• Title/Summary/Keyword: Glass composites

Search Result 910, Processing Time 0.022 seconds

Properties of Nano-Hybrid Coating Films Synthesized from Colloidal Silica-Silane (콜로이달 실리카와 실란으로부터 합성된 나노하이브리드 코팅 박막의 특성)

  • Na, Moon-Kyong;Ahn, Myeong-Sang;Kang, Dong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.232-233
    • /
    • 2006
  • In recent years the interest in organic/inorganic hybrid materials has increased at a fast rate. Nano organic-inorganic hybrid composites have shown advantages for preparing hard coating layers. Especially, nano hybrid composite has low environmental pollution. It has high transparency, hardness, toughness, thermal dissociation temperature, hydrophobicity by using nano sized inorganic material. There are many ways in which these materials may be synthesized, a typical one being the use of silica and silanes using the sol-gel process. The structure of sol-gel silica evolves as a result of these successive hydrolysis and condensation reactions and the subsequent drying and curing. The sol-gel reactions are catalyzed by acids and produce silica sol solutions. The silica sol grows until they reach a size where a gel transition occurs and a solid-like gel is formed. Colloidal silica(CS)/silane sol solutions were synthesized in variation with parameters such as different acidity and reaction time. In order to understand their physical and chemical properties, sol-gel coating films were fabricated on glass. From all sol-gel solutions, seasoning effect of sol-gel coating layer on glass was observed.

  • PDF

Influence of Styrene Contents on Retraction Behaviors of SBR Vulcanizates (SBR 가황물의 회복 거동에 미치는 스티렌 함량의 영향)

  • Choi, Sung-Seen;Woo, Chang-Su;Chang, Dong-Ho
    • Elastomers and Composites
    • /
    • v.40 no.4
    • /
    • pp.237-241
    • /
    • 2005
  • Influence of the styrene content on the retraction behaviors of SBR vulcanizates was studied. SBRs with different styrene contents of 15 and 21 wt% were used. The vulcanizate with low styrene content started to recover at lower temperature than that with high one. The recovery rate of the vulcanizate with low styrene content was slower than that with high one. The recovery difference between the two vulcanizates with different styrene contents was larger for the carbon black-filled vulcanizates than for the silica-filled ones. The experimental results were explained with the glass transition temperature and modulus.

Evaluation of the radiopacity of restorative materials with different structures and thicknesses using a digital radiography system

  • Yaylaci, Ayla;Karaarslan, Emine Sirin;Hatırli, Huseyin
    • Imaging Science in Dentistry
    • /
    • v.51 no.3
    • /
    • pp.261-269
    • /
    • 2021
  • Purpose: The aim of this study was to evaluate the radiopacities of various types of restorative materials with different thicknesses compared with enamel, dentin, and aluminum. Materials and Methods: Four bulk-fill resins, 2 hybrid ceramics, 2 micro-hybrid resin composites, 6 glass ionomer-based materials, 2 zinc phosphate cements, and an amalgam were used in the study. Twelve disk-shaped specimens were prepared from each of 17 restorative materials with thicknesses of 1 mm, 2 mm, and 4 mm (n=4). All the restorative material specimens with the same thickness, an aluminum (Al) step wedge, and enamel and dentin specimens were positioned on a phosphor storage plate and exposed using a dental X-ray unit. The mean gray values were measured on digital images and converted to equivalent Al thicknesses. Statistical analyses were performed using 2-way analysis of variance and the Bonferroni post hoc test(P<0.05). Results: Radiopacity was significantly affected by both the thickness and the material type (P<0.05). GCP Glass Fill had the lowest radiopacity value for samples of 1 mm thickness, while Vita Enamic had the lowest radiopacity value for 2-mm-thick and 4-mm-thick samples. The materials with the highest radiopacity values after the amalgam were zinc phosphate cements. Conclusion: Significant differences were observed in the radiopacities of restorative materials with different thicknesses. Radiopacity was affected by both the material type and thickness.

Electrical and Optical Properties of Carbon Nanotube Networks Formed on Glass Substrate by Dip-Coating Method (담지 방법을 통해 유리 기판 위에 형성된 탄소나노튜브 네트워크의 전기적 및 광학적 특성)

  • Jang, Eui-Yun;Kang, Tae-June;Im, Hyung-Wook;Kim, Dae-Weon;Kim, Yong-Hyup
    • Composites Research
    • /
    • v.21 no.1
    • /
    • pp.8-15
    • /
    • 2008
  • Single-walled carbon nanotube networks(SWNT-networks) were uniformly formed on a glass substrate by the dip-coating method. The changes of electrical and optical properties of SWNT-networks were investigated with respect to processing variables including number of dip, concentration of SWNT-colloidal solution, withdrawal velocity. Consequently, the sheet resistance and transmittance of the SWNTs-networks were sensitively controlled by the processing variables. The networks have highly uniform sheet resistance and optically excellent transmittance within the range of visible ray.

Epoxy Matrix with Adding Dopamine for Improving Mechanical Property and Interfacial Adhesion with Glass Fiber (도파민이 첨가된 에폭시 기지재의 기계적 물성 및 유리섬유 간 계면접착력 향상)

  • Shin, Pyeong-Su;Kim, Jong-Hyun;Baek, Yeong-Min;Park, Ha-Seung;Park, Joung-Man
    • Composites Research
    • /
    • v.32 no.2
    • /
    • pp.96-101
    • /
    • 2019
  • Interfacial adhesion between fiber and resin are related to composites performance, so it is very important to evaluate them accurately. In this study, the interfacial properties of microdroplets under fatigue loading conditions were evaluated. The mechanical properties and interfacial adhesion of epoxy resin with dopamine were studied. Tensile specimens were prepared to evaluate mechanical properties and epoxy microdroplets specimens were used for the evaluation of interfacial adhesion. In addition, in the microdroplet fatigue test, the same diameter of the microdroplet was used and the experiment was performed under the same conditions. As a result, it was confirmed that mechanical and interfacial properties were improved when dopamine was applied to epoxy resin through tensile and microdroplet experiments. It is considered that dopamine improves the degree of curing of the epoxy resin and imparts hydroxyl groups to the epoxy resin to increase the mechanical properties and the interfacial adhesion between the glass fibers.

Evaluation of Mechanical Performance Considering Prolonged Length of Glass Fiber-Reinforced Composite on Structure Weakness by Thermal Stress at Secondary Barrier in Cryogenic Liquified Gas Storage (극저온 액화가스 화물창 2차방벽 구조 열 응력 취약 부 Prolonged 길이 고려 유리섬유 강화 복합재 기계적 물성 평가)

  • Yeon-Jae Jeong;Hee-Tae Kim;Jeong-Dae Kim;Jeong-Hyun Kim;Seul-Kee Kim;Jae-Myung Lee
    • Composites Research
    • /
    • v.36 no.4
    • /
    • pp.246-252
    • /
    • 2023
  • A secondary barrier made of glass fiber reinforced composites has been installed infinitely using automatic bonding machine(ABM) in membrane type LNG cargo containment system (CCS). At the same time, significant thermal stress due to cryogenic heat shrinkage has occurred in the composite on the non-bonding area between the adhesive fixation at both ends. There have been studies from the perspective of structural safety evaluation taking this into account, but none that have analyzed mechanical property taking an prolonged length into account. In this study, 2-parameter Weibull distribution statistical analysis was used to standardize reliable mechanical property for actual length, taking into account the composite's brittle fracture of ceramic material with wide fracture strength dispersion. Related experimental data were obtained by performing uniaxial tensile tests at specific temperatures below cryogenic condition considering LNG environment. As a result, the mechanical strength increased about 1.5 times compared to -20℃ at -70℃ and initial non-linear behavior of fiber stretched was suppressed. As the temperature decreased until the cryogenic, the mechanical strength continued to increase due to cold brittleness. The suggested mechanical property in this study would be employed to secure reliable analysis support material property when assessing the safety of secondary barrier's structures.

Spring-back in GFR / CFR Unsymmetric Hybrid Composite Materials (유리섬유 / 탄소섬유 강화 비대칭 하이브리드 복합재료의 스프링 백)

  • Jung Woo-Kyun;Ahn Sung-Hoon;Won Myung-Shik
    • Composites Research
    • /
    • v.18 no.6
    • /
    • pp.1-8
    • /
    • 2005
  • The fiber-reinforced composite materials have been advanced for various applications because of their excellent mechanical and electromagnetic properties. On their manufacturing processes, however, thermo-curing inherently produces the undesired thermal deformation mainly from temperature drop from the process temperature to the room temperature, so called spring-back. The spring-back must be understood especially in the hybrid composites in order to design and fabricate desired shape. In this research, (glass fiber / epoxy) + (carbon fiber / epoxy) unsymmetric hybrid composites were fabricated under various conditions such as cure cycle, laminate thickness, stacking sequence and curing sequence. Coupons were made and spring-back were measured using coordinate measuring machine (CMM). Using the Classical Lamination Theory (CLT) and finite element analysis (ANSYS), the behavior of spring-back were predicted and compared with the experimental data. The results from CLT and FEA agreed well with the experimental data. Although, the spring-back could be reduced by lowering curing temperature, at any case, the spring-back could not be removed completely.

Fabricaton of PEMFC separators with conducting polymer composites by injection molding process and evaluation of moldability and electrical conductivity of the separators (전도성 복합재료를 이용한 PEMFC용 separator 사출성형 제조 및 전기전도성 평가)

  • Yoon, Yong-Hun;Lim, Seung-Hyun;Kim, Dong-Hak
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.11 no.4
    • /
    • pp.1361-1366
    • /
    • 2010
  • This research aims to develop polymer composites which can be used for PEMFC separators by injection molding process. Considering the moldability and stiffness, we used PPS(Poly(phenylene sulfide)) and PP(Polypropylene) as base resin. In order to improve electrical conductivity and physical properties, we chose glass fiber, carbon fiber, carbon black, and both expanded graphite and synthetic graphite. The 3 type composites are prepared for injection molding of PEMFC separators. and CAE(Computer Aided Engineering) analysis was conducted to optimize injection processing parameters(injection pressure, heat time, mold temperature etc.). We did successfully fabricate the separators by injection molding, and measure the electrical conductivity of the samples by using four point probe device. Conclusively, PP/SG/CB composite showed better both electrical conductivity and moldability than the others.

Nondestructive Evaluation and Interfacial Damage Sensing of PVDF embedded Polymer Composites using Micromechanical Techniques and Acoustic Emission (Micromechanical 시험법과 AE를 이용한 PVDF 함침 고분자 복합재료의 계면손상감지능 및 비파괴적 평가 연구)

  • Kong, Jin-Woo;Park, Joung-Man;Kim, Ki-Bok;Yoon, Dong-Jin
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2002.10a
    • /
    • pp.216-219
    • /
    • 2002
  • Conventional piezoelectric lead-zirconate-titanate (PZT) senor has high sensitivity, but it is very brittle. Recently polymer films such as polyvinylidene fluoride (PVDF) have been used use as a sensor. The advantages of PVDF are the flexibility and mechanical toughness. Simple process and possible several shapes are also additional advantages. PVDF sensor can be directly embedded and attached to a structure. In this study, PVDF sensor was embedded in single glass fiber/epoxy composites whereas PZT sensor with AE was attached to single fiber composites (SFC). Piezoelectric sensor responds to interfacial damage of SFC. The signals measured by PVDF sensor were compared to PZT sensor. PZT sensor detected the signals of fiber fracture, matrix crack, interfacial debonding and even sensor delamination, whereas PVDF sensor only detected fiber fracture signals so far, because PZT sensor is much more sensitive than current PVDF sensor. Wave voltage of fiber fracture measured by PVDF sensor was lower than that of PZT sensor, but the results of fast Fourier transform (FFT) analysis were same. Wave velocity using two PZT sensors was also studied to know the internal and surface damage effect of epoxy specimens.

  • PDF

A Study on the Crashworthiness Evaluation and Performance Improvement of Tilting Train Carbody Structure made of Sandwich Composites (틸팅열차의 샌드위치 복합재 차체 구조물에 대한 충돌안전도 평가 및 향상방안 연구)

  • Jang, Hyung-Jin;Shin, Kwang-Bok;Han, Sung-Ho
    • Composites Research
    • /
    • v.24 no.5
    • /
    • pp.9-16
    • /
    • 2011
  • This paper describes the crashworthiness evaluation and performance improvement of tilting train made of sandwich composites. The applied sandwich composite of carbody structure was composed of aluminum honeycomb core and glass/epoxy & carbon/epoxy laminate composite facesheet. Crashworthiness analysis of tilting train was carried out using explicit finite element analysis code LS-DYNA 3D. The 3D finite element model and 1D equivalent model were applied to save the finite element modeling and calculation time for crash analysis. The crash conditions of tilting train were conducted according to four crash scenarios of the Korean railway safety law. It found that the crashworthiness analysis results were satisfied with the performance requirements except the crash scenario-2. In order to meet the crashworthiness requirements for crash scenario-2, the stiffness reinforcement for the laminate composite cover and metal frames of cabmask structure was proposed. Consequentially, it has satisfied the requirement for crash scenario-2.