• Title/Summary/Keyword: Nano-hardness

Search Result 427, Processing Time 0.027 seconds

Strength Evaluation of Aluminum Alloy Bolt by Nano-Indentation Hardness Test

  • KUBOTA Yoshihiro;NAKAMURA Tamotsu;KOBAYASHI Mitsuo;FUKUDA Katsumi
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2003.10b
    • /
    • pp.123-126
    • /
    • 2003
  • A high strength aluminum alloy bolt (A7050, T7 temper treatment) has been developed by the authors. The bolt has a small grain size in the whole area of the bolt because of the large equivalent strain followed by thermo-mechanical treatment. As the bolt made of A 7050 has a risk of stress corrosion cracking, each grain should be strengthened the grain inside than the grain boundary in order to improve the stress corrosion cracking resistance. It has been confirmed that the nano-indentation hardness at each grain inside increased with the increasing equivalent strain by thermo-mechanical treatment processing.

  • PDF

Bonding structure of the DLC films deposited by RE-PECVD (RE-PECVD법에 의해 증착된 DLC박막의 결합 특성)

  • 최봉근;신재혁;안종일;심광보
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.14 no.1
    • /
    • pp.27-32
    • /
    • 2004
  • The diamond-like carbon (DLC) films were deposited on the Si (100) wafer by a rf-PECVD method as a function of the mixture rate of methane-hydrogen gas and bias voltage. The bonding structure and mechanical properties of these deposited DLC films were investigated using FT-IR, Raman, and nano-indenter. The deposition rates of DLC films increased with increased flow rate of methane in the gas mixtures and increased bias voltage. The $sp^3/sp^2$ bonding ratio of carbon in thin film and the hardness increased with increasing flow rate of hydrogen in the gas mixtures and increasing bias voltage.

Microstructure and Nano-hardness of SiC/C Multi-coated Layers on a Particulate Nuclear Fuel (입자 핵연료의 SiC/C 다층 도포층의 미세조직 및 극미세 경도 평가)

  • Choi, Young
    • Journal of the Korean institute of surface engineering
    • /
    • v.52 no.6
    • /
    • pp.321-325
    • /
    • 2019
  • Triso-type coating layers of silicon carbide and graphite on UO2 paticulate nuclear fuel were prepared by using fluidized bed type chemical vapor deposition and self-propagating high temperature synthesis methods to make a coated nuclear fuel of a power plant for hydrogen mass-production. The source and carrier gases were the mixture of methyltrichlorosilane and propane, and inert argon. Chemical analysis and microstructure observation showed that the coated layers were inner graphite, middle silicon carbide and outer graphite. The elastic modulus and nano-hardness of the silicon carbide layer were 503 [GPa] and 36 [GPa], respectively.

Characteristic Properties of TiN Thin Films Prepared by DC Magnetron Sputtering Method for Hard Coatings (Hard Coating 응용을 위한 DC 마그네트론 스퍼터링 방법을 이용하여 증착한 TiN 박막의 특성에 대한 연구)

  • Kim, Young-Ryeol;Park, Yong-Seob;Choi, Won-Seok;Hong, Byung-You
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.7
    • /
    • pp.660-664
    • /
    • 2008
  • Titanium nitride (TiN) thin films are widely used for hard coatings due to their superior hardness, chemical stability, low friction and good adhesion properties. In this study, we investigated the effect of DC power on the characteristics of TiN thin films deposited on Si and glass substrates by DC magnetron sputtering using TiN target. We made TiN films of 300 nm thickness with various DC powers. The structural properties of films are investigated by x-ray diffractions (XRD) and tribological properties are measured by nano-indentation, nano-scratch tester. The rms roughness was measured by atomic forced microscopy (AFM). In the result, TiN films had the smooth surface and exhibited (111) directions with the increase of DC Power. Also, especially in case of 175 W DC power, TiN film exhibited the maximum hardness about 8 GPa, and the critical load near 25.

Intermetallic Compounds Behavior at Laser Overlay Interface of Aluminum and Fe-based Powder (Al-Fe 레이저 오버레이층 경계면에서의 금속간화합물 거동)

  • Kang, Nam-Hyun;Yoo, Yeon-Gon;Lee, Chang-Woo;Kim, Jeong-Han
    • Journal of Welding and Joining
    • /
    • v.25 no.3
    • /
    • pp.51-56
    • /
    • 2007
  • A $CO_2$ laser overlay was conducted by using a Fe-based powder on the AC2B aluminum substrate. Cracks and intermetallic compounds (IMC) were observed inconsistently along the interface between the overlay and post-molten layer. A scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS) detected some Fe-rich IMC ($Fe_3Al$, FeAl) as well as the brittle Al-rich IMC ($Fe_2Al_5,\;FeAl_3$). Micro vickers hardness proved the formation of Al-rich IMC ($FeAl_3$) along the interface by showing HV0.1 $800{\sim}900$. Furthermore, nano indentation was successfully applied to investigate the behavior of IMC more precisely than the micro vickers hardness.

Effect of Si on Mechanical and Anti-oxidation Properties of Ti-Si-N Coating (Si가 Ti-Si-N 코팅막의 기계적 성밀 및 내산화특성에 미치는 영향)

  • 박범희;김정애;이종영;김광호
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.1
    • /
    • pp.96-101
    • /
    • 2000
  • Comparative studies on microstructure, and mechanical and anti-oxidation properties between TiN and Ti-Si-N films were performed. The Ti-Si-N films were deposited on high-speed steel and silicon wafer substrates by plasma-assisted chemcial vapor deposition(PACVD) technique. The Si addition to TiN film caused to change the microstructure such as grain size refinement, randomly multi-oriented microstructure, and nano-sized codeposition of silicon nitride in the TiN matrix. The Ti-Si-N film, contains Si content of ∼7 at.%, showed the micro-hardness value of ∼3400 HK, which was higher than the pure TiN film whose hardness was ∼1500HK. The Ti-Si(7 at.%)-N film also showed much improved anti-oxidation properties compared with those of the pure TiN film. These properties were also related to the microstructure of Ti-Si(7 at.%)-N film was formed and retarded further oxidation of the nitridelayer. These properties were also related to the microstructure of Ti-Si(7 at.%)-N film which was characterized by nano-sized precipitates of silicon nitride phase in the TiN matrix and randomly oriented grains.

  • PDF

Consolidation of Segment Powder for Diamond Tool by Magnetic Pulsed Compaction (자기펄스 압축성형법에 의한 다이아몬드 공구용 세그먼트 분말 성형)

  • Yun, J.S.;Lee, J.G.;Lee, M.K.;Rhee, C.K.;Park, M.S.;Hong, S.J.
    • Journal of Powder Materials
    • /
    • v.15 no.5
    • /
    • pp.378-385
    • /
    • 2008
  • This article presents the successful consolidation of the mixed Co and Diamond powders for a drilling segment by the combined application of magnetic pulsed compaction (MPC) and subsequent sintering, and their properties were analyzed. Homogeneous hardness (Hv 220) and density (97%) of sintered bulks fabricated by MPC were obtained by the new technique, where higher pressure has been employed for short period of time than that of general process. A fine microstructure and homogeneous hardness in the consolidated bulk were observed without cracks. Relatively higher drilling speed of 9.61 cm/min and life time of 6.55 m were found to the MPCed specimens, whereas the value of the specimens fabricated by general process was 11.71 cm/min and 7.96 m, respectively. A substantial improvement of mechanical properties of segment was achieved through this study.

Influence of Substrate on Mechanical Characteristics of ZnO Thin Film by NI Technology (NI법에 의한 기계적 특성에 미치는 ZnO박막의 기판재의 영향)

  • Jung Hun-Cbae;KIM Dong-Hyun;Yoon Han-Ki;Lim Hee-Sup;Yu Yun-Sik
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2004.05a
    • /
    • pp.342-346
    • /
    • 2004
  • Recently there has been a great world-wide interest in developing and characterizing new nano-structured materials. These newly developed materials are often prepared in limited quantities and shapes unsuitable for the extensive mechanical testing. The development of depth sensing indentation methods have introduced the advantage of load and depth measurement during the indentation cycle. In the present work, ZnO thin films are prepared on the Glass, GaAs(100), Si(111), and Si(100) substrates at different temperatures by pulsed laser deposition(PLD) method. Because the potential energy in c-axis is law, the films always shaw c-axis orientation at the optimized conditions in spite of the different substrates. Thin films are investigated by X-ray diffractometer and Nano indentation equipment. From these measurements it is possible to get elastic modulus and hardness of ZnO thin films on all substrates.

  • PDF

The Influence of Annealing Temperature on Mechanical Properties and Friction Coefficient of Coating Layer in Galvannealed Sheet Steel (용융아연도금강판에서 어닐링 온도변화에 따른 화합물화가 도금층 기계적 특성 및 마찰계수에 미치는 영향)

  • Jeon J.S.;Lee J. M.;;Kim D. J.;Kang Y.S.;Kim B. M.
    • Transactions of Materials Processing
    • /
    • v.14 no.8 s.80
    • /
    • pp.696-703
    • /
    • 2005
  • In the modern days, a galvannealed sheet steel (GA) instead of a cold rolled steel sheet has been widely used as an alternative to extend the life of automotive body. Accordingly, the mechanical properties of GA for automobiles were taken into account and studied by examining their variation with annealing temperature. To clarify the effect of surface features on the mechanical and frictional properties of GA, the several tests such as nanoindentation, Vickers hardness and nano scratch test were executed. The frictional characteristics of coating layers of GA were examined through nano scratch test in this study. The friction coefficient of coating layers on the surface was obtained from the nano scratch. The variation of friction coefficient versus velocity and pressure was taken into consideration in this paper. Hardness and elastic modulus of coating layer were increased as increasing annealing temperature.

Investigation on Age-hardening characteristic of thixo and rheocast by using Nano/Micro-probe Technology (나노/마이크로 프로브 기술을 통한 틱소/레오 캐스트의 시효경화 특성 조사)

  • Cho, S.H.;Lee, C.S.;Kang, C.G.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2006.05a
    • /
    • pp.322-325
    • /
    • 2006
  • The nano/microstructure and mechanical properties of the eutectic regions in thixo and rheo cast A356 alloy parts were investigated using nano/micro-indentation and mechanical scratching, combined with optical microscopy and atomic force microscope (AFM).Most eutectic Si crystals in the A356 alloy showed a modified morphology as fine-fibers, however Si particles of network in eutectic region was formed quickly with aging time increase in thixo-cast. The aging responses of the eutectic regions in both the thixo and rheo cast A356 alloys aged at $150^{\circ}C$ for different times (0, 2, 4, 8, 10, 16, 24, 36, and 72 h) were investigated. Both Vickers hardness ($H_V$) and indentation ($H_{IT}$) test results showed almost the same trend of aging curves, the peak was obtained at the same aging time of 10 h.

  • PDF