• 제목/요약/키워드: Natural zeolite

검색결과 232건 처리시간 0.044초

천연(天然) Zeolite의 CEC 증가(增加)와 입단화(粒團化)에 관(關)한 연구(硏究) -1. NaOH농도(濃度)와 조반비(曺礬比)(Na2O/Al2O3)의 영향(影響) (The Study on the CEC Increase and Granulation of Natural Zeolite -The Effect of NaOH Concentration and Na2O/Al2O3 Ratio)

  • 최정;허남호
    • 한국토양비료학회지
    • /
    • 제26권2호
    • /
    • pp.67-71
    • /
    • 1993
  • 부가가치(附加價値)가 낮은 천연(天然) Zeolite 미분(微分)을 이용(利用)하여 CEC가 높은 토양개량제(土壤改良劑) 혹은 흡착제(吸着劑)의 개발(開發)을 시도하였다. 천연(天然) Zeolite의 $SiO_2/Al_2O_3$의 비(比)는 6.78이었으며 CEC는 67.5mg/100g이었다. 그러나 3N-NaOH용액(溶液)으로 $Na_2O/Al_2O_3$의 비(比)를 9.5로 하여 8시간(時間) 처리(處理)한 반응생성물(反應生成物)의 CEC는 약 200me/100g이었으며 다른 조건(條件)으로 처리(處理)한 반응생성물(反應生成物)의 CEC보다 높았다. 천연(天然) Zeolite의 주(主)된 점토광물(粘土鑛物)은 Clinoptilolite, Mordenite 및 Smectite였으나 반응생성물(反應生成物)은 Philipsite로 동정(同定)되었다.

  • PDF

Zeolite의 특성 (Characteristics of Zeolites)

  • 임굉
    • 자연과학논문집
    • /
    • 제6권1호
    • /
    • pp.103-108
    • /
    • 1993
  • Zeolite는 기공을 통한 흡착과 분리작용의 특징을 지닌 흡착제.분리제로서는 물론, 기체나 액체의 건조제 및 촉매로 그리고 화학공학적 공정기술에있어서 혼합물의 분리정제공정에 널리 이용되고 있고, 다른 silica gel, 활성제, 활성 alumina 및 산성백토등에 비하여 독특한 특성을 가지고 있으며, aluminosilicate 광물의 일종인 천연 zeolite가 광물학적 특성과 화학적 표면활성으로 인하여 다방면에 있어서 공업적 이용도가 날로 증가하고 있다. 광물학상 zeolite는 Na, Ca등 양이온을 함유하는 규산염물질로서 산소환의 공경이 $3~11\AA$ 정도인 입체망상구조로 되어있어 탈착이 자유스러운 수분을 함유하고 있으며 광물중에서 양이온 교환능(C.E.C가 대략 100~300)이 대단히 높기 때문에 기체에 대한 선택적 흡착력이 큰 광물로 알려져 있다. 더욱이 천연 zeolite는 토양계량제나 가축사료용, 혼합비료 및 농약등에도 사용되고 있으며 공업용으로 제지원료로서 백색도가 높고 경도가 낮다는 특성뿐만 아니라 단열.보온재 및 건재등 공업재료로서의 활용성, 그리고 흡착제, 흡습제, 건조제, 이온교환체, 증량제 및 molecular sieve로서의 이용은 괄목할 만 하다. 특히 높은 양이온 교환능을 이용한 중금속 발수처리제나 방수성 발수의 처리제, 경수의 연화제로서의 이용도가 높아지고 있어 앞으로 zeolite의 공업화에 따른 새로운 제조방법과 활용가능성을 모색해야 한다.

  • PDF

혼화재로서 천연제올라이트 및 이암의 활용성 검토에 관한 연구 (The Investigation for the Possibility to Utility on the Natural Zeolite and Mud Stone as Admisxture)

  • 김화중;김태섭;박정민;한종훈
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1993년도 가을 학술발표회 논문집
    • /
    • pp.167-172
    • /
    • 1993
  • In domestic, there are not adequate admixtures for concrete now, so the study on that is required deeply, Accordingly the purpose of this study is to analyze the application possibilities of Natural Zeolite and Mud Stone as admixtures for concrete through comparing the compressive strength prorerties of mortar mixed with imported Silica Fume those mixed with domestic Zeolite and Mud Stone. As the results from this study, the optimum displacement rate of Silica Fume, Zeolite and Mud Stone is 15%, 5~10%, 15% respectively. In Zeolite and Mud Stone, the compressive strength is higher in proportion as the powder is fine. Consequentely, the application possibility the application possibility of Zeolite and Mud Stone is very sufficient as admixtures for concrete.

  • PDF

화학처리 및 금속이온 교환된 천연 제올라이트의 질소 흡착특성 (Nitrogen Adsorption Characteristics of Chemical-treated and Metal Ion-exchanged Natural Zeolite)

  • 이재영;심미자;김상욱
    • 공업화학
    • /
    • 제5권6호
    • /
    • pp.1024-1029
    • /
    • 1994
  • 경북 감포지역에서 산출되는 천연 제올라이트를 각기 다른 농도의 HCl과 NaOH로 화학처리한 시료와 금속양이온 교환한 시료를 제조 하였다. 이들 시료에 대한 질소의 흡착특성을 $25^{\circ}C$, 100~760 torr의 범위에서 조사하였다. 산처리한 시료의 질소 흡착량은 처리하기 전보다 감소하였으며, 알칼리 처리한 시료는 많이 증가하였다. 0.5N-HCl 처리 후 0.5N-NaOH로 연속처리한 경우 약 200% 정도 흡착량이 개선되었으나, 알칼리 처리 후 산으로 연속처리한 경우에는 오히려 감소하였다. $Na^+$, $K^+$, $Cs^+$를 이온교환한 경우 이온의 크기가 증가할수록 흡착량은 감소했으며, $Mg^{2+}$, $Ca^{2+}$, $Ba^{2+}$를 이온교환한 경우는 이온의 크기가 증가할수록 흡착량이 증가하였다.

  • PDF

천연 Zeolite와 산화철을 이용한 폐수 중 질소 및 인의 처리 (Removal Nitrogen and Phosphorus from Wastewater using Natural Zeolite and Iron Oxide)

  • 원성연;이상일
    • 한국물환경학회지
    • /
    • 제20권2호
    • /
    • pp.104-109
    • /
    • 2004
  • Removal of nutrients from domestic sewage or industrial wastewater is needed to protect surface waters from eutrophication. This research was carried out to remove the nitrogen (N) and phosphorus (P) from the wastewater using the iron oxide obtained from the steel industry and the natural zeolite, respectively. This research was conducted in both batch and continuous systems. The removal efficiency of the nutrients was evaluated in the batch system using the varying concentrations of zeolite and iron oxide added. The removal efficiency of N was 60% at the 8g of zeolite added. In the same condition, the removal efficiencies of N were 76% and 82% at 12g and 16g of zeolite added, respectively. Removal efficiency of P was 80% as 8g of iron oxide was added. The removal efficiency of P was correspondingly increased as the concentration of iron oxide was increased. Continuous column system was also used to evaluate the removal efficiency of N and P by the addition of zeolite and ferric oxide, respectively. Removal efficiencies of N were compared in the mixed packing, two stage, and four stage columns, respectively. The removal efficiencies (80%) of N in the separate packed columns (two and four stages) were higher than the mixed packing column (400%) after 90 hr. Whereas, the removal efficiencies of P were similar to each other in the three columns.

천연(天然)Zeolite의 CEC 증가(增加)와 입단화(粒團化)에 관(關)한 연구(硏究) -2. 반응(反應) 온도(溫度)와 반응(反應) 시간(時間)의 영향(影響) (The Study on the CEC Increase and Granulation of Natural Zeolite -2. Effects of Temperature and Time on the Recrystallization of Natural Zeolite)

  • 최정;허남호;이동훈
    • 한국토양비료학회지
    • /
    • 제26권3호
    • /
    • pp.151-154
    • /
    • 1993
  • CEC가 67me/100g되는 천연(天然)zeolite 미분(微粉)을 3N-NaOH용액(溶液)에서 $80^{\circ}C$로 30시간(時間) 처리(處理)한 결과(結果), 반응생성물(反應生成物)의 CEC는 약 260me/100g으로 증가(增加)하였으며 서로 다른 반응조건(反應條件) 하(下)의 반응(反應) 생성물(生成物)중 가장 높았다. NaOH용액(溶液)을 처리(處理)하여 생성(生成)된 반응생성물(反應生成物)에는 천연(天然) zeolite에 함유(含有)되었던 clinoptilolite, mordenite 및 smectite의 함량(含量)은 감소(減少)하였으나 phillipsite로 새롭게 나타났다. 반응온도(反應溫度)와 반응시간(反應時間)이 증가(增加)할수록 phillipsite의 함량(含量)이 증가(增加)하였다. 30시간반응(時間反應) 후(後)에는 phillipsite가 주(主)된 점토광물(粘土鑛物)로 나타났다.

  • PDF

실란 결합제 처리된 에폭시 수지 복합재료의 계면 특성 (Interface Characteristics of Epoxy Composite Treated with Silane Coupling Agent)

  • 이재영;이홍기;심미자;김상욱
    • 한국재료학회지
    • /
    • 제11권12호
    • /
    • pp.1009-1013
    • /
    • 2001
  • The effects of coupling agent on the interface characteristics between epoxy resin and natural zeolite were studied by SEM, optical microscope and universal testing machine (UTM). Epoxy resin as a matrix was diglycidyl ether of bisphenol A (DGEBA)/4,4'-methylene dianiline (MDA)/malononitrile (MN) system and natural zeolite as an inorganic fillet was produced in Korea. With the increment of zeolite content, tensile strength decreased and it was due to the different elastic moduli of two materials. When external stress was loaded on the composites, the stress concentrated on the weakly bonded interface and crack grew easily. To improve the interface characteristics, the surface of the natural zeolite was treated with the silane coupling agent and it was found that the tensile strength was increased. The morphology of the interface showed that the bonding characteristics were modified by coupling agent.

  • PDF

Montmorillonite가 섞인 천연 제올라이트를 이용한 중금속 이온의 제거 (Removal of Heavy Metal Ions by Using Natural Zeolite Comixed with Montmorillonite)

  • 문정호;김윤호;김영만;김천한;곽현태
    • 분석과학
    • /
    • 제13권3호
    • /
    • pp.394-398
    • /
    • 2000
  • The mineralogical properties of natural zeolite comixed with montmorillonite were investigated by the chemical composition analysis, X-ray diffraction analysis, and differential scanning calorimetry. The experimental results on the removal of heavy metal ions by using the natural sample are summerized as follows. The removal of the heavy metal in solution is greatly influenced by the pH. Also, the removal capacity of heavy metal ions by zeolite and montmorillonite have increased in order of $Cu^{2+}>Cd^{2+}>Ni^{2+}$.

  • PDF