• 제목/요약/키워드: Indentation system

검색결과 112건 처리시간 0.023초

한의사 맥진 가압력 재현에 대한 고찰 (Considerations on an Oriental Medical Doctor like Indentation System)

  • 이전;우영재;전영주;이유정;유현희;김종열
    • 한국한의학연구원논문집
    • /
    • 제14권3호
    • /
    • pp.113-119
    • /
    • 2008
  • In pulse diagnosis, the indentation pressure is one of the most important factors as well as the change of pulse shape and the distribution of pressure via time. But, on the oriental medical doctor's indentation pressure control, the understandings of the neurophysiological meanings and mechanisms have been lacked. So, in this paper, we considered on these issues and then proposed a proper system which can imitate the OMD's indentation pressure control mechanisms. As a result, both tactile information and kinesthetic information were found to be essential to the indentation pressure control so that a system, which can measure both the physical indent pressure and the displacement of an indentation arm, has been proposed. With this proposed system, while the indentation was being controlled through the moving step number of the step motor, the physical indentation pres sure and displacement of the indentation arm were measured. From these measured data, the relationships between the moving step number and both physical indentation pressure and displacement were revealed to have linear characteristics in early phase and to have nonlinear characteristics in latter phase. Additionally, three types of graph were generated whose X axis means the moving step number, the physical indentation pressure and the displacement respectively and Y axis means the pulse pressure. By comparing these graphs, we come to conclude that different concepts on indentation pressure control cause different diagnostic results on floating/sinking degrees for the same subject. Consequently, an indentation system for the pulse diagnosis should be able to provide both the tactile information and kinesthetic information, that is, the physical indentation pressure and the displacement of the indentation arm. In future, the proposed system should be optimized to the pulse diagnosis environment and how to combine the both information for more reliable diagnosis should be studied.

  • PDF

Advanced Indentation System을 이용한 천연가스배관 용접열영향부의 응력-변형률 변화 특성 분석 (Evaluation of Stress-Strain Characteristics of Weldment in Natural Gas Pipeline Using Advanced Indentation System)

  • 장재일;손동일;권동일;김우식;박주승
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.483-488
    • /
    • 2001
  • Until now, the tensile properties of materials can be obtained just in accordance with conventional tensile testing methods which are described in several standards such as ASTM (American Society for Testing and Materials) standard and BS (British Standard). For some cases including on-service facility materials, however, the standard testing methods cannot be applicable due to the destructive testing procedure and specimen size requirement. Therefore, simple, non-destructive and advanced indentation technique was proposed. This test measures indentation load-depth curve during indentation and analyzes the mechanical properties related to deformation and fracture. In this paper, the research trend of non-destructive evaluation of tensile properties using AIS (advanced indentation system) and its application fields are reviewed and discussed.

  • PDF

Cr-Mo 강의 열화도 평가를 위한 Advanced Indentation System의 응용 (Application of Advanced Indentation System for Evaluati Tensile Property Degradation of Cr-Mo Steel)

  • 장재일;최열;이윤희;권동일;김정태
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.231-236
    • /
    • 2001
  • A newly developed Advanced Indentation System (AIS), which is a portable and nondestructive system for evaluating tensile properties, was used to measure mechanical behavior of materials used under high temperature and pressure conditions. This test measures indentation load-depth curve during indentation and analyzes the mechanical properties related to deformation and fracture. Aging effects of Cr-Mo and Cr-Mo-V steel at high temperature were simulated. Tensile properties including yield strength and tensile strength at various temperature are obtained from the test. For all test materials and conditions, the AIS-derived results were in good agreement with those from conventional standard test method. Examples of the test results ate given and potential applications of the AIS to assess the integrity of aging structures are briefly discussed.

  • PDF

비파괴적 연속압입시험 기법을 응용한 구조용 강의 소성 물성 평가 (Evaluation of Flow Properties of Steel Using Advanced Indentation System)

  • 장재일;손동일;최열;박순찬;권동일
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.191-194
    • /
    • 2002
  • The tensile properties of materials can be obtained just in accordance with conventional tensile testing methods which are described in several standards. However, the standard testing methods cannot be applicable due to the destructive testing procedure and specimen size requirement for some cases including on-service facility materials. Therefore, simple, non-destructive and advanced indentation technique was proposed. This test measures indentation load-depth curve during indentation and analyzes the mechanical properties related to deformation and fracture. In this paper, the research trend of non-destructive evaluation of tensile properties using advanced indentation system and its application fields are reviewed and discussed.

  • PDF

요골동맥 직경 변화에 따른 맥파 측정 시스템 개발 (Development of an Measuring System for Pulse Wave Corresponding to Different Radial Artery Diameters Caused by Indentation)

  • 이전;우영재;전영주;이유정;김종열
    • 전기학회논문지
    • /
    • 제57권12호
    • /
    • pp.2351-2357
    • /
    • 2008
  • Noninvasive radial artery pulse wave has been widely used not only for the pulse wave analysis(PWA) itself but also for assessment of arterial stiffness with estimated aortic pulse wave from peripheral pulse wave. However, it has been found that the deformation of pulse shape can be caused readily by changing measuring position, indentation pressure, and so on. So, in this study, we have developed a system which can measure radial pulse wave and skin displacement simultaneously while the indentation body goes down to occlude subject's radial artery. This system can be divided into a measuring apparatus part, an indentation control hardware part, a data acquisition part and a control and computation part. And, the measuring apparatus consists of an arm-rest, a step motor, an indentation body, a laser displacement sensor(LK-G30, Keyence Co.) and pulse wave sensor. Under load-free condition and radial artery loaded condition, the evaluation of developed system has been performed. From these results, we can conclude: 1) The developed system can control the indentation body quantitatively and the adopted laser displacement sensor shows linear output characteristic even with skin as a reflector. 2) This system can measure the pulse wave and the displacement of indentation body, that is, skin displacement simultaneously at each specific level of indentation body. 3) This system can provide the number of motor steps used to get down the indentation body, the measured skin displacement, the calculated indentation pressure, the calculated pulse pressure and the pulse waveform as well as the information generated by combining these with each others. 4) This system can reveal the relationship between the morphological changes of pulse wave and the estimated displacement of radial artery wall by indentation. Consequently, the developed system can furnish more abundant information on radial artery than previous diagnosis systems based on tonometric measurement. In further study, we expect to setup the standard measuring process and to concrete the algorithm for the estimation of radial artery's diameter and of displacement of radial artery's wall. Furthermore, with well designed clinical studies, we hope to turn out the usefulness of developed system in the field of cardiovascular system evaluation.

브리넬 경도 표준 시험기 및 압입 자국 자동 측정장치의 특성 평가에 대한 연구 (A Study on the Evaluation of Brinell Standard Hardness Tester and Automatic Indentation Measurement System)

  • 방건웅;탁내형
    • 열처리공학회지
    • /
    • 제12권4호
    • /
    • pp.294-302
    • /
    • 1999
  • Evaluation of Brinell standard hardness tester was carried out to secure its application as a national standard for Brinell hardness. Accuracies and reliabilities in load application, indenter diameter and indentation measurement were tested through evaluation of these components. The accuracies of load application for various loading conditions were within the limit of ISO and KS specifications. Errors in the indentation measurement due to the difference in personnel characters were successfully removed by utilising automatic indentation measurement system. In overall, the tester and the indentation measuring system were found to be eligible as a national standard of Brinell hardness.

  • PDF

음향방출을 이용한 유리의 비커스 압입 균열 특성 (Characteristics of Cracks under Vickers Indentation in Glass Using Acoustic Emission)

  • 박혜연;이종규;박흥일;이병우
    • 동력기계공학회지
    • /
    • 제16권1호
    • /
    • pp.72-77
    • /
    • 2012
  • Acoustic emission (AE) is known to be sensitive to fracture process and so it was expected that AE data may propose as a means of monitoring the fracture information. The aim of this study is to analyze the characteristic of AE signal emitted from glass during Vickers indentation. To observe AE characteristics by surface effect, both glass and coating glass were studied. During Vickers indentation loading, AE signal resulted from penny-like crack is detected. During Vickers indentation unloading, AE signal resulted from both radial/median crack and lateral crack is detected. In case of indentation on glass, the emission energy(${\epsilon}$) is found to be approximately proportional to the fourth power of the crack length. In case of indentation on coating glass, the emission energy(${\epsilon}$) is approximately proportional to the crack length.

Advanced Indentation System을 이용한 현장에서의 구조강도 건전성 평가 (In-field Evaluation of Structural Strength and Reliability Using Advanced Indentation System)

  • 최열;손동일;장재일;권동일
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2001년도 춘계학술대회 논문집
    • /
    • pp.230-237
    • /
    • 2001
  • For the structural integrity of large and complex structures such as railway vehicle, the in-field diagnosis of mechanical properties of the structures is needed, and especially, the mechanical characteristics of the weldment must be carefully evaluated. But, conventional standard testing methods having destructive procedures are not applicable to in-field assessment of mechanical property variations within weldment because they needs the limitations of specimen size and geometry. In this paper, to overcome this problems, the advanced indentation technique (AIS) is introduced for simple and non-destructive/in-field testing of weldment of industrial structures. This test measures indentation load-depth curve during indentation and analyzes the mechanical properties related to deformation and fracture. First of all, flow properties such as yield strength, tensile strength and work hardening index can be evaluated through the analysis of the deformation behavior beneath the spherical indenter. Additionally, case studies of advanced indentation techniques are introduced.

  • PDF

초미세 위치결정시스템을 이용한 실리콘 웨이퍼의 파괴거동에 관한 연구 (A Study on the Fracture behavior in Silicon Wafer using the Ultra-Precision Micro Positioning System)

  • 이병룡
    • 한국생산제조학회지
    • /
    • 제9권1호
    • /
    • pp.38-44
    • /
    • 2000
  • The background of this study lies in he investigation of the formation mechanism of ductile mode(nkanometer-size) chips of brittle materials such as fine ceramics glass and silicon. As the first step to achieve this purpose this paper intends to observe the micro-deformation behavior of these materials in sub${\mu}{\textrm}{m}$ depth indentation tests using a diamond indentor. In this study it was developed Ultra-Micro Indentation. Device using the PZT actuator. Experimentally by using the Ultra-Micro Indentation device the micro fracture behavior of the silicon wafer was investigated. It was possible that ductile-brittle transition point in ultimate surface of brittle material can be detected by adding an acoustic emission sensor system to the Ultra-Micro Indentation appartus.

  • PDF

계장화 압입시험법을 이용한 차량용 컴프레서 저널 경도 평가 (Hardness Estimation of Compressor Journal for a Use of Instrumented Indentation Techniques)

  • 곽성종;진지원;김태성;노기한;강기원
    • 한국생산제조학회지
    • /
    • 제21권3호
    • /
    • pp.376-381
    • /
    • 2012
  • This paper deals with application of instrumented indentation technique for quality inspection methodology for automobile component. For this, the instrumented indentation tests were performed the normal and cracked compressor journal, which is made from spheroidal graphite cast iron and utilized in air-conditioning system. And the Brinell hardness was estimated using the unloading slope and maximum indentation force. With the aid of Normal distribution, this Brinell hardness was statistically compared and analyzed with hardness measured by indentation hardness tests. Also, application possibility of reliability-based quality inspection criteria for compressor journal was evaluated through the probabilistic analysis for the Brinell hardness estimated by instrumented indentation technique.