• Title/Summary/Keyword: MAXIMUM STRENGTH

Search Result 3,770, Processing Time 0.033 seconds

Performance of self-compacting concrete at room and after elevated temperature incorporating Silica fume

  • Ahmad, Subhan;Umar, Arshad;Masood, Amjad;Nayeem, Mohammad
    • Advances in concrete construction
    • /
    • v.7 no.1
    • /
    • pp.31-37
    • /
    • 2019
  • This paper evaluates the workability and hardened properties of self-compacting concrete (SCC) containing silica fume as the partial replacement of cement. SCC mixtures with 0, 2, 4, 6, 8 and 10% silica fume were tested for fresh and hardened properties. Slump flow with $T_{500}$ time, L-box and V-funnel tests were performed for evaluating the workability properties of SCC mixtures. Compressive strength, splitting tensile strength and modulus of rupture were performed on hardened SCC mixtures. Experiments revealed that replacement of cement by silica fume equal to and more than 4% reduced the slump flow diameter and increased the $T_{500}$ and V-funnel time linearly. Compressive strength, splitting tensile strength and modulus of rupture increased with increasing the replacement level of cement by silica fume and were found to be maximum for SCC mixture with 10% silica fume. Further, residual hardened properties of SCC mixture yielding maximum strengths (i.e., SCC with 10% silica fume) were determined experimentally after heating the concrete samples up to 200, 400, 600 and $800^{\circ}C$. Reductions in hardened properties up to $200^{\circ}C$ were found to be very close to normal vibrated concrete (NVC). For 400 and $600^{\circ}C$ reductions in hardened properties of SCC were found to be more than NVC of the same strength. Explosive spalling occurred in concrete specimens before reaching $800^{\circ}C$.

Development of a laboratory testing method for evaluating the loading capability of lattice girder (격자지보재(Lattice Girder)의 실내성능평가기법 개발)

  • Kim, Dong-Gyou;Bae, Gyu-Jin
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.10 no.4
    • /
    • pp.371-382
    • /
    • 2008
  • The objective of this study is to develop the laboratory testing method for evaluating the loading capacity of lattice girder used for support in tunnel structure. 3-point flexible strength test and 4-point flexible strength test were performed on three types of lattice girder, such as $LG-50{\times}20{\times}30$, $LG-70{\times}20{\times}30$, and $LG-95{\times}22{\times}32$, mainly used in Korea. Two types of loading position for each flexible strength test were used to analyze the behavior of load-deformation. The loading distribution in the lattice girder was analyzed by means of strains measured by strain gauges attached on chords and diagonal bars. In 3-point flexible strength test, the difference of the average of maximum flexible strength according to loading position had the range from 10% to 33%. In 4-point flexible strength test, the average of maximum flexible strength according to loading position was almost no difference. The difference between the average of maximum flexible strengths obtained from 3-point and 4-point flexible strength tests was from 13.56 to 31.55%. The load applied on the lattice girder was concentrated to the main chord in 3-point flexible strength test. The load applied on the lattice girder in 4-point flexible strength test was distributed to three chords and diagonal bars.

  • PDF

Study on engineering properties of xanthan gum reinforced kaolinite

  • Zhanbo Cheng;Xueyu Geng
    • Computers and Concrete
    • /
    • v.31 no.6
    • /
    • pp.501-511
    • /
    • 2023
  • The strengthening efficiency of biopolymer treated soil depends on biopolymer type, concentration ratio, soil type, initial water content, curing time and mixing method. In this study, the physical and mechanical properties of xanthan gum (XG) treated kaolinite were investigated through compaction test, Atterberg limit test, triaxial test and unconfined compression test. The results indicated that the optimum water content (OWC) increased from 30.3% of untreated clay to 33.5% of 5% XG treated clay, while the maximum dry density has a slight increase from 13.96 kg/m3 to 14 kg/m3 of 0.2% XG treated clay and decrease to 2.7 kg/m3 of 5% XG treated clay. Meanwhile, the plastic limit of XG treated clay increased with the increase of XG concentration, while 0.5% XG treated clay can be observed the maximum liquid limit with 79.5%. Moreover, there are the ideal water content about 1.3-1.5 times of the optimum water content achieving the maximum dry density and curing time to obtain the maximum compressive strength for different XG contents, which the UCS is 1.52 and 2.07 times of the maximum UCS of untreated soil for 0.5% and 1% XG treated clay, respectively. In addition, hot-dry mixing can achieve highest UCS than other mixing methods (e.g., dry mixing, wet mixing and hot-wet mixing).

The Investigation of Stress Block of C-Shaped Specimen for High-Strength Polymer Concrete (고강도 폴리머 콘크리트 C 형보의 응력블럭 고찰)

  • 김관호;연규석;김남길;박광수;신수균;이준구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.05a
    • /
    • pp.1023-1028
    • /
    • 2001
  • This study was conducted to develop a procedural method to produce a high strength polymer concrete using polyester resin to experimentally examine the stress block properties of the high strength polymer concrete. C-shaped specimens were Produced and test to compute parameter of the stress block. They were $k_{1}$ : 0.73 and $\gamma$ : 0.845, respectively. $k_{1}$ is the ratio of the depth of the maximum compressive strength of the beam

  • PDF

A Study on the Compactibility of Quick-lime Mixed with Soil (생석탄 혼합토의 다짐성에 관한 연구)

  • 김철규
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.12 no.1
    • /
    • pp.1883-1886
    • /
    • 1970
  • This study was made to obtain the optium compaction of quicklime mixed with soil and to find out the relation of the quicklime mix ratio, dry density and strength by changing the compaction rounds. The obtained results are as follows. 1. The maximun dry density of unmixed soil in not distinguishable, while that of mixed soil is distinguishable. 2. What the increase of quicklime mix ratio, the dry density and strength increase and the optimum quicklime mix ratio could be obtained. 3. With the increase of compaction rounds, the dry density and strength increase, while they decrease in a certain limit and maximum dry density and strength could be obtained.

  • PDF

Structural Strength Evaluation for Tank of Tank Car used for Carrying Asphalt (아스팔트 수송용 철도차량 탱크의 구조강도 평가)

  • Lim, C.H.;Goo, B.C.
    • Proceedings of the KSR Conference
    • /
    • 2007.11a
    • /
    • pp.1024-1030
    • /
    • 2007
  • We studied on the characteristics of many kinds of tank cars carrying hazard materials and performed structural strength evaluation for tank of asphalt tank car using finite element analysis. We analyzed the tank strength according to JIS E 7102(Design Method for Tanks of Tank Cars). It was found that the maximum stress obtained at the area supported by the saddle is much lower than the yield stress and the criteria of JIS E 7102.

  • PDF

Strengthening Effects of Epoxy Mortar Systems on Reinforced Concrete Beams by Flexural Tensile Strength (변성에폭시 모르터 휨인장강도가 단면증대 보에 미치는 영향)

  • 류현희;신영수;정혜교
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.04a
    • /
    • pp.787-790
    • /
    • 2000
  • This paper presents an experimental study on flexural behavior of structural member enlarged with epoxy mortar system. The main test variable is flexural tensile strength. A series of 4 test beams was tested to shoe the corresponding effect of each variables on maximum load capacity, load-deflection and moment-curvature relationship, interface behavior and failure mode. The results show that the flexural tensile strength of retrofitted materials have no relation load-deflection, but to load-strain, and failure mode.

  • PDF

A Study on Pore Pressure Evaluation of Concrete Lining in Road Tunnel Fire (도로터널 라이닝 화재조건 콘크리트 라이닝 공극압력 특성에 관한 연구)

  • Park, Kyung-Hoon;Kim, Heung-Youl;Yoo, Yong-Ho;Lee, Chul-Ho;Kim, Hyung-Jun
    • Proceedings of the Korea Institute of Fire Science and Engineering Conference
    • /
    • 2008.11a
    • /
    • pp.484-489
    • /
    • 2008
  • We carried out a one-way heating experiment on the PC panel manufactured by changing the filling depths(20,30,40,50mm) of concrete regarding the fire strength in order to measure the inner concrete pressure which is a direct cause of concrete spalling. This fire experiment was conducted under the fire strength conditions of ISO 834 Standard, Modified Hydrocarbon and the maximum value of Pore Pressure was measured. As a result of analyzing the time it took to reach maximum pressure, it showed that the time rising to the maximum pressure of high strength concrete of 40MPa is slower than that of a 24MPa tunnel lining. In case of ISO fire conditions, spalling damage might take place in heating period of $20{\sim}40$ minutes in the range of $100{\sim}200^{\circ}C$ temperature. In case of MHC fire conditions, the area damaged by fire can appear after a lapse of $25{\sim}50$ minutes in the range of $150{\sim}250^{\circ}C$ temperature.

  • PDF

Temperature and Mechanical Properties of Welded Joints Under Friction Stir Welding Conditions of Mg Alloy (AZ61) (Mg Alloy(AZ61) 마찰교반용접 조건에 따른 용접부의 온도와 기계적 특성변화)

  • Lee, Woo Geun;Kim, Jung Seok;Sun, Seung-Ju
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.26 no.4
    • /
    • pp.378-386
    • /
    • 2017
  • Friction stir welding was performed using six welding conditions to evaluate the mechanical properties and microstructure of the welded zone based on its temperature change in the extruded plate of magnesium alloy AZ61. The welded zone temperature was measured using a thermocouple, and the maximum temperature ranges for the advancing and retreating sides were approximately $210-315^{\circ}C$ and $254-339^{\circ}C$, respectively. Depending on the welding conditions, a temperature difference of more than $100^{\circ}C$ was observed. In addition, the maximum yield strength and maximum tensile strength of the welded component was 84.4% and 96.9%, respectively, of those of the base material. For the temperatures exceeding $300^{\circ}C$, oxidation defects occurred in the weld zone, which decreased the mechanical strength of the weld zone. The microstructure and texture confirmed that fracture occurred because of the grain size deviation of the welding tool and the severe anisotropy of the texture of the welded joints.

Durability Study on Structural Strength due to the Shape of Excavator Wheel (굴삭기휠의 형상별 구조 강도에 대한 내구성 연구)

  • Cho, Jaeung;Han, Moonsik
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.21 no.6
    • /
    • pp.166-174
    • /
    • 2013
  • This study investigates the strength durability on the results of structural and vibration analysis due to the shape of excavator wheel. As model 2 has the least stress by comparing three models with maximum equivalent stress, model 2 has most durability among three models at static analysis. Maximum equivalent stress is shown at the bottom part contacted with ground and this part on wheel is most affected by load in cases of all models. Safety factor can be decided with the value of 2.3 by considering the yield stress of this model. The range of maximum harmonic response frequencies becomes 6900 to 7000Hz. As model 2 has the least total deformation and equivalent stress at these critical frequencies, model 2 has the most durability at vibration analysis among three models. The structural and vibration analysis results in this study can be effectively utilized with the design of excavator wheel by investigating prevention and durability against its damage.