• Title/Summary/Keyword: Morphotropic phase boundary (MPB)

Search Result 44, Processing Time 0.174 seconds

The Effect of Mechanical Stress and Electric Field on the Morphotropic Tetragonal and Rhombohedr Phase Boundary in PZT System : Thermodynamic Consideration (PZT계의 정방정상과 능면체정상의 경계조성에 대한 기계적 응력과 전기장의 영향 : 열역학적 고찰)

  • 천채일;김호기
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.10
    • /
    • pp.859-865
    • /
    • 1993
  • Morphotropic tetragonal and rhombohederal phase boundary(MPB) in PZT system was calculated and the effect of mechanical stress and electric field on the MPB was examined using phenomenological thermodynamic theory proposed by Devonshire. Mechanical stress and electric field was calculated to change free energies of phases and shift MPB. The stable composition range of the phase, of which spontaneous strain and spontaneous polarization aligned to the direction of tensile stress or electirc field, was expanded.

  • PDF

Effects of Thermal Annealing on Dielectric and Piezoelectric Properties of Pb(Zn, Mg)1/3Nb2/3O3-PbTiO3 System in the Vicinity of Morphotropic Phase Boundary

  • Hyun M. Jang;Lee, Kyu-Mann
    • The Korean Journal of Ceramics
    • /
    • v.1 no.1
    • /
    • pp.13-20
    • /
    • 1995
  • Effects of thermal annealing on the dielectric/piezoelectric properties of $Pb(Zn, Mg)_{1/3}Nb_{2/3}O_3-PbTiO_3$ ceramics (PZMNPT) with Zn/Mg=6/4) were examined across the rhombohedral/tetragonal morphotropic phase boundary (MPB). Both the relative dielectric permittivity ($\varepsilon$r)and the piezoelectric constant($d_33$)/electromechanical coupling constant ($k_p$)were increased by thermal annealing ($800^{\circ}$~$900^{\circ}C$) after sintering at $1150^{\circ}C$ for 1 hr. Based on the dielectric analysis using the series mixing model and the concept of a random distribution of the local Curie points, the observed improvements in the dielectric and piezoelectric properties of PZMN-PT were interpreted in terms of the elimination of PbO-rich amorphous intergranular layers(~1nm) induced by thermal annealing. A concrete evidence of the presence of amorphous grain-boundary layers in the unannealed (as-sintered) specimen was obtained by examining the structure of intergranular region using a TEM.

  • PDF

Perspective on Ferroelectric Polymers Presenting Negative Longitudinal Piezoelectric Coefficient and Morphotropic Phase Boundary (강유전체 고분자의 음의 압전 물성 및 상공존경계(MPB)에 대한 고찰)

  • Im, Sungbin;Bu, Sang Don;Jeong, Chang Kyu
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.35 no.6
    • /
    • pp.523-546
    • /
    • 2022
  • Morphotropic phase boundary (MPB), which is a special boundary that separates two or multiple different phases in the phase diagram of some ferroelectric ceramics, is an important concept in identifying physics that includes piezoelectric responses. MPB, which had not been discovered in organic materials until recently, was discovered in poly(vinylidene fluoride-co-trifluoroethylene (P(VDF-TrFE)), resulting from a molecular approach. The piezoelectric coefficient of P(VDF-TrFE) in this MPB region was achieved up to -63.5 pC N-1, which is about two times as large as the conventional value of -30 pC N-1 of P(VDF-TrFE). An order-disorder arrangement greatly affects the rise of the piezoelectric effect and the ferroelectric, paraelectric and relaxor ferroelectric of P(VDF-TrFE), so the arrangement and shape of the polymer chain is important. In this review, we investigate the origin of negative longitudinal piezoelectric coefficients of piezoelectric polymers, which is definitely opposite to those of common piezoelectric ceramics. In addition to the mainly discussed issue about MPB behaviors of ferroelectric polymers, we also introduce the consideration about polymer chirality resulting in relaxor ferroelectric properties. When the physics of ferroelectric polymers is unveiled, we can improve the piezoelectric and pyroelectric properties of ferroelectric polymers and contribute to the development of next-generation sensor, energy, transducer and actuator applications.

Structural and piezoelectric properties of lead-free (1-x)$(Na_{0.5}\;K_{0.5})NbO_3$-xBa($Ti_{0.9}$, $Sn_{0.1}$)$O_3$ ceramics

  • Cha, Yu-Jeong;Nam, San;Kim, Chang-Il;Jeong, Yeong-Hun;Lee, Yeong-Jin;Baek, Jong-Hu
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2009.05a
    • /
    • pp.33.1-33.1
    • /
    • 2009
  • Lead-free (1-x)$(Na_{0.5}K_{0.5})NbO_3$-xBa($Ti_{0.9}Sn_{0.1})O_3$ [NKN-BTS-100x] ceramics doped with 1 mol% $MnO_2$ have been prepared by the conventional solid state method and their structural and piezoelectric properties were investigated. The NKN-BTS-100x ceramics exhibited a dense and homogeneous microstructure when they were sintered at $1030-1150^{\circ}C$. Grain growth was observed for the specimen sintered at relatively low temperature of $1050^{\circ}C$. A tetragonal/orthorhombic morphotropic phase boundary (MPB) in the perovskite structure was also appeared for the NKN-BTS-100x ceramics (0.04$1050^{\circ}C$. The enhanced piezoelectric properties in the NKN-BTS ceramics with a MPB composition were obtained. Especially, for the NKN-BTS-6 ceramics, a high dielectric constant (${\varepsilon}^T_3/\varepsilon_0=1,400$), piezoelectric constant ($d_{33}=237$) and electromechanical coupling factor ($k_p=0.42$) were obtained.

  • PDF

Ferroelectric Phase Transition Behavior in $(Na_{1/2}Bi_{1/2})TiO_3-PbTiO_3$ System ($(Na_{1/2}Bi_{1/2})TiO_3-PbTiO_3$ 고용체의 강유전 상전이 거동)

  • 홍국선;조서용;박승익
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.8
    • /
    • pp.915-921
    • /
    • 1995
  • The morphotropic phase boundary and phase transitions of the solid solutiion system, (1-x)(Na1/2Bi1/2)TiO3-PbTiO3+xPbTiO3 were studied by investigating changes in crystal structure, variations in permittivity with temperature, and calorimetric behavior. It was observed that the morphotropic phase boundary (MPB) of this solid solutiion system was at near 14 mol% of PbTiO3. Compositions containing less than 10mol% PbTiO3 (x<0.1) exhibited a phase transition, i.e. ferroelectric rhombohedrallongrightarrowparaelectric paraelectric cubic, with increasing temperature. Composition containing more than 14 mol% PbTiO3 (x 0.14) showed a phase transition from ferroelectric tetragonal to paraelectric cubic. In the composition range of 0.1$\varepsilon$ (T) curve, which coincided with a phase transition from ferroelectric rhombohedral to an intermediate phase, was also found.

  • PDF

Phase Transition Behavior and Dielectric Properties of Morphotropic Phase Boundary in (1-x)Pb(Yb1/2Nb1/2)O3-xPbTiO3 (0.40 ≤ x ≤ 0.60) Solid Solutions ((1-x)Pb(Yb1/2Nb1/2)O3-xPbTiO3 (0.40 ≤ x ≤ 0.60) 고용계에서의 PbTiO3 치환에 따른 상전이 영역의 상전이 거동과 유전특성)

  • Kim, Jung-Hyun
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.3
    • /
    • pp.253-259
    • /
    • 2012
  • In this study, crystal structural changes and dielectric properties of $(1-x)Pb(Yb_{1/2}Nb_{1/2})O_3-xPbTiO_3$ ((1-x)PYN-xPT) solid solutions were measured and analyzed with respect to the $PbTiO_3$ (PT) contents ($0.40{\leq}x{\leq}0.60$). From X-ray diffraction (XRD) measurements, (1-x)PYN-xPT solid solutions showed changes of the crystal structure from pseudocubic ($0.40{\leq}x{\leq}0.44$) to tetragonal ($0.52{\leq}x{\leq}0.60$) on increasing PT contents and exhibited the coexistence of pseudocubic and tetragonal phase near the morphotropic phase boundary (MPB) composition ($0.46{\leq}x{\leq}0.50$). The dielectric constant showed a maximum value at x = 0.46 and the maximum values in (1-x)PYN-xPT decreased with higher PT contents. The phase transition temperatures of (1-x)PYN-xPT solid solutions increased over the whole composition ranges tested ($0.40{\leq}x{\leq}0.60$).

Electrical Properties and Temperature Stability of resonant Frequency with Zr/Ti ratio in PSN-PMN-PZT Ceramics (PSN-PMN-PZT 세라믹스의 Zr/Ti 비에 따른 전기적 특성과 공진주파수의 온도안정성)

  • 류주현;윤광희;민석규;이명수;서성재
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.13 no.8
    • /
    • pp.675-680
    • /
    • 2000
  • In this study the temperature coefficient of resonant frequency(TC $F_{r}$) dielectric and piezoelectric properties of Pb[(S $b_{1}$2//N $b_{1}$2/)$_{0.065}$)-(Z $r_{x}$, $Ti_{1-x}$ )$_{0.90}$] $O_3$ceramics were investigated with Zr/Ti ratio. The compositions near the morphotropic phase boundary (MPB) appeared when Zr/Ti ratio was 49.5/50.5 The dielectric constant and electromechanical coupling factor( $k_{p}$) also showed the highest values of 1,257, 0.653 respectively when the Zr/Ti ratio was 49.5/50.5 Moreover the mechanical quality factor( $Q_{m}$) showed th lowest value of 713 when the Zr/Ti ratio. The temperature coefficient of resonant frequency(TC $F_{r}$) abruptly change at the morphotropic phase boundary(MPB) which existed between the rhombohedral phase with highly negative TC $F_{r}$ of -106ppm/$^{\circ}C$ and the tetragonal phase with highly positive TC $F_{r}$ of +64pp $m^{\circ}C$ as Zr/Ti ratio varied from 50/50 to 49.5/50.5.50.5..50.5.

  • PDF

Comparisons on Dielectric and Peizoelectric Proeprties of Rhombohedral, Tetragonal and Morphotropic Phase Boundary in Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3 System with MnO2 Addition (Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3계의 삼방정, 정방정 및 상경계조성에서의 MnO2 첨가에 따른 유전 및 압전특성에 비교)

  • 전구락;손정호;김정주;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.25 no.5
    • /
    • pp.488-494
    • /
    • 1988
  • Effects of MnO2 addition on themicrostructure, dielectric and piezoelectric properties of Rhombohedral, Tetragonal and Morphotropic phase boundary(MPB) in Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3 system were investigated and respectively the amount of MnO2 addition was 0, 0.2, 0.5, 1.0, 3.0wt%. In the tetragonal region, compared with the Rhombohedral and Morpotropic phase boundary, Mechanical quality factor(Qm), Curie temperature(Tc) and Dissipation factor were promoted by addition of MnO2. According to the results of the microstructure, dielectric and piezoelectric properties, the solid solution range of MnO2 addition in this system was 0.2-0.5wt%.

  • PDF

Field-Induced Strains and Polarization Switching Mechanisms in La-Modified $Pb(Sc_{1/2}Nb_{1/2})O_3-PbTiO_3$ Ceramics (La 변성 $Pb(Sc_{1/2}Nb_{1/2})O_3-PbTiO_3$계 요업체의 전계유기변위와 분극특성)

  • 장명철
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.1
    • /
    • pp.63-69
    • /
    • 2000
  • Electrically-induced strain(S) and polarization(P) for Pb(Sc1/2Nb1/2)O3-PbTiO3(1-x)PSN-xPT) crystalline solutions were studied. From the compositional dependence of S and P we could observe two maximum values at x=0.10 and x=0.425. It is considered that PSNT10(x=0.10) composition is the structural phase boundary to indicate the variable order-disorder[VOD] region. PSNT(x=0.425) composition is the morphotropic phase boundary[MPB] to indicate the rhombohedral to tetragonal phase transition. Higher S (0.437%) and P (0.3974$\mu$C/$\textrm{cm}^2$) values were attained by the La substitution (5 wt%) at Pb site in the MPB composition of 57.5PSN-42.5PT.

  • PDF

Dielectric and Piezoelectric Properties of Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3 Solid Solution Ceramics (Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3계의 유전 및 압전특성)

  • 손정호;남효덕;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.25 no.5
    • /
    • pp.523-531
    • /
    • 1988
  • The dielectric and piezoelectric properties with compositions in Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3-(PNN-PT-PZ)solid solution ceramics were investigated. In this study, the compsition ranges were 30 PNN 45mole%, 20 PT 50mole% and 50 PZ5mole%. As PT fraction were increased the grain size was increased and the fired density was decreased, but the changes of PNN fraction had no effect on the grain size. The Curie temperature was increased when PT and PNN fraction were increased. The displacement was increased but had a great hysteresis loss when PT fraction was increased. In morphotropic phase boundary, the maximum piezoelectric and electromechanical coupling factor were indicated. Morphotropic phase boundary(MPB) was 34 PT 36mole% in chang of compositions.

  • PDF