• 제목/요약/키워드: Hardened width and depth

검색결과 15건 처리시간 0.021초

레이저 표면 경화 공정에서 다점 온도 모니터링을 통한 경화층 크기 예측 (Estimation of Hardened Layer Dimensions Using Multi-Point Temperature Monitoring in Laser Surface Hardening Processes)

  • 우현구
    • 제어로봇시스템학회논문지
    • /
    • 제9권12호
    • /
    • pp.1048-1054
    • /
    • 2003
  • In laser surface hardening processes, the geometrical parameters such as the depth and the width of a hardened layer can be utilized to assess the hardened layer quality. However, accurate monitoring of the geometrical parameters for on-line process control as well as for on-line quality evaluation is very difficult because the hardened layer is formed beneath a material surface and is not visible. Therefore, temperature monitoring of a point of specimen surface has most frequently been used as a process monitoring method. But, a hardened layer depends on the temperature distribution and the thermal history of a specimen during laser surface hardening processing. So, this paper describes the estimation results of the geometric parameters using multi-point surface temperature monitoring. A series of hardening experiments were performed to find the relationships between the geometric parameters and the measured temperature. Estimation results using a neural network show the enhanced effectiveness of multi-point surface temperature monitoring compared to one-point monitoring.

금형용 합금공구강 STD11의 레이저 표면경화 특성 (The Laser hardening Characteristics of the Alloy Tool Steels STD11)

  • 조용무;김재도
    • 열처리공학회지
    • /
    • 제6권4호
    • /
    • pp.230-236
    • /
    • 1993
  • The laser beam hardening has been experimentally tried to find the hardened characteristics of STD11. Experiment was performed on the optimum hardening condition with 2kW $CO_2$ laser. The microstructure of the hardened layers was observed using the microscope. The hardened zones exhibits very high Vickers microhardness of 720 Hv, however, the deoxidation was observed under the surface of hardened area. The case depth of hardened zones is about 0.6mrn and case width is 4mm. FEM-simulation on laser surface hardening of STD11 steel are described. With the proper assumption of the absorbed energy density, the calculated case depth and width in 2 kW $CO_2$ laser hardening were in good agreement with the experimental result. It was found that there is optimum absorbed energy density of STD11.

  • PDF

YAG 레이저에 의한 SK5 표면경화 특성 (Surface Hardening Characteristics of SK5 Steel by Pulsed YAG LASER)

  • 강형식;문종현;전태옥;박홍식
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1995년도 추계학술대회 논문집
    • /
    • pp.921-924
    • /
    • 1995
  • Case hardening behavior of carbon tool steel(SK5) was investigated after pulsed YAG laser irradiation. In the case od beam passes,martensite formed in the melt zone and in former pearlite regions of the austenitization zone exhibits vary high Vickers hardness values. The molten depth and width decrease as the beam power density increase. The influence of depth and width of color painted specimen was also investigated. The molten zone of the black painted specimen was the largest. The were loss of the black painted specimen was smaller than any other painted or raw material.

  • PDF

실시간 출력 제어를 통한 구상흑연 주철의 레이저 표면경화 특성 (Characteristics of Surface Hardening by Laser Power Control in Real Time of Spheroidal Graphite Cast Iron)

  • 김종도;송무근
    • 한국레이저가공학회지
    • /
    • 제18권2호
    • /
    • pp.1-4
    • /
    • 2015
  • This study is related to the surface hardening treatment to spheroidal graphite cast iron for die by using high power diode laser. Laser device used in this experiment is capable of real-time laser power control. This is because the infrared temperature sensor (two color pyrometer) attached to the optical system measures the surface temperature of specimen and adjusts the laser power in real time. The surface treatment was carried out with the change of heat treatment temperature at the beam travel speed 3 mm/sec. Hardened width and depth was measured and hardened zone was analyzed by micro vickers hardness test in order to research the optimum condition of heat treatment. The changes in microstructure of the hardened zone also was examined. As a result of hardness measurement and observations on microstructure of hardened zone, hardness increased over three times as compared with base metal because the martensite was formed on the matrix structure.

물림조건에 따른 경화강의 절삭저항 특성에 관한 연구 (A Study on the Cutting Resistance Characteristics of Hardended Steel according to Engagement Condition)

    • 한국생산제조학회지
    • /
    • 제5권3호
    • /
    • pp.58-65
    • /
    • 1996
  • This thesis is concerned with the study on the characteristics of the cutting resistance occurring in finish machining of hardened steels such as carbon tool steel and alloy tool steel by a ceramic tool with nose radius. For the purpose, the shape of cutting cross-section made at nose part of the tool was analyzed geometrically and the wear mechanism on the flank face of the ceramic tool is investigated. In order to investigate the characteristics of cutting resistance two categories of cutting conditions are suggested, along with geometrical analysis. One category includes the conventional cutting parameters such as feed and depth of cut, another containing new cutting parameters of thickness of cut and width of cut etc. Thickness of cut width of cut and area of undeformed chip section formed by the condition of engagement between workpiece and cutting tool are determined as the function of feed, depth of cut and nose radius of cutting too, And an effective approach angle is determined by depth of cut and nose radius.

  • PDF

고출력 레이저에 의한 표면 경화 (Transformation Hardening of High Power Laser)

  • 김재도
    • 열처리공학회지
    • /
    • 제8권1호
    • /
    • pp.24-31
    • /
    • 1995
  • Heat flow equation and FEM have been used to calculate the hardening section of material in laser transformation hardening. SCM440 used as the diesel engine piston of vessel has been hardened by a $CO_2$ laser with the wavelength of $10.6{\mu}m$. The specimens were inclined from 0 to 70 degree to investigate the characteristics of laser hardening. The geometrical factor of heat flow equation affects the size of hardening area. The case width decreased with increasing travel speed and the case width increased with increasing inclined angle. Maximum case depth was achieved about 1.0mm and maximum hardness of laser hardened area was of 2.8 times than that of base metal. Experimental data show good agreement with the theoretical calculations for given laser hardening conditions.

  • PDF

SM 45C강의 레이저 표면경화처리에 관한 연구 (A study on the laser surface hardening of SM 45C steel)

  • 나석주;김성도;이건이;김태균
    • 대한기계학회논문집
    • /
    • 제11권1호
    • /
    • pp.53-62
    • /
    • 1987
  • 본 논문에서는 1 KW CW CO$_{2}$레이저 발생자장치를 사용하여 표면경화 처리 를 행할때 공정과 관련된 변수들이 용접부 및 표면경화층에 미치는 영향들을 이론과 실험을 통해서 규명하고, 이 결과들을 실제공정에 사용할 수 있는 기초자료로서 제시 하고자 한다. 이를 위해서 해석에 사용될 수 있는 유한요소법(Finite Element Meth- od)에 근거한 2차원 열유동 해석용 프로그램 및 데이타 처리 프로그램을 개발하고, 중 탄소강에 레이저 표면처리를 수행하여 실험 및 이론해석의 결과를 비교 검토하였다. 비교 검토하여 그 설정기준을 고찰하였다.

Yb:YAG 디스크로 레이저 표면 용융 경화된 SKD61 열간금형강의 경도와 미세조직에 미치는 레이저 출력의 영향 (Effects of laser power on hardness and microstructure of the surface melting hardened SKD61 hot die steel using Yb:YAG disk laser)

  • 이광현;최성원;강정윤
    • Journal of Welding and Joining
    • /
    • 제33권3호
    • /
    • pp.54-61
    • /
    • 2015
  • In this study, effect of laser power on hardness and microstructure of SKD61 Hot Die steel of which surface was melted and hardened with Yb:YAG disk laser was investigated. Beam speed was fixed at 70 mm/sec and distance between them was 0.8 mm about Laser surface melting. The only thing that was changed laser power. Laser powers were 2.0, 2.4 and 2.8 kW. No defect was found under all conditions. As the laser power increased, the penetration depth were deepened and the bead width was also widened. There was no hardness deviation of fusion zone at same laser power and it was higher than that of heat affected zone. In addition, the more laser power increased, the more hardness in fusion zone decreased. Fusion zone was macroscopically dendrite structure. However, core matric in dendrite was lath martensite of 100 nm size. There were $M_{23}C_6$ of 500 nm and the VC and $Mo_2C$ of a nano meters on boundary of dendrite.

고출력 다이오드 레이저(HPDL)를 이용한 탄소강 환봉의 표면변태경화 (Surface Transformation Hardening for Rod-shaped Carbon Steels by High Power Diode Laser)

  • 김종도;길병래;강운주
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제31권8호
    • /
    • pp.961-969
    • /
    • 2007
  • The laser material processing has replaced a conventional material processing such as a welding, cutting, drilling and surface modification and so on. LTH(Laser Transformation Hardening) is one branch of the laser surface modification process. A lot of energy is needed for the LTH process to elevate workpiece surface to temperature of the austenite transformation($A_3$), which results from utilizing a beam with a larger size and lower power intensity comparatively. The absorptivity of the laser energy with respect to material depends on the wave length of a beam. This study is related to the surface hardening for the rod-shaped carbon steel by the high power diode laser(HPDL) whose beam absorptivity is better than conventional types of lasers such as $CO_2$ or Nd:YAG laser. Because a beam proceeds on the rotating specimen the pretreated hardened-phase can be tempered and softened by the overlapping between hardened tracks. Accordingly, the longitudinal hardness measurement and observation of the micro structure was carried out for an assessment of the hardening characteristics. In addition, a hardening characteristics as a hardenability of materials was compared in the point of view of the hardness distribution and hardening depth and width.

다이오드 레이저를 이용한 탄소강 환봉의 표면변태 경화특성 (Characteristics of Surface Transformation Hardening for Rod-shaped Carbon Steels by Diode Laser)

  • 김종도;강운주;이수진;윤희종;이제훈
    • 한국레이저가공학회지
    • /
    • 제11권4호
    • /
    • pp.7-12
    • /
    • 2008
  • Laser Transformation Hardening(LTH) is one branch of the laser surface modification processes. A lot of energy is needed for the LTH process to elevate workpiece surface to temperature of the austenite transformation($A_3$), which results from utilizing a beam with a larger size and lower power density comparatively. This study is related to the surface hardening for the rod-shaped carbon steel by the high power diode laser whose beam absorptivity is better than conventional types of lasers such as $CO_2$ or Nd:YAG laser. Because a beam proceeds on the rotating specimen, the pretreated hardened-phase can be tempered and softened by the overlapping between hardened tracks. Accordingly, the longitudinal hardness measurement and observation of the micro structure was carried out for an assessment of the hardening characteristics. In addition, a hardening characteristics as a hardenability of materials was compared in the point of view of the hardness distribution and hardening depth and width.

  • PDF