Composite thin-walled members for civil engineering application are mainly produced by pultrusion technique, and they are generally made of a polymeric resin system reinforced by E-glass fibers due to economical reason. This material combination results in low elastic moduli of the composite materials and makes the design of composite members to be governed by stability limit state. Therefore the buckling behavior of composite thin-walled members was experimentally investigated in the present study. Axial compression was applied on each specimens by a hydraulic ram and knife edge fixtures were placed at both ends to simulate simple boundary condition. Axial compression, lateral displacements and twisting at the mid-height of each specimen were measured by a set of transducers during buckling test. The experimental buckling loads were compared with analytical results obtained through isotropic formulas. In the calculation of analytical results, elastic properties such as Young's modulus(E) and shear modulus(G) were replaced with EL and GLT obtained from coupon tests, respectively.
Polydimethylsiloxane(PDMS)-containing polyurethane coating materials were synthesized because PDMS-based elastomers have unique properties including an extremely low glass transition temperature, good thermal and oxidative stability, and good dielectric properties. In this experiment a vinyl copolymer which consisted of vinyl chloride, vinyl acetate, vinyl alcohol, and maleic acid was used, and Coronate L was used as a polyisocyanate. PDMS-containing polyurethane was synthesized from polydimethylsiloxane, MDI, and 1,4-butanediol. Films were casted by reaction of viny copolymer, Coronate L, and PDMS-containing polyurethane. Thickness of tile films were $150-170{\mu}m$ and the films were characterized by IR, DSC, and Instron.
Kim, Kong-Soo;Park, Jun-Ha;Kim, Ki-Wun;Kim, Young-Jun
Elastomers and Composites
/
v.33
no.1
/
pp.10-16
/
1998
In DGEBA/DDM system, the curing specimen are many curing factors which can affect on thermal and mechanical properties. This study was performed to prove the effect on curing specimen prepared by changing of the curing factors which are curing time and temperature of DGEBA/DDM system. As a result on thermal and mechanical properties, flexural strength, modulus and glass transition temperature (Tg) were increased with curing time and temperature were increased. It was found that the optimum curing condition of DGEBA/DDM system cure at $150^{\circ}C$ for 3hrs at equivalent ratio of 1/1.
The Transactions of the Korean Institute of Electrical Engineers C
/
v.50
no.4
/
pp.153-160
/
2001
In order to analyze the degradation process of epoxy/glass fiber for outdoor condition, FRP laminate was exposed to high temperature. Then, the degradation process was evaluated by comparing contact angle, surface potential, surface resistivity, and XPS. The experimental results showed that the amount of weight loss, contact angle, surface potential and surface resistivity increased up to 200 $^{\circ}C$ as a function of temperature. These phenomena show the existence of hydrophobic surface. With the change to the hydrophobic surface and the electrical potential and resistivity on FRP surface increased. In XPS to analyze surface chemical structures, the increased hydrophobicity in thermal increase of unsaturated double bond in carbon chains. Aslo, thermal treatment caused the discoloration on the point of treated surface. These phenomena were attributed to the generations of ether group.
Lee Eun Dong;Yoon Sung Ho;Shin Kwang Bok;Jeong Jong Cheol
Proceedings of the Korean Society For Composite Materials Conference
/
2004.04a
/
pp.51-54
/
2004
Testing methods for mechanical properties of the advanced composites were introduced. The mechanical properties, such as tensile properties, compressive properties, in-plane shear properties, flexural properties, and interlaminar shear properties, were evaluated along the warp and the fill directions. The CF3327 of the carbon fabric, the HG1581 of the glass fabric, and the HK285 of the aramid fabric were considered as reinforcements. Epoxy and phenolic resin were used as resin. The experimental results obtained in this study would be applicable in the design and structural analysis for the manufacture of the carbody of the tilting train.
Kim Young-keun;Shin Dong-hyok;Kim Young-min;Park Joung-wuk;Min Jae-Jun
Proceedings of the Korean Society For Composite Materials Conference
/
2004.04a
/
pp.55-58
/
2004
Phenolin resin, prepared form phenol and formaldehyde, is one of the oldest thermosetting resins available. Phenolic resins are cured via condensation polymerization with evolution of water, which in molding process is a big problem. The use of phenolic resins in glass fiber composites is growing, primarily due to their low flame spread, low smoke generation and low smoke toxicity properties. SMC of phenolics has been rearched since the 1986. The technology challenge was to match resin viscosity, handling and cure with those for the polyester SMC to avoid any special processing for fabricators and end users. Phenolic SMC was chosen because of the ease of molding to the required shape with light- weight, thin wall structure and with excellent fire protection.
Lee Chang-Hun;Kim Jin-Bong;Park Ji-Sang;Hwang Byung-Sun
Proceedings of the Korean Society For Composite Materials Conference
/
2004.04a
/
pp.258-261
/
2004
This paper contains the tension-tension, the tension-tension bearing and the tension-tension steel bolt joint fatigue characteristics of glass fabric/phenol composite laminates. The experimental results show that the bearing and the steel bolt joint fatigue characteristics of the material is so excellent compared with the simple tension fatigue characteristics, that there are no needs of additional strengthening for mechanical joint parts when the parts are properly designed.
As the first step in discussing the reliability of composite structures, a fundamental study was performed to obtain the scattering characteristics of glass-fiber reinforced plastics (GFRP) and woven carbon fiber reinforced plastics (WCFRP) as well as a reference metal. The Euler buckling load was obtained experimentally for each material. The experiments were conducted for specified rectangular specimens with simply supported edges. A new attachment to realize the simply support boundary conditions for composite materials have been prepared before these experiments. The scattering data in the results for GFRP and WCFRP composites were compared with those of a typical metal of aluminum alloy. The experimental data were also compared with numerical simulations including the uncertainties.
Polymeric composite structures used in ground transportation applications such as the carbody of tilting train may be exposed to a ground environmental conditions during long-term missions. In this study, the degradation of mechanical and physical properties of graphite/epoxy composite and glass fabric/phenol composite under ground environmental conditions was investigated. Accelerated environmental conditions of ultraviolet radiation, temperature, and moisture were considered. Several types of specimens were used to investigate the effects of environmental conditions on mechanical properties of the composites. Also, storage shear modulus, loss shear modulus, and tan 8 were measured as a function of exposure times through a dynamic mechanical analyzer. Finally, composite surfaces exposed to environmental conditions were examined using a scanning electron microscope.
Various materials are used as electrical barrier materials, such as glass, insulating oil, gas, paper and polymer. These materials shut off electricity from conductor as a barrier and separate as well as support conductor from outside environment while using electrical equipment. Polymers are generally used for cable insulation material. Recently environmental regulation are reinforced and eco-friendly materials are in trend.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.