• Title/Summary/Keyword: Interface shear strength

Search Result 492, Processing Time 0.026 seconds

The Effect of Processing Variables on Self-Bonding Strength in Amorphous PEEK Films (비정질 PEEK 필름의 Self-Bonding강도에 미치는 제조공정변수의 영향)

  • Jo, Beom-Rae;Kardos, J.L.
    • Korean Journal of Materials Research
    • /
    • v.5 no.2
    • /
    • pp.191-196
    • /
    • 1995
  • Self-bonding strength developed at the interface of amorphous PEEK films is highly sensitive to the processing variables(time, temperature, and pressure) during the bonding process. In order to examine the effects of these processing variables, amorphous PEEK films were bonded at various bonding conditions and the resultant interfacial bond strengths were measured using a modified single lap-shear test. Experimental results showed that the developed self-bonding strength increases with increase in bonding temperature and is directly proportional to the bonding time raised to the 1/4 power. The applied pressure seems only to produce better wetting at the beginning stage of the bonding process. Conclusively, the self-bonding of amorphous PEEK films provides a great potential for developing excellent bond strength approaching the strength of the parent material without any adhesives in structural applications.

  • PDF

Economic construction management of composite beam using the head stud shear connector with encased cold-formed steel built-up fix beam via efficient computer simulation

  • Yin, Jinzhao;Tong, Huizhi;Gholizadeh, Morteza;Zandi, Yousef;Selmi, Abdellatif;Roco-Videla, Angel;Issakhov, Alibek
    • Advances in concrete construction
    • /
    • v.11 no.5
    • /
    • pp.429-445
    • /
    • 2021
  • With regard to economic efficiency, composite fix beams are widely used to pass longitudinal shear forces across the interface. The current knowledge of the composite beam load-slip activity and shear capability are restricted to data from measurements of push-off. Modelling and analysis of the composite beams based on Euro-code 4 regarding to shear, bending, and deflection under differing loads were carried out using Finite Element through an efficient computer simulation and the final loading and sections capacity based on the failure modes was analysed. In bending, the section potential was increased by an improvement of the strength in both steel and concrete, but the flexural and compressive resistance growth is very weak (3.2% 3.1% and 3.0%), while the strength of the concrete has increased respectively from 25 N/mm2 to 30, 35, and 40 N/mm2 compared to the increment of steel strength by 27% and 21% when it was raised from 275 to 355 and 460 N/mm2, respectively. It was found that the final flexural load capacity of fix beams was declined with increase in the fix beam span for both three steel strength. The shear capacity of sections was remained unchanged at constant steel strength and different length, but raised with final yield strength increment of steel sections by 29%, and 67% when it was raised from 275 N/mm2 to 355 N/mm2 and 460 N/mm2, respectively.

The Comparison of Bonded/Unbonded Stem-Cement Interface in Total Hip Replacement -Experimental Study (인공 고관절 전치환술에서 주대-시멘트 경계층의 접착 및 비접착 고정술의 비교를 위한 실험적 연구)

  • Han, J.H.;Yoon, Y.S.;Lee, J.J.
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.951-955
    • /
    • 2001
  • The experimental comparison between bonded and unbonded types stem-cement interface was carried out on axisymmetric stem-cement-aluminum model of the femoral component of a total hip replacement. Human femur was modeled in non-tapered and tapered($7.5^{\circ}$) aluminum hollow cylinders to emulate the diaphyseal and metaphyseal segments of the femur. For unbonded type, we tested stems with three different taper angles($5^{\circ},\;7.5^{\circ},\;10^{\circ}$). In every case, the cement-aluminum interface was designed to endure 8MPa shear strength. (a measured value at cement-bone interface) We tested aluminum models under axial loading for both cases. As an experimental result, it was found that unbonded stem sustained more axial load as bonded stem in both cases, diaphyseal and metaphyseal models. The unbonded types failed in cement mantle under axial compressive load, while the bonded ones failed in shear at cement-aluminum interface. These results suggest that a polished stem will sustain much higher axial load than a roughened stem. And a polished stem will make more stable cement-bone interface that may promote better osteosythesis around the stem.

  • PDF

Computer modeling and analytical prediction of shear transfer in reinforced concrete structures

  • Kataoka, Marcela N.;El Debs, Ana Lucia H.C.;Araujo, Daniel de L.;Martins, Barbara G.
    • Computers and Concrete
    • /
    • v.26 no.2
    • /
    • pp.151-159
    • /
    • 2020
  • This paper presents an evaluation of shear transfer across cracks in reinforced concrete through finite element modelling (FEM) and analytical predictions. The aggregate interlock is one of the mechanisms responsible for the shear transfer between two slip surfaces of a crack; the others are the dowel action, when the reinforcement contributes resisting a parcel of shear displacement (reinforcement), and the uncracked concrete comprised by the shear resistance until the development of the first crack. The aim of this study deals with the development of a 3D numerical model, which describes the behavior of Z-type push-off specimen, in order to determine the properties of interface subjected to direct shear in terms cohesion and friction angle. The numerical model was validated based on experimental data and a parametric study was performed with the variation of the concrete strength. The numerical results were compared with analytical predictions and a new equation was proposed to predict the maximum shear stress in cracked concrete.

Effect of Resistance Spot Welding Parameters on AA1100 Aluminum Alloy and SGACD Zinc coated Lap Joint Properties

  • Chantasri, Sakchai;Poonnayom, Pramote;Kaewwichit, Jesada;Roybang, Waraporn;Kimapong, Kittipong
    • International Journal of Advanced Culture Technology
    • /
    • v.3 no.1
    • /
    • pp.153-160
    • /
    • 2015
  • This article is aimed to study the effects of resistance spot welding (RSW) on the lap joint properties between AA1100 aluminum alloy and SGACD zinc coated steel and its properties. The summarized experimental results are as follows. The summarized experimental results are as follows. The optimum welding parameters that produced maximum tensile shear strength of 2200 N was a welding current of 95 kA, a holding time of 10 cycles, and a welding pressure of 0.10 MPa. Increasing of welding current, increased the tensile shear strength of the joint and also increased the amount of aluminum dispersion at the joint interface. The lap joint of steel over the aluminum (Type I) showed the higher joint tensile shear strength than a lap joint of aluminum over the steel (Type II). The indentation depth and the ratio of the indentation depth to the plate thickness decreased when the welding current was increased in the type I lap joint and also decreased when the welding current was decreased in the type II lap joint. The interface structure showed the formation of the brittle $FeAl_3$ intermetallic compound that deteriorated the joint strength.

Performance of shear connectors at elevated temperatures - A review

  • Shahabi, S.E.M.;Sulong, N.H. Ramli;Shariati, M.;Shah, S.N.R.
    • Steel and Composite Structures
    • /
    • v.20 no.1
    • /
    • pp.185-203
    • /
    • 2016
  • Shear connectors are key components to ensure the efficient composite action and satisfactory transfer of shear forces at the steel-concrete interface in composite beams. Under hazardous circumstances, such as fire in a building, the performance of a composite beam significantly relies on the performance of shear connectors. Studies on the behavior of shear connectors subjected to elevated temperatures performed in the last decade are reviewed in this paper. The experimental testing of push-out specimens, the design approaches provided by researchers and different codes, the major failure modes, and the finite element modeling of shear connectors are highlighted. The critical research review showed that the strength of a shear connector decreases proportionally with the increase in temperature. Compared with the volume of work published on shear connectors at ambient temperatures, a few studies on the behavior of shear connectors under fire have been conducted. Several areas where additional research is needed are also identified in this paper.

Evaluation of tissue ingrowth and reaction of a porous polyethylene block as an onlay bone graft in rabbit posterior mandible

  • Sosakul, Teerapan;Tuchpramuk, Pongsatorn;Suvannapruk, Waraporn;Srion, Autcharaporn;Rungroungdouyboon, Bunyong;Suwanprateeb, Jintamai
    • Journal of Periodontal and Implant Science
    • /
    • v.50 no.2
    • /
    • pp.106-120
    • /
    • 2020
  • Purpose: A new form of porous polyethylene, characterized by higher porosity and pore interconnectivity, was developed for use as a tissue-integrated implant. This study evaluated the effectiveness of porous polyethylene blocks used as an onlay bone graft in rabbit mandible in terms of tissue reaction, bone ingrowth, fibrovascularization, and graft-bone interfacial integrity. Methods: Twelve New Zealand white rabbits were randomized into 3 treatment groups according to the study period (4, 12, or 24 weeks). Cylindrical specimens measuring 5 mm in diameter and 4.5 mm in thickness were placed directly on the body of the mandible without bone bed decortication, fixed in place with a titanium screw, and covered with a collagen membrane. Histologic and histomorphometric analyses were done using hematoxylin and eosin-stained bone slices. Interfacial shear strength was tested to quantify graft-bone interfacial integrity. Results: The porous polyethylene graft was observed to integrate with the mandibular bone and exhibited tissue-bridge connections. At all postoperative time points, it was noted that the host tissues had grown deep into the pores of the porous polyethylene in the direction from the interface to the center of the graft. Both fibrovascular tissue and bone were found within the pores, but most bone ingrowth was observed at the graft-mandibular bone interface. Bone ingrowth depth and interfacial shear strength were in the range of 2.76-3.89 mm and 1.11-1.43 MPa, respectively. No significant differences among post-implantation time points were found for tissue ingrowth percentage and interfacial shear strength (P>0.05). Conclusions: Within the limits of the study, the present study revealed that the new porous polyethylene did not provoke any adverse systemic reactions. The material promoted fibrovascularization and displayed osteoconductive and osteogenic properties within and outside the contact interface. Stable interfacial integration between the graft and bone also took place.

An Experimental Study on the Bonding Shear Performance Evaluation of the UHPC According to an Bonding Interface Treatment of the Construction Joint (시공이음부 계면처리방법에 따른 초고성능 콘크리트의 전단부착성능 평가에 관한 실험적 연구)

  • Jang, Hyun-O;Kim, Bo-Seok;Lee, Han-Seung
    • Journal of the Korea Institute of Building Construction
    • /
    • v.16 no.3
    • /
    • pp.237-245
    • /
    • 2016
  • Structural performance and durability of ultra high performance concrete could demonstrate optimal performance when unity was kept. Accordingly, it is necessary to involve the characteristics and quantitative surface treatment at the same time in order to retain oneness of Ultra-High-Performance Concrete(UHPC) according to construction joint occurrence. Therefore, this study derives a reasonable surface treatment method in a material's point of view through the shear adhesion performance evaluation according to the construction joints surface processing method as a part for securing the adhesion performance of the construction joints when casting UHPC. 180 MPa of required average strength was used for mix of UHPC and surface treatment method was set to totally 7 level that MN, GR-10-0, GR-20-0, GR-30-0, SH-30-5, SH-30-10. After the specimen were manufactured to a size of $150{\times}150{\times}150mm$, Direct shear test was performed to evaluate the shear adhesion strength. As a result, it was confirmed that the adhesion performance was improved when executing a surface treatment for the construction joint interface and standard of failure mode of specimen was over Type C. Also, It was considered that interface of cross section and depth of concavo-convex should be concerned.

Effects of Thermal and Mechanical Fatigue Stress on Bond Strength in Bracket Base Configurations (열적, 기계적 피로응력이 교정용 브라켓의 결합강도에 미치는 영향)

  • Kim, Jong-Ghee;Kim, Sang-Cheol
    • The korean journal of orthodontics
    • /
    • v.30 no.5 s.82
    • /
    • pp.625-642
    • /
    • 2000
  • The purpose of this study is to evaluate the effects of mechanical and thermal fatigue stress on the shear, tensile and shear-tensile combined bond strengths(SBS, TBS, CBS) in various orthodontic brackets bonded to human premolars with chemically cured adhesive(Ortho-one, Bisco, USA). Five types of commercially available metal brackets with various bracket base configurations of Photoetched base(Tomy, Japan), Non-Etched Foil Mesh base(Dentaurum, Germany), Micro-Etched Foil Mesh base(Ortho Organizers, USA), Chessboard base(Daesung, Korea), and Integral base(3M Unitek, USA) were used. Samples were divided into 3 groups, the first group was acted with shear-tensile combined loads($45^{\circ}$) of 200g for 4 weeks(mechanical fatigue stress), the second group was subjected to the 5,000 thermocycles of 15 second dwell time each in $5^{\circ}C\;and\;55^{\circ}C$ baths(thermal fatigue stress), and the third group was the control. Bond strengths were measured at the crosshead speed of 0.5mm/min. The cross-section of bracket base/adhesive interface and the fracture surface were examined with the stereoscope and the scanning electron microscope. The resin remnant on bracket base surface was assessed by ART(Adhesive Remnant Index). The obtained results were summarized as follows, 1. In static bond strength, Photoetched base bracket showed the maximum bond strength and Integral base bracket showed the minimum bond strength(p<0.05). In all brackets, shear bond strength(SBS) was in the greatest value and shear-tensile combined strength(CBS) was in the least value(p<0.05). 2. After mechanical fatigue test, Photoetched base bracket showed the maximum bond strength and Integral base bracket showed the minimum bond strength(p<0.05). In Photoetched base bracket and Micro-Etched Foil Mesh base bracket, shear bond strength(SBS), tensile bond strength(TBS) and shear-tensile combined strength(CBS) were decreased after mechanical fatigue test(p

  • PDF

Tooth surface treatment strategies for adhesive cementation

  • Rohr, Nadja;Fischer, Jens
    • The Journal of Advanced Prosthodontics
    • /
    • v.9 no.2
    • /
    • pp.85-92
    • /
    • 2017
  • PURPOSE. The aim of this study was to evaluate the effect of tooth surface pre-treatment steps on shear bond strength, which is essential for understanding the adhesive cementation process. MATERIALS AND METHODS. Shear bond strengths of different cements with various tooth surface treatments (none, etching, priming, or etching and priming) on enamel and dentin of human teeth were measured using the Swiss shear test design. Three adhesives (Permaflo DC, Panavia F 2.0, and Panavia V5) and one self-adhesive cement (Panavia SA plus) were included in this study. The interface of the cement and the tooth surface with the different pre-treatments was analyzed using SEM. pH values of the cements and primers were measured. RESULTS. The highest bond strength values for all cements were achieved with etching and primer on enamel ($25.6{\pm}5.3-32.3{\pm}10.4MPa$). On dentin, etching and priming produced the highest bond strength values for all cements ($8.6{\pm}2.9-11.7{\pm}3.5MPa$) except for Panavia V5, which achieved significantly higher bond strengths when pre-treated with primer only ($15.3{\pm}4.1MPa$). Shear bond strength values were correlated with the micro-retentive surface topography of enamel and the tag length on dentin except for Panavia V5, which revealed the highest bond strength with primer application only without etching, resulting in short but sturdy tags. CONCLUSION. The highest bond strength can be achieved for Panavia F 2.0, Permaflo DC, and Panavia SA plus when the tooth substrate is previously etched and the respective primer is applied. The new cement Panavia V5 displayed low technique-sensitivity and attained significantly higher adhesion of all tested cements to dentin when only primer was applied.