Effect of Assist Gas on Laser Induced Plasma and Bead Formation in Welding of Structural Steel by CW Nd:YAG Laser (철강재료 용접에서 보조가스가 레이저플라즈마와 용입특성에 미치는 영향)

  • 김기철;신현준
    • Journal of Welding and Joining
    • /
    • v.20 no.3
    • /
    • pp.109-115
    • /
    • 2002
  • In this study high power Nd:YAG laser welding of structural steel was investigated. For the test steel blocks of $50{\times}50{\times}200mm$ were cut and machined, and bead-on-plate weld was made on the machined surface. Argon, nitrogen, helium, dry air or mixed gases were used to find the effect of shielding conditions on the bead formation. Results demonstrated that there were Fe I rich region and Fe II rich region in the laser induced plasma column based on the spectral analysis with S-2000 field spectrometer The Fe I region was located at the root of the column near keyhole opening. On the other hand, Fe II region was found at the middle of the plasma column. In the Nd:YAG laser welding, Fe I region emitted continuum which had peak value at wave length of around 710nm, and Fe II region had the peak at 580nm. In the welding of steel by $CO_2$ laser, however, no continuum was observed. There showed two groups of strong spikes in the $CO_2$ laser welding; the first group was displayed at the wave band of 450-560nm. This spike group emitted stronger intensity of light and sharper peaks than those group at 680-800nm.

Lap Welding of Magnesium Alloy using Nd:YAG Laser (Nd:YAG 레이저를 이용한 마그네슘 합금의 겹치기 용접)

  • Kim, J.D.;Lee, J.H.;Suh, J.
    • Laser Solutions
    • /
    • v.14 no.3
    • /
    • pp.12-16
    • /
    • 2011
  • In automotive industry, because of the consideration of fuel economy, lightweight alloys have been adopted and are expected to be extensively used in the future. Magnesium alloys are among the promising materials, due to their lightweight and good mechanical properties. This study is related to the laser weldability of AZ31B magnesium alloy, an all-purpose wrought alloy with good strength and ductility. A 4kW Nd:YAG laser was used to join AZ31B sheet, and the effects of welding parameter on the quality of lap-welded joints were investigated. As a result of this study, the optimal condition was obtained, and the effect of gap distance was also revealed on the porosity control.

  • PDF

The Weldability of Aluminum Ball in Electrolyte Injection Hole by Nd:YAG Laser (리튬이온전지의 전해액 주입구 볼에 대한 Nd:YAG 레이저 용접성)

  • Kim, Jong-Do;Yoo, Seung-Jo;Kim, Jang-Soo
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.30 no.6
    • /
    • pp.740-745
    • /
    • 2006
  • This study suggested the occurrence source of weld-defects and its solution methods in a welding of Electrolyte injection hole by pulsed Nd:YAG laser. In experiment, the ramp down was used in order that solidification crack was removed. Furthermore. shrinkage stress and heat input were reduced by changing of weld trajectory and defocused distance. As a results of a experiment, a sound weld bead shape and crack-free weld bead can be obtained. In conclusion this show that the welding stability is greatly affected by modulation of laser pulse shape for the same laser energy and welding parameters.

Effect of Process Parameters on Bead Formation in Nd:YAG Laser Welding of Thin Steels (저탄소 박판 강재의 Nd:YAG 레이저 용접부 형성에 미치는 공정변수의 영향)

  • 김기철;허재협
    • Journal of Welding and Joining
    • /
    • v.19 no.3
    • /
    • pp.317-324
    • /
    • 2001
  • This study deals with high power Nd:YAG laser welding of thin steels for small pressure vessels. Full penetration welding at the overlap joint was performed so as to assure sufficient weld strength. Results showed that mid-depth weld size reduced drastically with increasing the travel speed. Position of focus had little effect on the bead formation even though short focal system was used. However, the shape factor and the bead width had closely related with the position of focus. Based on the microstructural inspection, acceptable weld was obtained when the overlap clearance was controlled up to 20% of the base metal thickness. In the case that the joint contained more clearance than the critical value, both the tensile shear strength and the tear strength were reduced. Results also demonstrated that shielding gases were proved to play a key role as far as the bead formation characteristics was taken into consideration. Blowing dry air through 5mm in diameter nozzle produced narrower bead cross-section than that of argon or nitrogen shielding.

  • PDF

Investigation of the Properties of Laser-Welded Amorphous Metal in a Deep Frozen Environment (극저온 환경하에서 레이저 용접된 비결정질 재료의 특성에 관한 연구)

  • 이건상
    • Journal of Welding and Joining
    • /
    • v.15 no.3
    • /
    • pp.99-108
    • /
    • 1997
  • For the conventional welding method, the high heat transfer makes the crystallization of the work material unavoidable. Whereas the laser is able to weld the amorphous metal without a crystallized zone, because heat transfer is limited withn a very small restricted volume. In this paper, the possibilities and the limits of the laser welding in a deep frozen environment by liquid nitrogen were studied to utilize the advantageous properties of amorphous metal foils. The author investigated, after laser welding in a deep frozen environment with a solid state laser (Nd:YAG-laser), the achievable strengths and the influences of the laser beam parameters on the strengths.

  • PDF

The Weldability of Laminated Stator Core for Motor by Pulsed Nd:YAG Laser [II] - Investigation of Mechanism on Formation of Weld Defect - (펄스 Nd:YAG 레이저를 이용한 모터용 스테이터 적층코어의 용접특성 [II] - 용접결함의 형성 메커니즘 규명 -)

  • Kim Jong-Do;Kil Byung-Lea;Lee Chang-Je
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.30 no.5
    • /
    • pp.636-644
    • /
    • 2006
  • Recently, there were some successful examples that the laser welding was introduced into production line. However, the spread of laser welding is not sufficient in many industries. There are several reasons why it is difficult to penetrate the laser welding into production lines. Because it is different from reflection, absorption and permeation of laser beam according to material and surface condition. Moreover, there are significant problems in processing such as absorption and scattering of beam by the induced plasma or plume. Therefore, understanding of mechanism on formation of weld defect in laser welding of the laminated core for motor is very important. In this paper, it was analyzed in terms of materials which was source of defect in laser welding and conventional arc welding. As a results of analysis, insulation coating film of the laminated core was judged to main factor of weld defect. it could be well aware as tracing carbon volume, and it was deduced that weld defect by insulation coating film was caused by difference of mechanism between the two heat sources.

Characteristics of Output Energy and Optical Parameters in Welding of Braun Tubes by Pulsed Nd:YAG Laser (펄스 Nd:YAG 레이저에 의한 브라운관 부품의 용접시 빔의 출력특성과 광학변수)

  • Kim Jong-Do;Ha Seung-Hyup
    • Laser Solutions
    • /
    • v.8 no.1
    • /
    • pp.27-37
    • /
    • 2005
  • During laser spot welding of the braun tube electron gun, phenomena such as serious spattering and oxidative reaction, etc. were occurred. The spatter occurred from weld pool affects the braun tube, namely it blocks up a very small hole on the shadow mask and causes short circuit between two poles of the electron gun. We guessed that high power density and oxidative reaction are main sources of these problems. So, we studied to prevent and to reduce spatter occurring in spot welding of the braun tube electron gun using pulsed Nd:YAG laser. The characteristics of laser output power was estimated, and the loss of laser energy by optical parameter and spatter was measured by powermeter. The effects of welding parameters, laser defocused distance and incident angle, were investigated on the shape and penetration depth of the laser welded bead in flare and flange joints. From these results, the laser peak power was a major factor to control penetration depth and to occur spatter. It was found that the losses of laser energy by optic parameter and sticked spatter affect seriously laser weldability of thin sheets.

  • PDF

Finite element analysis for prediction of weld bead shape of Nd:YAG pulse laser welding for AISI 304 stainless steel plate (AISI 304 스테인리스 강판의 Nd:YAG 펄스 레이저 용접비드 형상예측을 위한 유한요소해석)

  • Cho Haeyong;Kim Kwanwoo;Hong Jinuk;Lee Jaehoon;Suh Jeong
    • Laser Solutions
    • /
    • v.8 no.1
    • /
    • pp.19-25
    • /
    • 2005
  • Pulse laser welding of AISI 304 stainless steel plate was simulated to optimize welding conditions by using commercial finite element code MARC. Due to geometric symmetry, a half model of AISI 304 stainless steel plate was considered. for the heat transfer analysis, user subroutines were applied to boundary condition. The material properties such as conductivity, specific heat, and mass density were given as a function of temperature and the latent heat associated with a given temperature range was considered. A moving heat source was designed on the basis of experimental data. As a result, Nd:YAG laser welding for AISI 304 stainless steel was successfully simulated and it should be useful to determine optimal welding condition.

  • PDF

Development of a Nd;YAG Welding System and Its Applications (Nd:YAG 레이저 응접기의 국산화개발 및 응용)

  • 김철종;이종민
    • Proceedings of the Optical Society of Korea Conference
    • /
    • 1989.06a
    • /
    • pp.107-115
    • /
    • 1989
  • A 200 W industrial Nd:YAG laser was developed and its weding applications were investigated. The important factors in designing of an industrial Nd:YAG laser were analyzed and special sedign features were explained. Also, the performance of laser weldings of Zircaloy-4, stainless steel and fine thermocouples was presented.

  • PDF

A Study on the Manufacture of instrumented Irradiation Fuel by Nd:YAG Laser Welding (Nd:YAG 레이저 용접에 의한 계장 조사연료봉 제조에 관한 연구)

  • 이철용;이도연;김수성;송기찬
    • Proceedings of the KWS Conference
    • /
    • 2004.05a
    • /
    • pp.115-117
    • /
    • 2004
  • Nd:YAG laser welding system was used to manufacture instrumented irradiation fuel. The optimal condition of zircaloy-4 seal tube is charge voltage 180V and pulse per energy 51. We got good welding result in charge voltage 400V, pulse width 7ms, pulse frequency 5 in zircaloy-4 endcap welding.