• 제목/요약/키워드: Insert metal

검색결과 148건 처리시간 0.029초

Cu-8.6wt%Al 삽입금속을 사용한 페라이트계 스테인리스강의 아크 브레이징 접합부의 미세조직과 인장성질 (Microstructures and Tensile Properties in Arc Brazed Joints of Ferritic Stainless Steel using Cu-8.6%Al Insert Metal)

  • 조영호;정창은;강명창;강정윤
    • Journal of Welding and Joining
    • /
    • 제29권4호
    • /
    • pp.85-92
    • /
    • 2011
  • Microstructures and tensile properties in arc brazed joints of ferritic stainless steel, 429EM using Cu-8.6%Al insert metal was investigated as function of brazing current. The brazing speed was fixed at 800mm/min and brazing current varied in the range of 80A to 120A. The initial phase of filler metal was Cu single phase. However, the insert metal structures of brazed joints was composed of Cu matrix and intermetallic compound such as ${\gamma}_1(Al_4Cu_9)$, and flower-shape Fe-Cr. The fraction of ${\gamma}_1(Al_4Cu_9)$ phase was similar with 80A and 100A brazing currents while that of brazed with 120A was decreased. On the other hand, the fraction of Fe-Cr phase increased with increasing of the brazing current. A reaction layer at the base metal/insert metal interface was observed and this reaction layer was thickened with increasing of the brazing current. In the brazed joints with the current lower than 100A, crack was grew up along the interface which was perpendicular to the tensile stress, and then, passed through the insert metal in the final stage of fracture. As the brazing current increased to 120A, fracture occurred at the base metal.

볼 밀링법으로 제조된 브레이징 삽입금속 및 접합 특성 (Characteristics of the Powder Type Ag System Insert Metals Made by Ball Milling Method and Brazed Joints)

  • 김광수;이규도;황선효
    • Journal of Welding and Joining
    • /
    • 제20권1호
    • /
    • pp.47-54
    • /
    • 2002
  • Powder type Ag system insert metals were manufactured by ball milling process. The variables of milling process such as milling media, revolution speed and powder/ball weight ratio were constant except the milling time. The milling times were selected for 24, 48 and 72 hours. The insert metals made by milling process were evaluated by performing scanning electron microscope, x-ray and DSC(differential scanning calorimetry) analysis, and further in terms of wettability test. The selected insert metals that have the good characteristics compared to commercial insert metals were applied to make the brazed joints of the steel/steel and the steel/WC superhard particles. The characterizations of those brazed joints were also conducted by microstructural observations, shear tensile tests and microhardness measurements. The results indicated that milling time of 48 hours for making powder type insert metals was the best condition showing the small amount of oxides residue, low wetting angle and stable microstructure. The brazed joints that applied the 48 hours milled insert metal were very sound condition indicating the shear tensile value of $2.29{\times}102$ MPa and the microhardness of 138VHN. Further, the amount of the porosity was appeared to be lower than that of the commercial insert metals.

코팅공구를 사용한 Face Milling의 가공특성에 관한 연구 (A Study on Machining Characteristics of Face Milling Using Coated Tool)

  • 이위로;김성일;김태영
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1993년도 추계학술대회 논문집
    • /
    • pp.106-111
    • /
    • 1993
  • This experimental study mainly deal with the single and multi-insert cutting characteristics using coated tool. Because metal cutting of the single and multi-insert has a large relation to the improvement of productivity, the economic cutting process can be achieved by the analysis of proper metal cutting mechanism. Therefore, machining characteristics of face milling in this paper has been studied by investigating the role of different insert number which is concerned with mean cutting force, the RMS values of AE(acoustic emission) signal, tool life and surface roughness in milling SS 41 and SUS 304.

  • PDF

A$_2$O$_3$세라믹과 Ni-Cr-Mo鋼과의 인서트 合金을 이용한 擴散接合에 關한 硏究 (A study on the diffusion bonding of the $Al_2$O$_3$ ceramics to metal)

  • 김영식;박훈종;김정일
    • Journal of Welding and Joining
    • /
    • 제10권3호
    • /
    • pp.63-72
    • /
    • 1992
  • The joining methods of ceramics to metals which can be expected to obtain high temperature strength are mainly classified into the solid-state diffusion bonding method and the active brazing method. Between these two, the solid-state diffusion bonding method is given attentions as substituting method for active brazing method due to being capable of obtaining higher bonding strength at high temperature and accurate bonding. In this paper, the solid-state diffusion bonding of $Al_{2}$O$_{3}$ ceramics to Ni-Cr-Mo alloy steel (SNCM21) using insert metal was carried out. The insert metal employed in this study was experimentally home-made, Ag-Cu-Ti alloy. Influence of several bonding parameters of $Al_{2}$O$_{3}$SNCM21 joint was quantitatively evaluated by bonding strength test, and microstructural analyses at the interlayer were performed by SEM/EDX. From above experiments, the optimum bonding condition of the solid-state diffusion bonding of $Al_{2}$O$_{3}$/SNCM21 using Ag-Cu-Ti insert metal was determined. Futhermore, high temperature strength and thermal-shock properties of $Al_{2}$O$_{3}$/SNCM21 joint were also examined. The results obtained are as follows. 1. The maximum bonding strength was obtained at the temperature of 95% melting point of insert metal. 2. The high temperature strength of $Al_{2}$O$_{3}$/SNCM21 joint appeared to bemaximum value at test temperature 500.deg.C and the bonding strength with increasingtemperature showed parabolic curve. 3. The strength of thermal-shocked specimens was far deteriorated than those of as-bonded specimens. Especially, water-quenched specimen after heated up to 600.deg. C was directly fractured in quenching.

  • PDF

삽입재를 사용한 A2024-T6와 SM45C의 마찰용접에 관한 연구 (A Study on Friction Welding of A2024-T6 and SM45C using Insert Metals)

  • 강성보;윤병수;민택기
    • Journal of Welding and Joining
    • /
    • 제16권5호
    • /
    • pp.48-55
    • /
    • 1998
  • This study was undertaken to investigate the friction welding of A2024-T6 aluminum alloy and SM45C carbon steel using insert metals. The relationships among the friction welding conditions, the tensile strength of joints, the hardness distribution of welds, the microstructure of welds and the tensile fracture surfaces were mainly investigated through this experiment. When the A6063-T5 aluminum alloy of insert metal was used, the maximum tensile strengh of joint was obtained. In this case, the maximum joint efficiency was 75.3 percent and in the case of unusing the insert metals, it was 37.7 percent. Optimal welding conditions were N=2000rpm, P$_1$=40MPa, P$_2$=140MPa, t$_1$=1.0sec and t$_2$=5sec.

  • PDF

이종재 접합부에서의 응력집중현상에 관한 연구 (A Study on the Stress Concentration Phenomenon of a Dissimilar Joints)

  • 조상명;김영식
    • Journal of Welding and Joining
    • /
    • 제10권1호
    • /
    • pp.35-42
    • /
    • 1992
  • In this study, the stress concentration phenomenon for the dissimilar joints(ceramic-metal) bonded by thermal treating using a soft-insert metal(copper) was investigated with the aid of FEM(finite element method) under the load condition of uniform tension. The analysis was carried out by the supposing that stress states are plane stress or plane strain and elastic or elastic-plastic. And the Von Mises yield criterion and the incremental theory as plastic flow were adopted in this analysis. As the summarized results obtained, the stress concentration phenomenon was severer as the soft insert metal was thicker, in plane strain than in plane stress and in elastic-plastic state than in elastic state. Furthermore, the inducing mechanism of stress concentration was well expressed by the constraint forces(Fc) generated between the soft and the hard material.

  • PDF

질화알루미늄과 금속간 계면접합에 관한 연구: 계면반응과 미세구조 형성이 접합체 강도에 미치는 영향 (Joining of AIN Ceramics to Metals: Effect of Reactions and Microstructural Developments in the Bonded Interface on the Joint Strength)

  • 박성계
    • 한국분말재료학회지
    • /
    • 제4권3호
    • /
    • pp.196-204
    • /
    • 1997
  • Joining of AIN ceramics to W and Cu by active-metal brazing method was tried with use of (Ag-Cu)-Ti alloy as insert-metal. Joints were produced under various conditions of temperature, holding time and Ti-content in (Ag-Cu) alloy Reaction and microstructural development in bonded interface were investigated through observation and analysis by SEM/EDS, EPMA and XRD. Joint strengths were measured by shear test. Bonded interface consists of two layers: an insert-metal layer of eutectic Ag- and Cu-rich phases and a reaction layer of TiN. Thickness of reaction layer increases with bonding temperature, holding time and Ti-content of insert-metal. It was confirmed that the growth of reaction layer is a diffusion-controlled process. Activation energy for this process was 260 KJ/mol which is lower than that for N diffusion in TiN. Maximum shear strength of 108 MPa and 72 MPa were obtained for AIN/W and AIN/Cu joints, respectively. Relationship between processing variables, joint strength and thickness of reaction layer was also explained.

  • PDF

Ni기 인서트금속을 이용한 2상 스테인리스강의 브레이징 접합부에 관한 연구 (A Study on the Brazed Joint of Duplex Stainless Steel with Ni Base Insert Metal)

  • 이병호;마창익;김대업
    • 한국항공우주학회지
    • /
    • 제30권8호
    • /
    • pp.65-70
    • /
    • 2002
  • 본 연구에서는 로켓엔진에 사용되고 있는 2상 스테인리스강의 브레이징 접합성에 관하여 접합 현상과 기계적 강도의 두가지 측면의 고찰을 통하여 검증하였다. UNS32550을 모재로, MBF-50을 인서트금속으로 사용하여 브레이징 접합온도를 1473K, 1498K로 변화시키고, 접합 시간은 0~1.8ks로 변화시키면서 각 조건에서의 접합현상을 고찰한 결과, 접합부에서는 모재와 인서트금속간의 반응으로 인해 다양한 상이 생성되었다. 접합 초기에는 접합계면 및 접합부 근방의 모재에서 BN가 생성되고, 접합계면에서는 Cr질화물이 생성되어 접합 시간이 증가함에 따라 BN과 Cr질화물의 양이 감소하였다. 전단시험 결과 500MPa의 우수한 전단강도를 얻었다.

마찰용접에서 A2024와 SM45C의 삽입재에 관한 연구 (A Study on Insert Metal in Friction Welding of A2024 to SM45C)

  • 윤병수
    • 한국생산제조학회지
    • /
    • 제7권6호
    • /
    • pp.19-27
    • /
    • 1998
  • This study was investigated on the friction welding of A2024 aluminum alloy to SM45C carbon steel with insert metals. The tensile strength of welded joints, the hardness distribution of welds, the microstructure of welds and the tensile fracture surfaces were mainly investigated through this experiment. When aluminum alloy A6351 was used as insert metal, the maximum tensile strength of welded joint was obtained. In this case, the maximum joint efficiency was 76.2 percent of base metal. Optimal welding conditions were N=2,000rpm. $P_1$=40MPa, $P_2$, $t_1$=1.5 sec, $t_2$=5 sec.

  • PDF

박판 Insert 사출성형시 Insert 변형 특성에 관한 기초 연구 (A basic study on insert deformation characteristics of thin foil insert injection molding process)

  • 정우철;신광호;허영무;윤길상;이정원
    • Design & Manufacturing
    • /
    • 제2권5호
    • /
    • pp.5-10
    • /
    • 2008
  • Recently, ultra precision and light-weight micro products are needed in various industries. Injection molding products with metal insert material is often satisfied with light-weight and precision simultaneously. The researches on macro-size insert deformation have been performed but, a research on micro-size insert is meager. In this paper, the injection molding product with $300{\mu}m$ thin foil insert is designed and insert injection molding process is performed. Finally, the deformation of thin foil insert is analyzed according to insert feature and gate length.

  • PDF