Plastic Deformation Behavior of Al6061 depending on Heat Treatment Condition (연속주조 Al6061 합금의 열처리에 따른 소성변형거동)

  • Park J. H.;Kwon Y. N.;Lee Y. S.;Lee J. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.05a
    • /
    • pp.127-130
    • /
    • 2004
  • In the recent years, lightweight components fabricated with aluminum alloys have been applied into building the automobiles. Among the several competing fabrication methods, hot forging is taken as the most reliable technique to produce suspension parts such as control arms. Generally, Al forging products have been used widely for the aircraft building with the extruded stock as a starting material. For the economical base, however, the cast stocks turn to be as the forging stocks recently after a continuously casting technique was developed to produce quite a uniform microstructure enough to use for the forging process. Even more, there is a tendency to omit the homogenization step before forging, which is considered to be an indispensable process for all kinds of Al alloy, In the present study, a series of compression test was carried out to find out how the cast structure and the following heat treatments influence the deformation behavior, that is, forging characteristic.

  • PDF

High Temperature Deformation Behavior of Beta-gamma TiAl Alloy (Beta-gamma TiAl 합금의 고온변형거동)

  • Kim, J.S.;Kim, Y.W.;Lee, C.S.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2006.05a
    • /
    • pp.429-433
    • /
    • 2006
  • High Temperature deformation behavior of newly developed beta-gamma TiAl alloy was investigated in this study. The optimum processing condition was investigated with the aid of Dynamic Materials Model (DMM). Processing maps representing the efficiency of power dissipation for microstructural evolution and instability were constructed utilizing the results of hot compression test at temperatures ranging from $1000^{\circ}C$ to $1200^{\circ}C$ and strain rate ranging from $10^{-4}/s$ to $10^2/s$. The Artificial Neural Network (ANN) simulation was adopted to consider the deformation heating. With the help of processing map and microstructural analysis, the optimum processing condition was presented and the role of $\beta$ phase was also discussed in this study.

  • PDF

Deformation Behaviour of Ti-8Ta-3Nb During Hot Forging

  • Lee Kyung Won;Ban Jae Sam;Kim Sun Jin;Cho Kyu Zong
    • Journal of Mechanical Science and Technology
    • /
    • v.20 no.1
    • /
    • pp.13-18
    • /
    • 2006
  • Ti-8Ta-3Nb, as a new biomaterial, was prepared by cast and swaging process. Their deformation behavior of Ti-8Ta-3Nb alloy has been characterized on the basis of its flow stress variation obtained from the true strain rate compression testing in the temperature of $700-900^{\circ}C$ and strain rate of $0.001-10\;s^{-1}$. At the strain rates lower than $0.1\;s^{-1}$ and the all temperature ranges which consist of two phase ${\alpha}+{\beta}$ as well as single ${\beta}$ phase fields, the flow curves show a small degree of flow softening behavior. In contrast, the shapes of the flow curves at other strain rates indicate unstable behavior. The shapes of the flow curves were similar in both as-cast and swaged specimen as well as in both ${\alpha}+{\beta}$ phase and ${\beta}$ phase. The flow stress data did not obey the kinetic rate equation over the entire regime of testing but a good fit has been obtained in the intermediate range of temperatures ($750-850^{\circ}C$). In this range, a stress exponent value of about 7.7 in as-cast specimens and about 6.2 in swaged specimens with an apparent activation energy of about 300 kJ/mol and about 206 kJ/mol respectively have been evaluated.

Deformation Characteristics of Udimet 720Li during Isothermal Forging (Udimet 720Li 합금의 항온단조 변형특성)

  • Yeom J. T.;Na Y. S.;Park N. K.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2001.05a
    • /
    • pp.190-193
    • /
    • 2001
  • Hot deformation behavior of Udimet 720Li was characterized by compression tests in the temperature range of $1025^{\circ}C\;to\;1150^{\circ}C$ and the strain rate rage of $0.0005s^{-1}\;to\;5s^{-1}$. In order to characterize the dependence of flow stress on strain, strain rate and temperature, a constitutive equation based on hyperbolic sine formation was used. Isothermal forging of Udimet 720Li was performed in the temperature range $1050-1150^{\circ}C$ at strain rates of $0.05s^{-1}\;and\;0.005s^{-1}$. FE simulation was also carried out to predict deformation microstructures during isothermal forging.

  • PDF

Effect of Ca addition on the microstructure and mechanical properties of extruded AZ31 alloy (마그네슘합금 AZ31 압출재의 기계적특성에 미치는 Ca의 효과)

  • Kim, Jeoung-Han;Kang, Na-Eun;Lee, Sang-Bok;Yim, Chang-Dong;You, Bong-Sun;Kim, Byoung-Kee
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.10a
    • /
    • pp.281-284
    • /
    • 2007
  • The effect of Ca addition on the microstructure evolution and deformation behavior of AZ31 magnesium alloy produced by hot extrusion was investigated. For this purpose, Ca was added into AZ31 melts to the level of 0.7 and 2.0 wt.% Ca. Then, AZ31 base alloy and Ca modified AZ31 alloys were extruded at $383^{\circ}C$. Ca added alloys showed finer grain size and increased hardness value rather than AZ31 base alloy. After isothermal hot compression, the shape of tested specimen exhibited a noticeable anisotropy due to the crystallographic texture effect. The ratio of major and minor axes of ovality was not directly related to test condition and Ca amount. Flow stress level increases with the increase of Ca addition at temperature below $300^{\circ}C$ because of fine microstructure. However, at high temperature and low strain rate region ($400^{\circ}C$ and $10^{-3}s^{-1}$), reverse tendency was observed since main deformation mechanism changes from dislocation slip to grain boundary sliding or diffusional process at high temperature.

  • PDF

High Temperature Compressive Deformation Behavior of Ti-6Al-2Sn-4Zr-6Mo Alloy (Ti-6Al-2Sn-4Zr-6Mo 합금의 고온압축 변형거동)

  • Hyun, Yong-Taek;Lee, Yong-Tai;Lee, Chan-Gyu
    • Korean Journal of Materials Research
    • /
    • v.11 no.2
    • /
    • pp.82-87
    • /
    • 2001
  • The hot deformation behavior of Ti-6Al-2Sn-4Zr-6Mo(Ti6246) alloy was investigated in both the $\alpha$+$\beta$ and $\beta$-phase fields by conducting compression tests over a strain rate range of $10^{-3}s^{-1}$ to $10^0s^{-1}$. The flow stress was increased with increasing strain rate and decreasing test temperature. The flow curves obtained at temperatures below 90$0^{\circ}C$ exhibited a flow softening. However, in the $\beta$-phase field, above 95$0^{\circ}C$, the flow stress increased monotonically with plastic strain approaching steady state values. Constitutive equations for the dependence of flow stress on strain, strain rate, and temperature were developed through the analysis of the flow curves.

  • PDF

High Temperature Deformation Behavior of Microalloyed Hot Forging Steels (열간 단조용 비조질강의 고온 변형 거동에 관한 연구)

  • Wi, Gyeom-Bok;Lee, Gyeong-Seop
    • Korean Journal of Materials Research
    • /
    • v.2 no.5
    • /
    • pp.343-352
    • /
    • 1992
  • The high temperature deformation behavior of microalloyed hot forging steels has been examined as a function of the temperature, the strain rate, and the alloying element by using high temperature compression test. The high temperature deformation mechanism, which was obtained by analyzing the flow stress-strain curve and microstructure, could be considered to dynamic recrystallization. The peak stress of Nb-V-Mo steel was more increased and the dynamic recrystallization of Nb-V-Mo steel was faster than those of Nb-V steel. The peak stress of 1.2Mn-0.09Nb steel was more increased and the dynamic recrystallization of 1.2Mn-0.09Nb was delayed a little bit than those of 1.0Mn-0.05Nb. The peak stress of C-Nb-V steel was more increased and the dynamic recrystallization of C-Nb-V steel was delayed than those of C-steel. The constitutive equation of high temperature deformation had a power law type. The grain size of dynamic recrystallization was refined as the Zener-Hollomon parameter was increased. The relation of the dynamic recrystallization grain size and Zener-Hollomon parameter could be quantified to power law.

  • PDF

High temperature deformation behaviors of AZ31 Mg alloy by Artificial Neural Network (인공 신경망을 이용한 AZ31 Mg 합금의 고온 변형 거동연구)

  • Lee B. H.;Reddy N. S.;Lee C. S.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2005.10a
    • /
    • pp.231-234
    • /
    • 2005
  • The high temperature deformation behavior of AZ 31 Mg alloy was investigated by designing a back propagation neural network that uses a gradient descent-learning algorithm. A neural network modeling is an intelligent technique that can solve non-linear and complex problems by learning from the samples. Therefore, some experimental data have been firstly obtained from continuous compression tests performed on a thermo-mechanical simulator over a range of temperatures $(250-500^{\circ}C)$ with strain rates of $0.0001-100s^{-1}$ and true strains of 0.1 to 0.6. The inputs for neural network model are strain, strain rate, and temperature and the output is flow stress. It was found that the trained model could well predict the flow stress for some experimental data that have not been used in the training. Workability of a material can be evaluated by means of power dissipation map with respect to strain, strain rate and temperature. Power dissipation map was constructed using the flow stress predicted from the neural network model at finer Intervals of strain, strain rates and subsequently processing maps were developed for hot working processes for AZ 31 Mg alloy. The safe domains of hot working of AZ 31 Mg alloy were identified and validated through microstructural investigations.

  • PDF

Variation in Microstructural Homogeneity and Mechanical Properties of Extruded Mg-5Bi Alloy Via Controlling Billet Shape (빌렛 형상 제어를 통한 Mg-5Bi 합금 압출재의 조직 균일도 및 기계적 물성 변화)

  • Jin, S.C.;Cha, J.W.;Park, S.H.
    • Transactions of Materials Processing
    • /
    • v.31 no.6
    • /
    • pp.344-350
    • /
    • 2022
  • Extruded Mg-Bi binary alloys are known to have an undesirable bimodal grain structure containing a large amount of coarse unrecrystallized grains. Accordingly, to improve the microstructural homogeneity of extruded Mg-Bi alloys, it is necessary to promote the dynamic recrystallization (DRX) behavior during hot extrusion. An effective way to promote DRX is an increase in nucleation sites for DRX through a pre-deformation process before extrusion, such as cold pre-forging and hot pre-compression. However, the application of these pre-deformation processes increases the cost of final extruded Mg products because of an increase in energy consumption and decrease in productivity. Therefore, a low-cost new continuous process with high productivity is required to improve the microstructural homogeneity and mechanical properties of extruded Mg alloys without a drastic increase in the entire process cost. This study proposes a new extrusion method using an extrusion billet with a truncated cone shape (i.e., tapered billet) instead of a conventional extrusion billet with a cylindrical shape. When the hot extrusion of a Mg-5Bi alloy is conducted using the tapered billet, the DRX behavior during extrusion is considerably promoted. The DRX fraction and average grain size of the extruded alloy significantly increase and decrease from 65% to 91% and from 225 ㎛ to 49 ㎛, respectively. Consequently, the extruded Mg-5Bi alloy fabricated using the tapered billet has a finer homogeneous grain structure and higher tensile elongation than the extruded counterpart fabricated using the cylindrical billet.

Effect of Alloying Elements on Hardness Self-Control of Non-Heat-Treatable Steels (비조질강의 경도 자기제어에 미치는 합금원소의 영향)

  • Cho, Ki Sub;Kwon, Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.30 no.2
    • /
    • pp.67-73
    • /
    • 2017
  • Transformation behavior and hardness change were studied in five kinds of self-control steels; standard, high V, modified Ni, W, and high C-Ni steels. In the cooling rates of $10-100^{\circ}C/min$, the primary ferrite and bainite were formed, and the amount of the former increased with decreasing cooling rate. The bainite transformation temperature, Bs, was measured as 570, 560, 590, 575, and $565^{\circ}C$ in experimental steels, respectively, which was similar to the calculated temperature. The self-control, that is, the consistency in hardness, was observed, in which the hardness increased with the decrease in Bs. In the case of hot compression testing, the lower temperature deformation led to the enhancement in hardness.