• 제목/요약/키워드: Hysteresis curve

검색결과 287건 처리시간 0.025초

저전압 대회전을 위한 분리된 압전 구동기에 의한 미소거울 (Micromirrors Driven by Detached Piezoelectric Microactuators For Low-voltage and Wide-angle Rotation)

  • 김성진;진영현;이원철;남효진;부종욱;조영호
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제55권3호
    • /
    • pp.149-155
    • /
    • 2006
  • This paper presents a torsional micromirror detached from PZT actuators (TMD), whose rotational motion is achieved by push bars in the PZT actuators detached from the micromirror. The push bar mechanism is intended to reduce the bending, tensile and torsional constraints generated by the conventional bending bar mechanism, where the torsional micromirror is attached to the PZT actuators (TMA). We have designed, fabricated and tested prototypes of TMDs for single-axis and dual-axis rotation, respectively. The single-axis TMD generates the static rotational angle of $6.1^{\circ}$ at 16 VDC, which is 6 times larger than that of single-axis TMA, $0.9^{\circ}$. However, the rotational response curve of TMD shows hysteresis due to the static friction between the cover and the push bar in the PZT actuator. We have shown that 63.2% of the hysteresis is due to the static friction caused by the initial contact force of the PZT actuaor. Without the initial contact force, the rotational response curve of TMD shows linear voltage-angle characteristics. The dual-axis TMD generates the static rotational angles of $5.5^{\circ}$ and $4.7^{\circ}$ in x-axis and y-axis, respectively at 16 VDC. The measured resonant frequencies of dual-axis TMD are $2.1\pm0.1$ kHz in x-axis and $1.7\pm0.1$ kHz in y-axis. The dual-axis TMD shows stable operation without severe wear for 21.6 million cycles driven by 16 Vp-p sinusoidal wave signal at room temperature.

무기 박막을 이용한 이온빔 배향 FFS 셀의 전기광학특성에 관한 연구 (A Study on Electro-optical Characteristics of the Ion Beam Aligned FFS Cell on a Inorganic Thin Film)

  • 황정연;박창준;정연학;김경찬;안한진;백홍구;서대식
    • 한국전기전자재료학회논문지
    • /
    • 제17권10호
    • /
    • pp.1100-1106
    • /
    • 2004
  • In this paper, we intend to make fringe-field switching (FFS) mode cell by the ion beam (IB) alignment method on the a-C:H thin film, to analyze electro-optical characteristics in this cell. We studied on the suitable inorganic thin film for fringe-field switching (FFS) cell and the aligning capabilities of nematic liquid crystal (NLC) using the alignment material of a-C:H thin film as working gas at 30 W rf bias condition. A high pretilt angle of about 5 $^{\circ}C$ by ion beam (IB) exposure on the a-C:H thin film surface was measured. Consequently, the high pretilt angle and the good thermal stability of LC alignment by the IB alignment method on the a-C:H thin film surface as working gas at 30 W rf bias condition can be achieved. An excellent voltage-transmittance (V -T) and response time curve of the IE-aligned FFS-LCD was observed with oblique IB exposure on the a-C:H thin films. Also, AC V-T hysteresis characteristics of the IB-aligned FFS-LCD with IE exposure on the a-C:H thin films is almost the same as that of the rubbing-aligned FFS cell on a polyimide (PI) surface.

Preisach 모델을 이용한 강자성체의 탈자기법 연구 (A Study on the Deperm of Ferromagnetic Material using Preisach Model)

  • 주혜선;박관수;원혁
    • 한국자기학회지
    • /
    • 제23권2호
    • /
    • pp.54-61
    • /
    • 2013
  • 강자성체는 자구들의 상호작용으로 인해 잔류 자화가 남게 되는데, 전자전기 산업 및 국방 피탐지 분야에서는 이러한 잔류 자화량을 정밀하게 0으로 만드는 탈자기법이 요구된다. 하지만 현재 수행되는 탈자기법들은 경험과 실험에 의존한 방법들로, 새로운 재료의 개발에 따른 효율적인 탈자를 위해서는 강자성체의 히스테리시스 곡선을 반영한 탈자기법이 필요하다. 본 논문에서는 자성체의 물성적인 성질을 기반으로 정립된 Preisach 모델링 기법을 이용하여 Anhysteretic Deperm, Deperm-ME, Flash-Deperm에 따른 2차원 유한요소해석을 수행하였다. 탈자 전류에 의한 자기이력궤적의 분석을 통해 강자성체의 히스테리시스 곡선과 탈자 변수의 관계를 고찰하였으며, 이로써 탈자에 효율적인 전류 감소 형태를 제시하였다.

Dynamic experimental study on single and double beam-column joints in steel traditional-style buildings

  • Xue, Jianyang;Qi, Liangjie;Yang, Kun;Wu, Zhanjing
    • Structural Engineering and Mechanics
    • /
    • 제63권5호
    • /
    • pp.617-628
    • /
    • 2017
  • In order to study the failure mode and seismic behavior of the interior-joint in steel traditional-style buildings, a single beam-column joint and a double beam-column joint were produced according to the relevant building criterion of ancient architectural buildings and the engineering instances, and the dynamic horizontal loading test was conducted by controlling the displacement of the column top and the peak acceleration of the actuator. The failure process of the specimens was observed, the bearing capacity, ductility, energy dissipation capacity, strength and stiffness degradation of the specimens were analyzed by the load-displacement hysteresis curve and backbone curve. The results show that the beam end plastic hinge area deformed obviously during the loading process, and tearing fracture of the base metal at top and bottom flange of beam occurred. The hysteresis curves of the specimens are both spindle-shaped and plump. The ultimate loads of the single beam-column joint and double beam-column joint are 48.65 kN and 70.60 kN respectively, and the equivalent viscous damping coefficients are more than 0.2 when destroyed, which shows the two specimens have great energy dissipation capacity. In addition, the stiffness, bearing capacity and energy dissipation capacity of the double beam-column joint are significantly better than that of the single beam-column joint. The ductility coefficients of the single beam-column joint and double beam-column joint are 1.81 and 1.92, respectively. The cracks grow fast when subjected to dynamic loading, and the strength and stiffness degradation is also degenerated quickly.

Comparative analysis of damping ratio determination methods based on dynamic triaxial tests

  • Song Dongsong;Liu Hongshuai
    • Earthquakes and Structures
    • /
    • 제25권4호
    • /
    • pp.249-267
    • /
    • 2023
  • Various methods for determining the damping ratio have been proposed by scholars both domestically and abroad. However, no comparative analysis of different determination methods has been seen yet. In this study, typical sand (Fujian standard sand) and cohesive soils were selected as experimental objects, and undrained strain-controlled dynamic triaxial tests were conducted. The differences between existing damping ratio determination methods were theoretically compared and analyzed. The results showed that the hysteresis curve of cohesive soils had better symmetry and more closely conformed to the definition of equivalent linear viscoelasticity. For non-cohesive soils, the differences in damping ratio determined by six methods were significant. The differences decreased with increasing confining pressure and relative density, but increased gradually with increasing shear strain, especially at high shear strains, where the maximum relative error reached 200%. For cohesive soils, the differences in damping ratio determined by six methods were relatively small, with a maximum relative error of about 50%. Moreover, they were less affected by effective confining pressure and had the same changing trend under different effective confining pressures. The damping ratio determination method has a large effect on the seismic response of soils distributed by non-cohesive soils, with a maximum relative error of about 15% for the PGA and up to about 30% for the Sa. However, for soil layers distributed by cohesive soils, the damping ratio determination method has less influence on the seismic response. Therefore, it is necessary to adopt a unified damping ratio determination method for non-cohesive soils, which can effectively avoid artificial errors caused by different determination methods.

건조 및 습윤과정에서 보은 화강암 풍화토의 불포화특성곡선 비교 (Comparative Study on Unsaturated Characteristic Curves of Boeun Granite Weathered Soil during Drying and Wetting Paths)

  • 송영석
    • 한국지반공학회논문집
    • /
    • 제32권7호
    • /
    • pp.15-24
    • /
    • 2016
  • 보은 화강암 풍화토에 대한 불포화 특성을 조사하기 위하여 자동 흙-함수특성곡선 시험장치를 이용하여 건조 및 습윤과정에 따른 모관흡수력과 체적함수비를 측정하였다. 이를 토대로 van Genuchten(1980)의 방법을 이용하여 흙-함수특성곡선(SWCC)을 산정한 결과 유효포화도에 따른 모관흡수력은 S자형의 비선형적인 관계를 나타내며, 건조 및 습윤과정을 거치는 동안 이력현상이 발생되었다. Lu and Likos(2006)의 방법을 이용하여 흡입응력특성곡선(SSCC)을 산정한 결과 유효포화도가 낮은 경우 건조과정의 흡입응력은 일정하게 유지되나 습윤과정의 흡입응력은 증가하는 경향을 보인다. 그러나 유효포화도가 큰 경우에는 동일한 유효포화도에서 건조과정의 흡입응력이 습윤과정의 흡입응력보다 크게 발생되었다. 한편 계수추정방법의 하나인 van Genuchten(1980)의 방법을 이용하여 투수계수함수(HCF)를 산정한 결과 모관흡수력이 증가함에 따라 불포화 투수계수는 감소하며, 모관흡수력에 따른 불포화 투수계수의 감소 속도는 건조과정이 습윤과정보다 더 크게 발생됨을 알 수 있다.

불포화 모래의 흡입응력 이력현상에 대한 실험적 연구 (Experimental Study on the Hysteresis of Suction Stress in Unsaturated Sand)

  • 송영석;최진수;김교원
    • 지질공학
    • /
    • 제22권2호
    • /
    • pp.145-155
    • /
    • 2012
  • 자동 흙-함수특성곡선 시험장치를 이용하여 상대밀도 60%인 주문진표준사에 대한 건조 및 습윤과정에서의 모관흡수력과 체적함수비를 측정하였다. 습윤과정이 건조과정에 비해 상대적으로 많은 시간이 소요되며, 이것은 건조과정에서 간극에 갇힌 독립된 공기에 의한 흐름 저항에 의한 것으로 판단된다. 측정된 모관흡수력과 체적함수비를 토대로 van Genuchten (1980)의 방법을 이용하여 흙-함수특성곡선(SWCC)을 예측하였다. 불포화 관련계수는 건조과정의 경우 ${\alpha}$는 0.399, n은 8.586, m은 0.884이며, 습윤과정의 경우 ${\alpha}$는 0.548, n은 5.625, m은 0.822로 산정되었다. 그리고 건조과정과 포화과정에서의 흙-함수특성곡선(SSCC)이 일치하지 않는 이력현상이 발생되었다. 불포화 관련계수를 이용하여 유효포화도와 흡입응력의 상관관계인 흡입응력특성곡선(SSCC)을 예측하였다. 흡입응력은 모관흡수력이 공기함입치 이상으로 작용할 경우 급격하게 감소하는 것으로 나타났다. 따라서 불포화토의 유효응력은 공기함입치 이상의 모관흡수력이 작용할 경우 포화토의 유효응력과 다른 값을 갖게 된다. 그리고 불포화상태에서의 동일한 유효포화도에서는 건조과정의 흡입응력이 더 크게 발생된다. 즉 흡입응력특성곡선(SSCC)에서도 건조과정과 포화과정이 일치하지 않는 이력현상이 발생되었다. 이는 흙-함수특성곡선(SWCC)의 이력현상에 기인하는 것으로 판단되며, 잉크병 효과와 접촉각 이력현상에 의해 발생되는 것으로 예상할 수 있다. 따라서 모래로 구성된 사면의 경우 지반 내 물이 유입되면서 흡입응력의 영향으로 사면 안정성에 유리하게 작용하다가 일정 흡입응력 이상이 되면 사면안정성에 불리하게 작용됨을 알 수 있다. 또한 실제 지반내 강우가 침투하는 과정은 습윤과정과 동일하므로 건조과정의 결과보다는 습윤과정의 결과를 활용하는 것이 바람직하다.

Pilocarpine투여(投與) 가토폐장(家免肺臟)의 압력(壓力)-용적곡선(容積曲線) 및 폐포표면활성물질(肺胞表面活性物質)에 관(關)하여 (Effects of Pilocarpine on Pressure-Volume Curve of the Excised Rabbit Lung and Pulmonary Surfactant)

  • 이승정;채수희;이석강
    • The Korean Journal of Physiology
    • /
    • 제8권2호
    • /
    • pp.49-53
    • /
    • 1974
  • 제 II 형(第 II 型) 폐포세포(肺胞細胞)의 페포표면활성물질(肺胞表面活性物質) 분비기능(分泌機能)이 부교감신경성작용(副交感神經性作用)에 의(依)해서 영향(影響)을 받을 것인지를 구명(究明)하기 위해서 체중(體重) 매(每) kg 당(當) 0.5mg의 pilocarpine hydrochloride를 투여(投與)한 가토(家兎)에서 폐장(肺臟)의 압력(壓力)-용적곡선(容積曲線)및 폐세척액(肺洗滌液)의 표면활성도(表面活性度)를 측정(測定)한 결과(結果)는 다음과 같다. (1) 적출가토폐(摘出家兎肺)에 공기(空氣)를 주입(注入) 및 배출(排出)할 때의 압력(壓力)-용적곡선(容積曲線)은 정상(正常) 가토(家兎)의 그것보다 hysteresis현상(現象)이 더욱 심(甚)하였으며 특(特)히 배출곡선(排出曲線)이 좌측(左側)으로 편입(偏入)되어있었다. (2) 정상(正常) 가토폐세척액(家兎肺洗滌液)의 평균최대(平均最大) 및 최소표면장력(最小表面張力) 및 stability index는 각각(各各) 46.6 dyne/cm, 7.4 dyne/cm 및 1.5이었다. (3) Pilocarpine 투여가토폐세척액(投與家肺洗滌液)의 평균최대(平均最大) 및 최소표면장력(最小表面張力) 및 stability index는 각각(各各) 47.5 dyne/cm, 6.1 dyne/cm 및 1.5로서 최소표면장력(最小表面張力)은 감소(減少)하는 경향(傾向)을 보였다. (4) 이상의 실험결과(實驗結果)로 미루어 보아 pilocarpine 투여(投與)에 의(依)해서 제 II 형(第 II 型) 폐포세포(肺胞細胞)의 페포표면활성물질(肺胞表面活性物質)의 분비기능(分泌機能)이 증가(增加)되는 경향(傾向)을 보였다.

  • PDF

인공 체액 조건에서 임플랜트용 티타늄 소재의 부식 특성 (Corrosion Behavior of Titanium for Implant in Simulated Body Fluids)

  • 이중배;최기열
    • 한국표면공학회지
    • /
    • 제37권2호
    • /
    • pp.110-118
    • /
    • 2004
  • The corrosion of pure titanium (CP- Ti Grade 2) and titanium alloy (Ti6Al4V ELI) were studied under various conditions of simulated body fluids. The static immersion test and the electrochemical test were performed in accordance with ISO 10271 : 2001. For the electrochemical test, the open circuit potential was monitored as a function of time, and the cyclic polarization curve was recorded. The corrosion resistance was evaluated from the values of corrosion potential, passivation current density, breakdown potential, and the shape of hysteresis etc. The effects of alloy type, surface condition, temperature, oxygen, and constituents in the fluids such as acid, chloride were estimated. Both specimens had extremely low dissolution rate in the static immersion test. They showed strong passivation characteristics in the electrochemical test. They maintained negligible current density throughout the wide anodic potential range. The passive layer was not broken up to 2.0 V (vs. SCE). The hysteresis and the shift of passivation potential toward the anodic direction was observed during the reversed scan. The passivation process appeared to be accelerated by oxygen in air or that dissolved in the fluids. The passivation also proceeded without oxygen by the reaction of constituents in the fluids. Acid or chloride in the fluids, specially later weakened the passive layer, and then induced higher passivation current density and less shift of passivation potential in the reversed scan. CP-Ti Grade 2 was more reactive than Ti6Al4V ELI in the fluids containing acid or chloride, but thicker layer produced on its surface provided higher corrosion resistance.

측정용 전압 변성기 오차 보상 알고리즘 (Compensation Algorithm for a Measurement Voltage Transformer)

  • 강용철;박종민;이미선;장성일;김용균
    • 전기학회논문지
    • /
    • 제57권5호
    • /
    • pp.761-766
    • /
    • 2008
  • This paper describes a compensation algorithm for a measurement voltage transformer (VT) based on the hysteresis characteristics of the core. The error of the VT is caused by the voltages across the primary and secondary windings. The latter depends on the secondary current whilst the former depends on the primary current, i.e. the sum of the exciting current and the secondary current. The proposed algorithm calculates the voltages across the primary and secondary windings and add them to the measured secondary voltage for compensation. To do this, the primary and secondary currents should be estimated. The secondary current is obtained directly from the secondary voltage and used to calculate the voltage across the secondary winding. For the primary current, in this paper, the exciting current is decomposed into the two currents, i.e. the core-loss current and the magnetizing current. The core-loss current is obtained by dividing the primary induced voltage by the core-loss resistance. The magnetizing current is obtained by inserting the flux into the flux-magnetizing current curve. The calculated voltages across the primary and secondary windings are added to the measured secondary current for compensation. The proposed compensation algorithm improves the error of the VT significantly.