• 제목/요약/키워드: LCF

검색결과 76건 처리시간 0.034초

변형률제어 비대칭파형 하의 고온피로수명 및 파면 (High Temperature Fatigue Life and Fractography under Asymmetric Waveform in Strain Control)

  • 허정원;박원조;유재환
    • 한국안전학회지
    • /
    • 제18권1호
    • /
    • pp.38-43
    • /
    • 2003
  • In this paper, the low cycle fatigue(LCF) life tests were carried out under waveforms of asymmetric triangle($4{\times}10^{-3}$ and $4{\times}10^{-10}$ strain rate) and hold-time(1min and 10min) in strain control. In triangular waveform, the fatigue lives of fast-slow waveforms were decreased to about 63-73% and them of slow-fast waveforms were down to about 23-24% compared to them of fast-fast waveforms. The shapes of fracture surfaces were transgranular in fast-fast and fast-slow waveforms and intergranular in slow-fast ones. The fatigue lives of slow-fast waveforms were remarkedly shorter than them of hold-time waveforms even though cycle times of hold time waveforms were longer than them of slow-fast ones. The damage mechanisms of frature surfaces were mixed frature with both transgranular and intergranular, but intergranular fratures were r-type cavity in hold-time waveforms and w-type cavity in slow-fast ones.

화력발전소 증기터빈용 12Cr 강의 저주기 피로거동 (Low Cycle Fatigue Behavior of 12Cr Steel for Thermal Power Plant Steam Turbine)

  • 강명수
    • 한국정밀공학회지
    • /
    • 제19권8호
    • /
    • pp.71-76
    • /
    • 2002
  • In this study low cycle fatigue (LCF) behavior of 12Cr steel at high temperature are described. Secondly, comparisons between predicted lives and experimental lives are made for the several sample life prediction models. Two minute hold period in either tension or compression reduce the number of cycles to failure by about a factor of two. Twenty minute hold periods in compression lead to shorter lives than 2 minute hold periods in compression. Experiments showed that life predictions from classical phenomenological models have limitations. More LCF experiments should be pursued to gain understanding of the physical damage mechanisms and to allow the development of physically-based models which can enhance the accuracy of the predictions of components. From a design point-of-view, life prediction has been judged acceptable for these particular loading conditions but extrapolations to thermo-mechanical fatigue loading, for example, require more sophisticated models including physical damage mechanisms.

순수 비틀림 하중하에서 열화를 고려한 2상 스데인리스강의 저주기 피로특성 (Low Cycle Fatigue Characteristics of Duplex Stainless Steel with Degradation under Pure Torsional Load)

  • 권재도;박중철
    • 대한기계학회논문집A
    • /
    • 제26권9호
    • /
    • pp.1897-1904
    • /
    • 2002
  • Monotonic torsional and pure torsional low cycle fatigue(LCF) test with artificial degradation were performed on duplex stainless steel(CF8M). CF8M is used in pipes and valves in nuclear reactor coolant system. It was aged at 430$^{\circ}C$ for 3600hrs. Through the monotonic and LCF test, it is found that mechanical properties(i.e., yield strength, strain hardening exponent, strength coefficient etc.) increase and fatigue life(N$\sub$f/) decreases with degradation of material. The relationship between shear strain amplitude(${\gamma}$$\sub$a/)and N$\sub$f/ was proposed.

차륜 및 차축 재료의 저주기 피로특성 (Low Cycle Fatigue Characteristics of the Railway Wheels and Axles)

  • 김대진;석창성;서정원
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2005년도 춘계학술대회 논문집
    • /
    • pp.427-433
    • /
    • 2005
  • Railway wheelset is the most essential part which undergoes severe cyclic loadings. In recent years, there has been increasing need for insuring the safety of running as the speed of the railway vehicles is getting higher. So it is required on the assessment of fatigue characteristics of the wheelset to consider plastic deformation which might be probable in the severe loading condition. In this study, total-strain controlled low cycle fatigue(LCF) test were performed to observe the LCF behaviors of the railway wheels and axles using companion specimens method. From the experimental results, the cyclic mechanical properties have been evaluated and total strain amplitude versus life relationship have been derived using the empirical Coffin-Manson law.

  • PDF

표면부착형 가변 자속 전동기의 설계 및 동특성 해석 (Design and Dynamic Aanlaysis of Surface-Mounted Type Variable Flux Machines)

  • 김정만;최장영;이규석;이성호
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2015년도 제46회 하계학술대회
    • /
    • pp.740-741
    • /
    • 2015
  • This paper presents the design and dynamic analysis of surface-mounted type variable flux permanent magnet(VFPM) machines. VFPM machines with a low-coercive-force (LCF) magnetic material have been studied extensively for their potential to improve the efficiency and extend the flux-weakening range of permaennt magnet (PM) machines. In order to implement the design of the VFPM machines effectively, we perform a characteristic analysis of the LCF magnet with respect to design parameters. The analysis results of the designed VFPM machines are compared with measured results, and the validity of the design of the VFPM machines is confirmed.

  • PDF

터빈 디스크용 스테인리스강의 고온 인장 및 저주기 피로 물성 측정 (Evaluation of high temperature tensile behavior and LCF properties of stainless steel for turbine disks)

  • 임형대;박철규;이광주;임성한;김춘택
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.334-337
    • /
    • 2007
  • Austenitic stainless steel is used as high temperature components such as gas turbine blade and disk because of its good thermal resistance. In the present investigation, tensile and low cycle fatigue(LCF) behavior of stainless steel for turbine disks was studied at wide temperature range $20^{\circ}C\;{\sim}\;750^{\circ}C$. In the tensile tests, it was shown that elastic modulus, yield strength, ultimate tensile strength decreased when temperature increased. The effect on fatigue failure of the parameters such as plastic strain amplitude, stress amplitude and plastic strain energy density was also investigated. Coffin-Manson and Morrow models were used to adjust experimental data and predict the fatigue life behavior at different mean strain values during cyclic loading of high temperature components.

  • PDF

Detection of Low Cycle Fatigue in Type 316 Stainless Steel using HTS-SQUID

  • Park, D.G.;Kim, D.W.;Timofeev, V.P.;Hong, J.H.
    • Corrosion Science and Technology
    • /
    • 제3권5호
    • /
    • pp.222-225
    • /
    • 2004
  • A portable RF HTS SQUID-based susceptometer was applied to the measurement of fatigue behavior for type 316L(N) stainless steel containing 0.04% to 0.15% nitrogen content. Strain-controlled low cycle fatigue (LCF) tests were conducted at RT and $600^{\circ}C$ in air an atmosphere, and the magnetic moments were measured after the fatigue test using HTS SQUID. The magnetic moment of an as-received sample is higher than that of a fatigued sample in all the temperature ranges irrespective of the nitrogen content. The fatigue life decreased with an increasing test temperature up to $500^{\circ}C$, but increased at $600^{\circ}C$. The change of the magnetic moments by LCF test is attributed to the stress induced micro defects.

23Cr26Ni 내열강의 피로 특성 (Fatigue Behavior of 23Cr26Ni Heat Resistant Steel)

  • 이희웅;권숙인
    • 열처리공학회지
    • /
    • 제24권2호
    • /
    • pp.92-98
    • /
    • 2011
  • The influence of the cooling condition after solution treatment on the high temperature fatigue resistance of 23Cr-26Ni heat resistant steel was investigated. Two different cooling conditions were applied to the steel after solution treatment at $1200^{\circ}C$ for 3 hours. One specimen was water quenched immediately after the solution treatment. The other one was furnace cooled at a rate of $0.5^{\circ}C/min$ down to $750^{\circ}C$ after the solution treatment. Then, both specimens were aged at $750^{\circ}C$ for 5 hours. Under two different heat treatment conditions, the low cycle fatigue (LCF) test was performed at $600^{\circ}C$ and room temperature (RT). Only cyclic hardening continued from the beginning until fracture at all strain amplitudes during LCF at $600^{\circ}C$. This phenomenon was attributed to the increase in the dislocation density due to cyclic deformation, which resulted in the interaction between the newly created dislocations and precipitates. Cyclic hardening followed by saturation and cyclic softening was observed at RT. Cyclic softening was attributed to the dislocation annihilation rate exceeding the dislocation generation rate. Other probable factor for cyclic softening was some cavities formed around grain boundaries after 20 cycles. WQ and FC have a similar LCF behavior at RT and $600^{\circ}C$ as shown in the cyclic stress response curves.