• Title/Summary/Keyword: High-extrusion ratio

Search Result 48, Processing Time 0.021 seconds

The Characteristic of a Hydrostatic Extrusion of Magnesium Alloy(AZ31) (Mg 합금(AZ31)의 열간 정수압 압출 특성에 관한 연구(I))

  • Yoon D. J.;Seo Y. W.;Jeong H. G.;Na K. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.10a
    • /
    • pp.128-131
    • /
    • 2004
  • Magnesium alloys are being extensively used in weight-saving applications and as a potential replacement for plastics in electronic and computer applications. Magnesium alloy has some good characteristics, EMI shielding property and high specific strength. Nevertheless their high brittleness make it uneasy to process the magnesium. Magnesium alloys are extruded like aluminium alloys. The present work was done to find a characteristic of magnesium alloy(AZ31) changing the extrusion ratio 8.5, 19.1, 49 respectly and changing the die half angle $30^{\circ},\;45^{\circ},\;60^{\circ}$. Here this present done by the hydrostatic extrusion in the hot condition, $310^{\circ}$. The higher the extrusion ratio goes, the higher the extrusion force goes.

  • PDF

The Effect of Extrusion Temperature and Die Angle on Mechanical Properties of $SiC_p$/2024Al Composites Fabricated by Powder Extrusion Method (분말압출법으로 제조된 $SiC_p$/2024Al 복합재료에 있어서 압출온도와 다이각이 기계적 성질에 미치는 영향)

  • 성병진
    • Journal of Powder Materials
    • /
    • v.2 no.1
    • /
    • pp.44-52
    • /
    • 1995
  • Effects of the extrusion temperature and die angle on the tensile properties of SiCIyAl composites in powder extrusion have been investigated. SiCP/Al composites were extruded at various extrusion temperatures (450, 500, $550^{\circ}C$) under the extrusion ratio of 25 : 1. The ram speed was maintained at 13 cm/min for all the extrusion conditions. The surface of the extruded rod appeared to be smooth without tearing at 450 and 50$0^{\circ}C$, whereas it was very rough due to tearing at $550^{\circ}C$. It was found that the tensile strength and elongation of the composites extruded at $500^{\circ}C$ are greater than those of composites extruded at $450^{\circ}C$ This is due to the easier plastic deformation of composite extruded at $500^{\circ}C$, compared with the composites extruded at $450^{\circ}C$. The effect of die angle was examined under 20=60, 120, $180^{\circ}$die angles at extrusion temperature of $500^{\circ}C$ under 25:1 extrusion ratio. The tensile strength of the composites extruded with 20=$60^{\circ}$approved to be higher than that of the composties extruded with 28 : 120 and $180^{\circ}$This is attributable to the higher extrusion pressure, which mixed composite powders could be densely consolidated at elevated temperatures, resulting from high friction force between billet and sliding surface of conical die.

  • PDF

Extrusion Die Development of Interior & Exterior Parts for High Speed Train on Aluminum Alloys and Controls of Extrusion Conditions (고속전철 내·외장재용 알루미늄 합금의 압출 금형 개발 및 압출 조건의 제어)

  • Kim, Kee Joo
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.7
    • /
    • pp.50-55
    • /
    • 2018
  • The important thing in extrusion technology is the design and production of molds. Appropriate design of the molds is essential for achieving the desired extrusion of molds at the same time to maximize the life of the molds and increase their efficiency. The extrusion temperature and extrusion speed are the main parameters at the time of extrusion. Different extrusion conditions should be added depending on the extrusion ratio, physical properties of the material, and type of extrusion. In this study, the extrusion process of various 6xxx series aluminum cast alloys for high speed train interior or exterior parts were investigated. The extruded die design was performed for the 6063, 6061, 6N01, 6005, 5083 and 6060 alloy profiles and an extrusion test was conducted. In addition, the extrusion conditions, such as extrusion pressure following as the billet temperature, extrusion temperature, and materials change, were analyzed. Although the 6063 aluminum alloy can be extruded at the lowest temperature and pressure, the 6061 alloy can be extruded at the highest temperature and pressure. From these results, the successful extruded products were manufactured from these established conditions.

A Study on Extrusion Process of Cylindrical Product with Helical Fins Using Rotating Extrusion Die (회전압출다이를 사용한 헬리컬 핀붙이 원형단면 제품의 압출가공에 관한 연구)

  • Park S. M.;Jin I. T.
    • Transactions of Materials Processing
    • /
    • v.14 no.5 s.77
    • /
    • pp.444-451
    • /
    • 2005
  • A new extrusion process of the circular section product with helical fins could be developed by rotating extrusion die. The twisting of extruded product is caused by the twisted conical die surface connecting the die entrance section and the die exit section linearly. But, until now, because the process has used fixed extrusion die, it needs high pressure in order to twist billet and form fin shape on the surface of billet. So, during extruding billet, in order not to twist billet, the extrusion die is needed to rotate itself instead of twisting of billet. It is known that it is possible to reduce extrusion load of product with helical fins by analysis and experiments using rotating die. And it is known that, through the extrusion load analysis by $DEFORM^{TM}-3D$ software, optimal rotational velocity of rotating die can be obtained according to reduction ratio of area and twisted angle of die. And experiments and analysis using rotating extrusion die show that the twisted angle of product can be controlled by twisted angle of extrusion helical die and the rotational velocity of extrusion helical die.

Development of porthole Die on Aluminum Extrusion for the Automobile Control Arm (자동차용 컨트롤 암 알루미늄 열간 압출을 위한 포트홀 금형개발)

  • Joe, Young-June;Lee, Sang-Kon;Oh, Kae-Hee;Park, Sang-Woo;Lee, Woo-Sik;Jang, Gae-Won;Kim, Byung-Min
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.24 no.4 s.193
    • /
    • pp.102-108
    • /
    • 2007
  • The characteristic properties of aluminum, high strength stiffness to weight ratio, good formability, good corrosion resistence, and recycling potential make it the ideal candidate to replace heavier materials in the car to respond to the weight reduction demand within the automotive industry. In this paper, FE simulation was carried out to design an appropriate extrusion die for the automobile control arm. Based on the FE simulation result, a new die design has been proposed for uniform material flow in the cross section of extruded product. And then the welding pressure, extrusion load, and the tendency of mandrel deflection were estimated to verify high quality. In the extrusion experiment, it was possible to produce sound product without defects.

Effects of Initial Slug Design on the Earring of a Rectangular Battery Case During Impact Extrusion (충격압출 공정에서 초기 슬러그 디자인이 사각 배터리 케이스의 이어링에 미치는 영향 분석)

  • Lim, J. H.;Choi, S.;Chung, W. J.;Shin, J. H.;Lee, J.
    • Transactions of Materials Processing
    • /
    • v.24 no.6
    • /
    • pp.425-430
    • /
    • 2015
  • In the current paper, the effects of initial slug design on the earring of an Al rectangular battery case manufactured by impact extrusion were studied. During impact extrusion, non-uniform metal flow between the long and the short sides of the battery case leads to earring, which is subsequently trimmed. Process parameters such as friction, aspect ratio of the battery case, the die shape and the forming temperature tend to induce earring because they cause greater non-uniform metal flow. Large aspect ratio of the battery case and high friction between slug and die can greatly affect the earring of a rectangular battery case. To make a rectangular battery case without earring, it is necessary to control metal flow uniformly during impact extrusion. One of the ways to reduce the earring is to control the metal flow of slug at the initial upsetting stage. To analyze the effects of the initial slug design on earring, FE analysis was conducted using DEFORM 3D. Two types of initial slug designs were evaluated where volume was removed along either the width or thickness directions. The results show that the initial slug design can be effective in adjusting the uniformity of metal flow.

Fine Wire Extrusion Technology (극세선 압출 기술 개발)

  • Kim S. S.;Park H. J.;Jun D. J.;Lim S. J.;Choi T. H.;Na K. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2001.10a
    • /
    • pp.97-101
    • /
    • 2001
  • Fine metal (Au, Ag, Cu) wire was extruded with hydrostatic extrusion process in cold condition. A vertical type 900kN hydrostatic extruder has been developed. The extruder was facilitated with high pressure container which are available for hot and cold forming. The container endured 1400MPa internal pressure and extrusion ratio To was achieved in cold forming for Au fine wire which had $600{\mu}m$ diameter. In contrast to the conventional macroscopic-sized-billet fine-wire requires higher extrusion pressure and effect of friction is much more significant.

  • PDF

Strengthening of Rapidly Solidified and Extruded Mg Alloy Powders (압출공정을 이용한 급속응고 Mg 합금분말의 고강도화)

  • Kim, Taek-Soo
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.10a
    • /
    • pp.35-37
    • /
    • 2008
  • The light Mg alloys bearing the remarkably high strength, corrosion resistance and elevated temperature stability stand on the center of interest. The accomplishment so far is, however, only by alloy modification without any consideration on the rapid solidification effect. This work is to report not only the effect of rapid solidification of $MgZn_{4.3}Y_{0.7}$ alloy powders, but the extrusion behavior on the materials properties. The average grain size of the atomized powders was about $3-4{\mu}m$. The extrusion was carried out with the area reduction ratio of 10:1 to 15:1. As the ratio increased, homogeneous microstructure was obtained, and the mechanical properties such as tensile strength and elongation were simultaneously increased.

  • PDF

Fabrication of a Micro Die by LIGA Process and Hybrid Powder Extrusion Process of Micro-spur Gear (LIGA 공정을 이용한 초소형 스퍼기어 금형 제작 및 하이브리드 분말 압출성형)

  • Lee, K.H.;Hwang, D.W.;Kim, J.H.;Jang, S.S.;Kim, B.M.
    • Transactions of Materials Processing
    • /
    • v.19 no.6
    • /
    • pp.352-356
    • /
    • 2010
  • This paper was designed to fabricate the micro-spur gear by the LIGA and hybrid powder extrusion process. It is important to manufacture a micro-die with a high aspect ratio and determine appropriate extrusion conditions for a microforming. Ni has been used to fabricate micro-dies. LIGA process was capable to produce micro-extrusion dies with close tolerance, longer bearing length and adequate surface quality. Superplastic Al-78Zn powders have the great advantage in achieving deformation under low stresses and exhibiting good micro-formability with average strain rate raging from $10^{-3}$ to $10^{-2} s^{-1}$ and constant temperature ranging from 503 to 563K. Al-78Zn powders were compacted into a cylindrical shape ($\Phi3\times$h10mm) under compressive force of 10kN and, subsequently, the compacted powders were extruded by the hybrid powder extrusion process controlling of the temperature holing time for a improvement on formability of Al-22Zn powder. Micro-extrusion has succeeded in forming micro-gear shafts.