• 제목/요약/키워드: Metal matrix composites(MMC)

검색결과 44건 처리시간 0.026초

$Al/{Al_2}{O_3}$금속복합재료의 기계적 성질과 피로거동 (Mechanical Property and Fatigue Bahavior of $Al/{Al_2}{O_3}$ Metal Matrix Composite)

  • 송정일;임홍준;한경섭
    • 대한기계학회논문집A
    • /
    • 제20권3호
    • /
    • pp.753-764
    • /
    • 1996
  • The metal matrix composites(MMC) are currently receiving a great deal of attention. These composites possess exellent mechanical and physical properties such as modulus, strength, wear resistance and thermal stability, which make them very attractive for use in automotive piston. In this study, $Al/{Al_2}{O_3}$(15%) composites are fabricated by the squeeze casting method. Mechanical properties such as tensile strength and ductility are performed at room and elevated temperature($250^{\circ}C$ and $350^{\circ}C$), respectively. Through thermomechanical analyser, thermal expansion coefficient of $Al/{Al_2}{O_3}$ composites are conducted for ranging from room temperature to ($400^{\circ}C$.And bending fatigue tests are also performed by the rotary bending machine at room temperature.The tensile strength and elastic modulus have been improved up to 38% and 35% by the addition of the reinforcements, respectively. Thermal expansion coefficients of MMCs which is located normal and parralel to the applied pressure are showed slightly different less than 10%. Fatigue strengh of the composite was improved by about 20% compared with that of unreinforced Al alloy. The results of this study will be used to understand the basic fracture behavior of MMCs and eventually to expand the applocation of MMCs as a machine parts undertaken various loadings.

입자강화 금속기 복합재료의 고온 피로강도 향상에 관한 연구 (A Study on the Improvement of Fatigue Strength in Particulate Reinforced Metal Matrix Composites at Elevated Temperatures)

  • 신형섭
    • 대한기계학회논문집A
    • /
    • 제24권5호
    • /
    • pp.1146-1154
    • /
    • 2000
  • Fatigue strength of NiAl and Ni$_3$Al particulate reinforced aluminum alloy composites fabricated by the diecasting method was examined at room and elevated temperatures. The results were compared wit h that of SiC particulate reinforced one. The particulate reinforced composites showed some improvement in the static and fatigue strength at elevated temperatures when compared with that of Al alloy. The composites reinforced by intermetallic compound particles showed good fatigue strengths at elevated temperatures especially $Ni_3AI_{p}/Al$ alloy composite showed good fatigue limit up to high temperature of 30$0^{\circ}C$. Adopting intermetallic compound particle as a reinforcement phase, it will be possible to develop MMC representing better fatigue property at elevated temperature.

습식 교반 및 방전 플라즈마 소결 공정에 의한 CNT 분산 Cu 복합재료 제조 (Fabrication of CNT dispersed Cu matrix composites by wet mixing and spark plasma sintering process)

  • 조승찬;조일국;이상복;이상관;최문희;박재홍;권한상;김양도
    • 한국분말재료학회지
    • /
    • 제25권2호
    • /
    • pp.158-164
    • /
    • 2018
  • Multi-walled carbon nanotube (MWCNT)-copper (Cu) composites are successfully fabricated by a combination of a binder-free wet mixing and spark plasma sintering (SPS) process. The SPS is performed under various conditions to investigate optimized processing conditions for minimizing the structural defects of CNTs and densifying the MWCNT-Cu composites. The electrical conductivities of MWCNT-Cu composites are slightly increased for compositions containing up to 1 vol.% CNT and remain above the value for sintered Cu up to 2 vol.% CNT. Uniformly dispersed CNTs in the Cu matrix with clean interfaces between the treated MWCNT and Cu leading to effective electrical transfer from the treated MWCNT to the Cu is believed to be the origin of the improved electrical conductivity of the treated MWCNT-Cu composites. The results indicate the possibility of exploiting CNTs as a contributing reinforcement phase for improving the electrical conductivity and mechanical properties in the Cu matrix composites.

($\textrm{Al}_2\textrm{O}_3$+SiCp)/AZ91 하이브리드 Mg 복합재료의 기계적 특성에 미치는 SiCp크기의 영향 (The Effect of SiCp Size on the Mechanical Preperties of ($\textrm{Al}_2\textrm{O}_3$+SiCp)/AZ91 Hybrid Mg Composites)

  • 하창식;김봉룡;조경목;박익민;최일동
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2001년도 춘계학술발표대회 논문집
    • /
    • pp.29-33
    • /
    • 2001
  • In the present study, AZ91Mg/$\textrm{Al}_2\textrm{O}_3$ short fiber+SiC particulates hybrid metal matrix composites(MMCs) were fabricated by squeeze casting method. Different particulate sizes of 45, 29 and $9\mu\textrm{m}$ were hybridized with 5% volume fraction to investigate the effect of SiC particulates size on microstructure, mechanical and thermal properties such as hardness, flexural strength, wear resistance and thermal expansion. Results show that the microstructure of the hybrid composites were quite satisfactory, namely revealing relatively uniform distribution of reinforcements. Some aggregation of SiC particulates caused by particle pushing was observed especially in the hybrid composites containing in fine particulates($9\mu\textrm{m}$). The hardness and flexural strength were improved by decreasing particulates size, whereas wear resistance improved by increasing particulates size because of large particulates restricting matrix wear from contacted stress. Regardless of particulates size, thermal expansion of composites was the same. This may be because the content of particulates was in all cases 5 volume fraction.1

  • PDF

용탕단조법으로 제조된 니켈코팅흑연화이버 강화 금속복합재료의 미세조직에 대한 가압력의 영향 (Influence of Applied Pressure on the Microstructure of NCG Reinforced MMC Fabricated by Squeeze Casting)

  • 유용문;윤의박
    • 한국주조공학회지
    • /
    • 제19권1호
    • /
    • pp.66-70
    • /
    • 1999
  • In order to increase the wettability between ceramic fiber and metal matrix, ceramic fibers are generally coated with metal. In this paper, we examined how the nickel layers coated on continuous graphite fiber to increase the wettability are affected with variation applied pressure. In order to examine the behavior of nickel layer with variation of applied pressure, microstructure and nickel mapping of composites were investigated with SEM, and tensile properties of the composite were tested with UTM. As the applied pressure increases, nickel layers were resolved into the aluminum matrix and ultimate tensile strength of the composite decreased.

  • PDF

The Electrical Resistivity of a SiCw/Al Alloy Composite with Temperature

  • Kim Byung-Geol;Dong Shang-Li;Park Su-Dong;Lee Hee-Woong
    • 한국재료학회지
    • /
    • 제14권7호
    • /
    • pp.489-493
    • /
    • 2004
  • The electrical property of MMC is essentially important to some applications such as power transmission lines and cables, electronic and electrical components as well as electromagnetic shielding equipments. The behavior of electrical resistivity of $SiC_{w}/Al$ alloy composites under as-extruded and annealed conditions has been investigated within the temperature range from room temperature to $450^{\circ}C$. It can be seen that within entire temperature range, the electrical resistivity of composites was higher than that of an unreinforced matrix alloy under the same condition of either as-extrusion or annealing. The temperature dependence of both exhibited positive incline like a typical metal. The variation of electrical resistivity of an unreinforced matrix alloy with temperature from ambient temperature to $450^{\circ}C$ was nearly monotonous, while those of composites increased monotonously at low temperature and rose to a high level after about $250^{\circ}C or 275^{\circ}C$. The difference of these temperature dependences on electrical resistivity can be interpreted as qualitatively the interfaces of $SiC_{w}$ fibers and matrix, where act as nucleation sites.

금속기복합재료의 피로균열성장거동에 대한 응력비 영향에 관한 연구 (A Study on the Stress Ratio effect of Metal Matrix Composites on Fatigue Crack Growth Behavior)

  • 최용범;허선철;윤한기;박원조
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.155-160
    • /
    • 2002
  • Metal matrix composites had generated a lot of interest in recent times because of significant in specific properties. It was also highlighted as the materials of frontier industry because strength, heat-resistant, corrosion-resistant, wear-resistant were superiored. In this study the strength properties of $Al_{18}B_4O_{33}/AC4CH$ were represented mixing the binder of $Al_2O_3$ and $TiO_2$. It was also fabricated by squeeze casting. $Al_{18}B_4O_{33}/AC4CH$ was fabricated at the melt temperature of $760^{\circ}C$ the perform temperature of $700^{\circ}C$ and mold temperature of $200^{\circ}C$ under the pressure of 83.4MPa and observed SEM. Fatigue crack growth rate tests on compact tension specimen(half-size) of thickness 12.5mm were conducted by using sinusoidal waveform. Compact tension specimens(half-size) were used and fatigue crack growth rate da/dN and stress intensity factor range ${\Delta}K$ were analyzed concerning to the R value of 0.1 and 0.05. In order to find out the value of ${\Delta}K$, load amplitude constant method was applied by the standard fatigue testing method describes in ASTM E647-95a. As the results of this study, Fatigue crack growth rate increased with in creasing the load ratio, Consequently, At equivalent stress intensity factors, the fatigue crack growth rates in MMC were faster than those of AC4CH alloy. then the fatigue life and the fatigue crack growth rate was investigated using scanning election microscopy(SEM)

  • PDF

용탕단조법에 의하여 제조한 $SiC_p$/Al 복합재료의 2차 성형공정이 기계적 성질에 미치는 영향 (Effects of Secondary Forming Process on Mechanical Properties of $SiC_p$/Al Composites Fabricated by Squeeze Casting)

  • 서영호;강충길
    • 대한기계학회논문집A
    • /
    • 제20권11호
    • /
    • pp.3474-3490
    • /
    • 1996
  • A metal matrix composites(MMCs) for A16061 reinforced with silicon carbide particles is fabricated by melt-stirring method. The primary products of MMCs billets are prepared by volume fractions 5 vol% to 20 vol% and particle size $13\mu m$ to $22\mu m$.This paper will be made to examine the microstructure and mechanical properties of fabricated $SiC_p$/Al 6061 composite by melt-stirring and squeeze casting method. The MMC billets is extruded at $500^{\circ}C$ under the constant extrusion velocity $V_e$=2mm/min using curved shape die. Extrusion force, particle rearrangement, micro structure and mechanical properties of extruded composites will be investigated. The mechanical properties of primary billets manufactured by melt-stirring and squeeze casting method will be compared with extrusion specimen. The effect of volume fraction and size of the reinforcements will be studied. The increase in uniformity of particle dispersion is the major reason for an improvement in reliability due to hot extrusion with optimal shape die. Experimental Young's modulus and 0.2% offset yield strength for the extruded MMCs will be compared with theretical values calculated by the Eshelby method. A method will be proposed for the prediction of Young's modulus and yield strength in $SiC_p$ reinforced MMCs.

금속기지 복합재료의 제조 및 성형시에 발생하는 열적잔류응력의 정량적 평가 및 예측에 관한 이론적 연구 (제 1보 : 강화재가 2차원 평면상태로 분포하는 경우) (A Theoretical Study on Quantitative Prediction and Evaluation of Thermal Residual Stresses in Metal Matrix Composite (Case 1 : Two-Dimensional In-Plane Fiber Distribution))

  • 이준현;손봉진
    • 비파괴검사학회지
    • /
    • 제17권2호
    • /
    • pp.89-99
    • /
    • 1997
  • 단섬유강화금속복합재료는 최근 항공기, 자동차산업에 있어서 관심의 대상이 되고 있는 재료중의 하나이나 재료의 제조 및 성형중에 재료내의 기지재 및 강화재의 열팽창계수의 차이로 인해 재료 내부에 발생되는 열적잔류응력으로 인한 재료 특성의 변화로 실제적인 재료 적용상에 많은 문제점들이 보고되고 있다. 이와 같은 금속복합재료의 잔류응력의 평가에는 몇가지 비파괴적 방법이 적용되고 있으나 그 측정에 많은 어려움이 보고되고 있다. 따라서 금속복합재료의 보다 실제적인 응용을 위하여는 이와 같은 열적잔류응력을 평가하기 위한 이론적모델의 확립이 요구된다. 본 연구에 있어서는 비방향성을 가진 강화재가 2차원 평면 상태로 기지재내에 존재하는 단섬유강화금속복합재료에 있어서 재료에 균일한 온도 변화가 주어질 때 기지재와 강화재의 열팽창계수의 차로 인해 재료 내부에 발생하는 열적잔류응력을 평가, 예측하기 위한 이론적 탄성 모델을 확립하고자 한다. 본 연구에서 해석하고자 하는 이론 모델은 Eshelby의 등가 개재물 방법을 토대로 하고 있으며 과거 제안되고 있는 이론모델을 포함하는 보다 일반성을 가지는 해석 모델로서, 이 해석 모델을 이용하여 열적잔류응력에 미치는 강화재의 체적률, 종횡비, 분포 상태, 분포 cut-off 각도들에 대한 각 인자의 영향을 검토하였다. 그 결과 강화재의 체적률, 종횡비, cut-off 각도들이 강화재의 분포 상태보다도 금속복합재료의 열적잔류응력에 미치는 영향이 현저함을 알 수 있었다.

  • PDF

알루미늄 복합재료의 마찰용접시 브레이크 타이밍이 접합계면 효율에 미치는 영향 (Effect of Brake Timing on Joint Interface Efficiency of Aluminum Composites During Friction Welding)

  • 김현수;박인덕;소전강;김태규
    • 한국분말재료학회지
    • /
    • 제13권1호
    • /
    • pp.62-67
    • /
    • 2006
  • Friction welding of $Al_2O_3$ particulate reinforced aluminum composites was performed and the following conclusions were drawn from the study of interfacial bonding characteristics and the relationship between experimental parameters of friction welding and interfacial bond strength. Highest bonded joint efficiency (HBJE) approaching $100\%$ was obtained from the post-brake timing, indicating that the bonding strength of the joint is close to that of the base material. For the pre-brake timing, HBJE was $65\%$. Most region of the bonded interface obtained from post-brake timing exhibited similar microstructure with the matrix or with very thin, fine-grained $Al_2O_3$ layer. This was attributed to the fact that the fine-grained $Al_2O_3$ layer forming at the bonding interface was drawn out circumferentially in this process. Joint efficiency of post-brake timing was always higher than that of pre-brake timing regardless of rotation speed employed. In order to guarantee the performance of friction welded joint similar to the efficiency of matrix, it is necessary to push out the fine-grained $Al_2O_3$ layer forming at the bonding interface circumferentially. As a result, microstructure of the bonded joint similar to that of the matrix with very thin, fine-grained $Al_2O_3$ layer can be obtained.