A Durability Assessment on Complex Deterioration of Concrete with Ground Granulated Blast-Furnace Slag Replacement (복합열화 환경하에서의 고로슬래그미분말 사용 콘크리트의 내구성능 평가)

  • Lee, Seung-Hoon;Kim, Hyung-Doo
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.14 no.2
    • /
    • pp.171-175
    • /
    • 2010
  • This paper presents the experimental results of frost durability characteristics including freezing-thawing and de-icing salt scaling of the concrete for gutter of the road and marine structure. Mixtures were proportioned with the three level of water-binder ratio(W/B) and three binder compositions corresponding to Type I cement with 0%, 30% and 50% GGBS(Ground granulated blast furnace slag) replacement. Also, two different solutions of calcium chloride were used to evaluate their effect on the frost durability resistance. Specially, in case of complex of freezing and thawing with salt and carbonation, the deterioration of concrete surface is evaluated. Test results showed that the BFS30 and BFS50 mixture exhibited higher durability and lower mass loss values than those made with OPC mix and the use of GGBS can be used effectively in terms of economy and frost durability of the concrete to be in complex deterioration. Therefore, the resistance to complex deterioration with freezing-thawing was strongly influenced by the strength and the type of cement.

Characteristic Changes of ZnO Arrester Blocks by Multiple-lightning Impuse Currents (다중 뇌충격전류에 의한 산화아연형 피뢰기 소자의 특성 변화)

  • Gil, Gyeong-Seok;Han, Ju-Seop
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.49 no.12
    • /
    • pp.685-690
    • /
    • 2000
  • Multiple-lightning impulse currents are a general feature of the lightning ground f=flash. It is therefore necessary for lightning arresters used in power systems to be estimated by applying not only a single-lightning impulse current but also a multiple-lightning impulse currents. This paper presents the effects of multiple-lightning impulse currents on deterioration of ZnO arrester blocks. The multiple-lightning impulse generator which can produce quadruple 8/20$[\mus]$ 5[kA] with separation time of 30~120[ms] is designed and fabricated. The total energy applied to the arrester block at each impulse is about 1,200[J]. In experiment, various parameters such as leakage current component, reference voltage, and temperature are measured with the number of applied impulse current. Also, micro-structure changes of the ZnO blocks after applying the single and the multiple-lightning impulse currents of 200 times are compared. The experimental results indicate that the types of arrester blocks are more vulnerable to deterioration or damage by multiple-lightning impulse currents.

  • PDF

A Study on the Consecutive Failure Due to Deterioration in Surge Arresters of the Offshore Wind Farm (해상 풍력발전단지에서 뇌격 시 서지어레스터 열화로 인한 연계 고장 분석)

  • Kim, Jin-Hyuk;Kim, Kyu-Ho;Lee, Jea-Kyun;Woo, Jung-Wook
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.67 no.10
    • /
    • pp.1265-1270
    • /
    • 2018
  • One of the ways to improve the stability of power facilities used in power systems is to use power surge arresters and to protect against transient overvoltages and surges in normal operation. Also it is important to reduce the impact of lightning strikes because lightning can create overvoltage in the grid of the wind turbine and affect power quality. So This paper analyzes the effects of overvoltage and adjacent turbines due to single strike and multi strike to ground impedance changes when the surge arrester is deteriorated in a wind power farm.

Condition Evaluation of Concrete Bridge Decks using CPR (레이더를 이용한 콘크리트 교량의 바닥판 상태평가)

  • Suh, Jin-Won;Rhee, Ji-Young;Lee, Il-Yong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.4 no.4
    • /
    • pp.101-107
    • /
    • 2000
  • In this study, the Ground Penetrating Radar(GPR) was tested to evaluate the condition of concrete decks. Test results obtained by CPR were compared with values measured from drilled cores and damage mapping by the visual survey. It is shown that GPR can provide highly accurate measurements of layer properties of concrete decks and can map areas of deterioration in bridge decks by dielectric constants. The deck condition can be grouped into categories of "good" or "distressed". The ground penetrating radar data shows promise for producing rapid and accurate condition assessment for bridge decks. And these data can be used to evaluate highway bridge condition and make cost-effective bridge deck rehabilitation by accurately estimating the quantity of deteriorated concrete.

  • PDF

A Study on the Optimum Mixture for Reducing Combined Deterioration of Eco-Friendly Concrete Using Waste Fibe (폐섬유를 활용한 친환경 바탕 콘크리트의 복합열화 저감 최적 배합에 관한 연구)

  • Kim, Dae-Geon
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.05a
    • /
    • pp.37-38
    • /
    • 2023
  • As one of the resource recovery projects, this study aims to select natural fibers and synthetic fibers that can be used for concrete mixing among waste fibers and reuse them for the base concrete mixture. Using waste fiber, we seek a solution to the problem of reduced fluidity and hardening time of fiber-reinforced concrete and find the optimal mix of the ground concrete mixed with waste fiber.

  • PDF

Design of the secondary tunnel lining using a ground-primary support-secondary lining interaction model

  • Chang, Seok-Bue;Seo, Seong-Ho;Lee, Sang-Duk
    • 한국지구물리탐사학회:학술대회논문집
    • /
    • 2003.11a
    • /
    • pp.109-114
    • /
    • 2003
  • It is the common practice to reinforce excessively the secondary tunnel lining due to the lack of rational insights into the ground loosening loads. The main load of the secondary lining for drained-type tunnels is the ground loosening. The main cause of the load for secondary tunnel lining is the deterioration of the primary support members such as shotcrete, steel ribs, and rockbolts. Accordingly, the development of the analysis model to consider the ground-primary supports-secondary lining interaction is very important for the rational design of the secondary tunnel lining. In this paper, the interaction is conceptually described by the simple mass-spring model and the load transfer from the primary supports to the ground and the secondary lining is showed by the characteristic curves including the secondary lining reaction curve for the theoretical solution of a circular tunnel. And also, the application of this model to numerical analysis is verified in order to review the potential tool for practical tunnel problems with the complex conditions like non-circular shaped tunnels, multi-layered ground, sequential excavation and so on.

  • PDF

Assessment on the Seawater Attack Resistance of Antiwashout Underwater Concrete (수중불분리성 콘크리트의 해수침식에 대한저항성 평가)

  • 문한영;김성수;안태송;이승태;김종필
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.05a
    • /
    • pp.683-688
    • /
    • 2001
  • In case of constructing the concrete structures under seawater environment, the concrete suffers from deterioration due to penetration of various ions such as chloride, sulfate and magnesium in seawater. Tn the present study, Immersion tests with artificial seawater were carried out to investigate the resistance to seawater attack of antiwashout underwater concrete. From the results of compressive strength, it was found that blended cement concrete due to mineral admixtures such as fly ash(FA) and ground granulated blast-furnace slag(SGC), were superior to ordinary portland cement concrete with respect to the resistance to seawater attack. Moreover, XRD analysis indicated that the formed reactants of ordinary portland cement paste by sulfate and magnesium ions led to the deterioration of concrete. As expected, however, the blended cements with FA or SGC have a good resistance to seawater attack. This paper would discuss the mechanism of seawater deterioration and benefical effects of antiwashout underwater concretes with mineral admixtures.

  • PDF

Freeze-Thaw Resistance of Blended Cement Concrete using Seawater (해수를 사용한 혼합시멘트계 콘크리트의 동결융해 저항성)

  • 문한영;김성수;이승태;김종필;박광필
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.05a
    • /
    • pp.725-730
    • /
    • 2002
  • The durability of concrete involves resistance to freeze-thaw action, corrosion, permeation, carbonation, chemical attack and so on. Generally, properties of concrete have been well understood under the separate action of these deterioration mechanisms. However, in practice, the degradation of concrete usually is the result of combined action of physical and chemical attack and can be accelerated by the combined action of several deterioration mechanisms. In the present study, to evaluate the combined deterioration by freeze-thaw action and seawater attack, ground granulated blast-furnace slag or silica fume concrete with water or seawater as mixing water was exposed to 210 cycles of freeze-thaw action. Tests were conducted to determined the relative dynamic modulus of elasticity and compressive strength. Furthermore, The XRD, SEM and EDS analysis were performed on the deteriorated part of concrete due to freeze-thaw action and seawater attack.

  • PDF

Freeze-Thaw Resistance and Void Characteristic of Blended Cement Concrete using Seawater (해수를 사용한 혼합시멘트계 콘크리트의 동결융해 저항성 및 공극특성)

  • Kim, Seong-Soo;Lee, Seung-Tae;Jung, Ho-Seop;Park, Kwang-Pil
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.589-592
    • /
    • 2006
  • The durability of concrete involves resistance to freeze-thaw action, corrosion, permeation, carbonation, chemical attack and so on. Generally, properties of concrete have been well understood under the separate action of these deterioration mechanisms. However, in practice, the degradation of concrete usually is the result of combined action of physical and chemical attack and can be accelerated by the combined action of several deterioration mechanisms. In the present study, to evaluate the combined deterioration by freeze-thaw action and seawater attack, ground granulated blast-furnace slag or silica fume concrete with water or seawater as mixing water was exposed to 300 cycles of freeze-thaw action. Tests were conducted to determined the relative dynamic modulus of elasticity and compressive strength. Furthermore, The MIP analysis were performed on the deteriorated part of concrete due to freeze-thaw action and seawater attack.

  • PDF

Development of a Deterioration Diagnostic Device for ZnO Arrester by Leakage Current Detection (누설전류 검출에 의한 ZnO 피뢰기의 열화진단장치 개발)

  • Kim, Jae-Chul;Lee, Bo-Ho;Oh, Jung-Hwan;Lee, Young-Gil;Moon, Sun-Ho;Kim, Young-Chun
    • The Transactions of the Korean Institute of Electrical Engineers A
    • /
    • v.48 no.3
    • /
    • pp.184-189
    • /
    • 1999
  • In this paper, we develope a diagnosis device for ZnO arrester by detecting the leakage current in service. To diagnose the deterioration of ZnO arrester, the device detects the total leakage current which flows between an arrester and ground, and analyzes the resistive current(third harmonic current) which is an indicator of deterioration of ZnO arrester. We use the optical cable which can transfer a detected data without a noise, also use a microprocessor for a data storage, processing, and trend analysis. Experiment are executed to verify its performance in laboratory and the results show that the diagnosis device exactly detects the total leakage current and the resistive current, so it can diagnose the deterioration of ZnO arrester. Also the leakage current of ZnO arrester is detected using the developed diagnostic device in field, these results are presented.