  • The wear of partially coated pinion cutters under several cutting conditions was studied. In the realm of this experiment, chipping was a dominant tool wear mechanism and flank wear was much larger than crater wear. Under the condition of relatively low rotary feed and low radial feed rate, the wear due to chipping was concentrated at the nose part of pinion cutter. Increasing of rotary feed and radial feed rate alleviated the concentration of chipping at nose and prolonged tool life.

  • PDF

알루미늄 합금의 미끄럼마모 특성에 미치는 상대재 경도의 영향 (Analysis of Sliding Wear Properties for Aluminum Alloy According to the Hardness Values of the Mating Tool Steel)

  • 이한영;조용재;김태준;박원규
    • Tribology and Lubricants
    • /
    • 제26권2호
    • /
    • pp.105-110
    • /
    • 2010
  • In order to investigate the wear behavior of aluminum alloy depended on different hardness of the mating tool steel, sliding wear tests were conducted. It was found that the wear characteristics pattern of aluminum alloy for sliding speed was not affected by the hardness of the mating tool steel. However, the effects of the hardness of the mating tool steel exhibited only in relatively low sliding speed ranges. At these ranges, the wear rate of aluminum alloy decreased when increasing the hardness of the mating tool steel. This was attributed by the fact that $Al_2O_3$ particles released from the aluminum worn surface were crushed and embedded on the mating worn surface with high hardness level. At the high sliding speed ranges, wear of aluminum alloy was hardly occurred by the formation of thick $Al_2O_3$ film on the worn surface, regardless of the hardness of the mating tool steel.

A study on the machinability of SUS304

  • Lim, K.Y.;Yu, K.H.;Seo, N.S.
    • 한국정밀공학회지
    • /
    • 제10권1호
    • /
    • pp.34-41
    • /
    • 1993
  • SUS304 is wellknown as difficult-to-machine materials. It is easy to appear workhardened, and workhardening is one of the causes of groove wear on the tool. In this paper, the author would like to compare the width of flank wear with that of groove wear, and to find whether the groove wear can be used as a criterion of a tool life. The design of the twelve tests provides three levels for each variable (speed: 200m/min, 118m/min, 70m/min; feed: 0.3mm/rev, 0.17mm/rev, 0.1mm/rev; depth of cut: 0.4mm, 0.28mm, 0.2mm). The study of tool-life testing by statistical technique follows usual most scientific sequence. So the tool-life predicting equation is calculated by the method of least squares. The overall adequacy of the model can be verified by the analysis of variance. The results obtained are as follows : 1) When SUS304 is cut in 200(m/min), the width of flank wear is much larger than that of groove wear. 2) In cutting speed 118m/min, flank wear is a little larger than groove wear and in the cutting speed 70m/min, the latter is a little larger so that it is reasonable to determine the tool life according the crierion by groove wear in the low cutting speed (less than 70m/min). 3) Owing to the burr the depth of engagement along the cutting edge is extended toward the shank.

  • PDF

CBN 공구를 이용한 선삭에서의 절삭력과 공구마모 특성 (Cutting Forces and Tool Wear Characteristics in Hard Turning using CBN Tools)

  • 김태영;스기타;신형곤;김종택
    • 한국기계가공학회지
    • /
    • 제6권1호
    • /
    • pp.27-33
    • /
    • 2007
  • Hard turning on modern lathes becomes a realistic replacement for many grinding applications. Because CBN tools are expensive, excessive tool wear can eliminate economic advantages of hard turning. This paper describes a study of investigating the cutting force and the characteristics of tool wear in hard turning of hardened steels, AISI 52100. Cutting forces generated using CBN tools have been evaluated. The radial thrust cutting force was the largest among three cutting force components. It increased dramatically as a result of progressive tool wear. On the other hand, the result shows significantly different wear characteristics between high CBN and low CBN. Backpropagation neural network was used for the estimation of tool wear. The networks were achieved the reliability of 96.3% even when the spindle speed and feed rate are changed.

  • PDF

원형 톱날의 형태와 마모가 유리 탄소섬유 하이브리드 복합재료의 절단 품질에 미치는 영향 (Effect of the Circular Saw-Blade Type and Wear on the Cutting Quality of a Glass Carbon-Fiber Hybrid Composite)

  • 백종현;주창민;김수진;박윤옥
    • 한국기계가공학회지
    • /
    • 제20권10호
    • /
    • pp.72-79
    • /
    • 2021
  • A circular saw is an effective tool for cutting glass and carbon-fiber hybrid composites. This study investigated tool wear and cut quality when reusing saw blades. The carbide saws wear four times faster than the new ones, and polycrystalline diamond (PCD) is very resistant to tool wear, except at the end of its lifespan. The cut cross-section quality is affected by the blade type, tool wear, and spindle speed. Alternate top bevel (ATB)-type blades are suitable for cutting fiber-reinforced plastics, but triple-chip grind (TCG)-type blades are unsuitable because they cause fiber-pullout defects. Tool wear and low spindle speeds increase the occurrence of arc scratches, due to the rear saw blade. A microscopic examination showed that the burr, which is a mixture of fiber chips and epoxy matrix, was bonded on top, and glass-fiber delamination occurred on the bottom glass-fiber-reinforced polymer (GFRP) surface.

탭 형상에 따른 공구마모 특성에 관한 연구 (A Study About Tool Wear Characteristic on Geometry of Tap)

  • 최만성;윤홍기
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2000년도 추계학술대회 논문집
    • /
    • pp.892-897
    • /
    • 2000
  • In this study, tap wear was analyzed not only to predict the tap life time but also to propose an improved tap design. Because rake angle and thread relief of tap are the significant factors in geometry of tap, these two factors were picked as the experiment variables. The experiment was conducted with six types of tap which have 6$^{\circ}$ , 8$^{\circ}$ and 12$^{\circ}$ of rake angles with 0,08mm and 0.14 mm of thread relief. From the measured cutting force, it could be known that cutting torque was low at the large the rake thread relief and tool life was long as rake angle became large. Eventually, tool life is longest when rake angle is 12$^{\circ}$ and the with 0.08mm thread relief. Aand the width of crater wear and that of flank wear were measured when a tapping torque was 20 [$kg_f$-mm] . Most of the measured values were above the width of tool wear[$V_B$=O.O3m], which means that tool life is over.

  • PDF

신경망을 이용한 전극 저소모 방전조건 결정 (Determination of EDM parameters for low tool wears utilizing neural networks)

  • 주상윤
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 1997년도 추계학술대회 논문집
    • /
    • pp.43-47
    • /
    • 1997
  • Advances in EDM power supplies have made the process competitive in some areas dominated by conventional and numerically controlled machines. This paper will produce more comprehensive data than are presently available and will use this data in applying concepts of optimization based on manufacturer's guide lines utilizing neural networks. A method will be developed for determining the machining parameters of the EDM process considering the conflicting desirability of good surface finish, low tool wear and high rates of metal removal. By the proposed method, one can select machining parameters that can maintain permissible tool wear and obtain maximum machining rates on the system represented by the data.

  • PDF

Characterization of Tribolayers and Sliding wear at High Temperature between AlCrN Coated Tool Steels and Ultra-high Strength Boron Steels

  • Choi, Byung-Young;Gu, Yoon-Sik
    • 열처리공학회지
    • /
    • 제24권1호
    • /
    • pp.37-44
    • /
    • 2011
  • High temperature wear of AlCrN coated tool steels sliding against the ultra-high strength boron steels used for hot press forming has been studied. The sliding wear tests have been carried out using a pin-on-disc of configuration under applied normal load of 50 N for 20 min with heating the ultra-high strength boron steels up to $800^{\circ}C$. Characterizations of tribolayers formed on the contacting surfaces between the tribopairs of the AlCrN coated tool steels and the ultra-high strength boron steels have been studied. It was found on the tribolayers of the AlCrN coated tool steels that microcracking and oxides containing Fe and Cr to increase friction coefficient were formed at the early stage of sliding wear, followed by the generation of the smeared oxide layers containing Fe transferred from the tribopair to decrease friction coefficient. This may mainly contribute to very low specific wear rate of the AlCrN coated tool steels sliding against the ultra-high strength boron steels, resulting from oxideoxide contact between the tribopair.

상대재 내식성이 철강재료의 미끄럼마모 특성에 미치는 영향 (Effects of Corrosion Resistance Characteristics of Opponent Materials in relative Motion on Sliding Wear Behavior of Mild Carbon Steel)

  • 이한영
    • Tribology and Lubricants
    • /
    • 제35권2호
    • /
    • pp.139-147
    • /
    • 2019
  • This study investigates the effects of corrosion resistance characteristics of opponent materials in relative motion on the sliding wear behavior of mild carbon steel. Pin specimens made of mild carbon steel are tested at several sliding speeds against mating discs made of two types of alloyed steels, such as type D2 tool steel (STD11) and type 420 stainless steel (STS420J2), with different corrosion resistance characteristics in a pin-on-disc type sliding wear test machine. The results clearly show that the sliding wear behavior of mild carbon steel is influenced by the corrosion resistance characteristics of the mating disc materials at low sliding speeds. However, the sliding wear behavior at high sliding speeds is irrelevant to the characteristics because of the rising temperature. During the steady state wear period, the sliding wear rate of mild carbon steel against the type 420 stainless steel at a sliding speed of 0.5 m/s increases considerably unlike against the type D2 tool steel. This may be because the better corrosion resistance characteristics achieve a worse tribochemical reactivity. However, during the running-in wear period at low sliding speeds, the wear behavior of mild carbon steel is influenced by the microstructure after heat treatment of the mating disc materials rather than by their corrosion resistance characteristics.

단속 하드터님에 관한 연구 (I) : 절삭성과 CBN공구의 마모특성 (Research on the Intermittent Hard Turning (I) : Machinability and Characteristic of CBN Tools)

  • 전준용;고태조;김희술
    • 한국정밀공학회지
    • /
    • 제16권7호
    • /
    • pp.58-65
    • /
    • 1999
  • Hard turning offers many possible benefits over grinding such as lower equipment costs, shorter setup time, reduced process steps and better surface integrity. Despite the amount of research in this area, there exists no data in the intermittent hard turning. The objective of this paper is to investigate the effect of CBN tool materials and machinability to an intermittent hard turning. To this end, different CBN materials were tested to evaluate the tool wear and surface roughness in an intermittent hard turning. It is found that low-CBN-content tool is better than high-CBN-content tool. Then, we discussed a cutting force, vibration, and CBN tool wear mechanism from the hard turning.

  • PDF