• 제목/요약/키워드: NiMo

검색결과 656건 처리시간 0.027초

Evaluations of Si based ternary anode materials by using RF/DC magnetron sputtering for lithium ion batteries

  • 황창묵;박종완
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2010년도 제39회 하계학술대회 초록집
    • /
    • pp.302-303
    • /
    • 2010
  • Generally, the high energy lithium ion batteries depend intimately on the high capacity of electrode materials. For anode materials, the capacity of commercial graphite is unlike to increase much further due to its lower theoretical capacity of 372 mAhg-1. To improve upon graphite-based negative electrode materials for Li-ion rechargeable batteries, alternative anode materials with higher capacity are needed. Therefore, some metal anodes with high theoretic capacity, such as Si, Sn, Ge, Al, and Sb have been studied extensively. This work focuses on ternary Si-M1-M2 composite system, where M1 is Ge that alloys with Li, which has good cyclability and high specific capacity and M2 is Mo that does not alloy with Li. The Si shows the highest gravimetric capacity (up to 4000mAhg-1 for Li21Si5). Although Si is the most promising of the next generation anodes, it undergoes a large volume change during lithium insertion and extraction. It results in pulverization of the Si and loss of electrical contact between the Si and the current collector during the lithiation and delithiation. Thus, its capacity fades rapidly during cycling. Si thin film is more resistant to fracture than bulk Si because the film is firmly attached to the substrate. Thus, Si film could achieve good cycleability as well as high capacity. To improve the cycle performance of Si, Suzuki et al. prepared two components active (Si)-active(Sn, like Ge) elements film by vacuum deposition, where Sn particles dispersed homogeneously in the Si matrix. This film showed excellent rate capability than pure Si thin film. In this work, second element, Ge shows also high capacity (about 2500mAhg-1 for Li21Ge5) and has good cyclability although it undergoes a large volume change likewise Si. But only Ge does not use the anode due to its costs. Therefore, the electrode should be consisted of moderately Ge contents. Third element, Mo is an element that does not alloys with Li such as Co, Cr, Fe, Mn, Ni, V, Zr. In our previous research work, we have fabricated Si-Mo (active-inactive elements) composite negative electrodes by using RF/DC magnetron sputtering method. The electrodes showed excellent cycle characteristics. The Mo-silicide (inert matrix) dispersed homogeneously in the Si matrix and prevents the active material from aggregating. However, the thicker film than $3\;{\mu}m$ with high Mo contents showed poor cycling performance, which was attributed to the internal stress related to thickness. In order to deal with the large volume expansion of Si anode, great efforts were paid on material design. One of the effective ways is to find suitably three-elements (Si-Ge-Mo) contents. In this study, the Si based composites of 45~65 Si at.% and 23~43 Ge at.%, and 12~32 Mo at.% are evaluated the electrochemical characteristics and cycle performances as an anode. Results from six different compositions of Si-Ge-Mo are presented compared to only the Si and Ge negative electrodes.

  • PDF

인공시효시간에 따른 Ni 기판 Pb-free 솔더접합부의 기계적 물성평가 (Evaluation of Mechanical Property for Pb-free Solder/Ni Plate Joints with Artificial Aging Time)

  • 박소영;양성모;유효선
    • 대한기계학회논문집A
    • /
    • 제39권5호
    • /
    • pp.467-471
    • /
    • 2015
  • 최근까지, 전자제품에 사용되는 솔더는 납성분이 남아 있으며, 전자부품 및 시스템의 무연 (Pb-free) 솔더에 대한 관심은 반도체 및 전자산업에서 증가하고 있다. 본 논문에서 사용된 솔더접합부는 Sn-37Pb, Sn-4Ag 및 Sn-4Ag-0.5Cu/Ni 기판 이다. 인공시효처리는 $150^{\circ}C$에서 각각 0hr, 100hr, 200hr, 400hr, 600hr 그리고 1000hr 동안 수행되었으며, SP 시험을 이용해 $30^{\circ}C$$50^{\circ}C$에서 접합강도를 평가했다. 전단강도는 인공시효시간과 온도가 증가함에 따라 전반적으로 감소하였다. 무연솔더는 Sn-37Pb 보다 총파괴 에너지가 높았으며, Sn-4Ag-0.5Cu/Ni 접합부는 고온에서 기계적 물성치가 가장 우수하였다.

초음파를 이용한 Sn-3.5Ag 플립칩 접합부의 신뢰성 평가 - Si웨이퍼와 Sn-3.5Ag 솔더의 접합 계면 특성 연구 (Flip Chip Solder Joint Reliability of Sn-3.5Ag Solder Using Ultrasonic Bonding - Study of the interface between Si-wafer and Sn-3.5Ag solder)

  • 김정모;김숙환;정재필
    • 마이크로전자및패키징학회지
    • /
    • 제13권1호통권38호
    • /
    • pp.23-29
    • /
    • 2006
  • Si-웨이퍼와 FR-4 기판을 상온에서 초음파 접합한 후, 접합부의 신뢰성을 평가하였다. Si-웨이퍼 상의 UBM(Under Bump Metallization)은 위에서부터 Cu/ Ni/ Al을 각각 $0.4{\mu}m,\;0.4{\mu}m,\;0.3{\mu}m$의 두께로 전자빔으로 증착하였다. FR-4 기판위의 패드는 위에서부터 Au/ Ni/ Cu를 각각 $0.05{\mu}m,\;5{\mu}m,\;18{\mu}m$의 두께로 전해 도금하여 형성하였다. 접합용 솔도로는 Sn-3.5wt%Ag을 두께 $100{\mu}m$으로 압연하여 사용하였다. 시편의 초음파 접합을 위하여 초음파 접합 시간을 0.5초에서 3.0초까지 0.5초 단위로 증가시키면서 상온에서 접합하였으며, 이 때 출력은 1,400W로 하였다. 실험 결과, 상온 초음파 접합법에 의해 신뢰성 있는 'Si-웨이퍼/솔더/FR-4기판' 접합부를 얻을 수 있었다. 접합부의 전단 강도는 접합 시간에 따라 증가하여 접합 시간 2.5초에서 65N으로 가장 높게 측정되었다. 이 후 접합 시간 3.0초에서는 전단 강도가 34N으로 감소하였는데, 이는 초음파 접합시간이 과도해지면서 Si-웨이퍼와 솔더 사이의 계면을 따라 균열이 발생되었기 때문으로 판단된다. 초음파 접합에 의해 Si-웨이퍼와 솔더 사이에서 생성된 금속간 화합물은 ($(Cu,Ni)_{6}Sn_{5}$)으로 확인되었다.

  • PDF

마찰교반접합된 9% Ni 강의 미세조직 및 기계적 특성에 관한 연구 (Study on microstructure and mechanical properties of friction stir welded 9% Ni steel)

  • 최돈현;안병욱;최정현;;연윤모;송건;이종섭;정승부
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2009년 추계학술발표대회
    • /
    • pp.49-49
    • /
    • 2009
  • 마찰교반접합법은 특정한 회전수로 회전하는 용접 툴을 이용하여 접합하고자 하는 피접합재의 맞댄면에 삽입시킨 후 툴을 이동시키거나 혹은 시편을 견고하게 고정시킨 장치(backing plate)가 움직여 고상 상태에서 접합이 이루어진다. 알루미늄, 마그네슘 등 비교적 융점이 낮은 저융점 재료의 재료에 처음 적용이 되어 많은 연구가 활발히 진행되었고 타 용접방법에 비해 우수한 접합특성을 나타내었다. 최근 이러한 마찰교반접합은 이러한 저융점 재료를 넘어서 스틸, 타이타늄, 니켈 등과 같은 고융점 재료 등에 대한 적용이 늘어나고 있다. 마찰교반접합을 이용하여 이러한 고융점 재료의 접합 경우 내마모성 및 내열성 등의 내구성이 갖추어진 툴과 이러한 툴을 냉각시킬 수 있는 냉각 장치 등이 필요로 하나 경제적 측면이나 접합부의 우수한 특성 등을 고려 할 때 그 적용 및 발전 가능성이 매우 높다고 볼 수 있다. 최근 무공해 연료로 각광받고 있는 액화천연가스 (LNG)의 수요가 급증함에 따라 LNG 저장탱크 소재로 널리 사용되고 있는 9% Ni강의 수요 또한 증가하고 있는 상황이다. 하지만 9% Ni 강은 극저온용 소재로 용접부의 저온인성 ($-196^{\circ}C$)이 가장 중요하기 때문에 저온인성을 확보하고자 Inconel 계나 Hastelloy계 등의 니켈 기 합금을 용접재료로 사용하고 있으나 이러한 용접재료는 가격이 매우 고가이며 또한 용접 후 용접부의 강도가 낮다는 문제가 제기되고 있다. 또한 LNG 탱크 제작시 사용되는 용접법은 GTAW, SAW 및 SMAW 이지만 국내에서는 주로 SMAW에 의존하고 있는 실정인 관계로 보다 더 경제적인 용접 프로세스의 적용 가능성이 검토되고 있는 상황이다. 본 연구에서는 마찰교반용접을 이용하여 두께 4mm의 9% Ni 강에 대해 맞대기 마찰교반접합을 실시하였다. 툴 회전 속도 및 접합 속도를 고정한 상태에서 접합을 실시 하였으며 접합 시 툴은 $Si_3N_4$로 제작된 툴을 사용하였다. 접합 후 외관상태 점검, 미세조직 관찰, 경도, 인장 강도 및 저은 충격 측정 등의 실험을 실시하였고, 이러한 결과를 이용하여 미세조직과 기계적 특성과의 관련성을 조사하였다.

  • PDF

이종접합 Gate 구조를 갖는 수평형 NiO/Ga2O3 FET의 전기적 특성 연구 (Electrical Characterization of Lateral NiO/Ga2O3 FETs with Heterojunction Gate Structure)

  • 이건희;문수영;이형진;신명철;김예진;전가연;오종민;신원호;김민경;박철환;구상모
    • 한국전기전자재료학회논문지
    • /
    • 제36권4호
    • /
    • pp.413-417
    • /
    • 2023
  • Gallium Oxide (Ga2O3) is preferred as a material for next generation power semiconductors. The Ga2O3 should solve the disadvantages of low thermal resistance characteristics and difficulty in forming an inversion layer through p-type ion implantation. However, Ga2O3 is difficult to inject p-type ions, so it is being studied in a heterojunction structure using p-type oxides, such as NiO, SnO, and Cu2O. Research the lateral-type FET structure of NiO/Ga2O3 heterojunction under the Gate contact using the Sentaurus TCAD simulation. At this time, the VG-ID and VD-ID curves were identified by the thickness of the Epi-region (channel) and the doping concentration of NiO of 1×1017 to 1×1019 cm-3. The increase in Epi region thickness has a lower threshold voltage from -4.4 V to -9.3 V at ID = 1×10-8 mA/mm, as current does not flow only when the depletion of the PN junction extends to the Epi/Sub interface. As an increase of NiO doping concentration, increases the depletion area in Ga2O3 region and a high electric field distribution on PN junction, and thus the breakdown voltage increases from 512 V to 636 V at ID =1×10-3 A/mm.

Ni-Zn Ferrite의 조성성분 및 소결온도에 따른 물리적 특성의 실험적 연구 (The Effect of Chemical Composition and Sintering Temperature on the Experiment of Physical Properties of Ni-Zn Ferrite)

  • 고재귀
    • 한국자기학회지
    • /
    • 제16권5호
    • /
    • pp.255-260
    • /
    • 2006
  • 기본조성 $(Ni_{0.35}Cu_{0.2}Zn_{0.45})_{1.02}(Fe_2O_3)_{0.98}$과 NiO 비율을 증가시키고 ZnO을 감소시킨 또 다른 기본조성 $(Ni_{0.4}Cu_{0.2}Zn_{0.4})_{1.02}(Fe_2O_3)_{0.98}$에 grain boundary의 높은 저항층을 형성하고 flux로서 사용하기 위해서 0.1 mol% $CaCO_3$와 입자의 성장을 촉진시켜 낮은 손실, 높은 투자율을 얻기 위한 목적으로 $V_2O_5$를 0.03mo1% 첨가하였다. 이들 원료들을 혼합한 후 $600^{\circ}C$에서 2시간 동안 가소시킨 분말을 toroid 시편으로 만들어 소결온도 $1,050^{\circ}C,\;1,070^{\circ}C,\;1,100^{\circ}C$에서 각각 2시간 동안 공기 중에서 소결하였다. 각 시편들에 대한 밀도는 $4.90{\sim}5.10g/cm^3$으로 나타났고, 각 시편들의 고유저항은 $10^8{\sim}10^{12}{\Omega}-cm$으로 측정되었으며, 결정립의 크기는 대략 $3.0{\sim}8.0{\mu}m$이었다. 시편들의 자기유도 특성 값이 대부분 우수하게 나타났으며, 그 중에서도 기본조성 $(Ni_{0.4}Cu_{0.2}Zn_{0.4})_{1.02}(Fe_2O_3)_{0.98}$$CaCO_3$$V_2O_5$를 첨가하고 $1,070^{\circ}C$에서 소결한 시편의 특성 값이 잔류자기유도 1,660 G, 최대자기유도 4,000 G로 약간 더 우수하게 측정되었으며, 각각 시편들의 보자력은 $0.15{\sim}0.25\;Oe$로 전형적인 연자성 재료의 범위로 나타났다. 초투자율, 손실계수, 및 큐리온도는 각각 $2,948{\sim}2,997,\;171{\sim}208,\;191{\sim}202^{\circ}C$로 나타나 Ni-Zn ferrite에서 측정되는 값들과 대동소이했다. 물리적인 특성값(고유저항, 자기유도, 초투자율, 손실계수, 큐리온도 등)으로 미루어보아 각종 microwave 통신기기 core 및 고 투자율 deflection yoke core 등으로 사용이 가능하다.

전이금속-카본나이트라이드 나노튜브 혼성체: 화학적 수소화물 수용액의 수소발생 촉매 (Transition Metal Nanoparticles-Carbon Nitride Nanotube Hybrids: Direct Hydrogen Generation Catalyst of Chemical Hydride Aqueous Solution)

  • 신원호;정형모;강정구
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2009년도 춘계학술대회 논문집
    • /
    • pp.781-781
    • /
    • 2009
  • We demonstrate that trasition metal catalyst nanoparticle (NP) attached to carbon nitride nanotubes (CNNTs) show selective catalytic activities on hydrogen generation from the water solution including chemical hydride negative ions. The natural bonding orbitals (NBO) obtained from the first-principle calculations shows that the catalysts attached on CNNTs are quite differently polarized when they play for hydrogen generation from chemical hydride ions and hydrogen of water. For Co and Ni nanoparticles attached on CNNTs, their charges are more positively polarized when they interact with $BH_4^-Na^+$ and $H_2O$ while Pt atoms are less positively charged. In this matter, the increased positive charges on catlyst nanoparticles are proven to be more efficient in attracting hydride negative ions, thus improving hydrogen generate rates. Consequently, this result implies that these different charge polarization leads to selective catalytic activities of NPs-CNNTs. In the hydrogen generation experiments, Co-CNNTs shows the highest hydrogen generation rate when the similar amounts of catalyst nanoparticles (Co, Ni, and Pt) are dispersed on the sidewalls of CNNTs.

  • PDF

Alloy 617계 산화물 분산강화(ODS) 합금의 제조와 인장특성 (Fabrication and Tensile Properties of Alloy 617 base ODS Alloy)

  • 민형기;강석훈;김태규;한창희;김도향;장진성
    • 한국분말재료학회지
    • /
    • 제18권6호
    • /
    • pp.482-487
    • /
    • 2011
  • Alloy 617, Ni-22Cr-12Co-9Mo base oxide dispersion strengthened alloy was fabricated by using mechanical alloying, hot isostatic pressing and hot rolling. Uniaxial tensile tests were performed at room temperature and at $700^{\circ}C$. Compared with the conventional Alloy 617, ODS alloy showed much higher yield strength and tensile strength, but lower elongation. Fracture surfaces of the tensile tested specimens were investigated in order to find out the mechanism of fracture mode at each test temperature. Grain adjustment during tensile deformation was analyzed by electron backscattered diffraction mapping, inverse pole figures and TEM observation.

Maxillary molar derotation and distalization by using a nickel-titanium wire fabricated on a setup model

  • Jung, Jong Moon;Wi, Young Joo;Koo, Hyun Mo;Kim, Min Ji;Chun, Youn Sic
    • 대한치과교정학회지
    • /
    • 제47권4호
    • /
    • pp.268-274
    • /
    • 2017
  • The purpose of this article is to introduce a simple appliance that uses a setup model and a nickel-titanium (Ni-Ti) wire for correcting the mesial rotation and drift of the permanent maxillary first molar. The technique involves bonding a Ni-Ti wire to the proper position of the target tooth on a setup model, followed by the fabrication of the transfer cap for indirect bonding and its transfer to the patient's teeth. This appliance causes less discomfort and provides better oral hygiene for the patients than do conventional appliances such as the bracket, pendulum, and distal jet. The treatment time is also shorter with the new appliance than with full-fixed appliances. Moreover, the applicability of the new appliance can be expanded to many cases by using screws or splinting with adjacent teeth to improve anchorage.

티타늄과 니켈-크롬 합금의 도재결합강도 비교 (COMPARISON OF THE BOND STRENGTH OF CERAMICS FUSED TO TITANIUM AND Ni-Cr ALLOY)

  • 박세영;전영찬;정창모
    • 대한치과보철학회지
    • /
    • 제41권1호
    • /
    • pp.89-98
    • /
    • 2003
  • Titanium requires special ceramic system for veneering. Low fusing dental ceramics with coefficients of thermal expansion matching that of titanium have been developed. The purpose of this study was determine the bond strengths between cast and noncast pure titanium and two commercial titanium porcelains, and to compare the results with a conventional nickel-chromium alloy-ceramic system. The bond strengths were determined using a 3-point flexure test. Three-point flexure specimens $25{\times}3{\times}0.5mm$ were prepared After removal of ${\alpha}-case$ layer, they were veneered with $8{\times}3{\times}1mm$ of ceramics at the center of the bar. Specimens were tested in a universal testing machine. Within the limits of this study, the following conclusions were drawn: 1. The bond strengths between pure titanium and two commercial porcelains exceeded th lower limit of the bonding strength value in ISO 9693(25MPa). 2. There was no significant difference between cast and noncast titanium-porcelain bonds. 3. There was no significant difference between two commercial titanium porcelains. 4. The bond strengths of the titanium-porcelain systems ranged from 73% to 79% of that of the Ni-Cr-conventional porcelain system.