• 제목/요약/키워드: Local strain

검색결과 643건 처리시간 0.02초

지역 평량이 지역 변형률에 미치는 영향 (The Effect of Local Basis Weight on Local Strain)

  • 남원석;백기현
    • 펄프종이기술
    • /
    • 제31권3호
    • /
    • pp.105-109
    • /
    • 1999
  • The purpose of this experiment was to see the effect of local basis weight on the local strain during changing moisture content in handsheets. The averaged strain value of the whole size of paper sheet did not give more valuable information to explain non uniform deformation in the paper sheet. The combination of intact strain measurement system KISA (Linear Image Strain Analysis) and local basis weight measurement method using a scanner made it possible to compare local basis weight with local strain to explain moisture induced paper deformation . Usually higher basis weight local area showed higher moisture induced local strain. However, the hygro-induced strain values were highly affected by the behavior of neighbor local areas. Well distributed local basis weight paper would give more uniform local strains than those of non-uniformed local basis weight paper.

  • PDF

국부 변형률 근사를 이용한 원통형 노치시편의 피로균열 발생수명의 예측 (The Prediction of Fatigue Crack Initiation Life of Cylindrical Notch Specimens Using Local Strain Approximation)

  • 임재용;홍성구;이순복
    • 대한기계학회논문집A
    • /
    • 제28권6호
    • /
    • pp.791-798
    • /
    • 2004
  • Fatigue crack initiation lives of round cylindrical notch specimen were investigated. Firstly, local strain approximation methods, such as the modified incremental Neuber's rule and the modified incremental Glinka's equivalent strain energy density(ESED) rule, were used to get multiaxial stress and strain state components at the notch tip. Based on the history of local stress and strain, multiaxial fatigue models were used to obtain fatigue crack initiation lives. Because the solution of Neuber's rule and Glinka's ESED rule make the upper and lower bound of local strain approximations, fatigue crack initiation lives are expected to place between life predictions by two local strain approximations. Experimental data were compared with the fatigue crack initiation life prediction results.

화상계측기법에 의한 전단압축파괴형 보의 국부변형률분포 추정 (Estimation of Local Strain Distribution of Shear-Compressive Failure Type Beam Using Digital Image Processing Technology)

  • 권용길;한상훈;홍기남
    • 콘크리트학회논문집
    • /
    • 제21권2호
    • /
    • pp.121-127
    • /
    • 2009
  • 연화재료의 변형률 국부화 거동에 따른 파괴영역과 파괴영역 내에서의 변형률 추이는 구조물의 극한거동에 큰 영향을 미치지만 파괴영역의 예측과 영역 내에서의 변형률을 정량화하는 것은 실험적으로 명확히 구명되어 있다고 보기 어렵다. 이 연구에서는 국부화된 파괴영역 및 그 영역 내에서의 변형률 분포 추이를 추정하기 위해 화상처리기법을 이용하였다. 화상처리기법의 신뢰성 및 타당성을 검증하기 위해, 일축압축공시체를 대상으로 화상처리기법을 이용하여 변형률을 추정하고, 이를 콘크리트 게이지로부터 취득한 변형률과 비교분석하였다. 분석 결과를 바탕으로 전단압축파괴형 보의 정적파괴실험에 화상처리기법을 적용하여 실험체의 거동에 따른 주인장변형률 및 주압축변형률의 분포도를 작성하였다. 마지막으로 작성된 분포도를 이용하여 국부화영역 및 국부변형률을 추정하였다. 실험 결과, 화상처리기법을 이용하여 취득한 파괴영역 내에서의 변형률 분포 추이는 비교적 정확히 실험체의 거동을 예측할 수 있었으며 손상 정도에 따라 비교적 합리적인 국부변형률값을 얻을 수 있었다.

인장하중을 받는 직선 배관 감육부의 국부 탄소성 변형률 평가 방법 (Estimation Method of Local Elastic-Plastic Strain at Thinning Area of Straight Pipe Under Tension Loading)

  • 안중혁;김윤재;윤기봉;마영화
    • 대한기계학회논문집A
    • /
    • 제30권5호
    • /
    • pp.533-542
    • /
    • 2006
  • In order to assess the integrity of pipes with local thinning area, the plastic strain as well as the elastic strain at the root of thinned region are required particularly when fluctuating load is applied to the pipe. For estimating elastic-plastic strain at local wall thinning area in a straight pipe under tensile load, an estimation model with idealized fully circumferential constant depth wall thinning area is proposed. Based on the compatibility and equilibrium equations a nonlinear estimation equation, from which local elastic-plastic strain can be determined as a function of pipe/defect geometry, material and the applied strain was derived. Estimation results are compared with those from detailed elastic-plastic finite element analysis, which shows good agreements. Noting that practical wall thinning in nuclear piping has not only a circular shape but also a finite circumferential length, the proposed solution for the ideal geometry is extended based on two-dimensional and three-dimensional numerical analysis of pipes with circular wall thinning.

Local ratcheting behavior in notched 1045 steel plates

  • Kolasangiani, K.;Farhangdoost, K.;Shariati, M.;Varvani-Farahani, A.
    • Steel and Composite Structures
    • /
    • 제28권1호
    • /
    • pp.1-11
    • /
    • 2018
  • In this paper, local ratcheting behavior of 1045 steel plates with circular cutout was investigated. Experimental tests were carried out by a Zwick/Roell HB 100 servo hydraulic machine. In order to measure the local strain at notch root, a data acquisition system with strain gauge was used. Various notch diameters and distances of strain gauges mounted from the notch root were found influential in the magnitude of local ratcheting strain. It was found that the local maximum principal stress plays a crucial role in increasing the local plastic deformation. Numerical simulation was done by ABAQUS software using nonlinear isotropic/kinematic hardening model. Material parameters of hardening model were attained from several stabilized cycles of flat specimens subjected to symmetric strain cycles. The nonlinear kinematic hardening model along with the Neuber's rule was employed to assess local ratcheting at the notch root of steel plates. The results of the numerical simulations agreed closely with those measured values in this study. Both ratcheting progress and mean stress relaxation occurred simultaneously at the notch root.

국부변형률방법을 이용한 용접시험편의 피로수명 해석 (Fatigue Life Analysis of Butt-welded specimen by Local Strain Approach)

  • 이동형;서정원;구병춘;석창성
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2003년도 추계학술대회 논문집(III)
    • /
    • pp.73-78
    • /
    • 2003
  • The residual stresses and. distortions of structures by welding exert negative effect on the safety of railroad structures. This investigation performs a thermal elasto-plastic analysis using finite element techniques to evaluate residual stresses in butted-welded joint. Considering this initial residual stresses, local stress and strain at the critical location (weld toe) during the loading were analyzed by elastic plastic finite element analysis. Fatigue crack initiation life and fatigue crack propagation life of butt-welded specimen were predicted by local strain approach and Neuber's role and Paris law. It is demonstrated that fatigue life estimates by local strain approach closely approximate the experimental results.

  • PDF

금속 재료의 피로 균열 전파 속도(da/dN) 평가를 위한 변형율 확대 계수의 유효성 검토 (Evaluation of Fatigue Strain Intensity Factor on Fatigue Crack Propagation Rate (da/dN))

  • 유재환;최재강;손종동
    • 한국안전학회지
    • /
    • 제11권2호
    • /
    • pp.3-8
    • /
    • 1996
  • Fatigue fracture is the cyclic fracture phenomena at a very small local area near a crack tip. Therefore, the detailed quantitative experimental analysis about local cyclic strain distribution near a crack tip is prerequisite In order to make an effective parameter able to account for fatigue fracture problems. However, there are few reports on detailed quantitative experimental analysis of a local cyclic strain distribution near a crack tip, because of experimental difficulties. In this study, the distribution of local fatigue strains near a fatigue crack tip was in detail studied using by fine dot grid strain measurement method. From these results, a single parameter, which characterizes local fatigue strain field, was proposed. In addition, this parameter was applied to evaluate the fatigue crack propagation rate.

  • PDF

압축파괴에너지를 도입한 횡구속 고강도 콘크리트의 응력-변형률 모델 (Stress-strain Model of Laterally Confined High-strength Concrete with the Compressive Fracture Energy)

  • 홍기남;심원보
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제23권1호
    • /
    • pp.54-62
    • /
    • 2019
  • 본 논문에서는 압축파괴에너지를 이용하여 고강도 구속콘크리트에 대한 응력-변형률 모델을 제안하였다. 참고문헌[5]에서 저자가 실시한 압축실험에는 변형률 게이지를 부착한 아크릴 막대를 실험체의 중앙부에 매립하여 압축부재의 국부 변형률 측정을 시도하였다. 이 아크릴 막대를 이용한 국부 변형률 측정은 매우 효과적인 것으로 나타났다. 압축파괴영역길이는 아크릴 막대로부터 측정된 국부 변형률 분포에 기초하여 정의되었다. 구체적으로, 구속콘크리트의 국소파괴영역길이는 압축강도 발현시의 변형률 ${\varepsilon}_{cc}$의 2배 이상 변형률이 증가하는 영역으로 정의하였다. 또한, 동일한 횡구속압을 받는 압축부재에 흡수된 에너지양은 부재의 형상이나 크기에 관계없이 일정하다는 가정에서 압축 파괴에너지를 도입한 구속콘크리트의 응력-변형률 관계를 제안하였다. 본 연구에서 제안된 모델은 본 연구의 실험결과뿐만 아니라 타 연구자들의 실험결과를 대체적으로 잘 예측하는 것으로 나타났다.

국부적 변형 집중 저감을 통한 액압 성형성 개선연구 (Enhancement of Hydroformability Through the Reduction of the Local Strain Concentration)

  • 신세계로;주병돈;문영훈
    • 소성∙가공
    • /
    • 제23권5호
    • /
    • pp.317-322
    • /
    • 2014
  • Bursting during tube hydroforming is preceded by localized necking. The retardation of the initiation of necking is a means to enhance hydroformability. Since high strain gradients occur at the necking sites, a decrease in local strain gradients is an effective way to retard the initiation of necking. In the current study, the expansion at potential necking sites was intentionally restricted in order to reduce the strain gradient at potential necking sites. From the strain distribution obtained from FEM, it is possible to determine strain concentrated zones, which are the potential necking sites. Prior to the hydroforming of a trailing arm, an incompressible material(such as lead) is attached to the tube where the strain-concentrated zone would contact the die. Due to the incompressibility of lead, the tube expansion is locally restricted, and the resultant strain extends to adjacent regions of the tube during hydroforming. After the first stage of hydroforming, the lead is removed from the tube, and the hydroforming continues to the final targeted shape without any local restriction. This method was successfully used to fabricate a complex shaped automotive trailing arm that had previously failed during traditional hydroforming fabrication.

微小圓形格子變形率 測定法을 利용한 龜裂先端의 局所疲勞變形率分布 (The Local Fatigue Strain Distribution Near a Crack Tip by Using Fine Dot Grid Strain Measurement Method)

  • 박영철;오세욱;김광영
    • 대한기계학회논문집
    • /
    • 제15권1호
    • /
    • pp.209-217
    • /
    • 1991
  • 본 연구에서는 이러한 제반 문제점들을 보완하여 피로균열 선단의 국소영역에 서의 변형율상태를 실시간적으로 정도 높게 측정할 수 있는 새로운 변형율측정법인 미 소원형격자변형율측정법(fine dot grid strain measurement method)을 이용하였다. 그 결과, 균열선단의 국소영역에서의 피로변형율상태를 명확히 밝혀냄은 물론 이를 기 초로 하여 국소피로변형율장을 대표할 수 있는 피로변형율확대계수 .DELTA.A를 제안하였으 며 그 유효성에 대하여 명백히 하였다.