• Title/Summary/Keyword: Noritake powder

Search Result 4, Processing Time 0.021 seconds

Esthetic restoration using Noritake powder through communication with the dental clinic (진료실과의 소통과 Noritake powder를 이용한 심미보철제작)

  • Hwang, Boah
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.27 no.2
    • /
    • pp.105-115
    • /
    • 2018
  • Not to recreate the final prosthesis is the shortest way to get a successful outcome. In the case of an aesthetic prosthesis, it is important not only the condition of the oral cavity but also the whole harmony in the face such as the interpupillary line and the smile line. But the dental technician creates the prosthesis only based on the oral model. So if you want to prevent the failure of the prosthesis due to discordance with the face, it is a good idea to use patient's facial photography and provisional restorations to reproduce facial features, shapes and aesthetics before switching to a final prosthesis. To prevent the failure of the final prosthesis, it is important to communicate among the patient, the technician and the doctor according to the model diagnosis, facial and oral photos. Then all the technicians will get satisfactory results. In addition, the technician have to understand the form of natural teeth, to analyze and reproduce colors, and to understand materials in order to produce a successful aesthetic prosthesis. From now on, I will explain two parts. At first, the communication in the dental office for the successful production of aesthetic prosthesis through the clinical case. And the second, my opinion for the successful aesthetic prosthesis.

Manufacture of paste opaque porcelains using glycols as a solvent and evaluation of their physical properties (글리콜을 용매로 제조한 연고형 불투명 도재의 물성)

  • Kim, Sa-Hak
    • Journal of Technologic Dentistry
    • /
    • v.25 no.1
    • /
    • pp.41-62
    • /
    • 2003
  • In this research, we manufactured the paste opaque porcelains using Propylene Glycol (PG) and Buthylene Glycol (BG) as a solvent, and compared the composition of solvents, the coefficient of thermal expansion, the particle size distribution, the viscosity and bonding strength to metal, and the tone with those of the commercial products(Duceram Plus, Duceram GmbH; VMK 95, Vita Co.; Noritake EX-3, Noritake Co.)used in the clinical field. The results of the research were as follows: 1. The result of solvent analysis indicated that the solvents included in the paste opaque porcelains of the control group were mainly composed of Glycols. 2. From the Coefficient of thermal expansion measurement, we drew out the following results; testing group: $14.0\times10^{-6}/^{\circ}C$, Duceram Plus: $13.9\times10^{-6}/^{\circ}C$, VMK 95: $14.3\times10^{-6}/^{\circ}C$, and Noritake EX-3: $13.3\times10^{-6}/^{\circ}C$. 3. Seen from the result of particle size distribution measurement, the experimental group was similar to the control group in 1$\mu m$ below, but the experimental group marked the highest distribution of 61% in the case of between 1$\mu m$ and 5$\mu m$. Between 5$\mu m$ and 10$\mu m$, they showed relatively similar distribution, and Noritake EX-3 was turned out the highest distribution of 29% in 10$\mu m$ above. 4. From the result of viscosity measurement, Duceram plus showed the highest viscosity throughout all the measurements followed by Noritake Ex-3, experimental group and VMK 95 in decreasing order. 5. The result of bonding strength measurement was EX 35.53 $\beta\acute{A}$, DU 40.88 $\beta\acute{A}$, VM 39.43 $\beta\acute{A}$, and NO 35.39 $\beta\acute{A}$, and no significant difference was found between the experimental group and the control groups(P>0.05). 6. The measurement of the tone indicated that the $L^*$ value of the experimental group was 86.89 0.63 in average, which is higher than the control group in its brightness. In the case of the $a^*$ value, Duceram Plus, VMK 95 and EX-3 showed positive value, whereas the testing group was turned out negative value. In $b^*$ value, Duceram Plus proved the highest. From the results of this research, the paste opaque porcelains using Propylene Glycol (PG) and Buthylene Glycol (BG) as a solvent did not make differences from the commercial products that are actually used in the clinical fields. Therefore, it is possible to utilize Propylene Glycol (PG) and Buthylene Glycol (BG) for the paste opaque porcelains of P.F.M crown. It is also recommended that further researches concerning the compositions and forms of powder, the types of organic solvent components and the ratio of mixture proceeded in order to improve the level of productivity in the future.

  • PDF

An Experimental Study on Effect on Debonding Strength of Metal-porcelain by Painting Method of Opaque Porcelain (Opaque 도재의 도포 방법에 따른 금속-도재의 결합강도에 미치는 영향에 관한 실험적 연구)

  • Kim, Sa-Hak
    • Journal of Technologic Dentistry
    • /
    • v.22 no.1
    • /
    • pp.39-47
    • /
    • 2000
  • This study is the know the difference bond strength according to painting method of Opaque porcelain. Among Porcelain powder for Porcelain, Noritake powder, Bonding agent 1 class and metal are selected as Base metal alloy. And painting method of Opaque porcelain is divided by 4 groups : PG, WG, NG and DG. Also it is to manufacture 24 sheets of Specimen by 6 each every method and to measure Crack-initiation Strength of Metal-porcelain and it is to observe it by Scanning electron microscope. I come to get a conclusion as follows. 1. As for Debonding strength of every experiment groups, it showed that WS group which executed Wash bake had highest value, 44.25MPa and NG group which used Normal powder had value, 42.11MPa and DG group which used Bonding agent had value, 35.88MPa and PG group which used Paste opaque had value, 35.39MPa. 2. In four painting methods of Opaque porcelain, PG group, WG group, NG group and DG group, there is no significant difference statistically in Crack-initiation Strength. 3. As a result of observing fracture surface with Scanning electron microscope, it was showde that PG group remained a lot of particle of porcelain on the surface of metal than WG group, NG group and DG group.

  • PDF

In vitro evaluation of the bond strength between various ceramics and cobalt-chromium alloy fabricated by selective laser sintering

  • Bae, Eun-Jeong;Kim, Hae-Young;Kim, Woong-Chul;Kim, Ji-Hwan
    • The Journal of Advanced Prosthodontics
    • /
    • v.7 no.4
    • /
    • pp.312-316
    • /
    • 2015
  • PURPOSE. This study aimed to present the clinical applicability of restorations fabricated by a new method, by comparing the bond strength of between ceramic powder with different coefficient of thermal expansion and alloys fabricated by Selective laser sintering (SLS). MATERIALS AND METHODS. Fifty Co-Cr alloy specimens ($25.0{\times}3.0{\times}0.5mm$) were prepared by SLS and fired with the ceramic ($8.0{\times}3.0{\times}0.5mm$) (ISO 9693:1999). For comparison, ceramics with different coefficient of thermal expansion were used. The bond strength was measured by three-point bending testing and surfaces were observed with FE-SEM. Results were analyzed with a one-way ANOVA (${\alpha}$=.05). RESULTS. The mean values of Duceram Kiss ($61.18{\pm}6.86MPa$), Vita VM13 ($60.30{\pm}7.14MPa$), Ceramco 3 ($58.87{\pm}5.33MPa$), Noritake EX-3 ($55.86{\pm}7.53MPa$), and Vintage MP ($55.15{\pm}7.53MPa$) were found. No significant difference was observed between the bond strengths of the various metal-ceramics. The surfaces of the specimens possessed minute gaps between the additive manufactured layers. CONCLUSION. All the five powders have bond strengths higher than the required 25 MPa minimum (ISO 9693); therefore, various powders can be applied to metal structures fabricated by SLS.