• 제목/요약/키워드: Microbial Adsorbent Layer

검색결과 2건 처리시간 0.015초

미생물토양시트를 충진한 도로포장용 다공성 콘크리트의 제조 및 수질정화특성 (Preparation and Water Quality Purification of Permeable Concrete Pavement Filled with Microbial-Soil Sheet)

  • 강영현;황필기;강선홍
    • 상하수도학회지
    • /
    • 제23권6호
    • /
    • pp.727-733
    • /
    • 2009
  • This study was performed to investigate the physical characteristics like compressive strength, permeability, porosity and the water quality removal characteristics of permeable concrete pavement filled with microbial-soil sheet to remove SS, organic matter and nutrients in artificial rainfall. As a result, it can show the removal efficiency is SS 90~95%, COD 85~93%, BOD 80~83%, T-N 61~75%, T-P 71~78% on WAPS I(W1) and WAPS II(W2). Therefore, permeable concrete pavement filled with microbial-soil sheet shows higher removal efficiency(SS 10%, organic matter and nutrients 30%) than a conventional porous concrete(W3). By filling microbial-soil sheet to permeable concrete pavement, we confirm that the function and efficiency are improved significantly and that a naturally-friendly facility can be developed and applied to treat non-point sources.

화강풍화토와 미생물 혼합물의 고결 반응 메카니즘 (A Study on Cementation Reaction Mechanism for Weathered Granite Soil and Microbial Mixtures)

  • 오종신;이성열;김진영;권성진;정창성;이재수;이정훈;고화빈;백원진
    • 한국농공학회논문집
    • /
    • 제61권6호
    • /
    • pp.103-110
    • /
    • 2019
  • The purpose of this study is to investigate the reaction mechanism of soil and bacteria solution by various mixing ratios. For this purpose, in order to understand the reaction mechanisms of microorganisms and weathered granite soil, the tests were carried out under various mixing ratios additives such as soil, bacteria solution, $Ca(OH)_2$ and fixture. The test results from this study are summarized as follows. Firstly, the reaction between the bacteria solution and fixture produced a precipitate called vaterite, a type of silicate and calcium carbonate. Secondly, as a result of SEM analysis, the resulting precipitates generated from the test results using the specimens with various mixing ratios except SW condition and the irregular spherical microscopic shapes were formed in the size of $150{\mu}m$ to $20{\mu}m$. In addition, it can be seen that the bacteria solution and the fixture reacted between the granules to form an adsorbent material layer on the surface, and the microorganisms had a biological solidifying effect when the pores are combined into hard particles. Finally, The XRD analysis of the sediment resulting from the reaction between the microorganism and the deposit control agent confirmed the presence of a type of calcium carbonate ($CaCO_3$) vaterite, which affects soil strength formation, as well as silicate($SiO_2$).