The purpose of this study was to observe the thermal expansion of the inlay waxes at temperature. Inlay pattern wax shows not only a high coefficient of expansion but also a tendency to warp or distort when allowed to stand unrestrained. The thermal expansion of inlay waxes was tested according to the treatment conditions for 10 minutes at $40^{\circ}C$ The thermal expansion of inlay waxes at various temperatures was measured with an electro dial gauge. The results were as fellows: 1. It is shown that the rate of thermal expansion of wax A is 0.2%, wax B is 0.29%, wax C is 0.38%, and wax D is 0.22% at $40^{\circ}C$ 2. It is shown that the coefficient of thermal expansion of wax A is $106{\times}10^{-6}/^{\circ}C$, wax B is $152{\times}10^{-6}/^{\circ}C$, wax C is $199{\times}10^{-6}/^{\circ}C$, and wax D is $116{\times}10^{-6}/^{\circ}C$ at $40^{\circ}C$ 3. The thermal expansion of the inlay waxes at $40^{\circ}C$ was shown to increase in the order of wax C, B, D, A.
This study was performed to observe the flow change of the inlay waxes at various temperatures. The flow of inlay waxes was tested according to the treatment conditions, for 10 minutes at 40$^{\circ}C$, 41$^{\circ}C$, 42$^{\circ}C$, 43$^{\circ}C$, 44$^{\circ}C$, and 45$^{\circ}C$ The flow of inlay waxes at various temperatures was measured with an electro dial gauge. The results were as fellows: 1. The flow change of the inlay waxes at various temperatures was shown to increase in the order of wax A, B, D, C. 2. Wax A was close to ADA specification with 3% flow at 40$^{\circ}C$ and 71% flow at 45$^{\circ}C$, but wax B and D did not reach up to ADA specification with 40% flow at 45$^{\circ}C$. 3. Wax C came up with 3% flow at 40$^{\circ}C$ and 7% flow at 45$^{\circ}C$, and it revealed a very low flow change at 5$^{\circ}C$.
This study was aimed at obtaining a desirable wax pattern for inlay. The method used was to analyze, mix, and heat several kinds of waxes, comparing the temperatures of their components. The result was Type C wax. In type C the amount of paraffin was generally contained(60$\sim$70%) was reduced to 45% and there was mixed 10%-15% of carnauba, which was intended for the wax not to soften readily at low temperatures. The type C has some advantages for general use: handy preparation, high safety, and economy. The inlay waxes commonly used contracted if the temperature fell from 38 to 28, but the contraction of type C was observed to be 0.2%$\sim$0.4% in proportion to the 10 fall. This was more characteristic in mixing.
The purpose of this study was to evaluate the effects of bleaching agent through the dentinal tubules of cervical area in the intracoronal bleaching of pulpless teeth on cutured fibroblast cells. Extracted human incisors were enlarged to # 40 K-file and obturated with gutta-perella and AH 26 sealer. The gutta-percha was removed to 2mm below the cementoenamel junction of the root The teeth were divided into 3 experimental and control groups. Experimental groups; Experimental group 1: Temporary inlay wax filld with 30% $H_2O_2$ in pulp cavity. Experimental group 2: Temporary inlay wax filld with 30% $H_2O_2$ in pulp cavity after placement of ZOE cement to cementoenamel junction. Experimental group 3: Temporary inlay wax filld with 30% $H_2O_2$ in pulp cavity after application of Copalite to cementoenamel junction. Control group: Temporary inlay wax filled without 30% $H_2O_2$ in pulp cavity under the same condition at each experimental group. Each tooth was immersed in well of multidish cultured fibroblast cell for 48 hours. The cellular multiplication and cell viability were calculated at the interval of 1, 3, 5. 7 hours and the morphological changes in well were observed and their photographs were taken with inverted microscope. The obtained results were as follows : CD The cellurar multiplicaton and cell viability decreased in all experimental groups at 1 hour after experiment and the morphology of fibroblast cell was changed from star shape to round (2) The cell viability was lowered to 34 % in experemental group 1, 44 % in experimental group 2, and 38 % in experemental group 3 at 3 hours after experiment (3) The cell multiplication was decreased to 54% in experemental group 1. 47% in experimental group 2, and 40% in experemental group 3 at 7 hours after experiment. (4) The decrease of cell number and morphological changes of fibroblast cell were remarkable in experimental group 1, group 3 and 2 in order. These results suggest that the fibroblast cells receive severe damage by 30% $H_2O_2$ solution leaked through the dentinal tubules and the dentinal tubules are able to be obturated better by ZOE cement than by Copalite.
The object of this study was to measure of the distortion of various dental waxes under condition simulating clinical usage. Eleven commercial product (table) including the inlay and baseplate waxes were tested, and compared in the study. Test specimens were prepared $5{\times}5{\times}65mm$. split brass mold. Placed this rod wax specimens and the brass wax distortion test mold into the water bath and tested the distortion values for waxes at $35^{\circ}C,\;40^{\cric}C,\;45^{\circ}C\;and\;50^{\circ}C$. Measured the distortion as the difference between the final (Df) and original (Do) distance between the ends of the specimen. Recorded Df, Do and Df-Do (Distortion) to the nearest 0.5mm. A minimum of five specimens were tested for each material. The following conclusions may be drawn from this study. 1) It can be seen that, a significant wax distortion was obtained with the temperature of forming the pattern, and the length of time and the temperature at which it was stored. 2) It was found that, when the storage time was increased, the wax distortion was correspondingly increased. At the sametime, the higher the storage time was employed, the distortion was obviously much greater. 3) It can be observed that the higher the temperature at which the wax was manipulated, the less was the resulting distortion upon storage.
Purpose: The purpose of this study was to compare the marginal and internal fit of lithium disilicate ceramic inlay produced by heat pressing that inlay pattern made by subtractive manufacturing and additive manufacturing method. Methods: A mandibular lower first molar that mesial occlusal cavity (MO cavity) die was prepared. After fabricating an epoxy resin model using a silicone impression material, epoxy resin die was scanned with a dental model scanner to design an MO cavity inlay. The designed STL pile was used to fabricate wax patterns and resin patterns, and then lithium disilicate ceramic inlays were fabricated using hot-press method. For the measurement of the marginal and internal gap of the lithium disilicate, silicone replica method was applied, and gap was measured through an optical microscope (x 80). Data were tested for significant differences using the Mann-Whitney Utest. Results: The marginal fit was 103.56±9.92㎛ in the MIL-IN group and 81.57±9.33㎛ in the SLA-IN group, with a significant difference found between the two groups (p<0.05). The internal fit was 120.99±17.52㎛ in the MIL-IN group and 99.18±6.65㎛ in the SLA-IN group, with a significant difference found between the two groups (p<0.05). Conclusion: It is clinically more appropriate to apply the additive manufacturing than subtractive manufacturing method in producing lithium disilicate inlay using CAD/CAM system.
PURPOSE. The purpose of this study was to compare the cutting method and the lamination method to investigate whether the CAD data of the proposed inlay shape are machined correctly. MATERIALS AND METHODS. The Mesial-Occlusal shape of the inlay was modeled by changing the stereolithography (STL). Each group used SLS (metal powder) or SLA (photocurable resin) in the additive method, and wax or zirconia in the subtractive method (n=10 per group, total n=40). Three-dimensional (3D) analysis program (Geomagic Control X inspection software; 3D systems) was used for the alignment and analysis. The root mean square (RMS) in the 2D plane state was measured within $50{\mu}m$ radius of eight comparison measuring points (CMP). Differences were analyzed using one-way analysis of variance and post-hoc Tukey's test were used (${\alpha}=.05$). RESULTS. There was a significant difference in RMS only in SLA and SLS of 2D section (P<.05). In CMP mean, CMP 4 ($-5.3{\pm}46.7{\mu}m$) had a value closest to 0, while CMP 6 ($20.1{\pm}42.4{\mu}m$) and CMP 1 ($-89.2{\pm}61.4{\mu}m$) had the greatest positive value and the greatest negative value, respectively. CONCLUSION. Since the errors obtained from the study do not exceed the clinically acceptable values, the lamination method and the cutting method can be used clinically.
This investigation was designed to determine the effects of wire size, bracket width and the number of bracket on bracket-wire dynamic frictional resistance during simulating arch wire-guided tooth movement in vitro. For simulation of an arch wire-guided tooth movement, we simulated tooth, periodontal ligament and cancellous bone. Maxillary premolar and 1st molar were simulated as real sized resin teeth, the simulated resin teeth which its root was coated by polyether impression material which its elastic modulus is similar to periodontal ligament were embedded in steel housing with inlay wax which its elastic modulus is similar to cancellous bone. Stainless steel wires in four wire size (0.016, 0.018, $0.016\;{\times}\;0.022,\;0.019\;{\times}\;0.025$ inch) were examined with respect to three (stainless steel) bracket widths (2.4, 3.0, 4.3mm) and the number of medium bracket(one, two, three) included in the experimental assembly under dry condition. The wires were ligated into the brackets with elastomeric module. The results were as follows : 1. In all the brackets, frictional resistance increased with increase in wire size. But, statistically similar levels of frictional resistance were observed between 0.018 inch and $0.016\;{\times}\;0.022$ inch wires in narrow bracket and also between 0.016 inch and 0.018 inch wire in wide backet. 2. The frictional forces produced by 0.016 inch wire were statistically similar levels in all the brackets. In 0.018 inch round wire, wide bracket was associated with lower amounts of friction than both narrow and medium brackets. In $0.016\;{\times}\;0.022,\;0.019\;{\times}\;0.025$ inch rectangular wire, wide bracket produced target friction than both narrow and medium brackets. In all the wirer, narrow and medium bracket demonstrated no statistical difference in levels of frictional resistance. 3. Frictional resistance increased with increase In number of medium bracket. 0.016 inch round wire demonstrated the greatest increment in frictional resistance, followed by $0.019\;{\times}\;0.025,\;0.016\;{\times}\;0.022$ inch rectangular wire which were similar level in increment of frictional resistance, 0.018 inch wire demonstrated the least increment. The increments of frictional resistance were not constantly direct proportion to number of bracket.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.