• Title/Summary/Keyword: Low Alloy

Search Result 1,547, Processing Time 0.028 seconds

High-temperature Oxidation Kinetics and Scales Formed on Fe-2.3%Cr-1.6%W Alloy (Fe-2.3%Cr-1.6%W 합금의 고온산화 부식속도와 스케일 분석)

  • Bak, Sang-Hwan;Kim, Min-Jung;Lee, Jae-Ho;Bong, Sung-June;Kim, Seul-Ki;Lee, Dong-Bok
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.1
    • /
    • pp.57-62
    • /
    • 2011
  • The T23 steel, whose composition was Fe-2.3%Cr-1.6%W, was arc-melted, and oxidized between $600^{\circ}C$ and $900^{\circ}C$ in air for up to 7 months. The amount of precipitates in the arc-melted microstructure was as large as 11.4 vol.%. The precipitates increased the oxidation rate of the arc-melted T23 steel. Owing to the low amount of Cr in the T23 steel, breakaway oxidation occurred after a few hours during oxidation above $700^{\circ}C$ in both arc-melted and as-received T23 steels. The scales that formed on arc-melted and as-received T23 steels were similar to each other. They consisted primarily of the outer $Fe_2O_3$ layer and the inner ($Fe_2O_3$, $FeCr_2O_4$)-mixed layer. The precipitates increased the microhardness and the oxidation rates.

Production of Ultra-fine Metal Powder with Gas Atomization Processes

  • Wang, M. R.
    • Journal of ILASS-Korea
    • /
    • v.11 no.2
    • /
    • pp.59-68
    • /
    • 2006
  • Experimental results of the metal powder production with internal mixing, internal impinging and the atomizer coupled with substrate design are presented in this paper. In a test with internal mixing atomizer, mean powder size was decreased from $37{\mu}m\;to\;23{\mu}m$ for Pb65Sn35 alloy as the gas-to-melt mass ratio was increased from 0.04 to 0.17. The particle size further reduces to $16.01{\mu}m$ as the orifice area is increased to $24mm^2$. The micrograph of the metal powder indicates that very fine and spherical metal powder has been produced by this process. In a test program using the internal impinging atomizers, the mean particle size of the metal powder was decreased from $22{\mu}m\;to\;12{\mu}m$ as the gas-to-melt-mass ratio increased from 0.05 to 0.22. The test results of an atomizer coupled with a substrate indicates that the deposition rate of the molten spray on the substrate is controlled by the diameter of the substrate, the height of the substrate ring and the distance of the substrate from the outlet of the atomizer. This in rum determines the powder production rate of the spraying processes. Experimental results indicate that the deposition rate of the spray forming material decreases as the distance between the substrate and the atomizer increases. For example, the deposition rate decreases from 48% to 19% as the substrate is placed at a distance from 20cm to 40cm. On the other hand, the metal powder production rate and its particle size increases as the subsrate is placed far away from the atomizer. The production of metal powder with mean particle size as low as $3.13{\mu}m$ has been achieved, a level which is not achievable by the conventional gas atomization processes.

  • PDF

Wafer-Level MEMS Capping Process using Electrodeposition of Ni Cap and Debonding with SnBi Solder Layer (Ni 캡의 전기도금 및 SnBi 솔더 Debonding을 이용한 웨이퍼 레벨 MEMS Capping 공정)

  • Choi, J.Y.;Lee, J.H.;Moon, J.T.;Oh, T.S.
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.16 no.4
    • /
    • pp.23-28
    • /
    • 2009
  • We investigated the wafer-level MEMS capping process for which cavity formation in Si wafer was not required. Ni caps were formed by electrodeposition on 4" Si wafer and Ni rims of the Ni caps were bonded to the Cu rims of bottom Si wafer by using epoxy. Then, top Si wafer was debonded from the Ni cap structures by using SnBi layer of low melting temperature. As-evaporated SnBi layer was composed of double layers of Bi and Sn due to the large difference in vapor pressures of Bi and Sn. With keeping the as-evaporated SnBi layer at $150^{\circ}C$ for more than 15 sec, SnBi alloy composed of eutectic phase and Bi-rich $\beta$ phase was formed by interdiffusion of Sn and Bi. Debonding between top Si wafer and Ni cap structures was accomplished by melting of the SnBi layer at $150^{\circ}C$.

  • PDF

A Study on Inter-leaf Transmission and Cross-leaf Transmission for Clinical Applications of the Multileaf Collimator (다엽 콜리메이터의 임상적용을 위한 엽측간 투과선량 및 엽종단간 투과선량 연구)

  • 이규찬;최진호
    • Progress in Medical Physics
    • /
    • v.15 no.1
    • /
    • pp.17-22
    • /
    • 2004
  • Multileaf collimator (MLC) is now rapidly replacing the lead ahoy block to shape the radiation treatment field. In addition to its defect of rectangular field shaping and increased penumbra width, it has another possible problem, and that is of radiation transmission between leaves, which needs to be maintained at as low a level as is permissible. The authors measured and analyzed the inter-leaf and cross-leaf transmissions of MLC by Varian Associates Inc, before its clinical application. The inter-leaf and cross-leaf transmissions were calculated by comparing the measured point doses in the polystyrene phantom in the open field and in a total closure of MLC. The beam profile of the inter-leaf and cross-leaf transmissions were depicted by using a water phantom. A photon beam of 6 MV was used in the measurement. The inter-leaf transmission was 1.63∼1.67%, indicating that the shielding effect of MLC is excellent. However, the cross-leaf transmission in the central area was 18.4∼18.7% and this is well over the clinically acceptable limitation of 5%. The beam profile of cross-leaf transmission displayed 80∼90% transmission near the field edge, so that the cross-leaf transmission was 14∼17% in this area. The multileaf collimator has an excellent shi디ding effect and the inter-leaf transmission is negligible so that it can be used in clinic as a good replacement of the conventional lead alloy block. However, care must be taken to avoid the cross-leaf transmission in the radiation field.

  • PDF

Magnetic Properties of FePt:C Nanocomposite Film

  • Ko, Hyun-Seok;A. Perumal;Shin, Sung-Chul
    • Proceedings of the Korean Magnestics Society Conference
    • /
    • 2003.06a
    • /
    • pp.220-221
    • /
    • 2003
  • Equiatomic FePt and CoPt alloy thin films have received considerable attention as possible magnetic and magneto-optic recording because of their high magnetic anisotropy energy and high coercivity. The high coercivity in these thin films is due to the presence of finely dispersed ordered FePt phase mixed with disordered FePt phase. However, a high temperature treatment, either substrate heating during deposition or post annealing, is needed to obtain the ordered L1$\_$0/ phase with high value of magneto crystalline anisotropy. Recent microstructural studies on these films suggest that the average grain size ranges from 10-50 nm and the grains are magnetically coupled between each other. On the other hand, the ultrahigh-density magnetic recording media with low media noise imposes the need of a material, which consists of magnetically isolated grains with size below 10 nm. The magnetic grain isolation can be controlled by the amount of additional non-magnetic element in the system which determines the interparticle separation and therefore the interparticle interactions. Recently, much research work has been done on various non-magnetic matrices. Preliminary studies showed that the samples prepared in B$_2$O$_3$ and Carbon matrices have shown strong perpendicular anisotropy and fine grain size down to 4nm, which suggest these nanocomposite films are very promising and may lead to the realization of a magnetic medium capable of recording densities beyond 1 Tb/in$^2$. So, in this work, the effect of Carbon doping on the magnetic properties of FePt nanoparticles were investigated.

  • PDF

A Study on Metal Hydride Electrode of Ni/MH Battery(I) (니켈/금속수소 축전지의 금속수소 전극에 관한 연구(I))

  • Kim, Jeong-Seon;Cho, Won-Il;Cho, Byung-Won;Yun, Kyung-Suk;Kim, Sang-Ju;Shin, Chee-Burm
    • Applied Chemistry for Engineering
    • /
    • v.5 no.1
    • /
    • pp.81-89
    • /
    • 1994
  • A study on Mm type electrode which is relatively high in electrode capacity and low in material cost was performed to develope high performance nickel-metal hydride battery. The electrode characteristics were investigated by P-C-T, charge-discharge and microencapsulation treatment experiments. The plateau pressure and hydrogen absorption capacity obtained from the P-C-T experiment were 0.4 atm and 310 mAh/g, respectively. The electrode capacity and stability of microencapsulated electrode were improved than those of conductor mixed electrode and the microencapsulation was possible without pretreatment. The electrode capacity of microencapsulated Mm type alloy was 240~250 mAh/g(0.2 C).

  • PDF

Ultrasonic Nonlinearity Measurement in Heat Treated SA508 Alloy: Influences of Grains and Precipitates (열처리된 SA508 합금에서의 초음파 비선형성 측정: 결정립과 석출물 영향)

  • Baek, Seung-Hyun;Lee, Tae-Hun;Kim, Chung-Seok;Jhang, Kyung-Young
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.30 no.5
    • /
    • pp.451-457
    • /
    • 2010
  • In the present study, the influences of grains and precipitates of microstructural evolution on the ultrasonic nonlinearity have been experimentally investigated. The prior-austenite grain and precipitate size are controlled by the variation in austenitizing and tempering conditions in reactor pressure vessel materials of nuclear power plant, SA508 Gr.3 low alloys. The ultrasonic nonlinearity was found to have strong correlations with grains and precipitates since the ultrasonic nonlinear parameter $\beta$ shows decrease trend with coarsening of grains and precipitates. Although the prior-austenite grain size increased, the $\beta$ changed little due to the effects of subgrains, packets and laths. For the preciptate effects, the $\beta$ decreased sharply due to decrease in $Mo_2C$ causing the coherency stain in addition to the precipitate size. The results in this study may provide a potential for characterizing the microstructural evolution, grains and precipitates, by measuring the ultrasonic nonlinearity.

Characteristics of Two-Step Plasma-Assisted Boronizing Process in an Atmosphere of BCl3-H2-Ar (BCl3-H2-Ar 분위기를 이용한 2단계 플라즈마 보로나이징 특성)

  • Nam, Kee-Seok;Lee, Gu-Hyun;Shin, Pyung-Woo;Song, Yo-Seung;Kim, Bae-Yeon;Lee, Deuk-Yong
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.6 s.289
    • /
    • pp.358-361
    • /
    • 2006
  • A two-step plasma-assisted boronizing process was carried out on the AISI 1045 steel substrate to reduce the pore density introduced by a conventional single plasma boronizing process. The specimens were plasma boronized for 1 h at $650^{\circ}C$ and subsequently far 7 h at $800^{\circ}C$ in an atmosphere of $BCl_3-H_2-Ar$. The boride layer thickness was parabolic in boronizing time, a high HV reading of 1540 was found up to the boride layer thickness of $25{\mu}m$. It was found that the morphology of the boride layer prepared by the two-step boronizing process was changed from a columnar to a tooth-like structure and the pores in the borided steel were eliminated completely in comparison to those synthesized by the conventional single boronizing process, implying that it is highly applicable for enhancing the dense and compact coating properties of the low-alloy steel.

Fabrication and Evaluations of Hydrogenation Properties of TiH2/TiH2-Al agents on Aluminum Foam Alloy (알루미늄 발포용 TiH2/TiH2-Al의 제조와 수소화 특성 평가)

  • Hong, T.-W.;Cho, G.-W.;Kweon, S.-Y.;Kim, I.-H.;Lee, J.-I.;Ur, S.-C.;Lee, Y.-G.;Ryu, S.-L.
    • Journal of Hydrogen and New Energy
    • /
    • v.15 no.3
    • /
    • pp.235-243
    • /
    • 2004
  • A number of potential applications of aluminum foams are being identified and renewed interest in these engineering materials is also reflected by several current research projects. One of the key issues for industrial exploitation of aluminum foams is the development of cost-effective manufacturing strategies facilitating, preferably, net shape production of foams with controlled porosity and cell size, and minimized structural imperfection. Especially, melt route to aluminum foam production based on the foaming agents offer attraction of low cost and the potential for good microstructure. The present paper is focused mainly on foaming agents of melt-foam aluminum such as $TiH_2$ or $TiH_2-Al$ mixture. For the purpose of economical manufacturing, we are proposed to hydrogen induced mechanical alloying (HIMA) process. Thermo-physical properties of particles synthesized are compared with conventional methods. Specimens synthesized are characterized by scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS), thermo- gravimetry-differential scanning calorymetry (TG-DSC), pressure-composition-isotherm. (PCI).

Effect of Melt-Spinning Process on Hydrogen Storage Properties of Mass-Produced Ti0.85Zr0.13(Fex-V)0.56Mn1.47Ni0.05 Alloy (대량용해 Ti0.85Zr0.13(Fex-V)0.56Mn1.47Ni0.05 수소저장합금의 용융방사공정을 통한 수소저장특성)

  • Kim, Jinho;Han, Kyusung
    • Journal of Hydrogen and New Energy
    • /
    • v.24 no.5
    • /
    • pp.367-372
    • /
    • 2013
  • Hydrogen storage as a metal hydride is the most promising alternative because of its relatively large hydrogen storage capacities near room temperature. TiMn2-based C14 Laves phases alloys are one of the promising hydrogen storage materials with easy activation, good hydriding-dehydriding kinetics, high hydrogen storage capacity and relatively low cost. In this work, multi-component, hyper-stoichiometric $Ti_{0.85}Zr_{0.13}(Fe_x-V)_{0.56}Mn_{1.47}Ni_{0.05}$ C14 Laves phase alloys were prepared by a vacuum induction melting for a hydrogen storage tank. Since pure vanadium (V) is quite expensive, the substitution of the V element in these alloys has been tried and some interesting results were achieved by replacing V by commercial ferrovanadium (FeV) raw material. In addition, the melt-spinning process, which was applied to the manufacturing of some of these alloys, could make the plateau slopes much flatter, which resulted in the increase of reversible hydrogen storage capacity. The improvement of sloping properties of melt-spun $Ti_{0.85}Zr_{0.13}(Fe_x-V)_{0.56}Mn_{1.47}Ni_{0.05}$ alloys was mainly attributed to the homogeneity of chemical composition.