Heterogeneous nucleations in the polyol process for the preparation of fine cobalt particles (미립 코발트분말 합성을 위한 polyol공정에서 비균질계 핵생성 반응)

  • 김동진;정헌생;우상덕;이재장;안종관
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.12 no.2
    • /
    • pp.73-79
    • /
    • 2002
  • The polyol process which applies to cobalt, nickel. copper and precious metals is a interesting and unexpected example of such a method for preparing uniform metal powders. The reaction proceeds via dissolution, and the polyol acts simultaneously as a solvent, a reducing agent, and to some extent a protective agent. Submicrometer uniform cobalt particles can be obtained by seeding the reactive medium ($AgNO_3$) to achieve a complete substitution of homogeneous by heterogeneous nucleation. By varying the number of nuclei it is possible to control to some extent the average particle size in the submicrometer (0.5$\mu$m) range.

Production of Fine Cobalt Metal Powders from Superalloy Scrap(1) (Treating Superalloy Scrap with Zinc) (Superalloy 스크랩으로부터 Co 미분말의 제조(1) (Superalloy 스크랩의 아연처리))

  • 박문경;이영근
    • Resources Recycling
    • /
    • v.4 no.1
    • /
    • pp.52-59
    • /
    • 1995
  • Treating bulk superalloy scrap with molten zinc has been studled to facililate recycling and recovery- of cobalt.Superalloys investigated were the cobalt-base Mar-M-509 and X45 and the nickel-base Rene 80. Charges withZnlscrap ratlos of 1.5-6.5 were heated to 750-9002 far 1-7.5 hours in a nitrogen atmosphere. The moltenzinc dissolved superalloy scrap and zinc was removed by vacuum distillation at 850-Wk for 4-6 hours. Ithas been concluded that the optimum conditions of decomposition for Mar-M-509 and Rene 80 \"ere dissolutiontemperature of about 850k, Znlscrap ratlo of about 5, and dissalution time of about 5.5 hours. The zinc-treatedsuperalloy prouducts were friable and reacted rapidly with acid solutions. Leaching 9mm pieces of unalloyedMar-M-509 or Rene 80 with 5 times the stolchlometric amount oi 6N HCI at 90t ior 3 hours dissolved about1.5-7.270, while leachmg of the minus 20-mesh products dissolved about 89.0-93.0%.ved about 89.0-93.0%.