Microstructural evolution during a heat treatment and high-temperature tensile properties have been investigated in conventionally cast CM247LC. In as-cast specimens, MC carbides with high amounts of Ta, Ti, Hf, and W were found to exist in the interdendritic regions, and γ' was observed in the form of cubes and octocubes prior to decomposition into cubes. In the heat-treated condition, some portion of eutectic γ-γ' remained, and uniform cubic γ' was observed in both interdendritic regions and dendrite core. Three types of carbides with different stoichiometries and compositions were found at the grain boundaries. MC carbides with high Hf contents were observed in the vicinity of eutectic γ-γ'. The highest tensile strength value was found at 750℃, whereas the greatest ductility appeared at 649℃. The effect of the temperature on the tensile properties was closely related to the dislocation structure. With increase in the test temperature, the density of dislocations inside γ' decreased, whereas that in the γ matrix increased. Stacking faults generated in γ' at 750℃ had a strengthening effect, whereas thermally activated dislocation motion at a high temperature was considered to have the opposite effect.
In this study, solid solution heat treatment of consolidated nickel-based superalloy powders is carried out by hot isotactic pressing. The effects of the cooling rate of salt quenching, and air cooling on the microstructures and the mechanical properties of the specimens are analyzed. The specimen that is air cooled shows the formation of serrated grain boundaries due to their obstruction by the carbide particles. Moreover, the specimen that is salt quenched shows higher strength than the one that is air cooled due to the presence of fine and close-packed tertiary gamma prime phase. The tensile elongation at high temperatures improves due to the presence of grain boundary serrations in the specimen that is air cooled. On the contrary, the specimen that is salt quenched and consists of unserrated grain boundaries shows better creep properties than the air cooled specimen with the serrated grain boundaries, due to the negative creep phenomenon.
The Ni-based superalloy, Inconel 740, was corroded between 800 and 1100℃ for up to 100 hr in air and Ar-0.2%SO2 gas in order to study its corrosion behavior in air and sulfur/oxygen environment. It displayed relatively good corrosion resistance in both environment, because its corrosion was primarily dominated by not sulfidation but oxidation especially in Ar-0.2%SO2 gas. Such was attributed to the thermodynamic stability of oxides of alloying elements when compared to corresponding sulfides. The scales consisted primarily of Cr2O3, together with some NiAl2O4, MnCr2O4, NiCrMnO4, and rutile-TiO2. Sulfur from SO2 gas made scales prone to spallation, and thicker. It also widened the internal corrosion zone when compared to air. The corrosion resistance of IN740 was mainly indebted to the formation of protective Cr2O3-rich oxides, and suppression of the sulfide formation.
Hot gas path components, which are made of nickel based superalloys, are subject to periodic replacement due to degradation of thermomechanical properties that might bring catastrophic failure during normal operation of gas turbine units. In order to rejuvenate the metallurgical condition of the serviced components, heat treating techniques such as solution annealing and aging heat treatments have widely been employed. However, the effectiveness of those typical heat treatments is not apparent enough in terms of quantitative grounds. On the other hand the demand of the rejuvenation heat treatment and hot isostatic pressing (HIP) have constantly been raised by the end users. Therefore it is necessary to verify how the typical heat treating techniques affect to the aged and degraded material. As the result of experimental work in this study, GTD-111 and GTD-222 Ni-based superalloys were collected and analyzed quantitatively through microscopic observation, microhardness evaluation and creep test.
Alloy 617 is considered as a candidate Ni-based superalloy for the intermediate heat exchanger (IHX) of a very high-temperature gas reactor (VHTR) because of its good creep strength and corrosion resistance at high temperatures. Helium is used as a coolant in a VHTR owing to its high thermal conductivity, inertness, and low neutron absorption. However, helium inevitably includes impurities that create an imbalance in the surface reactivity at the interface of the coolant and the exposed materials. As the Alloy 617 has been exposed to high temperatures at $950^{\circ}C$ in the impure helium environment of a VHTR, the degradation of material is accelerated and mechanical properties decreased. The high-temperature strength, creep, and corrosion properties of the structural material for an IHX are highly important to maintain the integrity in a harsh environment for a 60 year period. Therefore, an alloy superior to alloy 617 should be developed. In this study, the mechanical and high-temperature corrosion properties for Ni-Cr alloys fabricated in the laboratory were evaluated as a function of the grain boundary strengthening and alloying elements. The ductility increased and decreased by increasing the amount of Mo and Cr, respectively. Surface oxide was detached during the corrosion test, when Al was not added to alloy. However the alloy with Al showed improved oxide adhesive property without significant degradation and mechanical property. Aluminum seems to act as an anti-corrosive role in the Ni-based alloy.
The silicon nitride based ceramic cutting tool materials have been fabricated by gas pressure sintering (GPS) or hot pressing (HP). Their mechanical properties were measured and the effect of the fabrication variables on the properties were examined. Also, effect of adding TiN or TiC particulates on the mechanical properties of the silicon nitride ceramics were investigated. Ceramic cutting tools (ISO 120408) were made of the sintered bodies. Cutting performance test were performed on either conventional or NC lathe. The workpieces were grey cast iron, hardened alloy steel (AISI 4140, HRc>60) and Ni-based superalloy (Inconel 718). The results showed that fabrication variables, namely, sintering temperature and time, exerted a strong influence on the microstincture and mechanical properties of the sintered body, which, however, did not make much difference in wear resistance of the tools. High hardness of the tool containing TiC particulates exhibited good cutting performance. Extensive crater wear was observed on both monolithic and TiN-containing silicon nitride tools after cutting the hardened alloy steel. Inconel 718 was extremely difficult to cut by the current cutting tools.
일방향응고로 제조된 니켈기 초내열합금 CM247LC의 다양한 온도 및 응력조건에서 크리프 특성에 대해 고찰하였다. 열처리 후 일부 공정조직이 남아 있었으며 비교적 균일한 육면체의 γ'이 수지상 내부와 수지상간 영역에서 관찰되었다. 상대적 저온인 750℃의 고응력 크리프 영역에서는 1차 크리프 동안 많은 변형이 발생하였으나 고온으로 갈수록 3차 크리프 구간이 크리프 변형시간의 대부분을 차지함을 알 수 있었다. 저온 고응력에서는 부분 전위가 γ'으로 진입하며 적층결함을 γ'내에 생성시켰으며 초기 크리프 변형속도가 증가하는 부분이 있었으나 850℃ 이상의 온도에서는 γ' 내부에서 적층결함이 관찰되지 않았으며 이는 적층결함에너지의 온도의존성 때문인 것으로 판단된다. 고온이어서 확산속도가 빠른 950℃와 1000℃에서는 γ'의 래프팅이 관찰되었다. 온도가 좀 더 낮은 850℃에서는 변형기구가 응력에 따라 다르게 나타나서 상대적으로 크리프 시간이 긴 저응력에서만 래프팅이 관찰되었다.
The effects of the brazing temperature and homogenizing time for brazed specimens on the joint of Ni-based superalloys such as Haynes 250, Inconel 617 and Hastelloy-X were investigated. The brazing alloy is nickel base MBF 15. The foil had a thickness of $38{\mu}m$, which was used two sheets of that for the all experiments. The experimental brazing was carried out by a brazing process in a vacuum of approximately $2{\times}10^{-5}$ Torr, an applied pressure of about 0.74MPa and the three kinds of brazing temperatures were 1100, 1150, and $1190^{\circ}C$ for a holding time of 5 to 1440 minutes. Microstructural observations were made on the cross-sectional samples by using an optical microscope(OM), scanning electron microscope(SEM), and electron probe X-ray microanalyzer(EPMA). The tensile tests were performed at room temperature with a cross head speed 1.5 mm/min according to ASTM E8M. The results show that excellent joint tensile strengths of as high as 788MPa were obtained when processed at $1190^{\circ}C$ for 5 minutes.
단련용 다결정 Ni기 초내열합금은 우수한 가공성, 내산화성, 고온특성 등으로 가스터빈 연소기, 디스크, 증기발생기 전열관 등 발전용 고온부품 소재에 널리 적용되고 있다. 최근 발전설비의 고효율화를 꾀하기 위해 작동 온도를 현격히 증가시키는 기술방향으로 발전하고 있고, 소재측면에서는 기존의 초내열합금 대비 고기능성을 확보할 수 있는 차세대 Ni기 초내열합금 개발이 유럽, 미국, 일본, 중국 등을 중심으로 활발히 이루어지고 있다. 이러한 소재의 고온강도 (온도수용성)를 향상시키기 위해서는 통상 규칙격자 금속간화합물인 $Ni_3(Al,Ti)-{\gamma}'$상의 분율을 증가시킬 수 있지만, ${\gamma}'$상분율이 증가할 경우 용접 및 후열처리 동안 용접열영향부 (HAZ)에서 액화균열이 발생할 가능성이 높아진다. 결정립계를 따라 발생하는 HAZ 액화균열은 입계특성에 의해 크게 영향을 받을 것으로 판단된다. 한편, 본 연구자들은 최근 입계 serration 현상을 단련용 합금에 도입시키는 특별한 열처리를 이론적 접근법을 통해 개발하였다. 형성된 파형입계는 결정학적인 관점에서 조밀 {111} 입계면을 갖도록 분해 (dissociation)되어 낮은 계면에너지를 갖게 됨을 확인하였으며, 입계형상 변화뿐만 아니라 탄화물 특성변화까지 유도하여 크리프 수명을 기존대비 약 40% 정도 향상시킴을 확인하였다. 이러한 직선형 입계 대비 'special boundary'로 간주되는 파형입계가 도입될 경우, HAZ 결정립크기 변화 및 액화거동에 미치는 영향을 고찰하고, 아울러 입계특성 제어가 용접성/용접부 품질 향상에 기여할 수 있는 가능성도 토의하고자 하였다. 본 연구에서는 재현 HAZ 열사이클 시험을 통해 미세구조를 정량적으로 비교하였다. 상대적으로 입계구조가 안정된 파형입계의 이동속도가 高계면 에너지를 갖는 직선형 입계보다 느려 HAZ 결정립 성장이 효과적으로 억제됨을 확인할 수 있었다. 입계 액화거동을 살펴보면, 두 시편 모두 $M_{23}C_6$, MC 등 입계탄화물 계면이 빠른 승온중 액화반응 (constitutional liquation)에 의해 입계가 액화되었으며, 이후 급냉에 의해 입계에 액상막이 존재한 흔적이 발견되었다. 최고온도별로 입계액화 폭/비율을 정량적으로 비교한 결과, 파형입계가 직선입계 대비 대체로 낮음을 확인할 수 있었으며, 때때로 액화되지 않고 잔존하는 입계 탄화물이 관찰되었다. 재현 HAZ 미세조직을 통해 Hot ductility 시험 결과를 유추하자면, 파형입계가 직선입계 보다 좁은 취성온도영역 (Brittle Temperature Range)을 나타낼 것으로 예상되어, 입계특성제어에 의해 Ni기 초내열합금의 용접성을 향상 가능성을 확인하였다.
This study used optical and scanning electron microscopy to analyze the surface oxidation phenomenon that accompanies a γ'-precipitate free zone in a directional solidified CM247LC high temperature creep specimen. Surface oxidation occurs on nickel-based superalloy gas turbine blades due to high temperature during use. Among the superalloy components, Al and Cr are greatly affected by diffusion and movement, and Al is a major component of the surface oxidation products. This out-diffusion of Al was accompanied by γ' (Ni3Al) deficiency in the matrix, and formed a γ'-precipitate free zone at the boundary of the surface oxide layer. Among the components of CM247LC, Cr and Al related to surface oxidation consist of 8 % and 5.6 %, respectively. When Al, the main component of the γ' precipitation phase, diffused out to the surface, a high content of Cr was observed in these PFZs. This is because the PFZ is made of a high Cr γ phase. Surface oxidation of DS CM247LC was observed in high temperature creep specimens, and γ'-rafting occurred due to stress applied to the creep specimens. However, the stress states applied to the grip and gauge length of the creep specimen were different, and accordingly, different γ'-rafting patterns were observed. Such surface oxidation and PFZ and γ'-rafting are shown to affect CM247LC creep lifetime. Mapping the microstructure and composition of major components such as Al and Cr and their role in surface oxidation, revealed in this study, will be utilized in the development of alloys to improve creep life.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.