Experimental Investigation of Porous Bearings Under Different Lubricant and Lubricating Conditions

  • Durak, Ertugrul
    • Journal of Mechanical Science and Technology
    • /
    • v.17 no.9
    • /
    • pp.1276-1286
    • /
    • 2003
  • The performance of porous bearing under different lubricants and lubricating conditions was experimentally investigated in this study. In order to carry out the experiments, a new test rig was designed to determine the tribological properties of based sintered bronze journal bearings that were manufactured by powder metallurgy (P/M) techniques. To determine the effects of lubricating conditions with and without oil supplement (OS) on the tribological characteristics of these bearings under static loading and periodic loadings, some experiments were carried out using different lubricants. In the tests, pure base oil (SAE 20W50), two fully formulated commercial engine oils (SAE20W50) and lubricating oils with commercial additive concentration ratio of 3% were used. The worn surfaces of test bearings were examined using optical microscopy. Experimental results showed that the change in friction coefficient was more stable and in smaller magnitude under static loading than that of periodic loading. In addition, the friction coefficient and the wear rate conducted with base oil resulted in higher values than those of fully formulated oils with and without OS lubricating conditions. The experimental results obtained in this study indicated that the correct selection of lubricant and suitable running conditions were very important on the tribological characteristics of porous bearings.

Fatigue Crack Growth Characteristics of the Pressure Vessel Steel SA 508 Cl. 3 in Various Environments

  • Lee, S. G.;Kim, I. S.;Park, Y. S.;Kim, J. W.;Park, C. Y.
    • Nuclear Engineering and Technology
    • /
    • v.33 no.5
    • /
    • pp.526-538
    • /
    • 2001
  • Fatigue tests in air and in room temperature water were performed to obtain comparable data and stable crack measuring conditions. In air environment, fatigue crack growth rate was increased with increasing temperature due to an increase in crack tip oxidation rate. In room temperature water, the fatigue crack growth rate was faster than in air and crack path varied on loading conditions. In simulated light water reactor (LWR) conditions, there was little environmental effect on the fatigue crack growth rate (FCGR) at low dissolved oxygen or at high loading frequency conditions. While the FCGR was enhanced at high oxygen condition, and the enhancement of crack growth rate increased as loading frequency decreased to a critical value. In fractography, environmentally assisted cracks, such as semi-cleavage and secondary intergranular crack, were found near sulfide inclusions only at high dissolved oxygen and low loading frequency condition. The high crack growth rate was related to environmentally assisted crack. These results indicated that environmentally assisted crack could be formed by the Electrochemical effect in specific loading condition.

  • PDF

PIV Measurements of Hull Wake behind a Container Ship Model with Varying Loading Condition and Reynolds number (선박 모형의 하중 (loading)조건 및 Reynolds 수의 변화에 따른 선미 반류의 PIV 속도장 측정)

  • Lee Jung-Yeop;Paik Bu-Geun;Lee Sang-Joon
    • 한국가시화정보학회:학술대회논문집
    • /
    • 2005.12a
    • /
    • pp.54-57
    • /
    • 2005
  • Flow characteristics of hull wake behind a container ship model were investigated experimentally with varying loading condition and Reynolds number. Large-scale bilge vortices of nearly the same strength are formed in the near-wake region. They are symmetric and counter-rotating with respect to the wake centerline for all loading conditions tested. With going downstream for both design and ballast loading conditions, the strength of the bilge vortices decreases and the wake region expands due to diffusion and viscous dissipation. Under the design loading condition, the bilge vortices start to appear at St=0.363 transverse plane above the propeller-boss. For the ballast loading condition, however, the bilge vortices start to appear at St=0.591 below the propeller-boss. They move upward as the hull wake goes downstream and Reynolds number increases. These wake characteristics, under the ballast loading condition, may weaken the propulsion and cavitation performances of the propeller, which are usually optimized for the design loading condition.

  • PDF

Experimental study of rockburst under true-triaxial gradient loading conditions

  • Liu, Xiqi;Xia, Yuanyou;Lin, Manqing;Benzerzour, Mahfoud
    • Geomechanics and Engineering
    • /
    • v.18 no.5
    • /
    • pp.481-492
    • /
    • 2019
  • Due to the underground openings, the tangentially concentrated stress of the tunnel remains larger at excavation boundary and decreases toward the interior of the surrounding rock with a certain gradient. In order to study the effect of different gradient stress on rockburst, the true-triaxial gradient and hydraulic-pneumatic combined test apparatus were carried out to simulate the rockburst processes. Under the different gradient stress conditions, the rock-like specimen (gypsum) was tested independently through three principal stress directions loading--fast unloading of single surface--top gradient and hydraulic-pneumatic combined loading, which systematically analyzed the macro-mesoscopic damage phenomena, force characteristics and acoustic emission (AE) signals of the specimen during rockburst. The experimental results indicated that the rockburst test under the gradient and hydraulic-pneumatic combined loading conditions could perfectly reflect the rockburst processes and their stress characteristics; Relatively high stress loading could cause specimen failure, but could not determine its mode. The rockburst under the action of gradient stress suggested that the failure mode of specimen mainly depended on the stress gradient. When the stress gradient was lower, progressive and static spalling failure occured and the rockburst grades were relatively slight. On the other hand, shear fractures occurred in rockbursts accounted for increasingly large proportion as the stress gradient increased and the rockburst occurred more intensely and suddenly, the progressive failure process became unconspicuous, and the rockburst grades were moderate or even stronger.

Characteristics of Pressure Confined Concrete under Monotonic Compression

  • Rhim, Hong-Chul;Buyukozturk, Oral;Soon, K. A;Kim, Gwang-Ho
    • KCI Concrete Journal
    • /
    • v.13 no.1
    • /
    • pp.53-60
    • /
    • 2001
  • Tests of cylindrical concrete specimens under lateral confining pressure of up to 5,000 psi were conducted for two different axial loading cases: monotonic compression and monotonic tension. The purpose of this experimental investigation is to provide stress-strain characteristics of plain concrete in triaxial stress conditions. Lateral confining pressure levels, loading rates, and strength of concrete specimens are varied as parameters. The loading rates are $34.75$\times$10^{-5}$ in/in/sec for fast, $\times$$6.95x10^{-5}$ in/in/sec for normal. and $0.579$\times$10^{-5}$ in/in/sec for slow loading cases. The concrete specimens used in the experiment have compressive strength of 3,500 psi and 6,500 psi, respectively. Findings of this experiment include dependency of the stress-strain behavior of concrete on the above parameters under two different types of loading conditions. The parametric study includes a series of 106 triaxial tests.

  • PDF

Transient heat transfer analysis using Galerkin finite element method for reinforced concrete slab exposed to high elevated temperature

  • Han, Byung-Chan;Kwon, Young-Jin;Lee, Byung-Jae;Kwon, Seung-Jun;Chae, Young-Suk
    • Computers and Concrete
    • /
    • v.18 no.6
    • /
    • pp.1097-1112
    • /
    • 2016
  • Fire loading causes a critical collapse of RC (Reinforced Concrete) Structures since the embedded steels inside are relative week against high elevated temperature. Several numerical frameworks for fire resistance have been proposed, however they have limitations such as unstable convergence and long calculation period. In the work, 2-D nonlinear FE technique is proposed using Galerkin method for RC structures under fire loading. Closed-form element stiffness with a triangular element is adopted and verified with fire test on three RC slabs with different fire loading conditions. Several simulations are also performed considering fire loading conditions, water contents, and cover depth. The proposed numerical technique can handle time-dependent fire loading, convection, radiation, and material properties. The proposed technique can be improved through early-aged concrete behavior like moisture transport which varies with external temperature.

Wheel Off-loading test procedure and result (단차 상태 차량 윤중 감소율 시험 절차 및 결과)

  • 김진태;이원상
    • Proceedings of the KSR Conference
    • /
    • 2002.10b
    • /
    • pp.857-862
    • /
    • 2002
  • The bogie, when run on the twist track develops the wheel off-loading factor. This will be comfirmed by testing under different loading conditions and air springs inflated and deflated in all conditions. Under the most extreme twist track condition, EMU (Electrical Multiple Unit) shall not over the wheel off-loading requirement 60% defined on UIC / ORE report. This paper describes the wheel off-loading test procedure according to UIC / ORE and test result of DMRC EMU of INDIA carried out to find out to meet the requirement defined in UIC / ORE.

  • PDF

Dynamic Compressive Deformation Characteristics of Free-Cutting Brass And Yellow Brass at High Strain Rates (고변형률 압축 하중에서 쾌삭 황동과 황동의 동적 변형 거동 특성)

  • Lee, Ouk-Sub;Kim, Kyoung-Joon;Lee, Jong-Won
    • Proceedings of the KSME Conference
    • /
    • 2003.04a
    • /
    • pp.107-112
    • /
    • 2003
  • Mechanical properties of the materials used for transportations and industrial machinery under high strain rate loading conditions such as high impact loading are required to provide appropriate safety assessment to varying dynamically loaded mechanical structures. The Split Hopkinson Pressure Bar(SHPB) technique with a special experimental apparatus can be used to obtain the material behavior under high strain rate loading conditions. In this paper, the dynamic deformation behavior of a brass under both high strain rate compressive loading conditions has been determined using the SHPB technique.

  • PDF

Simplified approach for the evaluation of critical stresses in concrete pavement

  • Vishwakarma, Rameshwar J.;Ingle, Ramakant K.
    • Structural Engineering and Mechanics
    • /
    • v.61 no.3
    • /
    • pp.389-396
    • /
    • 2017
  • Concrete pavements are subjected to traffic and environmental loadings. Repetitive type of such loading cause fatigue distress which leads to failure by forming cracks in pavement. Fatigue life of concrete pavement is calculated from the stress ratio (i.e. the ratio of applied flexural stress to the flexural strength of concrete). For the correct estimation of fatigue life, it is necessary to determine the maximum flexural tensile stress developed for practical loading conditions. Portland cement association PCA (1984) and Indian road congress IRC 58 (2015) has given charts and tables to determine maximum edge stresses for particular loading and subgrade conditions. It is difficult to determine maximum stresses for intermediate loading and subgrade conditions. The main purpose of this study is to simplify the analysis of rigid pavement without compromising the accuracy. Equations proposed for determination of maximum flexural tensile stress of pavement are verified by finite element analysis.

Liquefaction Behaviour of Saturated Silty Sand Under Monotonic Loading Conditions (정적하중 상태에서 포화된 실트질 모래의 액상화 거동)

  • Lee Dal-Won
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.48 no.4
    • /
    • pp.67-74
    • /
    • 2006
  • This study was carried out to investigate the liquefaction behaviour of saturated silty sand under monotonic loading conditions. The undrained soil tests were conducted using a modified triaxial cell and specimens were prepared using the moisture tamping method. Undrained triaxial compression tests were performed at different confining pressures, void ratios and overconsolidation ratios and the samples were sheared to axial strains of about 20% to obtain monotonic loading conditions. It is shown that increasing confining pressures, void ratios and overconsoildation ratios increases the deviator stress, but it has no effect on increasing the dilatant tendencies. It is shown that complete static liquefaction was observed regardless of increases in the confining pressure, void ratio and overconsolidation ratio. Therefore, the confining pressure, void ratio and overconsoildation ratio does not provide significant effects on the liquefaction resistance of the silty sand. The presence of fines in the soil was shown to greatly increase the potential for static liquefaction and creates a particle structure with high compressibility for all cases.