• 제목/요약/키워드: Hot pressing

검색결과 581건 처리시간 0.03초

기계적 합금화된 ODS NiAl에서 분산상 및 기지상의 조대화 거동 (Coarsening of Dispersoid and Matrix Phase in Mechanically Alloyed ODS NiAl)

  • 어순철
    • 한국분말재료학회지
    • /
    • 제4권1호
    • /
    • pp.48-54
    • /
    • 1997
  • NiAl powders containing oxide dispersoids have been produced by mechanical alloying process in a controlled atmosphere using high energy attrition mill. The powders have been consolidated by hot extrusion and hot pressing followed by isothermal annealing to induce microstructure coarsening to improve high temperature properties. Grain growth and dispersoid coarsening kinetics have been investigated as functions of annealing time and temperature. Coarsening of dispersion strengthen NiAl and dispersoid has been discussed. Some clues of secondary recrystallization have been investigated. Mechanical property measurements have been also made and correlated with the microstructures.

  • PDF

Magnetic Properties of $Nd_{12}Dy_2Fe_{73.2}Co_{6.6}Ga_{0.6}B_{5.6}$ magnets fabricated by current-applied pressure-assisted method

  • Kim, H. T.;S. H. Cho;Kim, Y. B.;G. A. Kapustin;Kim, H. S.
    • 한국자기학회:학술대회 개요집
    • /
    • 한국자기학회 2002년도 동계연구발표회 논문개요집
    • /
    • pp.232-233
    • /
    • 2002
  • Nanostructed high energy Nd-Fe-B based bulk magnet can be prepared by hot-working process (hot press and die-upset) from melt-spun amorphous or nanocrystalline powder.[1] Recently, we have investigated a modified method, current-applied pressure-assisted (CAPA) process, to produce nanocrystalline isotropic and anisotropic NdFeB magnets. The process consists of current-applied pressing the melt-spun powders to obtain isotropic precursor subsequent current-applied deforming the precursor to obtain textured magnet.[2-3] (omitted)

  • PDF

Skutterudite CoSb3의 합성 및 열전특성 (Synthesis and Thermoelectric Properties of Skutterudite CoSb3)

  • 김일호;유신욱;박종범;이정일;어순철;장경욱;최국선;김준수;김현주
    • 한국재료학회지
    • /
    • 제15권10호
    • /
    • pp.667-670
    • /
    • 2005
  • Binary skutterudite $CoSb_3$ compounds were prepared by the arc melting and hot pressing processes and their thermoelectric properties were investigated in the range from 300 to 600 K. Annealing effect was correlated to phase transformation and homogenization. Thermoelectric properties of the arc-melted and hot-pressed $CoSb_3$ were discussed and compared. Undoped intrinsic $CoSb_3$ prepared by the arc melting showed p-type conduction, while it showed metallic behavior with increasing measuring temperature. However, hot pressed specimens showed n-type conduction, possibly due to Sb evaporation. Thermoelectric properties were remarkably improved by annealing In vacuum and they were closely related to phase transformation.

신발용 직물의 투습방수 및 내열성 가공 (Water Vapour Permeable/Water Resistant and Heat Resistant Finishing of Footwear Fabric)

  • 이재호;최해욱
    • 접착 및 계면
    • /
    • 제7권3호
    • /
    • pp.16-25
    • /
    • 2006
  • 내열성 및 투습방수기능을 가진 신발용 직물 및 부직포를 제조하기 위하여 스크린 방식으로 공정조건을 검토하고 투습방수 필름을 라미네이팅 한 후, 최종제품의 물성을 평가하였다. 결과는 다음과 같다. 열가소성 핫 멜트와는 달리 반응형 폴리우레탄 핫 멜트는 작업 이후에 적정한 내열성을 보유하는 것으로 나타났다. 최적의 용융접착 공정조건은 다음과 같다 ; 드럼 온도 $95^{\circ}C$, 호스 온도 $97^{\circ}C$, 공급파이프 온도 $100^{\circ}C$, 스크린 온도 $105^{\circ}C$이고, opposite roller의 압력은 $1kgf/cm^2$, laminating roller의 압력은 $3kgf/cm^2$이며, 가공속도는 15 m/min이다. 투습도는 필름의 두께가 증가함에 따라 투습도는 감소하였으나, 내수도는 증가하였고, 공기투과도는 필름의 영향이 지배적이었다.

  • PDF

소결분위기 제어에 의한 Al2O3/Fe-Ni 나노복합재료의 제조 및 특성 (Fabrication of Al2O3/Fe-Ni Nanocomposites by Atmosphere-controlled Sintering and their Properties)

  • 이홍재;정영근;오승탁;이재성
    • 한국세라믹학회지
    • /
    • 제39권2호
    • /
    • pp.199-203
    • /
    • 2002
  • 소결 분위기가 금속입자분산 세라믹스기 복합체의 미세 조직 및 물성에 미치는 영향에 대하여 조사하고자 화학적 방법으로 합성한 $Al_2O_3$/Fe-Ni 나노복합분말을 수소 및 아르곤 가스 분위기, 또한 소결온도 등으로 제어하여 열간가압 소결하였다. 수소분위기에서 소결한 복합체는 아르곤분위기의 경우보다 반응상 $FeAl_2O_4$의 형성이 억제되었으며, 증가된 파괴강도 및 인성 값을 나타내었다. 또한, 소결 온도를 낮추었을 경우 기지상 및 금속 분산상의 미세화와 향상된 기계적 성질을 얻을 수 있었다. 소결 조건에 따른 기계적 특성의 변화는 주로 반응상의 형성과 관련된 미세조직 특성에 의존하는 것으로 해석하였다.

PLZT세라믹스에서의 입성장 분석 (Analysis on the Grain Growth of PLZT Ceramics)

  • 송병무;김도연
    • 한국세라믹학회지
    • /
    • 제25권4호
    • /
    • pp.329-334
    • /
    • 1988
  • Kinetics of grain growth in PLZT ceramics during isothermal heat treatment and hot-pressing were investigated and the published data on grain growth were reanalyzed. It was found, in many cases, that the errors were introduced by ignoring the initial grain size. The grain growth of PLZT ceramics was confirmed to follow the parabolic normal growth : D2-Do2=Kt.