elements(Si/Mn) ratio on the coating quality including wettabilty with molten zinc, galvannealing kinetics and crater has been investigated in interstitial-free high strength steel(IFHSS) containing Si and Mn. When the Si/Mn ratio was below 0.75, IF-HSS exhibited a good wettability leading to a good galvannealed coating quality after annealing at $800^{\circ}C$ for 40s in $15%H_2-N_2$ mixed gas with dew point $-60^{\circ}C$. In contrast, the wettability and galvannealed coating quality were deteriorated in the Si/ Mn ratio above 0.75. It is shown that they have relevance to oxides forms by selective oxidation on the steel surface. The oxide particles dispersed on the steel surface with a surface coverage of below 40% resulted in good wettability and galvannealed coating quality. The oxide particle is mainly consisted of $Mn_2SiO_4$ with low contact angle in molten zinc. On the other hand, the continuous oxide layer on the steel surface, such as network- and film-type,caused to poor wettability and galvannealed coating quality. The coverage of oxide layer was above 80%, and its chemical species was $SiO_2$ with high contact angle in molten zinc. Consequently, the Si/Mn alloy ratio played an importance role in galvannealed coating quality of IF-HSS.
이번 연구는 광미시료를 대상으로 반응시간(1, 2, 4, 7, 14, 21 및 30일)과 반응용액의 pH(1, 3 및 5)를 달리하여 실내 용출실험을 실시하였다. pH 5와 pH 3의 반응용액과의 용출실험에서는 반응 2일 후 최종 pH가 4.6-6.1 혹은 2.8-3.5로 안정화되었으며, 반응시간이 지남에 따라 점진적으로 낮아졌다. 황산염 농도와 산도는 7일 이후 증가하는 것이 관찰되었는데, 이는 황화광물의 산화작용때문인 것으로 판단된다 pH 5와 pH 3에서 용출된 Pb 함량은 반응기 간(1-30일) 동안 뚜렷한 변화가 보이지 않은 반면에 Zn, Cd 및 Cu는 시간이 지남에 따라 용출함량이 증가하는 경향을 보였다. 반응용액 pH 1에서의 용출특성은 Zn 형태(Zn, Cd, 및 Cu)와 Pb 형태(Pb)로 구분되었다. Zn 형태는 시간에 따라 용출함량이 증가되었고, 이는 지속적인 용해작용에 의한 것이다. Pb 형태는 시간에 따라 용출농도가 감소하였으며, 이는 황산염의 용출함량이 높아짐에 따라 용해된 Pb가 앵글레사이트(anglesit)로 침전됨을 지시한다. 높은 황산염 농도는 Fe, Zn, 및 Cd의 높은 용출함량과 밀접한 관련이 있다. 이들 용출실험 결과 Zn과 Cd의 용출과 산도는 광산주변 환경의 지표수와 지하수 수질에 악영향을 주는 요인이 될 수 있다. 용출반응에서 kinetics 문제는 광미가 빗물과 반응하여 유출수에서의 중금속 농도를 증가시킬 수 있는 중요한 요인이 된다.
In this study, the corrosion characteristics of T22 and T92 steel were investigated in 6O2 + 16CO2 + 2SO2 gas environment at 650 ℃. Corrosion characteristics were characterized by weight gain, oxide layer thickness, scanning electron microscope, optical microscope, energy dispersive X-ray spectroscopy, and X-ray diffraction. T22 and T92 steel tended to stagnate oxide layer growth over time. Oxidation kinetics were analyzed using the data of oxide layer thickness, and a regression model was presented. The regression model was significantly acceptable. The corrosion rate between the two steels through the regression model showed significant difference. The T92 steel was approximately twice as large as the time exponent and showed very good corrosion resistance compared to the T22 steel. In both steels, the oxide layer mainly formed a Fe-rich oxide layer composed of hematite (Fe2O3), magnetite (Fe3O4), and spinel (FeCr2O4). Sulfide segregation occurred in the oxide layer due to SO2 gas. However, the locations of segregation for the T22 and T92 steel were different.
$Cu_xFe_{3-x}O_4$ catalyst and $Zn_xFe_{3-x}O_4$ catalyst were synthesized by the air oxidation method with various C(II) and Zn(II) weights. Activated catalysts decomposed carbon dioxide to carbon at $350^{\circ}C$, $380^{\circ}C$, $410^{\circ}C$ and $440^{\circ}C$. The value of carbon dioxide decomposition rate for $Cu_{0.003}Fe_{2.997}O_4$ and $Zn_{0.003}Fe_{2.997}O_4$ catslysts than was better catalysts. The decomposed rate of the catalysts is about 85%${\sim}$90%. The reaction rate constant(4.00 $psi^{1-{\alpha}}/min$) and activation energy(2.62 kcal/mole) of $Cu_{0.003}Fe_{2.997}O_4$ catalyst are better than $Zn_{0.003}Fe_{2.997}O_4$
The color of Congo red hinders the spectrometric measurements of a concentration of hydrogen peroxide and enzyme activity (Horseradish peroxidase; HRP) during enzymatic decoloring of Congo red. In this study, a method was developed to measure peroxidase activity and hydrogen peroxide concentration in the presence of Congo red. The oxidation product of HRP/hydrogen peroxide and ABTS(2,2'-azino-bis-(3-ethylbenzotriazoline-6-sulfonic acid)) formed a dark green color. The spectrum of this product showed absorption bands at 420 nm and 734 nm. When compared with the Congo red spectrum, the absorption at 734 nm of this product did not overlap with Congo red, thus making the hydrogen peroxide measurement possible even in the presence of Congo red. Kinetic study of decoloring of Congo red performed by this method showed that the decoloring reaction followed the Michaelis-Menten kinetics. Pulse feeding of hydrogen peroxide, upon depletion, significantly increased the decoloring of Congo red. This result shows that this newly developed technique can monitor, predict, and improve the enzymatic decoloring process.
대한약학회 2002년도 Proceedings of the Convention of the Pharmaceutical Society of Korea Vol.2
/
pp.383.3-384
/
2002
Rosmarinic acid (1) and methyl rosmarinic acid (2), isolated from the ethyl acetate soluble fraction of the methanolic extract of Salvia miltiorrhiza Bunge (Lamiaceae) were found to be the tyrosinase inhibitors and scavengers of 1, 1-diphenyl-2-picrylhydrzyl (DPPH) radical. Compounds 1 and 2 inhibited the oxidation of L-tyrosine catalyzed by mushroom tyrosinase with $IC_{50}$/ of 16.8 $\mu\textrm{M}$ and 21.5 $\mu\textrm{M}$. respectively. It compared well with kojic acid. a well-known tyrosinase inhibitor. with an $IC_{50}$ of 22.4 $\mu\textrm{M}$. The inhibitory kinetics, analyzed by a Lineweaver-Burk plot, found rosmarinic acid and its methyl ester to be competitive inhibitors with $K_{i}$ of $2.35{\times}10^{-5}M$ and $1.52{\times}10^{-5}M$ respectively. In addition, compounds 1 and 2 showed the scavenging activities on DPPH radical, with $IC_{50}$ of 4.27 $\mu\textrm{M}$ and 3.05 $\mu\textrm{M}$. respectively. These scavenging effects were more potent than that of L-ascorbic acid ($IC_{50}$ = 11.75$\mu\textrm{M}$).
Study on the HDDr Characteristics of Nd16Fe76-xB8Zrx (x=0-2.0) Alloys and the Magnetic Properties of the HDDR Materials Nd16Fe76-xB8Zrx (where x=0-2.0) have been studied to see the effect of Zr addition on HDDR characteristics. A particular emphasis was place upon the anisotropy of the HDDR material. Anisotropy of the HDDR powder material has been evaluated by comparing the remanence values of the aligned sample measured along the aligning direction and the direction perpendicular to it. The HDDR characteristics of the alloys were investigated by means of DAT and TPA. Magnetic chracterisation of the HDDR processed materials was performed using a VSM and a TMA. The magnetic domain structure of the HDDR materials was examined by means of polarised microscope using a solid HDDR processed material. It has veen found that small addition (0.1 at %) of Zr to Nd-Fe-B-type alloy retards thedisproportionatio kinetics of the hydrogenated material. Desorption characteristic of the disproportionated materials has been found not to be affected significantly by the Zr addition. The Zr addition has been found to facilitate size of the powder. As the particle size decreases, the intrinsic coercivity decreases radically, and this is explained in terms of structural damage and/or oxidation caused during mechanical milling. It has also been found that the degree of alignment representing the anisotropic character of the HDDR powder is enhanced with decreasing particle size. Alloys with compositions based on
한국환경보건학회 2003년도 Challenges and Achievements in Environmental Health
/
pp.123-127
/
2003
This experiment was performed to investigate the characteristics of sonolytic reaction as the basic data for development of the ultrasonic AOP(Advanced Oxidation Process) process from which the refractory organic compounds in aqueous solution which are not readily removed by the existing conventional wastewater treatment processes can be destructed and removed. Trichloroethylene (TCE), benzene, and 2,4-dichlorophenol(DCP) were used as the samples, and their destruction efficiency were measured in terms of experimental parameters of the initial solution concentration, initial solution pH, reaction temperature, acoustic frequencies and intensities. Results showed that the destruction efficiencies of all of the sample materials were above 80% within 120 minutes of sonolytic reaction in all reaction condition. The reaction order of these three compounds was verified as Pseudo first order. From the fore-mentioned results, it can be concluded that the refractory organic compounds could be removed by the ultrasonic irradiation with radicals, such as H$.$and OH$.$causing the high increase of pressure and temperature. Finally, it appears that the new AOP technology using ultrasonic irradiation can be applied to the treatment of refractory substances which are difficult to be decomposed by the conventional methods.
Isotactic polyacrylonitrile (PAN) with triad isotacticity of 0.53, which was determined by $^{13}C$ NMR, using dialkylmagnesium as an initiator, was successfully synthesized. Isothermal treatment of iso-PAN was conducted in air at 200, 220, 250 and $280^{\circ}C$. Structural evolutions and chemical changes were studied with Fourier transformation infrared and wide-angle X-ray diffraction during stabilization. A new parameter $CNF={I_{2240cm}}^{-1}/ ({I_{1595cm}}^{-1}+f^*{I_{1595cm}}^{-1})$ was defined to evaluate residual nitrile groups. Crystallinity and crystal size were calculated with X-ray diffraction dates. The results indicated that the nitrile groups had partly converted into a ladder structure as stabilization proceeded. The rate of reaction increased with treatment temperature; crystallinity and crystal size decreased proportionally to pyrolysis temperature. The iso-conversional method coupled with the Kissinger and Flynn-Wall-Ozawa methods were used to determine kinetic parameters via differential scanning calorimetry analysis with different heating rates. The active energy of the reaction was 171.1 and 169.1 kJ/mol, calculated with the two methods respectively and implied the sensitivity of the reaction with temperature.
Singlet oxygen ($^1O_2$) is highly reactive form of molecular oxygen that may harm living systems by oxidizing critical cellular macromolecules. The oxyR gene product regulates the expression of the enzymes and proteins that are needed for cellular protection against oxidative stress. In this study, the role of oxyR in cellular defense against a singlet oxygen was investigated using Escherichia coli oxyR mutant strains. Upon exposure to methylene blue and visible light, which generates singlet oxygen, the oxyR overexpression mutant was much more resistant to singlet oxygen-mediated cellular damage when compared to the oxyR deletion mutant in regard to growth kinetics, viability and protein oxidation. Induction and inactivation of major antioxidant enzymes, such as superoxide desmutase and catalase, were observed after their exposure to a singlet oxygen generating system in both oxyR strains. However, the oxyR overexpression mutant maintained significantly higher activities of anticxidant enzymes than did the oxyR deletion mutant. These results suggest that the oxyR regulon plays an important protective role in singlet oxygen-mediated cellular damage, presumably through the protection of antioxidant enzymes.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.