• 제목/요약/키워드: Low temperature oxidation

검색결과 589건 처리시간 0.028초

황산제일철 용액의 오존 처리에 의한 산화철 합성 (Synthesis of Iron Oxide Using Ferrous Sulfate by Ozone Treatment)

  • 김삼중;서동수;엄태형;송경섭;노재승
    • 한국재료학회지
    • /
    • 제14권5호
    • /
    • pp.353-357
    • /
    • 2004
  • The influences of the ozone oxidation, reaction temperature and NaOH equivalent ratio on the iron oxide formation were studied with fixed ferrous sulfate concentration(0.5M $FeSO_4$$7H_2$O). Geothite($\alpha$-FeOOH) and/or Magnetite ($Fe_3$$O_4$) were synthesized depending on the reaction conditions. The characteristics of the synthesized powders were evaluated by XRD, SEM and quantitative phase analysis. The synthetic conditions to get Goethite were quite different from the results of Kiyama's and the Goethite was conveniently synthesized at low temperature and at low NaOH equivalent ratio.

Microstructural characterization of accident tolerant fuel cladding with Cr-Al alloy coating layer after oxidation at 1200 ℃ in a steam environment

  • Park, Dong Jun;Jung, Yang Il;Park, Jung Hwan;Lee, Young Ho;Choi, Byoung Kwon;Kim, Hyun Gil
    • Nuclear Engineering and Technology
    • /
    • 제52권10호
    • /
    • pp.2299-2305
    • /
    • 2020
  • Zr alloy specimens were coated with Cr-Al alloy to enhance their resistance to oxidation. The coated samples were oxidized at 1200 ℃ in a steam environment for 300 s and showed extremely low oxidation when compared to uncoated Zr alloy specimens. The microstructure and elemental distribution of the oxides formed on the surface of Cr-Al alloys have been investigated by transmission electron microscopy (TEM) and X-ray photoelectron spectroscopy (XPS). A very thin protective layer of Cr2O3 formed on the outer surface of the Cr-Al alloy, and a thin Al2O3 layer was also observed in the Cr-Al alloy matrix, near the surface. Our results suggest that these two oxide layers near the surface confers excellent oxidation resistance to the Cr-Al alloy. Even after exposure to a high temperature of 1200 ℃, inter-diffusion between the Cr-Al alloy and the Zr alloy occurred in very few regions near the interface. Analysis of the inter-diffusion layer by high-resolution transmission electron microscopy (HRTEM) and energy dispersive X-ray spectroscopy (EDS) measurement confirmed its identity as Cr2Zr.

Cu/CeO2 촉매의 구조적 특성이 일산화탄소 저온 산화반응에 미치는 영향 연구 (A Study on the Influence of the Structural Characteristics of Cu/CeO2 Catalyst on the Low-Temperature Oxidation of Carbon Monoxide)

  • 김민수;최경륜;김세원;홍성창
    • 청정기술
    • /
    • 제26권4호
    • /
    • pp.286-292
    • /
    • 2020
  • 본 연구는 Cu/CeO2-X 촉매의 저온 CO 산화 활성에 미치는 영향을 촉매의 구조적 특성, 반응 특성을 통해 확인하였다. 사용된 촉매는 습윤 함침법으로 제조되었으며, 각기 다른 소성온도(300~600 ℃)에서 형성된 CeO2 (지지체)를 이용하여 Cu (활성금속)를 담지함으로써 Cu/CeO2-X 촉매를 제조하였다. 제조된 Cu/CeO2-X 촉매는 저온 CO 산화 활성을 평가하였다. 125 ℃에서 Cu/CeO2_300 촉매는 90% 이상의 활성을 나타냈으며, CeO2의 소성온도가 증가됨에 따라 활성이 점차 감소하여, Cu/CeO2_600 촉매는 65%를 나타냈다. 다음으로 촉매의 물리/화학적 특성을 Raman, BET, XRD, H2-TPR, XPS 분석으로 확인하였다. XPS 분석 결과, CeO2-X의 소성온도가 낮을 수록 불안정한 Ce3+ 종(비 화학양론 종) 비율이 증가하였다. 증가된 Ce3+종은 Cu와 결합함으로 써 치환결합을 형성하였으며 Raman 분석의 CeO2 peak 변화와 H2-TPR 분석의 치환결합 구조의 환원 peak를 통해 확인하였다. 결과적으로 Cu와 CeO2의 치환 결합 형성은 촉매의 redox 특성 및 저온 CO 산화 활성을 증진시켰다고 판단된다.

오존산화에 의한 염색체수의 색도 제거에 관한 연구 (A Study on Removal of Color in Dyeing Wastewater by Ozone Oxidation)

  • 정순형;최준호
    • 환경위생공학
    • /
    • 제18권4호
    • /
    • pp.45-51
    • /
    • 2003
  • This study was conducted to remove the color in dyeing wastewater by ozone oxidation process, and the results were summarized as follows ; The 18.3% of BOD and 56.3% TOC were removed as decreasing with pH 1 in dyeing wastewater, containing the polyester reducing process. It showed that terephthalic acid was precipitated at low pH. The color of dyeing wastewater was removed by the first order reaction, and the reaction rate constants at pH 3, 7, 12 were investigated $0.234{\;}min^{-1},{\;}0.215{\;}min^{-1}{\;}and{\;}0.201{\;}min^{-1}$ respectively. It showed that color was more effectively removed with direct reaction of ozone than radical reaction(non-direct reaction). As increasing of the water temperature, the reaction rate constants were increased slightly. It indicated that activity of ozone was improved at high water temperature.

PRESERVATION OF QUALITY AFTER BROWN RICE DRYING

  • Goto, Kiyokazu;Miwa, Yoshihiro
    • 한국농업기계학회:학술대회논문집
    • /
    • 한국농업기계학회 1996년도 International Conference on Agricultural Machinery Engineering Proceedings
    • /
    • pp.878-885
    • /
    • 1996
  • The brown rice drying is effective for energy saving and cost reduction. However, deterioration after drying is one problem, because the skin damage occurs during the drying. So, the measures to preserve the quality has been investigated. One of major quality deteriorations is the oxidation of fat which is contained in the bran layer. So, milling should be carried out to remove the fat as soon as possible after brown rice drying. And the low temperature storage is also worth to be examined for prevention of oxidation. The effect of skin damage on the increase of fat oxidation was clarified. For the grain of skin damage, the increased of fatty acid vaule was remarkable after 70 days elapsed from occurrence of skin damage even in $15\;^{\circ}C$ condition. Therefore it is impossible to keep grain as brown rice form after brown rice drying. For the clean rice and excessively milled rice, the quality can be preserved even in high temperature of $30\;^{\circ}C$. Therefore the brown rice drying can b applied practically using the clean rice technique.

  • PDF

Effect of SiC on the Mullite-Cordierite Composite Properties

  • Motaman, A.;Amin, S.A.;Jahangir, A.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1067-1070
    • /
    • 2006
  • Experimental samples were produced with mullite and cordierite powders with SiC. Effects of temperature, atmosphere and additive on the composite properties were investigated by XRD, STA and PSA methods. Results show that samples containing calcinate cordierite and calcinate mullite with SiC baked in air atmosphere have not suitable properties at the temperature range of $1380-1450^{\circ}C$ due to SiC intensive oxidation, while argon atmosphere decrease SiC oxidation. Using $Bi_2O_3$ as the additive, cordierite phase formation and prevention from SiC oxidation at low temperatures were achieved, leading to the improvement of physical and mechanical properties

  • PDF

쌀과자의 자연발화 특성에 관한 연구 (A Study on the Characteristics of Spontaneous Ignition for Rice Cracker)

  • 김홍;강영구
    • 한국안전학회지
    • /
    • 제10권4호
    • /
    • pp.75-80
    • /
    • 1995
  • Spontaneous ignition characteristics of rice cracker were observed by preforming experiments at constant ambient temperature. As the results of the experiments, the critical spontaneous ignition temperature were exponentially decreased with the increase of ambient temperature. Type of combustion of rice cracker are smouldering combustion at low ignition temperature and flame combustion at high temperature. The rice cracker containing pam oil showed lower spontaneous ignition temperature than pure rice cracker because of oxidation heat of pam oil.

  • PDF

일산화탄소 저감을 위한 개질가스의 전이반응 연구 (Investigation of the Water Gas Shift from Reforming Gas for CO Removal)

  • 김성천;윤문중;전영남
    • 대한기계학회논문집B
    • /
    • 제31권10호
    • /
    • pp.855-859
    • /
    • 2007
  • Hydrogen as an energy carrier in fuel cell offers perhaps the largest potential benefits of reduced emissions of pollutants and greenhouse gases. The generation of high-purity hydrogen from hydrocarbon fuels is essential for efficient operation of fuel cell. Reduction of carbon monoxide to an acceptable level of 10ppm involves high temperature and low temperature water gas shift (WGS), followed by selective oxidation of residual carbon monoxide. The WGS reactor was designed and tested in this study to produce hydrogen-rich gas with CO to less than 5000 ppm. In the water gas shift operation, gas emerges from the reformer is taken through a high temperature shift (HTS) catalyst to reduce the CO concentration to about $2{\sim}4%$ followed to about 5000 ppm via a low temperature shift (LTS) catalyst.

디젤자동차용 산화촉매의 성능 평가 (Performance Evaluation of Diesel Oxidation Catalysts for Diesel Vehicles)

  • 최병철;박희주;정명근
    • 한국자동차공학회논문집
    • /
    • 제11권6호
    • /
    • pp.59-64
    • /
    • 2003
  • Recently, as people pay attention to the environmental pollution, the emissions of diesel engine have been a serious problem. We carried out the performance evaluation test of Diesel Oxidation Catalysts (DOC) for HSDI diesel engine equipped vehicles. The DOC, basically coated with Pt catalyst, was manufactured with various washcoat materials. It was found that CO conversion efficiency depends on temperature, but THC conversion efficiency is dominated by temperature and space velocity. The THC and CO conversion efficiencies of aged catalysts were increased with additions of $ZrO_2$ and zeolite B in the washcoat. We found that DOC performance changes with coating techniques, even through it has same washcoat materials. The DOC coated by high temperature washcoat coating technology showed good conversion efficiency than low temperature washcoat coated DOC.

Mo-DTP와 Zn-DTP를 혼합 첨가한 엔진 오일의 마찰 마모특성에 관한 연구 (A Study on the Friction and Wear Characteristics Engine Oil with Mo-DTP and Zn-DTP)

  • 김종호;강석춘;정근우;조원오
    • Tribology and Lubricants
    • /
    • 제7권1호
    • /
    • pp.46-54
    • /
    • 1991
  • As the additives of engine oil, Mo-DTP and Zn-DTP were studied by experimental works. These additives were added to the engine oil with various ratios, which was an attempt to find out the best ratio at which the wear and friction can be reduced effectively; Mo-DTP is belived to be able to decrease the frictioh of the sliding metal, while Zn-DTP is known as a very stable additive for oxidation at high temperature in addition to the good antiwear property. This study showed that the optimum addition ratio of Mo-DTP and Zn-DTP is 3:2. This oil made it possible to slide steel with minimum wear and low friction over various lovels of load at moderate temperature. But as the oil temperature increased, the wear slid with Mo-DTP oil was increased more. The reason of this result was that Mo-DTP deteriorated the property of oil at high temperature by the higher oxidation and viscosity of Mo-DTP oil than that of Zn-DTP oil.