A study on the fracture strength of collarless metal-ceramic fixed partial dentures

  • Yoon, Jong-Wook;Kim, Sung-Hun;Lee, Jai-Bong;Han, Jung-Suk;Yang, Jae-Ho
    • The Journal of Advanced Prosthodontics
    • /
    • v.2 no.4
    • /
    • pp.134-141
    • /
    • 2010
  • PURPOSE. The objective of this study was to evaluate fracture strength of collarless metal-ceramic FPDs according to their metal coping designs. MATERIALS AND METHODS. Four different facial margin design groups were investigated. Group A was a coping with a thin facial metal collar, group B was a collarless coping with its facial metal to the shoulder, group C was a collarless coping with its facial metal 1 mm short of the shoulder, and group D was a collarless coping with its facial metal 2 mm short of the shoulder. Fifteen 3-unit collarless metal-ceramic FPDs were fabricated in each group. Finished FPDs were cemented to PBT (Polybutylene terephthalate) dies with resin cement. The fracture strength test was carried out using universal testing machine (Instron 4465, Instron Co., Norwood MA, USA) at a cross head speed of 0.5 mm/min. Aluminum foil folded to about 1 mm of thickness was inserted between the plunger tip and the incisal edge of the pontic. Vertical load was applied until catastrophic porcelain fracture occurred. RESULTS. The greater the bulk of unsupported facial shoulder porcelain was, the lower the fracture strength became. However, there were no significant differences between experimental groups (P > .05). CONCLUSION. All groups of collarless metal-ceramic FPDs had higher fracture strength than maximum incisive biting force. Modified collarless metal-ceramic FPD can be an alternative to all-ceramic FPDs in clinical situations.

A Study on the Fracture Strength of All-Ceramic Crown according to the Zirconia Coping Design using CAD/CAM System (CAD/CAM을 이용하여 제작한 전부도재관의 지르코니아 코핑 디자인에 따른 파절강도에 관한 연구)

  • Bulgan, L.;Cho, In-Ho;Shin, Soo-Yeon
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.22 no.2
    • /
    • pp.111-123
    • /
    • 2006
  • A Study on the Fracture Strength of All-Ceramic Crown according to the Zirconia Coping Design using CAD/CAM System L. Bulgan, In-Ho Cho, Soo-Yeon Shin Department of Prosthodontics, Graduate School, Dankook University The fracture strength of prosthesis is important, because it affects the function, and long term success of prosthesis and teeth. The purpose of this study was to compare the fracture strength of zirconia coping designs. Experimental test group were classified into three designs according to coping design, Modified design: Zirconia coping margin was located at 1mm above the axiogingival line angle. Collarless design: The coping margin terminated at the axiogingival line angle Butt design: The coping margin was extended to the finishing line of prepared margin. A $Cercon^{(R)}$(Degussa, Germany) CAD/CAM system was used to make the zirconia coping. Fracture strength was measured using loading machine at a cross head speed of 1mm/min. The results were statistically analyzed using the one-way ANOVA and multiple comparison test. Statistical significance was set in advance at the probability level of less than 0.05. The result : I. Collarless($738N{\pm}155N$) and Modified($755N{\pm}185N$) groups showed significantly a lower fracture strength than Butt($1057N{\pm}262N$) group(p<0.05). II. There were no statistical differences of the fracture strength between Modified($755N{\pm}185N$) and Collarless($738N{\pm}155N$) groups. III. When comparing the fractured surface, all the group showed porcelain fracture, which were fractured at the labial surface of baked porcelain The butt design of the zirconia coping has higher fracture strength than modified and collarless design.

A STUDY ON THE MARGINAL FIT OF COLLARLESS METAL CERAMIC FIXED PARTIAL DENTURES

  • Yoon Jong-Wook;Yang Jae-Ho;Han Jung-Seok;Lee Jae-Bong
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.43 no.6
    • /
    • pp.707-716
    • /
    • 2005
  • Statement of problem. Collarless metal ceramic fixed partial dentures(FPDs) had an esthetic problem such as opaque reflection in cervical region. To overcome this, modified coping which removed its facial cervical metal could be used. The marginal quality could be worsen according to the amount of its facial metal reduction. Purpose. The purpose of this study was to evaluate marginal fits of collarless metal ceramic FPDs with retainers of modified copings. Material and method. Dentoform maxillary left central incisor and right lateral incisor were prepared for 3-unit collarless metal ceramic FPD and fixed in yellow stone. This model was duplicated to PBT resin dies via CAD/CAM and injection molding. Four different facial margin design groups were investigated. Group A was a coping with a thin facial metal collar, group B was a collarless coping with its facial metal to the shoulder, group C was a collarless coping with its facial metal 1 mm short of the shoulder, and group D was a collarless coping with its facial metal 2 mm short of the shoulder. Seven collarless metal ceramic FPDs per group were fabricated. They were cemented to PBT resin dies with resin cement. After removal of pontics, each retainers were separated and observed under Accura 2000 optical microscope. Then, retainers were embeded in orthodontic resin and cross sectioned faciopalatally. Internal marginal fits of midfacial porcelain margins were observed under FE-SEM. Result and conclusion. Within the limitations of this in vitro study. The following conclusions were drawn. 1. Mean marginal gaps of collarless FPDs were in the $50-60{\mu}m$ range. 2. In midfacial margin, marginal discrepancies were greater in group A than in the experimental groups(p<0.05). 3. In midpalatal margin, marginal gaps were greater in group C and D than in group A and B(p<0.05). 4. Marginal fits of porcelain margins were better than those of metal margins in collarless metal ceramic FPDs. 5. In both teeth, internal marginal gaps of group C and D were greater than those of group A and B(p<0.05).

A STUDY ON FRACTURE STRENGTH AND COLOR BY THE DESIGN OF METAL COPING IN CERAMO METAL CROWN (내부금속관 형태에 따른 도재전장금관의 파절강도와 도재색조에 관한 연구)

  • Lee Myung-Ho;Jeon Young-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.30 no.1
    • /
    • pp.103-124
    • /
    • 1992
  • The purpose of this study was to investigate the effect on the fracture strength and color of ceramic by the design of the metal coping in ceramo metal crown. In this study, four types of ceramic crowns were made for fracture strength : standard ceramo metal crown, collariess ceramo metal crown, modified ceramo metal crown, and ceramic jacket crown. And three types of disk formed-specimens were made to compare the dentin shade owing to aluminous opaque powder and palladium alloy. Fracture strength was measured by universal testing machine(Instron Co. Ltd., U.S.A) and color was measured by color and color difference meter(Yasuda Seiki Seisakusho, Ltd., Japan). The results were as follows : 1. The fracture strength of ceramic was affected significantly by the design of metal coping in ceramo metal crown. The mean fracture strength(192.0 Kg) of standard ceramo metal crown was about 1.7 times higher than that(111.5 Kg) of collarless ceramo metal crown, and about 2.8 times higher than that(67.8 Kg) of ceramic jacket crown. 2. Modified ceramo metal crown that has metal band in the labio cervical had the lowest fracture strength. 3. Lightness, yellowness and redness of the dentin fired were decreased by the metal coping.