Coating of Cobalt Over Tungsten Carbide Powder by Wet Chemical Reduction Method

  • Hong, Hyun-Seon;Yoon, Jin-Ho
    • 한국분말재료학회지
    • /
    • 제21권2호
    • /
    • pp.93-96
    • /
    • 2014
  • Cobalt coated tungsten carbide-cobalt composite powder has been prepared through wet chemical reduction method. The cobalt sulfate solution was converted to the cobalt chloride then the cobalt hydroxide. The tungsten carbide powders were added in to the cobalt hydroxide, the cobalt hydroxide was reduced and coated over tungsten carbide powder using hypo-phosphorous acid. Both the cobalt and the tungsten carbide phase peaks were evident in the tungsten carbide-cobalt composite powder by X-ray diffraction. The average particle size measured via scanning electron microscope, particle size analysis was around 380 nm and the thickness of coated cobalt was determined to be 30~40 nm by transmission electron microscopy.

디알킬아미노알킬 포스폰산과 비스-디알킬아미노알킬 포스핀산 유도체의 합성 (Synthesis of Dialklyaminoalkyl Phosphonic Acid and Bis(dialklyaminoalkyl) Phosphinic Acid Derivatives)

  • 정영진;진의
    • 공업화학
    • /
    • 제23권6호
    • /
    • pp.583-587
    • /
    • 2012
  • 모노-디알킬 아미노 또는 디-디알킬 아미노 기능기를 분자 내에 갖는 6종의 새로운 아미노알킬 포스폰산 또는 아미노알킬 포스핀산 유도체들을 합성하고, 그들의 연기밀도를 측정하였다. 이 화합물들은 아민 및 알데히드에 아인산 또는 하이포 아인산을 첨가하여 한 단계로 반응시켜 인산에 한 개 또는 2개의 아미노기를 갖는 화합물로서 거의 정량적으로 90-98.6%의 수율을 얻었다. 이들의 연기밀도 시험은 ASTM E 662의 방법으로 측정하였으며, 시험결과 연기밀도 (Ds)값이 224.5~256.6으로 측정되었으며, 인산구조에 2개의 아미노기를 갖는 화합물이 1개의 아미노기를 갖는 화합물 보다 연기밀도가 감소되었다. 또한 아미노기에 연결된 알킬기의 탄소수와 연기밀도 사이에는 특별한 관련이 없었다.