• 제목/요약/키워드: Mechanical alloying Method

검색결과 103건 처리시간 0.029초

기계적 합금화방법으로 만들어진 Ag계 삽입금속의 젖음성과 미세조직 (Wettability and Microstructures of Ag System Insert Metals Manufactured by Mechanical Alloying Method:)

  • 김광수;노기식;황선효
    • 한국재료학회지
    • /
    • 제11권12호
    • /
    • pp.1020-1027
    • /
    • 2001
  • Powder type Ag system insert metals were manufactured by mechanical alloying method. Alloying method was the ball milling process using zirconia ball media, and all alloying variables were constant except the milling time. The milling times were selected 24, 48 and 72 hours. The insert metals made by milling method were observed using scanning electron microscope and x-ray analyses. And also, the evaluation of wettability and microstructures of the insert metals were conducted to investigate the characteristics of the brazed joint. The wettability of the insert metals made by milling of 48 hours, was the best condition. And the insert metals contained Cd shows good wettability, however, there was the oxides residue on the brazing test specimen. The microstructures of the manufactured and the commercial insert metals were almost same displaying the Cu- rich proeutectic and Ag-rich eutectic. Further, there were some porosities. The 48 hours alloyed insert metal was exhibited the most sound brazed joint without containing porosity due to the superior wettability and good alloying condition.

  • PDF

기계적 합금화법으로 제조된 Cu/TiO2 촉매용 분말의 상변화 특성 (Phase Transformation Properties of Cu/TiO2 Photocatalyst Powders Fabricated by Mechanical Alloying)

  • 안인섭;배승열;이영란;고봉석
    • 한국분말재료학회지
    • /
    • 제9권2호
    • /
    • pp.110-115
    • /
    • 2002
  • In order to obtain the nano size $10wt%Cu-TiO_2$composite powders by mechanical alloying method for useful composite catalysis, the effects of mechanical alloying time on the formationof $10wt%Cu-TiO_2$ composite powders were analyzed. The phase transformation behaviors were experimented as the heat treating temperature increased. Homogeneous 10wt% Cu-rutile type $TiO_2$composite powders were synthesized in 40 hours by mechanical alloying. After 60 hours mechanical alloying 50 nm size $TiO_2$powders were obtained. Both the phase of mechanically alloyed 10 wt% $Cu-TiO_2$ and pure $TiO_2$ powders were not transformed to anatase after annealing at the temperature range between 350 to 500 $^{\circ}C$. The intermetallic compound of $Cu_2Ti_4$O was formed after 10 hours mechanical alloying, however it could be considered that this intemetallic phase dose not prevent the transformation of rutile $TiO_2$ to the anatase phase after heat treatment at the temperature between 350 and $550^{\circ}C$.

Mechanical Alloying Method로 제조된 고온수전해용 Ni/YSZ cermet의 제조 및 특성 (Synthesis and Characteristic of Ni/VSZ Cermet for High Temperature Electrolysis Prepared by Mechanical Alloying Method)

  • 채의석;홍현선;추수태
    • 한국수소및신에너지학회논문집
    • /
    • 제16권4호
    • /
    • pp.372-378
    • /
    • 2005
  • Ni/YSZ ($Y_2O_3$-stabilized $ZrO_2$) composite powder for a cathode material in high temperature electrolysis(HTE) was synthesized by a mechanical alloying method with Ni and YSZ powder. Microstructure of the composite and cell thickness for HTE reaction has been analyzed with various techniques of XRD, SEM to investigate effects of fabrication conditions. Employing the composite material, furthermore, the unit cell for HTE has been studied to evolve hydrogen from water. XRD patterns showed that the composites after wet mechanical alloying were composed of respective nano-sized crystalline Ni and YSZ. While ethanol as additive for mechanical alloying increased to $20\;{\mu}m$ of average particle size of the composites, alpha-terpineol effectively decreased to sub-micro size of that. This study has been found out the evolution of hydrogen by HTE reaction employing the fabricated cathode material, showing 1.4 ml/min of $H_2$ generation rate as increasing $20\;{\mu}m$ of cathode thickness.

급속냉각한 Al-(1, 3, 5)Cr 합금의 조직에 미치는 기계적 합금화의 영향 (Effects of Mechanical Alloying on the Structure of Rapid Solidified Al-(1, 3, 5 )Cr Alloys)

  • 지태구;김완철
    • 열처리공학회지
    • /
    • 제6권4호
    • /
    • pp.194-203
    • /
    • 1993
  • Rapid solidified splats Al-(1, 3, 5Cr) Alloys were produced by atomization-splat quenching method. Effects of mechanical alloying on the structure and mechanical properties of rapidly solidified Al-(1, 3, 5)Cr alloys were studied. Degree of mechanical alloying of Al-(1, 3, 5)Cr alloys can be determined by observing the microstructural refinement, microhardness and microstructure of Al-(l, 3, 5)Cr splats during processing. In the initial stage of mechanical alloying of the Al-(1, 3, 5)Cr splats fracturing of the grain boundaries occured first, followed after fracturing of zone A regions. Saturation hardness of Al-(1, 3, 5)Cr alloys increased proportionally with increasing concentration of the solute (Cr). Age hardening was not observed in these alloys. Decomposition temperature of Al-1Cr splats after mechanical alloying was higher than that of Al-5Cr splats. The density of $Al_7$ Cr precipitates increased proportionally with increasing chromium content, as a result, there was a transition to finely and spherically dispersed phase after mechanical alloying.

  • PDF

기계적 합금화법에 의한 ${\beta}-FeSi_2$ 분말 함성 (Synthesis of ${\beta}-FeSi_2$ Powder by Mechanical Alloying Process)

  • 이충효;조재문;김환태;권영순
    • 한국분말재료학회지
    • /
    • 제8권2호
    • /
    • pp.104-109
    • /
    • 2001
  • The semiconducting ${\beta}-FeSi_2$ compound has been recognized as a thermoelectric material with excel-lent oxidation resistance and stable characteristics at elevated temperature. In the present work, we applied mechanical alloying(MA) technique to produce ${\beta}-FeSi_2$ compound using a mixture of elemental iron and silicon powders. The mechanical alloying was carried out using a Fritsch P-5 planetary mill under Ar gas atmosphere. The MA powders were characterized by the X-ray diffraction with Cu-K $\alpha$ radiation, thermal analysis and scanning electron microscopy. The single ${\beta}-FeSi_2$ phase has been obtained by mechanical alloying of $Fe_{33}Si_{67}$ mixture powders for 120 hrs or for 70 hrs coupled with the subsequent heat treatment up to $700^{\circ}C$. The grain size of ${\beta}-FeSi_2$ powders analyzed by Hall plot method was 44nm.

  • PDF

기계적 합금화법에 의해 제조된 Cu-l0wt%W 소결재의 미세조직 및 물성 (Microstructure and Physical Properties of Cu-l0wt%W Sintered Material Fabricated by Mechanical Alloying Method)

  • 김보수
    • 한국분말재료학회지
    • /
    • 제1권2호
    • /
    • pp.167-173
    • /
    • 1994
  • Cu-10wt%W composite powders have been manufactured by a high energy ball milling technique. The composite powders were pressed at 250 MPa and sintered in a dry hydrogen at 103$0^{\circ}C$ for 4 hours. After sintering, Cu-10wt%W composite materials were forged. And the arc-resistance of forged materials which have the same relative density of 94% has been tested. Composite particles, i.e. tungsten particles distributed homogeneously in the copper matrix, was formed after 480 min mechanical alloying. Densities of these sintered materials were ranged from 74 to 84%. Densification degree was due to the formation of composite powders. As the mechanical alloying time increased, the hardness was increased and tungsten particle size was decreased. Arc loss of the forged specimens was decreased as increasing the mechanical alloying time.

  • PDF

기계적 합금법에 의한 $BaO_2-TiO_2$ :$Eu^{3+}$ 분말의 합성 (Formation of $Eu^{3+}$ - doped $BaO_2-TiO_2$ Powders Produced by Mechanical Alloying)

  • 김현구
    • 통합자연과학논문집
    • /
    • 제1권2호
    • /
    • pp.84-88
    • /
    • 2008
  • The formation and thermal properties of the $BaO_2$ and $TiO_2$ mixtures were prepared by mechanical alloying method was investigated by X-ray diffractometry (XRD), scanning electron microscopy (SEM), and thermogravimetric/differential thermal analysis (TG/DTA). The rotating speed of 750 rpm shows more effects on the formation of $BaTiO_3$ single phase. The internal strain calculated using Williamson-Hall method was $4.27{\times}10^{-3}$ for the mixture milled for 300 min, the crystallite size was calculated using the Scherrer method decreased with milling time. The $BaTiO_3$ crystal improved crystallinity was formed by thermal annealing at a temperature of $600^{\circ}C$ for 1 h for the mixture milled for 300 min.

  • PDF

MA법에 의한 Mn-Si계 초미세 열전재료의 제조 및 평가 (Fabrication and characterization of Mn-Si thermoelectric materials by mechanical alloying)

  • 이충효
    • 한국결정성장학회지
    • /
    • 제21권6호
    • /
    • pp.246-252
    • /
    • 2011
  • 반도성 $MnSi_{1.73}$ 화합물은 고온 특성이 우수하고 뛰어난 내산화성을 가진 열전재료로서 알려져 있다. 본 연구에서는 순 Mn 및 Si 분말재료를 출발 원료로 기계적 합금화법(MA)을 적용하여 $MnSi_{1.73}$ 화합물 합성을 실시하였다. MA 처리는 P-5 유성형 볼밀장치를 이용하여 Ar 중에서 행하였다. MA 분말재료의 X선 회절, 열분석 및 전자현미경 분석을 통하여 고상반응을 관찰하였다. MA 공정 중 Si의 손실을 고려하여 화학양론 조성에서 Si 양을 증가시켜 $MnSi_{1.73}$ 화합물 합성을 시도하였다. 그 결과 $MnSi_{1.73}$ 화합물 단상은 $MnSi_{1.88}$ 조성의 혼합 분말을 200시간 볼밀 처리함으로써 얻을 수 있었다. 또한 200시간 볼밀 처리에 의하여 제조된 $MnSi_{1.73}$ 화합물의 평균결정립 크기는 40 nm 임을 X 선 회절피크의 Hall plot으로 부터 알 수 있었다.

기계적 합금화법으로 제조된 $Bi_2Te_3$계 열전화합물 분말의 열분석 (Thermal Analysis of $Bi_2Te_3$ Based Thernoelectric Compound Powder Produced by Mechanical Alloying)

  • 김봉서;양준혁;오민욱;박수동;이희웅;박규섭;배동식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.151-152
    • /
    • 2006
  • Bi-Te thermoelectric powder was fabricated by mechanical alloying method for 1 to 10 hours under vacuum in planetary mill. We investigated the properties of mechanically alloyed Bi-Te powder by thermal analysis, X-ray diffractometer and FESEM with EDS Bi-Te raw material was formed to $Bi_2Te_3$ phase at condition over 3.5 hours of mechanical alloying time.

  • PDF

기계적 합금화 공정을 이용한 초미세 자성연마입자의 제조 및 특성 평가 (Fabrication of the Fine Magnetic Abrasives by using Mechanical Alloying Process and Its Polishing Characteristics)

  • 박성준;이상조
    • 한국정밀공학회지
    • /
    • 제21권10호
    • /
    • pp.34-41
    • /
    • 2004
  • A new method to fabricate the fine magnetic abrasives by using mechanical alloying is proposed. The mechanical alloying process is a solid powder process where the powder particles are subjected to high energetic impact by the balls in a vial. As the powder particles in the vial are continuously impacted by the balls, cold welding between particles and fracturing of the particles take place repeatedly during the ball milling process using a planetary mill. After the manufacturing process, fine magnetic abrasives which the guest abrasive particles c lung to the base metal matrix without bonding material can be obtained. The shape of the newly fabricated fine magnetic abrasives was investigated using SEM and its polishing performance was verified by experiment. It is very helpful to finishing the injection mold steel in final polishing stage. The areal ms surface roughness of the workpiece after several polishing processes has decreased to a few nanometer scales.