• Title/Summary/Keyword: Lead Ions

Search Result 232, Processing Time 0.033 seconds

Investigation on optimum protection potential of high-strength Al alloy(5456-H116) for application in ships (선박용 고강도 Al합금(5456-H116)의 최적 방식 전위결정에 관한 연구)

  • Kim Sung-Jong;Ko Jae-Yong
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.30 no.1
    • /
    • pp.157-168
    • /
    • 2006
  • Recently, interest in using Al alloys in ship construction instead of fiber-reinforced plastic (FRP) has increased because of the advantages of A) alloy ships over FRP ships, including high speed, increased load capacity. and ease of recycling. This paper investigated the mechanical and electrochemical properties of Al alloys in a slow strain rate test under various potential conditions. These results will provide reference data for ship design by determining the optimum protection potential regarding hydrogen embrittlement and stress corrosion cracking. In general, Al and Al alloys do not corrode on formation of a film that has resistance to corrosion in neutral solutions. In seawater, however, $Cl^-$ ions lead to the formation and destruction of a Passive film. In a potentiostatic experiment. the current density after 1200 sec in the Potential range of $-0.68\~-1.5\;V$ was low. This low current density indicates the protection potential range. Elongation at an applied potential of 0 V was high in this SSRT. However, corrosion protection under these conditions is impossible because the mechanical properties are worse owing to decreased strength resulting from the active dissolution reaction in parallel parts of the specimen. A film composed of $CaCO_3\;and\;Mg(OH)_2$ confers corrosion resistance. However, at potentials below -1.6 V forms non-uniform electrodeposition coating, since there is too little time to form a coating. Therefore, we concluded that the mechanical properties are poor because the effect of hydrogen gas generation exceeds that of electrodeposition. Comparison of the maximum tensile strength, elongation, and time to fracture indicated that the optimum protection potential range was from -1.45 to -0.9 V (SSCE).

Heavy Metal Contamination in Surface Water Used for Irrigation: Functional Assessment of the Turag River in Bangladesh

  • Arefin, M. Taufique;Rahman, M. Mokhlesur;Wahid-U-Zzaman, M.;Kim, Jang-Eok
    • Journal of Applied Biological Chemistry
    • /
    • v.59 no.1
    • /
    • pp.83-90
    • /
    • 2016
  • The aim of the present study was to evaluate the degree of metal contamination of the Turag River water and its suitability for irrigation. Twenty water samples were analyzed for physicochemical parameters and metals viz., calcium, magnesium, potassium (K), sodium, copper (Cu), zinc (Zn), iron (Fe), manganese (Mn), lead (Pb), cadmium (Cd), chromium (Cr), and nickel (Ni). All water samples were slightly alkaline to alkaline. Regarding electrical conductivity (EC), all samples were suitable for crop in soils with moderate permeability and leaching. Water samples were medium salinity and low alkalinity hazard classes. In terms of total dissolved solids (TDS), all samples were classified as freshwater. As per sodium adsorption ratio (SAR) and soluble sodium percentage (SSP), all samples were classified as excellent. No residual sodium carbonate (RSC) was detected in any of the samples, indicating suitability for irrigation; and all samples were considered very hard. Cr and Mn contents in all samples were above FAO guideline values and, therefore, these metals were considered toxic. Zn, Cu, Pb, Cd, and Ni concentrations were below acceptable limit for irrigation and do not pose a threat to soil environment. Significant relationships were found between EC and TDS, SAR and SSP, SAR and RSC, and SSP and RSC. The combinations of ions such as K-Zn, K-Fe, K-Cu, K-Mn, K-Pb, Zn-Fe, Zn-Cu, Zn-Mn, Fe-Mn, Cu-Mn, Cu-Pb and Mn-Pb exhibited significant correlation. This study revealed that Turag River water samples are contaminated with Cr and Mn. This fact should not be ignored because water contamination by metals may pose a threat to human health through food chain.

Analysis of Arsenic(III) by the Cathodic Stripping Voltammetry (음극 벗김 전류법을 이용한 비소(III) 분석에 관한 연구)

  • Yun, Young Ja;Lee, Hyung Sook;Ko, Weon Bae;Kim, Chung Hee
    • Analytical Science and Technology
    • /
    • v.5 no.4
    • /
    • pp.417-423
    • /
    • 1992
  • The effects of metal ions on the arsenic(III) stripping peak were examined by the cathodic stripping voltammetry. The reduction stripping peak potential and current of arsenic(III) value were -0.79V(vs. Ag/AgCl). $0.86{\mu}A$ by using 0.1N-hydrochloric acid solution. When 10 times of Cu(II) was added to the solution, the reduction stripping peak potential of arsenic(III) was the value of -0.84V(vs. Ag/Cl), which showed a good agreement with theoretical value -0.84V(vs. Ag/Cl) by using 0.1N hydrochloric acid solution. Lead(II) and copper(II) increased the stripping peak heigh of arsenic(III), Among them, the copper(II) extremely enhanced it.

  • PDF

A study on reduction of excess sludge in activated sludge system from a petrochemical plant using electro fenton process (전기펜톤공정을 이용한 석유화학공장 폐활성슬러지의 감량화 가능성 평가)

  • Chung, Chong Min;Kim, Kyung Il;Shim, Natalia;Park, Chul Hee;Lee, Sang Hyup
    • Journal of Korean Society of Water and Wastewater
    • /
    • v.23 no.5
    • /
    • pp.669-678
    • /
    • 2009
  • The reduction of excess activated sludge from petrochemical plant was investigated by the electro fenton (E-Fenton) process using electrogenerated hydroxyl radicals which lead to mineralization of activated sludge to $CO_2$, water and inorganic ions. Factors affecting the disintegration efficiency of excess activated sludge in E-Fenton process were examined in terms of five criteria: pH, $H_2O_2/Fe^{2+}$ molar ratio, current density, initial MLSS (mixed liquid suspended solids) concentration, $H_2O_2$ feeding mode. TSS total suspended solid and $TCOD_{cr}$ reduction rate increased with the increasing $H_2O_2/Fe^{2+}$ molar ratio and current density until 42 and $6.7 mA/cm^2$, respectively but further increase of $H_2O_2/Fe^{2+}$ molar ratio and current density would reduce the reduction rate. On the other hand, as expected, increasing pH and initial MLSS concentration of activated sludge decreas TSS and $TCOD_{cr}$ reduction rate. The E-Fenton process was gradually increased during first 30 minutes and then linearly proceed till 120 minutes. The optimal E-Fenton condition showed TSS reduction rate of 62~63% and $TCOD_{cr}$ (total chemical oxygen demand) reduction rate of 55~56%. Molar ratio $H_2O_2/Fe^{2+} = 42$ was determined as optimal E-Fenton condition with initial $Fe^{2+}$ dose of 5.4 mM and current density of $6.7{\sim}13.3 mA/cm^2$, initial MLSS of 7,600 mg/L and pH 2 were chosen as the most efficient E-Fenton condition.

Voltammetric Determination of Copper(II) Using Glassy Carbon Electrodes Modified with Nafion-DTPA-Glycerol

  • Park, Chan-Ju;Park, Eun-Heui;Chung, Keun-Ho
    • Proceedings of the Korean Environmental Health Society Conference
    • /
    • 2003.06a
    • /
    • pp.177-180
    • /
    • 2003
  • A glassy carbon electrode(GCE) modified with nafion-DTPA-glycerol was used for the highly selective and sensitive determination of a trace amount of Cu$\^$2+/. Various experimental parameters, which influenced the response of nafion-DTPA-glycerol modified electrode to Cu$\^$2+/, were optimized. The copper(II) was accumulated on the electrode surface by the formation of the complex in an open circuit, and the resulting surface was characterized by medium exchange, electrochemical reduction, and differential pulse voltammetry, A linear range was obtained in the concentration range 1.0${\times}$10$\^$-8/M∼1.0${\times}$10$\^$-6/M Cu(II) with 7 min preconcentration. Further, when an approximate amount of lead(II) is added to the test solution, nafion-DTPA-glycerol modified glassy carbon electrode has a dynamic range of 2 orders magnitude(1.0${\times}$10$\^$-9/M∼1.0${\times}$10$\^$-7/M). The detection limit(3 $\sigma$) was as low as 5.0${\times}$10$\^$-6/M(0.032ppb). The interferences from other metal ions could be reduced by adding KCN into the sample solutions. This method was applied to the determination of coppe,(II) in certified reference material(3.23${\times}$10$\^$-7/M, 21ppb), sea water(9.50${\times}$10/sup-7/M, 60ppb). The result agrees satisfactorily with the value measured by Korea Research Institute of Standard and Science.

  • PDF

QTL analysis of for micronutrient content in rice grain

  • Lee, Hyun-Sook;Shim, Kyu-Chan;Jeon, Yun-A;Ahn, Sang-Nag
    • Proceedings of the Korean Society of Crop Science Conference
    • /
    • 2017.06a
    • /
    • pp.144-144
    • /
    • 2017
  • Micronutrients such as zinc (Zn), iron (Fe), manganese (Mn) have important roles for development and growth in plants but it also have roles in animals and humans. In previous studies, a Korean weedy rice, KH2J was selected to have tolerance to heavy metal, lead (Pb) compared with a cultivar, Milyang23. To identify QTLs for micronutrients concentration in grain, an F2 population (120 plants) were developed from a cross between KH2J and an indica rice cultivar, Milyang23. To measure the concentration of eight ions, Zn, Fe, Mn, Pb, calcium (Ca), copper (Cu), cadmium (Cd) and arsenic (As), grains were collected and digested with 65% nitric acid, and the ion contents were measured using inductively coupled plasma mass spectrometry. A total 27 putative quantitative trait loci (QTLs) were detected on 12 chromosomes by single point analysis and 22 putative QTLs were detected by composite interval mapping. The co-locations of QTL for Zn, Fe and Mn were observed on chromosome 5. The QTLs for Cd, Cu and Zn were co-localized on chromosome 10, and QTLs for Zn, As and Mn was on chromosome 12. The Zn concentration in F2 generation showed significant correlation with concentrations of As (r = -0.4), Cu (r = 0.5) and Fe (r = 0.2) (P < 0.01). Also, the Ca concentration was significantly related with Mn and Fe concentrations (P < 0.01). Fine mapping of these QTLs is underway to analyze their functional relationship.

  • PDF

Surface Safety Characteristics of Polypropylene Surface Treatment by Variation of Rolling Speed and The Electric Power of Corona Discharge (코로나방전 표면 처리시 이동속도 및 공급전력 변화에 따른 폴리프로필렌 표면 안전성 특성)

  • Lee, Su Hwan;Lee, Dong Hoon
    • Journal of the Korean Society of Safety
    • /
    • v.33 no.1
    • /
    • pp.41-46
    • /
    • 2018
  • Experiments were carried out the phenomenal observation on effect of corona treated hotmelt laminating film in process of manufacture by 2 kinds of rolling speed and electric power variatons. Surface treatment by corona which is exposure of film surface to electron of ion bombardment, rather than mere exposure to active species, like atomic oxygen or ozone, can enhance adhesion by removing contaminant, electret, roughening surface, and introducing reactive chemical group. Reactive neutrals, ions, electron and photons generated during the corona treatment interact simultaneously with polymers to alter surface chemical composition, wettability, and thus film adhesion. However, it is highly recommended that extensive chains scission is avoided because it can lead to side-effect by forming sticky matter, resulting in dropouts. This paper reviews principles of surface preparation of polypropylene substrate by corona discharging. In addition, the experimental section provides a description of parameter optimization on corona discharging treatment and its side-effect. Experimental results are discussed in terms of surface wetting as determined by contact angle and SEM measurements. When the rolling speed of the film decreased from 1.666 [m / sec] to 0.083 [m / sec], contact angle decreased from $80[^{\circ}]$ to $64[^{\circ}]$, and the wettability was greatly improved. As the supply power increased from 0.4 [kVA] to 2 [kVA] at the corona discharge surface treatment, the contact angle decreased from $77[^{\circ}]$ to $65[^{\circ}]$, and the wettability was greatly improved.

Sapphire Enhancement with BeO Powder Source (BeO를 확산원으로 한 사파이어의 향상처리)

  • Song, Oh-Sung;Kim, Sang-Yeop
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.6 no.2
    • /
    • pp.105-109
    • /
    • 2005
  • We heat treated pure sapphire samples at $1800^{\circ}C{\sim}100$ hours in BeO-${Al_2}{O_3}$ powder by varying BeO contents of $5{\sim}50\;wt%$ in order to quantify the BeO diffusion enhancement for corundum gem stones. We investigated the heat treated samples with visual evaluation, color coordination analysis, and surface roughness measurement. We confirmed that $Be^{2+}$ ions did not lead to orange color but to dark gray. The lightness in CIE Lab index decreased while surface roughness increased rapidly as BeO contents increased. We propose that BeO yellow color enhancement may be feasible only for $Fe^{3+}$ rich blue sapphires and sub-5% BeO content be appropriate to shorten post re- cutting process.

  • PDF

Adsorption of Uranium (VI) Ion on Synthetic Resin Adsorbent with Styrene Hazardous Materials (Styrene 위험물을 포함한 합성수지 흡착제에 의한 우라늄(VI) 이온의 흡착)

  • Kim, Joon-Tae
    • Applied Chemistry for Engineering
    • /
    • v.20 no.2
    • /
    • pp.165-171
    • /
    • 2009
  • Resins were synthesized by mixing 1-aza-15-crown-5 macrocyclic ligand attached to styrene (2th petroleum in 4th class hazardous materials) and divinylbenzene (DVB) copolymer with crosslinkage of 1%, 2%, 8%, and 16% by substitution reaction. The characteristic of these resins was confirmed by content of chlorine, element analysis, thermogravimetric analysis (TGA), surface area (BET), and IR-spectroscopy. The effects of pH, time, dielectric constant of solvent and crosslinkage on adsorption of metal ion by the synthetic resin adsorbent were investigated. The metal ion showed a fast adsorption on the resins above pH 3. The optimum equilibrium time for adsorption of metallic ions was about two hours. The adsorption selectivity determined in ethanol was in an increasing order of uranium $(UO_2^{2+})$ > lead $(Pb^{2+})$ > chromium $(Cr^{3+})$ ion. The adsorption was in the order of 1%, 2%, 8%, and 16% crosslinkage resin and adsorption of resin decreased in proportion to the order of dielectric constant of solvents.

Haloperidol Induces Calcium Ion Influx Via L-Type Calcium Channels in Hippocampal HN33 Cells and Renders the Neurons More Susceptible to Oxidative Stress

  • Kim, Hyeon Soo;Yumkham, Sanatombi;Choi, Jang Hyun;Kim, Eung-Kyun;Kim, Yong Sik;Ryu, Sung Ho;Suh, Pann-Ghill
    • Molecules and Cells
    • /
    • v.22 no.1
    • /
    • pp.51-57
    • /
    • 2006
  • Haloperidol is a classical neuroleptic drug that is still in clinical use and can lead to abnormal motor activity following repeated administration. However, there is little knowledge of how it triggers neuronal impairment. In this study, we report that it induced calcium ion influx via L-type calcium channels and that the elevation of calcium ions induced by haloperidol appeared to render hippocampal cells more susceptible to oxidative stress. Indeed, the level of cytotoxic reactive oxygen species (ROS) and the expression of pro-apoptotic Bax increased in response to oxidative stress in haloperidol-treated cells, and these effects were inhibited by verapamil, a specific L-type calcium channel blocker, but not by the T-type calcium channel blocker, mibefradil. These findings indicate that haloperidol induces calcium ion influx via L-type calcium channels and that this calcium influx influences neuronal fate.