Clad강의 debonding 현상에 대한 연구 2

  • 윤중근;김희진
    • Journal of Welding and Joining
    • /
    • v.5 no.4
    • /
    • pp.22-27
    • /
    • 1987
  • The debonding of clad steel was often occurred at interface between stainless steel and carbon steel during the fabrication of pressure vessel. In order to clarify the causes of debonding phenomena, the fabrication sequences were fully analyzed. As a result, possible factors were noticed for causing the debonding of clad steel, that is, thermal treatment on weldment and welding. Moreover the existence of hydrogen diffused from surroundings also expedites the debonding of clad steel. In this stud, the effect of welding thermal cycle, hydrogen and mixed condition under thermal treatment on the interfacial strength of clad steel were investigated to understand the debonding mechanism of clad steel. From this study, it has been confirmed that the interfacial strength of clad steel was remarkablely deteriorated due to welding and/or existence of hydrogen under thermal treatment. In the case of welding thermal cycle effect, the higher temperature at interface experienced by welding, the more reduction in interfacial strength of clad steel resulted in. And the existence of diffusible hydrogen also reduced the interfacial strength. It is also found that the interfacial strength of clad steel became much lower value than that of the as-received plate under coexistence of above mentioned factors.

  • PDF

A study on pre-bonding mechanism of Si wafer at HF pre-treatment (HF 전처리시 실리콘 기판의 초기접합 메카니즘에 관한 연구)

  • Kang, Kyung-Doo;Park, Chin-Sung;Lee, Chae-Bong;Ju, Byung-Kwon;Chung, Gwiy-Sang
    • Proceedings of the KIEE Conference
    • /
    • 1999.07g
    • /
    • pp.3313-3315
    • /
    • 1999
  • Si direct bonding(SDB) technology is very attractive for both Si-on-insulator(SOI) electric devices and MEMS applications because of its stress free structure and stability. This paper presents on pre-bonding according to HF pre-treatment conditions in Si wafer direct bonding. The characteristics of bonded sample were measured under different bonding conditions of HF concentration, and applied pressure. The bonding strength was evaluated by tensile strength method. The bonded interface and the void were analyzed by using SEM and IR camera respectively. A bond characteristic on the interface was analyzed by using IT- IR. Si-F bonds on Si surface after HF pre-treatment are replaced by Si-OH during a DI water rinse. Consequently, hydrophobic wafer was bonded by hydrogen bonding of Si $OH{\cdots}(HOH{\cdots}HOH{\cdots}HOH){\cdots}OH-Si$. The bond strength depends on the HF pre-treatment condition before pre- bonding (Min:$2.4kgf/crn^2{\sim}Max:14.9kgf/crn^2$)

  • PDF

Optimal Post Heat-treatment Conditions for Improving Bonding Strength of Roll-bonded 3-ply Ti/Al/Ti Sheets (롤 본딩된 Ti/Al/Ti 3-ply 다층금속 판재의 접합강도 향상을 위한 최적 후열처리 조건 도출)

  • Kim, M.H.;Bong, H.J.;Kim, J.H.;Lee, K.S.
    • Transactions of Materials Processing
    • /
    • v.31 no.4
    • /
    • pp.179-185
    • /
    • 2022
  • The influence of post-roll bonding heat treatment conditions such as temperature and time on the variation in the diffusion layer, generated at the bonding interface and the subsequent mechanical properties of the roll-bonded Ti grade 1/Al1050/Ti grade 1 sheets, was systematically investigated. The intermetallic compound (IMC) phase generated by post heat treatment conditions adopted in this study was obviously indexed as monolithic TiAl3. Whereas the thickness of IMC layer generated by annealing at 500 ℃ was approximately 100 nm scale, it drastically increased above 1.5 ㎛ when annealed at 600 ℃. Uniaxial tensile and peel tests were then performed to compare mechanical properties. As a result, the bonding strength drastically increased above 7.9 N/mm by annealing at 600 ℃, which implies that proper annealing condition was a prerequisite, to improving interface bonding strength as well as global elongation properties for Ti/Al/Ti 3-ply sheet.

Implementation of Man-made Tongue Immobilization Devices in Treating Head and Neck Cancer Patients (두 경부 암 환자의 방사선치료 시 자체 제작한 고정 기구 유용성의 고찰)

  • Baek, Jong-Geal;Kim, Joo-Ho;Lee, Sang-Kyu;Lee, Won-Joo;Yoon, Jong-Won;Cho, Jeong-Hee
    • The Journal of Korean Society for Radiation Therapy
    • /
    • v.20 no.1
    • /
    • pp.1-9
    • /
    • 2008
  • Purpose: For head and neck cancer patients treated with radiation therapy, proper immobilization of intra-oral structures is crucial in reproducing treatment positions and optimizing dose distribution. We produced a man-made tongue immobilization device for each patient subjected to this study. Reproducibility of treatment positions and dose distributions at air-and-tissue interface were compared using man-made tongue immobilization devices and conventional tongue-bites. Materials and Methods: Dental alginate and putty were used in producing man-made tongue immobilization devices. In order to evaluate reproducibility of treatment positions, all patients were CT-simulated, and linac-gram was repeated 5 times with each patient in the treatment position. An acrylic phantom was devised in order to evaluate safety of man-made tongue immobilization devices. Air, water, alginate and putty were placed in the phantom and dose distributions at air-and-tissue interface were calculated using Pinnacle (version 7.6c, Phillips, USA) and measured with EBT film. Two different field sizes (3$\times$3 cm and 5$\times$5 cm) were used for comparison. Results: Evaluation of linac grams showed reproducibility of a treatment position was 4 times more accurate with man-made tongue immobilization devices compared with conventional tongue bites. Patients felt more comfortable using customized tongue immobilization devices during radiation treatment. Air-and-tissue interface dose distributions calculated using Pinnacle were 7.78% and 0.56% for 3$\times$3 cm field and 5$\times$5 cm field respectively. Dose distributions measured with EBT (international specialty products, USA) film were 36.5% and 11.8% for 3$\times$3 cm field and 5$\times$5 cm field respectively. Values from EBT film were higher. Conclusion: Using man-made tongue immobilization devices made of dental alginate and putty in treatment of head and neck cancer patients showed higher reproducibility of treatment position compared with using conventional mouth pieces. Man-made immobilization devices can help optimizing air-and-tissue interface dose distributions and compensating limited accuracy of radiotherapy planning systems in calculating air-tissue interface dose distributions.

  • PDF

Effect of Post Heat Treatment on Bonding Interfaces in Ti/STS409L/Ti Cold Rolled Clad Materials (Ti/STS409L/Ti 냉연 클래드재의 접합계면특성에 미치는 후열처리의 영향)

  • Bae, D.S.;Kim, W.J.;Eom, S.C.;Park, J.H.;Lee, S.P.;Kim, M.J.;Kang, C.Y.
    • Transactions of Materials Processing
    • /
    • v.20 no.2
    • /
    • pp.140-145
    • /
    • 2011
  • The aim of the present study is to derive optimized post heat treatment temperatures to get a proper formability for Ti/STS409L/Ti clad materials. These clad materials were fabricated by cold rolling followed by a post heat treatment process for 10 minutes at temperatures ranging from $500^{\circ}C$ to $850^{\circ}C$. The microstructure of the interface was observed using a Scanning Electron Microscope(SEM) and an Energy Dispersive X-ray Analyser(EDX) in order to investigate the effects of post heat treatment on the bonding properties of the Ti/STS409L/Ti clad materials. Diffusion bonding was observed at the interfaces with a diffusion layer thickness increasing with the post heat treatment temperature. The diffusion layer was composed of a type of(${\varepsilon}+{\zeta}$) intermetallic compound containing additional elements, namely, Fe, Ti and Ni. The micro Knoop hardness of the Ti/STS409L interfaces was found to increase with heat treatment up to $800^{\circ}C$ and then decrease for temperatures rising up to $850^{\circ}C$. The tensile strength was shown to decrease for heat treatment temperature increasing to $750^{\circ}C$ and then increase rapidly for temperature rising up to $850^{\circ}C$. A post heat treatment temperature range of $700{\sim}750^{\circ}C$ was found to optimize the formability of Ti/STS409L/Ti clad materials.

Fabrication of the interface-treated ramp-edge Josephson junctions using Sr$_2AlTaO_6$ insulating layers (Sr$_2AlTaO_6$ 절연막을 이용한 계면처리된 경사형 모서리 조셉슨 접합의 제작)

  • Choi, Chi-Hong;Sung, Gun-Yong;Han, Seok-Kil;Suh, Jeong-Dae;Kang, Kwang-Yong
    • 한국초전도학회:학술대회논문집
    • /
    • v.9
    • /
    • pp.63-66
    • /
    • 1999
  • We fabricated ramp-edge Josephson junctions with barriers formed by interface treatments instead of epitaxially grown barrier layers. Low-dielectric Sr$_2AITaO_6$(SAT) layer was used as an ion-milling mask as well as an insulating layer for the ramp-edge junctions. An ion-milled YBa$_2Cu_3O_{7-x}$ (YBCO)-edge surface was not exposed to solvent through all fabrication procedures. The barriers were produced by structural modification at the bottom YBCO edge using plasma treatment prior to deposition of the top YBCO electrode. We investigated the effects of pre-annealing and post-annealing on the characteristics of the interface-treated Josephson junctions. The junction parameters were improved by using in-situ RF plasma cleaning treatment.

  • PDF

Suppression of Interfacial Segregation and Control of Microstructure for Improvement of Mechanical Properties of W-Ni-Fe Heavy Alloy (계면편석 억제와 미세구조 조절에 의한 중합금의 기계적성질 향상)

  • 강석중
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 1993.11a
    • /
    • pp.3-3
    • /
    • 1993
  • In mechanical testing of W-Ni-Pe heavy alloys, the cracks nucleate at W/W interface and propagate through W/ Imatrix interface or through matrix phase together with the cleavage of W grains. The mechanical properties can therefore be improved by control of the interfacial strength and area. In this presentation, some experimental result and techniques on this subject will be reviewed and discussed. The hydrogen embrittlement caused by the hydrogen segregation at interfaces during sintering in an hydrogen atmosphere can be removed by an heat-treattnent in vacuum or in an inert atmosphere. The heat-treatment condition can be estimated by using a diffusion equation for a cylindrical shape. The mechanical properties, in particular the impact property, are degraded by the segregation of non-metallic impurities, such as Sand P. The degradation can be prevented by adding a fourth element, such as La or Ca, active with the non-metallic impurities. The cyclic heat-treatment at usual heat-treattnent tempemture causes the penetration of matrix between W/W grain boundaries and results in remarkable increase in impact energy. This is due to an increase in the area of ductile failure during the impact test. The instability of W/matrix interface casued by addition of Mo or Re can be controlled by using W powders of different size. The increase in the interfacial area in found to be related to the presence of non-equilibrium pure W gmins among W(Mo or Re) solid solution gmins.

  • PDF

Sludge Thickening using Electro-Flotation in Water Treatment Plant (전해부상에 의한 상수 슬러지 농축효율)

  • Lee, Jun;Han, Mooyoung;Dockko, Seok;Park, Yonghyo;Kim, Tschungil;Kim, Mikyung
    • Journal of Korean Society of Water and Wastewater
    • /
    • v.19 no.2
    • /
    • pp.155-160
    • /
    • 2005
  • Gravity thickening process has been widely used in WTP sludge thickening at domestic water treatment plant. The operation method of the process is very simple, however, the process requires long detention time about 24~48 hours for sludge thickening, uses polymer, and low total solids of thickened sludge to increase sludge thickening efficiency. To solve there problems, we studied about flotation process, especially, electro-flotation (EF) process in WTP sludge thickening. Electro-flotation process is simpler than dissolved-air-flotation(DAF) process because EF needs only electrode and current to generate micro-bubbles and the operation is easy. This study was performed at two batch columns to compare interface height, total solids, effluent turbidity between an electro-flotation thickening and a gravity thickening. According to the result, an electro-flotation thickening was that interface height was decreasing, total solids had high concentration, and effluent turbidity was low in comparison with a gravity thickening. Also, it will make the high efficiency of following process, such as a dehydrating process and digestive process. because of high total solids and low moisture content in the sludge.

Evaluating Nanomechanical Properties on Interface of Friction-welded TiAl and SCM440 Alloys with Cu as an Insert Metal (삽입금속 Cu를 적용한 TiAl 합금과 SCM440의 마찰용접 계면의 나노역학물성 평가)

  • Kim, Ki-Young;Oh, Myung-Hoon;Choi, In-Chul
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.34 no.6
    • /
    • pp.309-314
    • /
    • 2021
  • Due to the superior corrosion resistance and mechanical properties of TiAl alloy at high temperature, it has been utilized as a turbine wheel of a turbocharger. The dissimilar metallic bonding is usually applied to combine the TiAl turbine wheel with the SCM440 structural steel which is used as a driving shaft. In this study, the TiAl and SCM440 joint were fabricated by using a friction welding technique. During bonding process, to suppress the martensitic transformation and the formation of cracks, which might reduce a strength of the joints, Cu was used as an insert metal to relieve stress. As a result, the intermetallic compounds (IMCs) layer was observed at TiAl/Cu interface while no IMC formation was formed at SCM440/Cu interface. Since understanding of the IMCs effects on the mechanical performance of welded joint is also essential for ensuring the reliability and integrity of the turbocharger system, we estimated the nanohardness of welded joint region through nanoindentation. The relation between the microstructural feature and its mechanical property is discussed in detail.

Chitosan-induced biomodification on demineralized dentin to improve the adhesive interface

  • Isabella Rodrigues Ziotti;Vitoria Leite Paschoini;Silmara Aparecida Milori Corona;Aline Evangelista Souza-Gabriel
    • Restorative Dentistry and Endodontics
    • /
    • v.47 no.3
    • /
    • pp.28.1-28.12
    • /
    • 2022
  • Objectives: Metalloproteinase-inhibiting agents, such as chitosan, can prevent collagen degradation in demineralized dental substrates, thereby improving the adhesive interface. This study evaluated the bond strength (BS) and chemical and morphological characterization of the adhesive interface after applying chitosan solution to demineralized dentin. Materials and Methods: The 80 third molars were selected. Forty teeth underwent caries induction using the pH cycling method. The teeth were divided according to the treatment: distilled water (control) and 2.5% chitosan solution. The surfaces were restored using adhesive and composite resins. Half of the specimens in each group were aged, and the other half underwent immediate analyses. The teeth were sectioned and underwent the microtensile bond strength test (µTBS), and chemical and morphological analyses using energy-dispersive spectroscopy and scanning electron microscopy, respectively. Data analysis was performed using 3-way analysis of variance. Results: For µTBS, sound dentin was superior to demineralized dentin (p < 0.001), chitosan-treated specimens had higher bond strength than the untreated ones (p < 0.001), and those that underwent immediate analysis had higher values than the aged specimens (p = 0.019). No significant differences were observed in the chemical or morphological compositions. Conclusions: Chitosan treatment improved bond strength both immediately and after aging, even in demineralized dentin.