• 제목/요약/키워드: Nonmetallic inclusion

검색결과 26건 처리시간 0.045초

SM45C와 SCM440의 피삭성 검토에 관한 연구 (A Study on the Machinability Charateristic of SM45C and SCM440)

  • 김남훈;이용성
    • 대한기계학회논문집A
    • /
    • 제20권12호
    • /
    • pp.3899-3908
    • /
    • 1996
  • In order to clarify the effects of nonmetallic inclusion contents insteels (SM45C & SCM440) on the tool life, cutting experiment was performed under various cutting conditions. Tool life, cutting force, roughness of machined surface and cutting mechanism are examined on these two kinds of steel. The following conclusions were obtained from the analysis (1) Cutting force of the steels was not affected by chemical component and nonmetallic inclusion. (2) If the rate of amount, Ca/S has a value grater than about 0.2 and addition of less amount of Al, Mn, tool wear of tips decreasesinturning. (3) It is also proved that higher contents of nonmetallic inclusion improve roughness of the surface. (4) Less amount of Ca, higher amount of S, Mn and Al improve the chip breakability.

트럭용 커넥팅 로드 소재의 내부 품질에 따른 기계적 특성 연구 (A study on the Mechanical Characteristics by the Internal Quality of Connecting Rod Materials for Trucks)

  • 김동현
    • 한국생산제조학회지
    • /
    • 제7권1호
    • /
    • pp.75-81
    • /
    • 1998
  • We have studied internal quality including chemical compositions, microscopic structure and nonmetallic inclusion of test materials. We have analyzed tensile strength value, hardness value, impact value etc. In analyzing internal quality, all of the test materials showed typical ferrite+pearlite structure. But nonmetallic inclusion showed oxide and sulfide inclusions in medium carbon steels, and sulfide inclusion is S-free cutting steels. In ca+ S-free cutting steels, the calcium aluminate and sulfide complex inclusion had low-melting points as deformation of sulfide and oxide inclusion is existed. It was found that tensile strength and hardness give maximum value in medium carbon steels, where as minimum in Ca + -free cutting steels. But values of elongation, reduction of area impact are reverse. Fracture surface of impact specimen is ductile in free cutting steels but brittle in medium cabon steels.

  • PDF

대형강괴 주조공정 중 비금속개재물 저감연구 (Nonmetallic Inclusion in the Large Steel Ingot Casting Process)

  • 남궁정;김용찬;김문철;오상훈;김남수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 춘계학술대회 논문집
    • /
    • pp.52-56
    • /
    • 2008
  • Inclusions in forged large steel ingots of plan carbon steel and tool steel are investigated using optical microscop observation and WDX analysis. The large nonmetallic inclusions which is over $30\sim300{\mu}m$ in their diameter were observed in the samples that has been no good on a nondestructive test. The most of the inclusions were consist of some kind of oxides, ${Al_2}{O_3}$, $SiO_2$, CaO, MgO in forms of particles and glassy with an iron particles. The experimental large steel ingot was cast with a pouring temperature which is about ten centigrade higher than the field standard. The inclusions were observed in the test ingot are the smaller than that was in a usual forged steel ingot and is spherical shape with a glassy agglomerated ${Al_2}{O_3}-SiO_2-CaO-MgO$ particle. The pouring temperature is affected on removing the nonmetallic inclusions during the solidification by a floating mechanism.

  • PDF

SUP7-50CrV4강의 피로강도에 미치는 압축잔류응력의 영향 (The effect of compress residual stresses for fatigue strength of SUP7-50CrV4 Steel)

  • 박경동;정찬기
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2001년도 추계학술대회 논문집
    • /
    • pp.247-252
    • /
    • 2001
  • Recently the steel parts used at automobiles are required to be used under high stress more than ever before in need of the weight down. To achieve this requirement of a high strength steel, it must be necessary to decrease inclusion content and surface defect as like decarburization, surface roughness etc.. In this study, the surface conditions are measured to know the influence on fatigue properties by two cases of shot peening of two-stage shot peening and single-stage shot peening. And for this study, two kinds of spring steel (SUP7, 50CrV4) are used. This study shows the outstanding improvement of fatigue properties at the case of two-stage shot peening in the rotary bending fatigue test and this is assumed to be from on low stress condition, the 1st stage shot peening is not affected by nonmetallic inclusion under metal. it is possible that the 2nd stage shot peening increases the fatigue life and the high stress but that is affected by nonmetallic inclusion under metal. so far beeasily 50CrV4 have made high stress. But, results also show fatigue failures originated at inclusion near surface, and this inclusion type is turned out to be a alumina of high hardness.

  • PDF

DIN50CrV4-SAE9254강의 피로강도에 미치는 압축잔류응력의 영향 (The Effect of Compressive Residual Stresses on Fatigue Strength in DIN50CrV4-SAE9254 Steel)

  • 박경동;정찬기
    • 한국해양공학회지
    • /
    • 제15권3호
    • /
    • pp.93-99
    • /
    • 2001
  • Recently the steel parts used at automobils are required to be used under high stress more than ever before in need of the weight down. To achieve this requirement of a high strength steel, it must be necessary to decrease inclusion content and surface defect as like decarburization, surface roughness etc.. In this study, the surface conditions are measured to know the influence on fatigue properties by two cases of shot peening of two-stage shot peening and single-stage shot peening. And for this study, two kinds of spring steel (SAE 9254, DIN50CrV4) are used. This study shows the outstanding improvement of fatigue properties at the case of two-stage shot peening in the rotary bending fatigue test and this is assumed to be from (1) on low stress condition, th 1st stage shot peening is not affected by nonmetallic inclusion under metal.(2) it is possible that the 2nd stage shot peening increases the fatigue life and the high stress but that is affected by nonmetallic inclusion under metal. (3) so far beeasily DIN50CrV4 have made high stress. But, results also show fatigue failures originated at inclusion near surface, and this inclusion type is turned out to be a alumina of high hardness.

  • PDF

JISG4081SUP7-DIN50CrV4강의 피로강도에 미치는 쇼트피이닝의 영향 (Effect of Shot Peening on Fatigue Strength of JISG4081SUP7-DIN50CrV4 Steel)

  • 박경동;정찬기
    • 한국해양공학회지
    • /
    • 제15권4호
    • /
    • pp.66-72
    • /
    • 2001
  • Recently the steel parts used at automobiles are required to be used under high stress more than ever before in need of the weight down. To achieve this requirement of a high strength steel, it must be necessary to decrease inclusion content and surface defect as like decarburization, surface roughness etc.. In this study, the surface conditions are measured to know the influence on fatigue properties by two cases of shot peening of two-stage shot peening and single-stage shot peening. And for this study, two kinds of spring steel (JISG4081SUP7, DIN 50CrV4) are used. This study shows the outstanding improvement of fatigue properties at the case of two-stage shot peening in the rotary bending fatigue test and this is assumed to be from on low stress condition, the 1st stage shot peening is not affected by nonmetallic inclusion under metal. it is possible that the 2nd stage shot peening increases the fatigue life and the high stress but that is affected by nonmetallic inclusion under metal. so far beeasily DIN50CrV4 have made high stress. But, results also show fatigue failures originated at inclusion near surface, and this inclusion type is turned out to be a alumina of high hardness.

  • PDF

스프링강의 피로강도에 미치는 압축잔유응력의 영향 (The effect of compress residual stresses for fatigue strength of Spring Steel)

  • 박경동;정찬기
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.338-343
    • /
    • 2001
  • Recently the steel parts used at automobiles are required to be used under high stress more than ever before in need of the weight down. To achieve this requirement of a high strength steel, it must be necessary to decrease inclusion content and surface defect as like decarburization, surface roughness etc., In this study, the surface conditions are measured to know the influence on fatigue properties by two cases of shot peening of two-stage shot peening and single-stage shot peening. And for this study, two kinds of spring steel(SAE 9254, DIN 50CrV4) are made. This study shows the outstanding improvement of fatigue properties at the case of two-stage shot peening in the rotary bending fatigue test and this is assumed to be from (1) on low stress condition, the single stage shot peening is not affected by nonmetallic inclusion under metal. (2) it is possible that the two-stage shot peening increases the fatigue life and the high stress, but, that is affected by nonmetallic inclusion under metal. (3) so far, beeasily 50CrV4 have made high stress. But, results also show fatigue failures originated at inclusion near surface, and this inclusion type is turned out to be a alumina of high hardness.

  • PDF

Effect of Microstructure on Hydrogen Induced Cracking Resistance of High Strength Low Alloy Steels

  • Koh, Seong Ung;Jung, Hwan Gyo;Kim, Kyoo Young
    • Corrosion Science and Technology
    • /
    • 제6권4호
    • /
    • pp.164-169
    • /
    • 2007
  • Hydrogen induced cracking (HIC) was studied phenomenologically and the effect of microstructure on HIC was discussed for the steels having two different levels of nonmetallic inclusions. Steels having different microstructures were produced by thermomechanically controlled processes (TMCP) from two different heats which had the different level of nonmetallic inclusions. Ferrite/pearlite (F/P), ferrite/acicular ferrite (F/AF), ferrite/bainite (F/B) were three representative microstructures for all tested steels. For the steels with higher level of inclusions, permissible inclusion level for HIC not to develop was different according to steelmicrostructure. On the contrary, HIC occurred also at the martensite/austenite (M/A) constituents regardless of steel microstructure when they accumulated to a certain degree. It was proved that M/A constituents were easily embrittled by hydrogen atoms. Steels having F/AF is resistant to HIC at a given actual service condition since they covers a wide range of diffusible hydrogen content without developing HIC.

디젤 엔진용 캠축 소재의 금속적 특성 및 선삭 가공 특성에 관한 연구 (Turning and Metalic Characterization for CAM Shaft Materials of Diessel Engine)

  • 채왕석;김경우;김동현
    • 한국정밀공학회지
    • /
    • 제14권7호
    • /
    • pp.22-28
    • /
    • 1997
  • In this paper, We have studied internal quality incluiding chemical compositions, microscopic structure and nonmetalic inclusion of test material. We have analyzed dynamic characteristics of cutting resistence and compared chip treatment of the test material. In analyzing internal quality, all of the test material have typical ferrite+pearlite structure. But, nonmetallic inclusion has oxide and sulfide inclusion has oxide and sulfide inclusion in medium carbon steel, mainly sulfide inclusion is existed in S-free cutting steel. In Ca+S-free cutting steel, calcium aluminate and sulfide complex inclusion, had low-melting point, as deformation of sulfide and oxide inclusion is existed. Machining characteristics, cutting resistence is maximum in medium carbon steel. Chip treatement are excellent in S-free cutting steel, similar to the Ca+S free cutting steel and medium carbon steel.

  • PDF

트럭용 커낵팅 로드 소재의 내부 품질에 따른 절삭 특성 연구 (A Study on the Machining Characteristics by the Internal Quality of Conecting Rod's Meterials for Trucks)

  • 김동현
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1996년도 춘계학술대회 논문집
    • /
    • pp.97-101
    • /
    • 1996
  • In this paper, We have studied internal quality incluiding chemical compositions, microscopic structrue and nonmetalic inclusion of test materials. We have analyzed dynamic characteristics of cutting resistence including tensile strength value, hardeness value, impact value etcs. We have compared chip treatments of test materials. In analyzing internal quality, all of test materials have typical ferrite+pearlite structure. But, nonmetallic inclusion have oxide and sulfide inclusion in medium carbon steels, mainly sulfide inclusion is existed in S-free cutting steels. In Ca+S-free cutting steels, calcium aluminate and sulfide complex inclusion, had low-melting points, as deformation of sulfide and oxide inclusion is existed. machining characteristics, cutting resistence is maximum in Ca+S-free cutting steels, minimum in medium carbon steels. Chip treatements are excellent in S-free cutting steels, similar to the Ca+S free cutting steels and medium carbon steels.

  • PDF