• Title/Summary/Keyword: High-temperature compression test

Search Result 136, Processing Time 0.029 seconds

The effect of temperature in high temperature SHPB test (고온 SHPB실험에서 온도의 영향)

  • Park, Kyoung-Joon;Yang, Hyun-Mo;Min, Oak-Key
    • Proceedings of the KSME Conference
    • /
    • 2001.11a
    • /
    • pp.349-354
    • /
    • 2001
  • The split Hopkinson pressure bar has been used for a high strain rate impact test. Also it has been developed and modified for compression, shear, tension, elevated temperature and subzero tests. In this paper, SHPB compression tests have been performed with pure titanium at elevated temperatures. The range of temperature is from room temperature to $1000^{\circ}C$ with interval of $200^{\circ}C$. To raise temperature of the specimen, a radiant heater which is composed of a pair of ellipsoidal cavities and halogen lamps is developed at high temperature SHPB test. There are some difficulties in a high temperature test such as temperature gradient, lubrication and prevention of oxidation of specimen. The temperature gradient of specimen is affected by the variation of temperature. Barreling occurred at not properly lubricated specimen. Stress-strain relations of pure titanium have been obtained in the range of strain rate at $1900/sec{\sim}2000/sec$ and temperature at $25^{\circ}C{\sim}1000^{\circ}C$.

  • PDF

High Temperature Compressive Properties of Tungsten Activated Sintered Pare Prepared by 0.4 wt.% Ni-doped Tungsten Powder Compacts (0.4 wt% Ni을 첨가한 W 활성소결체의 고온압축 특성 연구)

  • 이승익;김순욱;박영삼;문인형
    • Journal of Powder Materials
    • /
    • v.9 no.5
    • /
    • pp.307-314
    • /
    • 2002
  • The high temperature deformation behavior of the activated sintered W powder compacts was investigated. The W compact showed the relative density of 94% with the average W grain size of $23\mutextrm{m}$ by activated sintering at $1400^{\circ}C$ for 1 hour. Compression tests were carried out in the temperature range of $900-1100^{\circ}C$ at the strain rate range of $10^{0}$/sec - $10^{-3}$/sec. True stress-strain curve and microstructure exhibited the grain boundary brittleness which was dependent on the compression test temperature. The activated sintered W compact showed that the maximum stress as well as the strain at the maximum stress was abruptly decreased as the test temperature increase from $900^{\circ}C$ to 1000 and $1100^{\circ}C$ regardless of the strain rate. The discrepancy of the microstructure in the specimen center was obviously observed with the increase of the test temperature. After compression test at $900^{\circ}C$ the W grain was severely deformed normally against the compression axis. However, after compression test at $1000^{\circ}C$ and $1100^{\circ}C$ the W grain was not deformed, but the microcrack was formed in the W grain boundary. The Ni-rich second phase segregated along the W grain boundary could be partly unstable over $900^{\circ}C$ and affect the poor mechanical property of the activated sintered W compact.

An Experimental Study on Quality Management of Strength in High Strength Mass Concrete Structure Using Thermal Insulation Material (보온재를 사용한 고강도 매스 콘크리트의 품질관리에 관한 연구)

  • Cho, Kyu-Hyun;Back, Min-Soo;Kim, Sung-Sik;Lim, Nam-Gi;Lee, Young-Do
    • Journal of the Korea Institute of Building Construction
    • /
    • v.4 no.2
    • /
    • pp.113-118
    • /
    • 2004
  • This study is a basic experiment on quality management of the compression strength of high strength concrete, aiming. at quality management of high strength mass concrete by giving the temperature hysteresis of the mass test pieces to managerial test pieces. Different from ordinary concrete, high strength concrete generally shows the temperature high rising caused by hydration heat inside the concrete. It is known that, in mass concrete, thermal stress occurs due to the difference in temperature between the inside and the outside, which causes a significant difference in compression strength between structure beams and managerial test pieces. It is also reported that there is a large difference between the compression strength of cylindrical managerial test pieces of standard underwater curing and the strength of structure beam concrete. Thus, this study made concrete test pieces in an optimal mix ratio for each strength level, and also created thermal insulation curing box and managerial test pieces. Then it carried out comparative analysis in relation to core strength and suggested equipment and a technique that can control the strength of high strength concrete mass more conveniently and accurately.

Deformation Property of TiC-Mo Solid Solution Single Crystal at High Temperature by Compression Test (TiC-Mo 고용체 단결정의 고온 압축변형 특성)

  • Shin, Soon-Gi
    • Korean Journal of Materials Research
    • /
    • v.24 no.11
    • /
    • pp.625-631
    • /
    • 2014
  • To investigate the deformation properties of TiC-(5-20) mol% Mo solid solution single crystals at high temperature by compression testing, single crystals of various compositions were grown by the radio frequency floating zone technique and were deformed by compression at temperature from 1250K to 2270K at strain rates from $5.1{\times}10^{-5}$ to $5.9{\times}10^{-3}/s$. The plastic flow property of solid solution single crystals was found to be clearly different among a three-temperature range (low, intermediate and high temperature ranges) whose boundaries were dependent on the strain rate. From the observed property, we conclude that the deformation in the low temperature range is controlled by the Peierls mechanism, in the intermediate temperature range by the dynamic strain aging and in the high temperature range by the solute atmosphere dragging mechanism. The work softening tends to become less evident with an increasing experimental temperature and with a decreasing strain rate. The temperature and strain rate dependence of the critical resolved shear stress is the strongest in the high temperature range. The curves are divided into three parts with different slopes by a transition temperature. The critical resolved shear stress (${\tau}_{0.2}$) at the high temperature range showed that Mo content dependence of ${\tau}_{0.2}$ with temperature and the dependence is very marked at lower temperature. In the higher temperature range, ${\tau}_{0.2}$ increases monotonously with an increasing Mo content.

Temperature Dependence of Dynamic Behavior of Commercially Pure Titanium by the Compression Test (CP-Ti의 동적거동에 미치는 온도의 영향)

  • Lee, Su-Min;Seo, Song-Won;Park, Kyoung-Joon;Min, Oak-Key
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.27 no.7
    • /
    • pp.1152-1158
    • /
    • 2003
  • The mechanical behavior of a commercially pure titanium (CP-Ti) is investigated at high temperature Split Hopkinson Pressure Bar (SHPB) compression test with high strain-rate. Tests are performed over a temperature range from room temperature to 1000$^{\circ}C$ with interval of 200$^{\circ}C$ and a strain-rate range of 1900 ∼ 2000/sec. The true flow stress-true strain relations depending on temperature are achieved in these tests. For construction of constitutive equation from the true flow stress-true strain relation, parameters for the Johnson-Cook constitutive equation is determined. And the modified Johnson-Cook equation is used for investigation of behavior of flow stress in vicinity of recrystalization temperature. The Modified Johnson-Cook constitutive equation is more suitable in expressing the dynamic behavior of a CP-Ti at high temperature, i.e. about recrystalization temperature.

Deformation Properties of TiC-Mo Eutectic Composite at High Temperature (TiC-Mo 공정복합재료의 고온 변형특성)

  • Shin, Soon-Gi
    • Korean Journal of Materials Research
    • /
    • v.23 no.10
    • /
    • pp.568-573
    • /
    • 2013
  • The deformation properties of a TiC-Mo eutectic composite were investigated in a compression test at temperatures ranging from room temperature to 2053 K and at strain rates ranging from $3.9{\times}10^{-5}s^{-1}$ to $4.9{\times}10^{-3}s^{-1}$. It was found that this material shows excellent high-temperature strength as well as appreciable room-temperature toughness, suggesting that the material is a good candidate for high-temperature application as a structure material. At a low-temperature, high strength is observed. The deformation behavior is different among the three temperature ranges tested here, i.e., low, intermediate and high. At an intermediate temperature, no yield drop occurs, and from the beginning the work hardening level is high. At a high temperature, a yield drop occurs again, after which deformation proceeds with nearly constant stress. The temperature- and yield-stress-dependence of the strain is the strongest in this case among the three temperature ranges. The observed high-temperature deformation behavior suggests that the excellent high-temperature strength is due to the constraining of the deformation in the Mo phase by the thin TiC components, which is considerably stronger than bulk TiC. It is also concluded that the appreciable room-temperature toughness is ascribed to the frequent branching of crack paths as well as to the plastic deformation of the Mo phase.

Investigation of High Temperature Deformation Behavior in Compression and Torsion of Ti-6Al-4V Alloy (Ti-6Al-4V합금의 비틀림 및 압축변형에 따른 고온변형거동 고찰)

  • Yeom, J.T.;Jung, E.J.;Kim, J.H.;Hong, J.K.;Park, N.K.;Lee, C.S.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.05a
    • /
    • pp.435-438
    • /
    • 2008
  • High temperature deformation of Ti-6Al-4V alloy with a lamellar colony microstructure was investigated by hot compression and torsion tests. The torsion and compression tests were carried out under a wide range of temperatures and strain rates with true strain up to 2 and 0.7, respectively. The processing maps were generated on the basis of compression and torsion test data and using the principles of dynamic materials modeling (DMM). The shapes of the strain-stress curves in alpha-beta region and processing maps obtained on the two different tests have been compared with a view to evaluate the effect of the microstructure evolution on the flow softening behavior of Ti-6Al-4V alloy with a lamellar colony microstructure.

  • PDF

Behaviors of UHPC-filled Q960 high strength steel tubes under low-temperature compression

  • Yan, Jia-Bao;Hu, Shunnian;Luo, Yan-Li;Lin, Xuchuan;Luo, Yun-Biao;Zhang, Lingxin
    • Steel and Composite Structures
    • /
    • v.43 no.2
    • /
    • pp.201-219
    • /
    • 2022
  • This paper firstly proposed high performance composite columns for cold-region infrastructures using ultra-high performance concrete (UHPC) and ultra-high strength steel (UHSS) Q960E. Then, 24 square UHPC-filled UHSS tubes (UHSTCs) at low temperatures of -80, -60, -30, and 30℃ were performed under axial loads. The key influencing parameters on axial compression performance of UHSS were studied, i.e., temperature level and UHSS-tube wall thickness (t). In addition, mechanical properties of Q960E at low temperatures were also studied. Test results revealed low temperatures improved the yield/ultimate strength of Q960E. Axial compression tests on UHSTCs revealed that the dropping environmental temperature increased the compression strength and stiffness, but compromised the ductility of UHSTCs; increasing t significantly increased the strength, stiffness, and ductility of UHSTCs. This study developed numerical and theoretical models to reproduce axial compression performances of UHSTCs at low temperatures. Validations against 24 tests proved that both two methods provided reasonable simulations on axial compression performance of UHSTCs. Finally, simplified theoretical models (STMs) and modified prediction equations in AISC 360, ACI 318, and Eurocode 4 were developed to estimate the axial load capacity of UHSTCs at low temperatures.

A Study on Microstructure and High Temperature Compression Characteristics of Silicide Eutectics (실리사이드 복합 공정합금의 미세조직 및 고온 압축특성)

  • Lee, Je-Hyun;Cho, Yong-Seong;Kang, Soo-Hyeon;Park, Jang-Sik;Kim, Sang-Sik
    • Journal of Korea Foundry Society
    • /
    • v.17 no.1
    • /
    • pp.85-92
    • /
    • 1997
  • There has been a considerable interest to develop the silicide alloys as high temperature structural materials because of their excellent high temperature stability and strength, however, their lack of room temperature ductility and toughness was a main obstacle for the application. In order to improve ductility while maintaining good high temperature properties, possible refractory metal-silicide eutectic alloys composed of fine two phases were prepared by VAR(Vacuum Arc Remelting). Three silicide alloys, $Nb-Nb_3Si$, $Ti-Ti_5Si_3$, $V-V_3Si$, were selected as prospecting silicide eutectics and those high temperature characteristics were evaluated by high temperature compression test.

  • PDF

Compression D/B for Liquid Segregation Control in Semi-Solid Forming Process and Its Application (반용융 성형공정에 있어서 액상편석제어를 위한 압축 D/B 및 응용)

  • 정경득
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1999.06a
    • /
    • pp.15-32
    • /
    • 1999
  • A relationship between stress and stain is very important to design a die to avoid defects of products during semi-solid forming process. Since the liquid will be of eutectic composition in alloys liquid segregation will result in significant or undesirable situation. The materials used in this experiment are A 357. A390, Al2024 alloys that is fabricated by the electro-magnetic stirring process from Pechiney in France. The compression test was performed by induction heating equipment and MTS. In order to prevent the liquid segregation these measured temperature would be useful to control of strain rate during compression test. The liquid segregation is controlled as change of the strain rate and solid fraction during the compression process, The characteristics of flow between solid and liquid phase considering liquid segregation is examined through the above experiments. In the case of medium and high volume fractions of solid the distribution of strain rate is calculated by using compression test data of semi-solid materials (SSM). The thixoforming experiments with the designed die are carried out successfully. The die filling patterns of SSM for variation of die temperature and pressing force have been investigated. The hardness of the thixoformed scroll products is evaluated in terms of the microstructure for each position.

  • PDF