An Electrochemical Evaluation on the Corrosion of Weld Zone in Cold Arc Welding Process of the Cast Iron (주철의 냉간 아크용접시 용접부의 부식에 관한 전기화학적 평가)

  • Kim, Jin-Gyeong;Mun, Gyeong-Man
    • Proceedings of the KWS Conference
    • /
    • 2005.06a
    • /
    • pp.273-275
    • /
    • 2005
  • Variation of hardness and corrosion potential of welding zone was investigated when cold arc welding of cast iron was carried out with a parameter of Ni electrode. Hardness of HAZ was the highest compared to other welding zone. And corrosion potential of HAZ was also more negative value than other welding zone. However there was not a proportional relation between hardness and corrosion potential. Local corrosion of HAZ was clearly appeared than other welding zone by small anode and large cathode in seal water solution.

  • PDF

Electrical and Optical Properties of Electrochromic Window with Both Lithium and Proton Conducting Polymer Electrolytic Media (리튬 및 프로톤 전도성 고분자전해질을 사용하여 제작한 Electrochromic 창의 전기 및 광학적 특성)

  • 박성용;이철환;김형선;조원일;조병원;윤경석;안춘호;우경근
    • Journal of the Korean institute of surface engineering
    • /
    • v.28 no.1
    • /
    • pp.46-54
    • /
    • 1995
  • An electrochromic(EC) cell was constructed using $WO_3$ as a electrochromic material and NiO as a counter electrode, deposited onto ITO-coated glass by the implementation of electron beam evaporation. The electrolytic media were both lithium and proton conducting polymers such as poly-acrylonitrile(PAN)-$LiClO_4$, poly-ethylene oxide(PEO)-$LiClO_4$, poly-vinyl butyral(PVB)-LiCl and PVB-H$_3$$PO_4$. Potentiodynamic cycling of the cells using PAN-$LiClO_4$, or PVB-$H_3$$PO_4$ electrolyte yielded a transmission variation of more than 40% at the wavelength of 632.8 nm within less than 10 sec response time at room temperature. These results indicate that these electrolytes, transparent in gel type, are premising for the application in large area electrochromic windows.

  • PDF

Spin Transport in a Ferromagnet/Semiconductor/Ferromagnet Structure: a Spin Transistor

  • Lee, W.Y;Bland, J.A.C
    • Journal of Magnetics
    • /
    • v.7 no.1
    • /
    • pp.4-8
    • /
    • 2002
  • The magnetoresistance (MR) and the magnetization reversal of a lateral spin-injection device based on a spin-polarized field effect transistor (spin FET) have been investigated. The device consists of a two-dimensional electron gas (2DEG) system in an InAs single quantum well (SQW) and two ferromagnetic $(Ni_{80}Fe_{20})$ contacts: all injector (source) and a detector (drain). Spin-polarized electrons are injected from the first contact and, after propagating through the InAs SQW are collected by the second contact. By engineering the shape of the permalloy contacts, we were able to observe distinct switching fields $(H_c)$ from the injector and the collector by using scanning Kerr microscopy and MR measurements. Magneto-optic Kerr effect (MOKE) hysteresis loops demonstrate that there is a range of magnetic field (20~60 Oe), at room temperature, over which the magnetization in one contact is aligned antiparallel to that in the other. The MOKE results are consistent with the variation of the magnetoresistance in the spin-injection device.

Trace elements in the rainwater runoff of the urban catchment of Guwahati, India

  • Devi, Upama;Bhattacharyya, Krishna G.
    • Advances in environmental research
    • /
    • v.2 no.2
    • /
    • pp.99-118
    • /
    • 2013
  • Rainwater runoff has been identified as a significant source of contaminants having tremendous impact on the receiving aquatic environment. In the present study, trace element transport by the surface runoff in the predominantly urban catchment of Guwahati city, India was monitored with a view to determine the chemical denudation rates of the land surface. A number of trace metals, namely Cd, Co, Cr, Cu, Fe, Mn, Ni, Pb and Zn were measured in the runoff after 70 major rain events within the city. Cadmium was found to be the least abundant metal and Iron was the most abundant metal in the runoff. The results are interpreted on the basis of temporal and spatial variations in their concentrations. These variations are quite large in some of the events and reflect changes in the local environmental setting, differences in water utilization, variations in runoff volume, gradient and quality.

Piezoelectric properties of PNW-PMN-PZT ceramics for High power Piezoelectric transformer with Manufacturing process (고출력 압전트랜스포머용 PNW-PMN-PZT 세라믹스의 제조 Process에 따른 압전 특성)

  • 황상모;이정선;류주현;박창엽;김종선;유충식
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.238-241
    • /
    • 2000
  • In this paper, we manufactured Pb($Ni_{1/2}$ $W_{1/2}$)$O_3$-Pb($Mn_{1/3}$$Nb_{2/3}$)$O_3$-Pb($Zr_3$Ti)$O_3$ceramics with variation of milling time and investigated its dielectric and piezoelectric properties. Density was increased with the increase of milling time because the sinterability of specimens were improved with the decrease of particle size. The highest value of electromechanical coupling factor was 0.518 at milling time 5hour. The highest values of mechanical quality factor and dielectric constant were 1566, 1590 at milling time 4hour, respectively.

  • PDF

Tensile Strain Characteristics of Critical Current in YBCO Coated Conductors (YBCO CC테이프 임계전류의 인장변형률 특성)

  • Shin, Hyung-Seop;Kim, Ki-Hyun;Oh, Sang-Soo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.274-275
    • /
    • 2005
  • The tensile strain dependency of critical current in YBCO coated conductors was examined at 77K and in the self magnetic field. A commercially available YBCO sample with Cu stabilizer layer was supplied. There existed a peak in the relation between the Ie and tensile strain, and the reversible variation of $I_c$ with applied tensile strain was found. In the neutral axis Ni alloy RABiTS-$Y_2O_3$/YSZ/$CeO_2$ buffered YBCO tape, the $I_c$ recovered reversibly until the applied strain reached to about 0.5%, representing that a significant residual compressive strain induced during cooling to 77 K influenced the axial strain tolerance of YBCO conductors. To investigate the strain and stress influence on the $I_c$, the stress-strain characteristics of YBCO conductors measured at 77 K were discussed.

  • PDF

A study on the formation and mechanical properties of the spray deposits by thermal spray (용사법에 의한 용사층의 형성과 기계적 성질에 관한 연구)

  • 최기영;박동환;김명호
    • Journal of Welding and Joining
    • /
    • v.7 no.3
    • /
    • pp.55-62
    • /
    • 1989
  • Variation of the spray droplet velocity with spraying distance and the microstructural characteristics of spray deposits fromed by oxy-fuel thermal spraying with Ni-base alloy powder contained chrome boride for hard facing were examined. Measurements of spray droplet velocity as a function of distance from the nozzle tip were inexcellent agreement with computer simulated predictions. Optimum condition for thermal spray deposits in this experiment was found to be under #10kg/cm^2$ of acceleration gas pressure with 15cm of spraying distance. Fine microstructure and higher microhardness of the initial part of the deposits due to rapid solidification were found to be able to maintained in a thickness up to 0.4mm, and this initial microstructure and properties could be maintained throughout the thickness of a thick spray deposits by performing the multipass spraying with 0.4mm thickness of each pass.

  • PDF

Cyclic fatigue resistance tests of Nickel-Titanium rotary files using simulated canal and weight loading conditions

  • Cho, Ok-In;Versluis, Antheunis;Cheung, Gary S.P.;Ha, Jung-Hong;Hur, Bock;Kim, Hyeon-Cheol
    • Restorative Dentistry and Endodontics
    • /
    • v.38 no.1
    • /
    • pp.31-35
    • /
    • 2013
  • Objectives: This study compared the cyclic fatigue resistance of nickel-titanium (NiTi) files obtained in a conventional test using a simulated canal with a newly developed method that allows the application of constant fatigue load conditions. Materials and Methods: ProFile and K3 files of #25/.06, #30/.06, and #40/.04 were selected. Two types of testing devices were built to test their fatigue performance. The first (conventional) device prescribed curvature inside a simulated canal (C-test), the second new device exerted a constant load (L-test) whilst allowing any resulting curvature. Ten new instruments of each size and brand were tested with each device. The files were rotated until fracture and the number of cycles to failure (NCF) was determined. The NCF were subjected to one-way ANOVA and Duncan's post-hoc test for each method. Spearman's rank correlation coefficient was computed to examine any association between methods. Results: Spearman's rank correlation coefficient (${\rho}$ = -0.905) showed a significant negative correlation between methods. Groups with significant difference after the L-test divided into 4 clusters, whilst the C-test gave just 2 clusters. From the L-test, considering the negative correlation of NCF, K3 gave a significantly lower fatigue resistance than ProFile as in the C-test. K3 #30/.06 showed a lower fatigue resistance than K3 #25/.06, which was not found by the C-test. Variation in fatigue test methodology resulted in different cyclic fatigue resistance rankings for various NiTi files. Conclusions: The new methodology standardized the load during fatigue testing, allowing determination fatigue behavior under constant load conditions.

Microstructure Generation and Linearly Elastic Characteristic Analysis of Hierarchical Models for Dual-Phase Composite Materials (이종 입자복합재의 미세구조 생성과 계층적 모델의 선형 탄성적 응답특성 해석)

  • Cho, Jin-Rae
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.31 no.3
    • /
    • pp.133-140
    • /
    • 2018
  • This paper is concerned with the 2-D micostructure generation for $Ni-A{\ell}_2O_3$ dual-phase composite materials and the numerical analysis of mechanical characteristic of hierarchical models of microstructure which are defined in terms of the scale of microstructure. The microstructures of dual-phase composite materials were generated by applying the mathematical RMDF(random morphology description functions) technique to a 2-D RVE of composite materials. And, the hierarchical models of microstructure were defined by the number of Gaussian points. Meanwhile, the volume fractions of metal and ceramic particles were set by adjusting the level of RMD functions. The microstructures which were generated by RMDF technique are definitely random even though the total number of Gaussian points is the same. The randomly generated microstructures were applied to a 2-D beam model, and the variation of normal and shear stresses to the scale of microstructure was numerically investigated. In addition, through the crack analyses, the influence of RMDF randomness and Gauss point number on the crack-tip stress is investigated.

Phase Changes of the STS 431 Martensitic Stainless Steel after High Temperature Gas Nitriding Treatment (STS 431 마르텐사이트계 스테인리스강의 고온 가스 질화 열처리에 따른 상변화)

  • Yoo, D.K.;Kong, J.H.;Lee, H.W.;Kang, C.Y.;Kim, Y.H.;Sung, J.H.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.21 no.5
    • /
    • pp.244-250
    • /
    • 2008
  • This study has investigated the surface phase change, hardness variation, surface precipitates, nitrogen content and corrosion resistance in STS 431 (17Cr-2Ni-0.2C-0.01Nb) martensitic stainless steel after high temperature gas nitriding (HTGN) treatment at the temperature range between $1050^{\circ}C$ and $1150^{\circ}C$. The HTGN-treated surface layer appeared $Cr_2N$ of rod type, carbo-nitride of round type and fine precipitates in the austenite matrix. On the other hand the interior region where the nitrogen was not permeated, exhibited martensite phase. The surface hardness showed 250~590 HV, depending on the HTGN treatment conditions, while the interior martensitic phase represented 520 HV. The permeation depth of nitrogen increased with increasing the HTGN-treated temperature. The nitrogen concentration of the surface layer appeared approximately ~0.17% at $1100^{\circ}C$. On comparing the corrosion resistance between solution-annealed and HTGN-treated steels, the corrosion resistance of HTGN-treated steel was superior to that of solution-annealed specimens.