• 제목/요약/키워드: Microstructural Analysis

검색결과 523건 처리시간 0.026초

알루미늄과 탄소 함량에 따른 Fe-23Mn계 고망간강의 열간 압연 시 발생하는 균열 현상 분석 (Analysis of Cracking Phenomenon Occurring During Hot Rolling of Fe-23Mn High-manganese Steels with Different Aluminium and Carbon Contents)

  • 임현석;이승완;황병철
    • 열처리공학회지
    • /
    • 제29권4호
    • /
    • pp.176-180
    • /
    • 2016
  • In this study, a microstructural investigation was conducted on the cracking phenonmenon occurring during hot rolling of Fe-23Mn high-manganese steels with different aluminium and carbon contents. Particular emphasis was placed on the phase stability of austenite and ferrite dependent on the chemical composition. An increase in the aluminum content promoted the formation of ferrite band structures which were easily deformed or cracked. In the steels containing high carbon contents of 0.4 wt.% or higher, on the other hand, the volume fraction and thickness of ferrite bands decreased and thus the cracking frequency was significantly reduced. Based on these findings, it is said that the microstructural evolution occurring during hot rolling of high-manganese steels with different aluminium and carbon contents plays an important role in the cracking phenomenon. To prevent the cracking, therefore, the formation of second phases such as ferrite should be minimized during the hot rolling by the appropriate control of the chemical composition and process parameters

Fabrication of FeCuNi alloy by mechanical alloying followed by consolidation using high-pressure torsion

  • Asghari-Rad, Peyman;Kim, Yongju;Nguyen, Nhung Thi-Cam;Kim, Hyoung Seop
    • 한국분말재료학회지
    • /
    • 제27권1호
    • /
    • pp.1-7
    • /
    • 2020
  • In this research, a new medium-entropy alloy with an equiatomic composition of FeCuNi was designed using a phase diagram (CALPHAD) technique. The FeCuNi MEA was produced from pure iron, copper, and nickel powders through mechanical alloying. The alloy powders were consolidated via a high-pressure torsion process to obtain a rigid bulk specimen. Subsequently, annealing treatment at different conditions was conducted on the four turn HPT-processed specimen. The microstructural analysis indicates that an ultrafine-grained microstructure is achieved after post-HPT annealing, and microstructural evolutions at various stages of processing were consistent with the thermodynamic calculations. The results indicate that the post-HPT-annealed microstructure consists of a dual-phase structure with two FCC phases: one rich in Cu and the other rich in Fe and Ni. The kernel average misorientation value decreases with the increase in the annealing time and temperature, indicating the recovery of HPT-induced dislocations.

$WO_3$가 첨가된 ZNO 바리스터의 미세구조적, 전기적 특성 (A Microstructural and Electrical Properties of $WO_3$-Doped ZnO Varistors)

  • 정순철;박춘현;남춘우
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1998년도 추계학술대회 논문집
    • /
    • pp.275-279
    • /
    • 1998
  • The influence of $WO_3$ (0.5-4.0mol%) on the microstructural and electrical properties of ZnO varistors was investigated. The major part of a tungsten segregated to the nodal point. SEM, EDAX, and XRD analysis revealed that three phase, such as W-rich phase, Bi-rich phase, and spinel phase, coexist at the nodal point. The average grain size increased in the range of 15.5-29.9pm with increasing $WO_3$ content. This may be probably attributed to liquid phase formed by $WO_3$, $WO_3$ acted as promotion additive of grain growth. As $WO_3$ content increase, the varistor voltage greatly decreased in the range 186.82-35.87V/mm due to the increase of grain growth. The barrier height decreased in the range 1.93-0.42eV with increasing $WO_3$content.

  • PDF

Wood Identification of Historical Architecture in Korea by Synchrotron X-ray Microtomography-Based Three-Dimensional Microstructural Imaging

  • HWANG, Sung-Wook;TAZURU, Suyako;SUGIYAMA, Junji
    • Journal of the Korean Wood Science and Technology
    • /
    • 제48권3호
    • /
    • pp.283-290
    • /
    • 2020
  • For visual inspection-based wood identification, optical microscopy techniques typically require a relatively large sample size, and a scanning electron microscope requires a clean surface. These novel techniques experience limitations for objects with highly limited sampling capabilities such as important and registered wooden cultural properties. Synchrotron X-ray microtomography (SR-µCT) has been suggested as an effective alternative to avoid such limitations and various other imaging issues. In this study, four pieces of wood fragments from wooden members used in the Manseru pavilion of Bongjeongsa temple in Andong, Korea, wereused for identification. Three-dimensional microstructural images were reconstructed from these small wood samples using SR-µCT at SPring-8. From the analysis of the reconstructed images, the samples were identified as Zelkova serrata, Quercus sect. Cerris, and Pinus koraiensis. The images displayed sufficient spatial resolution to clearly observe the anatomical features of each species. In addition, the three-dimensional imaging allowed unlimited image processing.

$ZrO_2$를 이차상으로한 복합체의 기계적 특성 (A Study on the Mechanical Properties of $ZrO_2$ Based Composite)

  • 신동우;김종희
    • 한국세라믹학회지
    • /
    • 제22권5호
    • /
    • pp.76-84
    • /
    • 1985
  • Mechanical property enhancing mechanisms of $Al_2O_3-ZrO_2$ two phase ceramic composites were studied for several compositions of different $ZrO_2$/$Al_2O_3$ ratio. Microstructural analysis of $Al_2O_3-ZrO_3$(pure) composites indicated that pre-existing microcrack due to larger $ZrO_2$ particle at grain boundary extended along alumina grain boundaries within process zone. Microcracks also nucleated when very small $ZrO_2$ particles at the grain boundaries transformed to monoclinic phase at near of main crack tip. These types of microcracks could contribute to the toughening achieved by creating additional crack surface area during crack propagation. Microstructural analyses also showed that the average grain size and abnormal grain size of $Al_2O_3$ were decreased with increasing $ZrO_2$ vol% in $Al_2O_3$ matrix. As a result it could be concluded as follows In TEX>$Al_2O_3-ZrO_3$(pure) system 1. Microcrack nucleation (stress-induced microcracking) and extension was effective mechanism for absorpiton of fracture energy 2, More narrow distribution and smaller grain size of $Al_2O_3$ due to $ZrO_2$particles mainly contributed to main-tatin the strength and hardness.

  • PDF

Strength enhancement of concrete incorporating alccofine and SNF based admixture

  • Reddy, Panga Narasimha;Jindal, Bharat Bhushan;Kavyateja, Bode Venkata;Reddy, A. Narender
    • Advances in concrete construction
    • /
    • 제9권4호
    • /
    • pp.345-354
    • /
    • 2020
  • Cement is the most significant component in concrete. Large scale manufacturing of cement consumes more energy and release harmful products (Carbon dioxide) into the atmosphere that adversely affect the environment and depletes the natural resources. A lot of research is going on in globally concentrating on the recycling and reuse of waste materials from many industries. A major share of research is focused on finding cementitious materials alternatives to ordinary Portland cement. Many industrial waste by-products such as quartz powder, metakaolin, ground granulated blast furnace slag, silica fume, and fly ash etc. are under investigations for replacement of cement in concrete to minimize greenhouse gases and improve the sustainable construction. In current research, the effects of a new generation, ultra-fine material i.e., alccofine which is obtained from ground granulated blast furnace slag are studied as partial replacement by 25% and with varying amounts of sulfonated naphthalene formaldehyde (i.e., 0.3%, 0.35% and 0.40%) on mechanical, water absorption, thermal and microstructural properties of concrete. The results showed moderate improvement in all concrete properties. Addition of SNF with combination of alccofine showed a significant enhancement in fresh, hardened properties and water absorption test as well as thermal and microstructural properties of concrete.

투과전자현미경을 이용한 상전이형 광디스크의 미세조직 관찰 (Microstructural Observation of Phase Change Optical Disk by TEM)

  • 김수철;김긍호
    • Applied Microscopy
    • /
    • 제29권4호
    • /
    • pp.493-498
    • /
    • 1999
  • 기억저장매체로서 광디스크의 개발이 활발히 진행되고 있으며 최근의 레이저 기술의 발전, 제조기술의 발전에 따른 기억밀도의 증가로서 기존의 자기기록매체와 경쟁을 하고 있다. 기록밀도의 증대와 신뢰성의 향상을 위하여 다층박막 구조를 가지는 광디스크의 미세구조는 더욱 복잡하며 소형화되고 있다. 이종의 물질로 구성된 다층박막형 광디스크의 미세구조 관찰 및 분석을 위해서는 투과전자현미경과 같은 미소영역 분석법이 필수적이며 비교적 간단하고 신뢰성 높은 시편준비법의 확립이 선행되어야 한다. 본 연구에서는 투과전자현미경 분석을 위한 광디스크의 평면 및 단면시료 제작법을 제시하고 제조된 시편으로부터 얻어진 광디스크의 미세구조 분석결과를 보고한다.

  • PDF

용탕단조 Mg-Zn-Zr 합금의 미세조직 및 강화기구 (Microstructure and Strengthening Behavior in Squeeze Cast Mg-Zn by Addition of Zr)

  • 오상섭;황영하;김도향;홍준표;박익민
    • 한국주조공학회지
    • /
    • 제19권1호
    • /
    • pp.38-46
    • /
    • 1999
  • Microstructural characteristics and strengthening behavior in Mg-5wt%Zn-0.6wtZr alloys have been investigated by a combination of optical, secondary electron and transmission electron microscopy, differential thermal analysis, and hardness and tensile, creep property measurements. The result have been compared with those of Mg-5wt%Zn alloys. The as-squeeze cast microstructure consisted of dendrite ${\alpha}-Mg$, interdendrite or intergranular $Mg_7Zn_3$ and fine dispersoids of $ZnZr_2$. The size of secondary solidification phases in Mg-5wt%Zn-0.6wtZr alloys was significantly smaller than that of the Mg-5wt%Zn alloys due to the existence of fine dispersoid of $ZnZr_2$ which also effected the refinement of grain size. TEM study showed that the main cause of age hardening is formation of fine rodlike ${\beta}_1\;'$ precipitates as well as fine $ZnZr_2$ dispersoids. Due to the observed microstructural characteristics mechanical propeties of Mg-5wt%Zn-0.6wtZr alloys was found to be superior to those of Mg-5wt%Zn alloys.

  • PDF

고액공존 과공정 Al-Si합금의 교반응고시 미세조직변화 (Microstructural changes during semi-solid state processing of hypereutectic Al-Si alloys)

  • 유영호;김도향
    • 한국주조공학회지
    • /
    • 제15권5호
    • /
    • pp.483-493
    • /
    • 1995
  • The microstructural changes during semi-solid state processing of hypereutectic Al-Si alloy has been investigated in the present study. Stirring of semi-solid slurry results in the morphological changes of the primary Si particles, i.e. from angular rod shape to near-spherical shape. Besides the spherodization of primary Si particles, the average particle size increases, especially, at much higher rate in the final stage than that in the early stage of stirring. Various microstructure characterization techniques, such as anisotropic etching, SEM imaging and ECP analysis, reveal that the spherodization of primary Si particles occurs by the combinations of the mechanisms of coalescence, fracture, and wear of the individual particles. Isothermal shearing of hypereutectic Al-Si at $580^{\circ}C$ shows that spherical ${\alpha}-Al$ particles are formed by the dissociation of Al-Si eutectic structure at the early stage of isothermal shearing. The spherical ${\alpha}-Al$ particles gradually grow by the mechanisms of Ostwald ripening and coalescence of the particles.

  • PDF

소결분위기 변환온도가 Al2O3/Cu 나노복합재료의 미세조직과 파괴강도에 미치는 영향 (Effect of Sintering Atmosphere Changing Temperature on Microstructure and Mechanical Property of Al2O3/Cu Nanocomposites)

  • 오승탁;윤세중
    • 한국분말재료학회지
    • /
    • 제11권5호
    • /
    • pp.421-426
    • /
    • 2004
  • The microstructure and mechanical property of hot-pressed $Al_2O_3/Cu$ composites with a different temperature for atmosphere changing from H$_{2}$ to Ar have been studied. When atmosphere-changed from H$_{2}$ to Ar gas at 145$0^{\circ}C$, the hot-pressed composite was characterized by inhomogeneous microstructure and low fracture strength. On the contrary, when atmosphere-changed at low temperature of 110$0^{\circ}C$ the composite showed more homogeneous microstructure, higher fracture strength and smaller deviation in strength. Based on the thermodynamic consideration and microstructural analysis, it was interpreted that the Cu wetting behavior relating to the formation of CuAlO$_{2}$ is probably responsible for strong dependence of microstructure on atmosphere changing temperature. The reason for a strong sensitivity of fracture strength and especially of its deviation to atmosphere changing temperature was explained by the microstructural inhomogeneity and by the role of CuAlO$_{2}$ phase on the interfacial bonding strength.