고로슬래그를 혼화재로 혼입한 투수콘크리트의 물리적 특성에 과한 실험적 연구 (An Experimental Study on the Physical Properties of Porous Cement Concrete Using Blast-furnace Slag as an Admixture)

  • 심종우;채창우
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.144-149
    • /
    • 2000
  • Porous cement concrete was developed to prevent hydroplaning of airway pavement or to reduce noise emission in highway. In has been introduced in domestic since early 1980' and applied to a pedestrian road or bike way. The concrete, however, has problems such as lack of optimized mix design, low strength and deterioration, etc. The purpose of this study is to manufacture porous cement concrete using blast-furnace slag to enhance mechanical properties. The results of this study are as follows; the compressive strength range is 102∼247kgf/㎠, the tensile strength range is 16∼70kgf/㎠, the bending strength range is 43∼70kgf/㎠, and the coefficient permeability range is 6.79 ×10-2∼1.17∼10-1cm/sec. To develope high-performance porous concrete, further studies are needed on optimum mixture of fineness modulus and admixture.

  • PDF

동절기 무양생 콘크리트의 현장적용 성능 평가에 관한 연구 (Study on the Properties of Field Applied Non-Curing Concrete in Winter Season)

  • 유조형;김우재;홍석범;김형철;이한승
    • 한국건축시공학회지
    • /
    • 제16권5호
    • /
    • pp.413-419
    • /
    • 2016
  • 동절기 콘크리트 공사에서는 무엇보다도 저온환경에서의 콘크리트의 안정적인 품질 확보가 중요하다. 따라서 본 연구에서는 고분말도 발열분체를 적용하여 동절기($0^{\circ}C$이하)에서도 양생 없이 강도발현이 가능한 콘크리트를 개발하였으며, 이를 현장에 적용하기 위해 실 부재 사이즈의 Mock-Up 부재를 제작하여 개발기술의 현장적용 성능평가를 실시하였다.

저열 포틀랜드 시멘트를 사용한 초고강도 분체 콘크리트 개발에 관한 실험적 연구 (An Experimental Study on Developing Ultra-High Strength Powder Concrete Using Low-heat Portland Cement)

  • 조병완;윤광원;김헌;박진모
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제13권6호통권58호
    • /
    • pp.135-147
    • /
    • 2009
  • 본 논문에서는 저열포틀랜드 시멘트와 steel aggregates인 Ferro-Silicon, 실리카흄, 충전재로서 미세 석영과 고강도화에 따른 취성파괴 문제를 개선하기위해 강섬유를 사용하여 압축강도 400MPa이상의 초고강도 분체 콘크리트를 개발 하고자 하였다. 콘크리트의 초고강도화의 영향을 고려하여 물-시멘트비 저감이 가능한 저열포틀랜드 시멘트와 비교대상으로 보통포틀랜드 시멘트를 사용하고, 골재 대체 재료로 Ferro Silicon을 각각의 배합비, 양생조건을 달리하여 압축강도를 비교분석 하였다. 초고강도 콘크리트는 보통콘크리트와 달리 사용재료의 영향이 대단히 중요하며, SEM 촬영결과 Type III, Type IV의 C-S-H수화물이 비교적 많이 생성되었고, 고온고압양생으로 토버모라이트와 조놀라이트가 생성된것을 확인 하였다. 또한 골재의 세립화, 분체의 치밀충전화 및 반응성 재료의 사용으로 인해 페이스트가 고강도화 되고, 강섬유를 사용하여 인성을 보강하므로써, 28일 압축강도 420Mpa의 초고강도 분체콘크리트를 성공적으로 개발 하였다.

Analysis of Characteristics of Slurry and Thermal Insulation Materials Using Hauyne Cement

  • Kim, Tae Yeon;Jo, Ki Sic;Chu, Yong Sik
    • 한국세라믹학회지
    • /
    • 제56권5호
    • /
    • pp.468-473
    • /
    • 2019
  • This study focused on manufacturing an inorganic insulation material set with various amounts of calcium-sulfoaluminate (CSA) (hauyne) content for enhancing both workability (demolding, handling) and the high thermal insulating property. To carry out the experiment, the amounts of CSA utilized were 5%, 10%, 15%, and 20%, with anhydrous gypsum added in equal proportion to produce a stable formation. As the content of CSA increased, a sinking phenomenon occurred because of the hydration reaction from the slurry, so it was difficult to utilize a retarder normally used in the cement manufacturing process. However, an RCOOM surfactant was able to solve the local clumping problem from cement and CSA and obtain a rapid retarding effect, so it was included in this process at 0.3%. Furthermore, the cement fineness was not 7000 ㎠/g but rather 3300 ~ 4000 ㎠/g to prevent a rapid temperature increase in the slurry. The specific gravity of the sample manufactured with 20% CSA was approximately 0.11 g/㎤, and its thermal conductivity was 0.041 W/m·K, providing an excellent insulating property.

알칼리 자극제로서 미분시멘트와 순환골재가 고로슬래그 다량치환 콘크리트의 공학적 특성 및 미세구조에 미치는 영향 (Effect of Fine Particle Cement and Recycled Aggregates as Alkali Activator on the Engineering Properties and Micro-Structure of High Volume Blast Furnace Slag Concrete)

  • 한민철;이향재;한천구
    • 한국건축시공학회지
    • /
    • 제13권6호
    • /
    • pp.602-608
    • /
    • 2013
  • 본 연구에서는 BS다량 치환 콘크리트의 알칼리자극제로서 순환골재 및 고분말도의 FC를 복합 사용한 콘크리트의 제반 공학적 특성 및 미시적 분석을 실시하였다. FC 치환에 따른 슬럼프 및 공기량은 큰 차이가 없었으며, 응결시간은 FC 치환에 따라 비례적으로 단축되는 것으로 나타났다. FC 치환에 따른 압축강도는 고분말도의 FC가 치환됨에 따라 촉진된 수화반응 및 순환골재의 미수화 시멘트의 알칼리 용출로 인해 BS의 잠재수경성 반응을 촉진시켜 초기 및 28일 재령에서의 Plain 대비 강도저하를 상당부분 회복할 수 있었으며, 특히 향후 재령이 경과함에 따라 포졸란 반응의 활성화로 추가적인 강도향상이 기대된다. 탄산화 저항성의 경우 큰 차이가 없으며, 세공분포의 경우 FC 치환률이 증가함에 따라 $0.1{\mu}m$이하의 미세 공극분포가 급격히 증가하는 경향을 보였고, SEM 측정결과 FC 치환에 따른 7일 및 28일에서의 C-S-H 및 $Ca(OH)_2$의 생성을 확인하여 FC가 BS 다량치환 순환골재 콘크리트의 알칼리 자극에 기여함을 확인 할 수 있었다.

세골재의 조립율에 따른 고유동콘크리트의 유동특성에 관한 실험적 연구 (An Experimental Study on the Fludity of High Flowing Concrete according to the Fineness Modulus of Fine Aggregate)

  • 박유신;강석표;조성현;최세진;김규용;김무한
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 가을 학술발표회 논문집
    • /
    • pp.385-390
    • /
    • 1997
  • In the mixing proportion of high flowing concrete we have to use quantity of power such as cement and superplasticizer, and increase the proportion of fine aggregate more than that of plain concrete to increase flowability and segregation resistance. Therefore, the fresh state of high flowing concrete is largely affected by superplasticizer and change of grade the percentage of surface water. This study aims at development of self-filling up high flowing concrete without compaction, in case of using the fine aggregate of standard grade range, by examination on the influence of fresh state of high flowing concrete, and by understanding influence on various fluidity such as flowability, reinforcement passibility, fillingability, segregation resistance.

  • PDF

폴리머를 혼화재로 혼입한 투수콘크리트의 물리적 특성에 관한 실험적 연구 (An Experimental Study on the Physical Properties of Porous Cement Concrete Using Polymer as an Admixture)

  • 채창우;민병렬;심종우
    • 콘크리트학회논문집
    • /
    • 제12권5호
    • /
    • pp.131-139
    • /
    • 2000
  • Porous Concrete usually contains large amount of voids(about 10∼20%) after compaction so that it has relatively high permeability. It has been introduced in domestic since early 1980's but it has problems such as lack of optimized mixture, low strength and durability, and other defects, etc. The purpose of this study is to manufacture high-performance porous concrete using polymer to enhance the mechanical properties. The results of this study are as follows; the compressive strength range 12 92∼207kgf/㎠, the tensile strength range is 14∼28kgf/㎠, the bending stength range is 42∼73kgf/㎠, and the coefficient permeability range is 5.77×10-2∼6.79×10-1cm/sec. To develope high-performance porous concrete. further studies are needed on optimum mixture of fineness modulus and admixture.

나노슬래그와 알칼리 자극제를 활용한 비소성 시멘트 모르타르에 관한 연구 (Study of Non Sintered Cement Mortar Using Nanoslag and Alkali Activator)

  • 정성욱;임남기
    • 한국건축시공학회지
    • /
    • 제10권6호
    • /
    • pp.61-66
    • /
    • 2010
  • 현재 지구촌 온난화에 의하여 환경이 열악해지고 있으며 그에 따라 건설분야에도 시멘트 제조에 따른 $CO_2$ 발생 저감하기 위한 노력을 하고 있다. 이에 시멘트 대체할 재료가 필요하다. 본 연구에서는 기존 비소성 시멘트의 문제점으로 지적 되는 경제성 및 초기강도 확보를 위해 산업부산물인 고로슬래그를 대상으로 연구를 진행하였으며 고가의 알칼리 자극제량을 최소화함으로서 실용화 가능한 비소성 시멘트 기술을 진행하고자 한다. 그리고 NT를 사용하여 분말도를 최대화 하여 고로슬래그의 초기강도를 개선시켰다. 본 연구는 알칼리 자극제를 사용한 나로슬래그를 치환한 비소성시멘트를 기초로 하고 있으며, 현장에서 사용가능한 비소성시멘트의 기초적 물성 및 품질을 조사하였다. 여러 자극제가 슬래그 중량의 10%로 사용되었으며 휨강도, 압축강도, 응결시간, 단열온도, 상승열등을 비교 분석하였으며 그 기초적 자료를 제시하는데 목적이 있다.

Mix Design for Pervious Recycled Aggregate Concrete

  • Sriravindrarajah, Rasiah;Wang, Neo Derek Huai;Ervin, Lai Jian Wen
    • International Journal of Concrete Structures and Materials
    • /
    • 제6권4호
    • /
    • pp.239-246
    • /
    • 2012
  • Pervious concrete is a tailored-property concrete with high water permeability which allow the passage of water to flow through easily through the existing interconnected large pore structure. This paper reports the results of an experimental investigation into the development of pervious concrete with reduced cement content and recycled concrete aggregate for sustainable permeable pavement construction. High fineness ground granulated blast furnace slag was used to replace up to 70 % cement by weight. The properties of the pervious concrete were evaluated by determining the compressive strength at 7 and 28 days, void content and water permeability under falling head. The compressive strength of pervious concrete increased with a reduction in the maximum aggregate size from 20 to 13 mm. The relationship between 28-day compressive strength and porosity for pervious concrete was adversely affected by the use of recycled concrete aggregate instead of natural aggregate. However, the binder materials type, age, aggregate size and test specimen shape had marginal effect on the strength-porosity relationship. The results also showed that the water permeability of pervious concrete is primarily influenced by the porosity and not affected by the use of recycled concrete aggregate in place of natural aggregate. The empirical inter-relationships developed among porosity, compressive strength and water permeability could be used in the mix design of pervious concrete with either natural or recycled concrete aggregates to meet the specification requirements of compressive strength and water permeability.

흙도로포장용 재료로서 폐콘크리트 미분말의 활용성 연구 (Utilizability of Waste Concrete Powder as a Material for Soil Pavement)

  • 김용직;최연왕;김영진
    • 한국건설순환자원학회논문집
    • /
    • 제3권3호
    • /
    • pp.277-282
    • /
    • 2015
  • 본 연구는 고품질의 재생골재 제조시 발생하는 폐콘크리트 미분말을 콘크리트용 혼화재료로 활용하기 위한 연구이며, 분말도는 $928cm^2/g$인 폐콘크리트 미분말에 대하여 검토하였다. 폐콘크리트 분말의 주요 특징은 시멘트와 유사한 각진 입형을 나타내고 있었으나 입자 표면에 수화생성물들이 부착되어 있었다. 또한 시멘트와 비교하여 폐콘크리트 분말의 입자 크기는 크게 나타났으며, 화학성분은 $SiO_2$ 함량이 높게 나타났다. 한편, 도로포장은 대부분이 표층에 불투수층인 아스팔트 및 시멘트 콘크리트를 사용한 포장으로 노상과 표층이 차단됨에 따라 노상의 흙은 점진적으로 산성화가 진행되어 영양물질이 부족하여 미생물이 서식하지 못하게 될 뿐만 아니라 토양의 건조화가 진행되어 여러 가지 환경문제가 발생하고 있다. 연구 결과 개발된 Road Compound 및 New Road Compound로써 표층흙을 고화시킬 목적으로 사용할 경우 압축강도를 5MPa에서 최대 29MPa정도까지 발현시킬 수 있으므로 흙포장 도로의 사용목적에 따라 즉 압축강도가 12~15MPa 범위에서는 보도 및 자전거도로용, 15~18MPa 범위에서는 경교통로 및 주차장용, 18~25MPa 범위에서는 일반도로용으로 사용이 가능할 수 있을 것으로 판단된다. 또한, Road Compound 및 New Road Compound의 혼합률을 조정하면 지반개량공사에 있어 연약지반 개량 및 안정처리용 등으로 폭 넓게 활용할 수 있을 것으로 판단된다.