Hard coatings playa continuously increasing role in the field of tribology as well as for decorative applications. In both areas they are often also exposed to corrosive media. While especially hard nitride coatings show a high corrosion resistance for themselves, hard $coating_strate systems may suffer from a severe corrosion attack due to the defects in the coating structure (pores, pinholes) resulting from the PVD-typical film morphology. While a huge number of investigations cover the tribological properties, only limited studies deal with the corrosion behavjour of coating substrate systems and attempts are made to improve their corrosion resistance. The present paper shortly describes the corrosion mechanisms and repots characteristic examples of the system behaviour. Special emphasis is laid on recent investigations to improve the corrosion resistance by alloying, interlayers or multilayered coating structures.es.
Poly(urethane acrylate) siloxane oligomers with Interpenetrating polymer netwoked nanoparticles were prepared to synthesize hard coating solution by reaction with diisocyanates. The diisocyanate combined siloxane hard coating solution showed more flexibility than the siloxane solution. In addition, diisocyanate resulted in improvement of curl property and surface hardness in the siloxane solution. Of the used diisocyanates, isophorone diisocyanate and acryloyloxy ethyl diisocyanate were good for UV hard coating solution. This effect will decrease brittleness in the siloxane solution using for plastic display plate.
UV curable transparent hard coating materials have been developed to improve the mechanical and optical properties of PET substrate. The coating materials were synthesized using various urethane acrylate oligomers, monomers, photo initiators, and leveling agents. The materials were coated on PET substrates and UV cured. The hard coated PET films were shown to have the good scratch resistance and transparency. When the urethane acrylate oligomer with more functional groups was introduced into the coating solution, the mechanical and optical properties were improved. However the higher concentration of 9-functional oligomer resulted in the decrease of workability. The addition of trimethylolpropane ethoxylate$(EO/OH)_9$ triacrylate(TMPETA) to coating solution improved the workability and properties. As a result, the UV cured film from the formulation of urethane acrylate oligomer with 9-functional groups, TMPETA as a monomer, IRACURE 754 as a photo initiator and BYK-340 as a leveling agent showed the best mechanical and optical properties in this study.
본 연구는 건축자재로 널리 사용되는 PVC 바닥상재의 표면을 스크래치로부터 보호하기 위하여 기존에 사용하는 광경화형 우레탄-아크릴 수지에 내마모성을 향상시킨 광경화형 하드 코팅액 개발에 관한 것이다. PVC 바닥상재용으로 사용되는 내마모성이 없는 우레탄-아크릴 수지에 $Al_2O_3$(Al-160SG-3), $Al(OH)_3$(SH-8W) 및 $SiO_2$(KS-5000) 등 서로 다른 내마모성을 지닌 물질을 분말 형태로 수지의 양 대비 함량(wt%)을 $10{\sim}30%$로 변화하여 첨가한 후 링밀(Ring Mill)을 사용, 배합하여 수지의 내마모성을 향상시킨 하드 코팅액을 제조하였다. 제조한 하드 코팅액은 코팅층의 두께조절이 가능한 코팅(Bar-coating)을 사용하여 PVC 바닥상재에 코팅 한 후 내마모성, 연필경도, 부착력, 코팅두께 등의 코팅층 표면물성을 평가하였다. 연구결과, 수지에 $Al_2O_3$ 분말 30%를 혼합하여 제조한 하드 코팅액이 내마모성 1등급, 연필경도 H, 부착력 100%로 가장 좋은 물성을 보였으며, 전반적으로 입자크기가 작고, 분말 함량이 많을수록 또한 코팅두께가 두꺼워 질수록 경도 및 내마모성이 우수한 것으로 나타났다.
Our team works on mixture of hard magnetic materials. As hard magnetic material we used mixture of powders: melt-spun ribbon Nd-Fe-B, ferrite and Alnico. Their different mixtures are basic material for dielectromagnets under our investigation. Main disadvantage of dielectromagnets with Nd-Fe-B alloy powder as a component is a low corrosion resistance. Protection against corrosion is covering dielectromagnets with metallic or organic coating film. The coating film protects dielectromagnets from free particles on the surface and low resistance for mechanical stresses too. The surface of dielectromagnets prepared from mixture of powders if formed by metallic particles - powder of Nd-Fe-B and Alnico, particles of oxide - powder of ferrite and particles of resin - bonding materials. Team work on technology of laying the metallic coating on dielectromagnets prepared from mixture of mentioned powders. Papers show the results of initial investigation on metallic coating technology. It shows influence of type and used technology of the metallic coating film on magnetic properties of dielectromagnets.
폴리카보네이트(polycarbonate)는 가볍고, 내충격성 및 가공성이 우수하여 광학기기의 렌즈 및 각종 건축물의 투명 소재 등에 유리의 대체품으로서 널리 이용되고 있으나 낮은 표면경도를 가지고 있어 유통 또는 사용시의 접촉으로 인하여 제품에 손상을 줄 염려가 있다. 따라서 본 연구에서는 폴리카보네이트 필름에 아크릴레이트 올리고머, 모노머, 용매, 염료, 실리콘 아크릴레이트, 그리고 광개시제 등을 다양한 함량비율에 따라 혼합한 코팅용액을 제조하고, 구성 성분의 비율에 따른 폴리카보네이트 필름의 표면 경도, 접착력, 그리고 투과율의 변화를 실험하였다. 그 결과 최대 연필 경도가 2H이고, 접착력과 가시광선 투과율이 우수한 코팅용액의 조성을 얻었다. 색상코팅 실험 결과, 기존 산화물 증착에 의해 구현하던 색상을 본 실험에서 제조한 코팅 용액을 사용하여 거의 대부분 구현할 수 있었으며, 이를 바탕으로 색상 윈도우 렌즈를 제작한 결과, 매우 깨끗하고 균일한 색상과 표면을 가졌다.
Kim, Sun-Hyung;Kim, Jae-Hong;Ahn, Kyung-Hyun;Lee, Seung-Jong
Korea-Australia Rheology Journal
/
제21권2호
/
pp.83-89
/
2009
Coating process plays an important role in information technology such as display, battery, chip manufacturing and so on. However, due to complexity of coating material and fast deformation of the coating flow, the process is hard to control and it is difficult to maintain the desired quality of the products. Moreover, it is hard to measure the coating process because of severe processing conditions such as high drying temperature, high deformation coating flow, and sensitivity to the processing variables etc. In this article, the coating process is to be re-illuminated from the rheological perspectives. The practical approach to analyze and quantify the coating process is discussed with respect to coating materials, coating flow and drying process. The ideas on the rheology control of coating materials, pressure and wet thickness control in patch coating process, and stress measurement during drying process will be discussed.
In this study, 2,5-dichlorobenzophenone was synthesized as a monomer using 1,4-dichlorbenzene, and subsequently, copolymers of benzoyl-p-phenylene and p-phenylene were prepared. The average molecular weight was improved using the low-molecular-weight polymer cutting method. The average molecular weight and glass transition temperature of the synthesized polymers were estimated. The as-prepared polymer was used as a hard coating material, and the coating was conducted on a poly(methyl methacrylate) plate. Furthermore, physical properties of the coatings, such as pencil hardness, adhesive strength, and abrasion resistance, were estimated. As the amount of p-phenylene in the copolymer increased, pencil hardness and abrasion resistance improved. The amount of p-phenylene in the copolymer can be increased to 30 mol% in order to increase the hardness of the coating, and the adhesive strength was insufficient for the copolymers with p-phenylene ratio greater than 35 mol%.
Weatherstrip coatings of urethane and silicon type which are fit to EPDM and thermoplastic materials are used in sealing systems for automotive applications for noise reduction and high slip characteristics for external applications, respectively. Polyurethane binder was successfully synthesized from poly(butyladiphate)diol (PBAD), poly(tetramethylene)glycol (PTMG) and isocyanate as starting materials. Then, polyurethane coating agents were prepared by using various additives. To investigate effects of segment types on the abrasion resistance of polyurethane coating agents, thin films based on polyurethane coating materials were fabricated. With increasing the amount of hard segment in the coating agent, abrasion resistance, modulus and tensile strength of the coating films were improved, but the elongation of the coating films was decreased.
금속염인 lanthanum nitrate를 증류수에 용해시킨 후 실란커플링제인 ${\gamma}$-glycidyloxypropyl trimethoxysilane과 금속산화물인 colloidal silica를 이 용액에 첨가하여 sol-gel법에 의해 유-무기 혼성 용액을 제조하였다. 또한 spiropyran계 광변색 염료를 용매인 tetrahydrofuran에 용해시킨 후 앞서 제조한 혼성 용액과 혼합하여 광 변색 코팅 용액을 제조하였다. 그 후 기재인 polycarbonate 시트에 코팅시키고 열 경화시켜 광 변색성을 갖는 하드 코팅 막을 제조하였다. 이 과정 중 colloidal silica의 첨가량이 코팅 막의 광변색 특성에 미치는 영향을 조사하였다. Colloidal silica의 첨가량이 증가할수록 코팅 막의 소색속도가 빨라졌으며 연필경도가 증가하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.