서울市 一部 水道栓水中 重金屬에 관한 調査硏究 (A Study on Heavy Metals at the Consumer s Tap in Seoul)

  • Lee, Byung Mu
    • 한국환경보건학회지
    • /
    • 제10권2호
    • /
    • pp.41-51
    • /
    • 1984
  • This study was performed using samples collected at Myungryundong and at Reservoirs. The purpose of this study was to investigate the differences of water quality between tap and raw water, and to analyse drinking water quality by Fe, Zn from corroded galvanized steel pipe. Results were as follows 1. The older the pipe was, the higher the concentration of Ferrum and Zinc was (t-test : p<0.05). Ferrum and Zinc also exceeded the limits in the older galvanized steel pipe. I think that this comes from the corrosion of pipe. 2. Mercury, Arsenic, Cadmium, Lead, Chomium, Argentum and Aurum not detected in raw water were not detected in tap water. Cobalt, Bismuth and Molybudenum detected in raw water were not detected in tap water. I think that this comes from the quality of raw water, the result of water treatment and the improbability of detection of above metals in water delivery system. 3. Silicon measured 2.4698ppm in raw water, but it ranged from 0.4769ppm to 1.982 ppm in tap water. Manganese measured 0.0638ppm in raw water, but it ranged from 0.0026ppm to 0.0198ppm in 17cases(31%) out of 55samples in tap water. I think that this comes from the water treatment. 4. Aluminium not detected in raw water was found in 17 cases (31%) out of the samples (55cases). It may be considered as the use of coagulants $Al_2(SO_4)_3$. $18H_2O$ and PAC (Poly Aluminium Chloride). The concentration of copper in tap water was much higher in 2 cases(3.6%) out of the samples(55) than that of copper in raw water. I think that this may come from the use of ${CuSO}_4$, the preventive of algae growth, and the result of chlorination, but further study must be necoessary to support the proof.

  • PDF

상·하수 배관재의 수 환경에서 부식진전도 연구 (Research of Corrosion Growth Degree According in Liquid Environment of Waterworks and Sewer Piping Material)

  • 박경동;기우태;유형주;김동욱
    • 한국기계가공학회지
    • /
    • 제5권4호
    • /
    • pp.33-40
    • /
    • 2006
  • The quality of the supply water which is supplied to consumer is not the thing of water after filtrating but the thing of water from faucet through pipe. As a result, heavy metals and microorganism, that is the major materials, which cause the distrust of the supply water is generated by supply process. Especially, the heavy metal is generated by the corrosion of waterworks. Besides, rupture by corrosion of pipe becomes the factor of supply water's pollution in waterworks and the factor of pollution of the soil and environment in drain pipe. Therefore, this research examined the weight reduction electric potential measure to measure the corrosion degree of piping materials after testing the corrosion of piping materials(Copper Pipe, Galvanized Steel Pipe, Stainless Steel Pipe) which is generally used at the moment in various corrosion environments(subterranean water, supply water, 3.5% NaCl, 3.5% $HNO_3$). And let me show basic design data about problem occurrence such as leakage water, rust water, inside and outside corrosion from this.

  • PDF

플라스틱 온실의 폭설피해 방지를 위한 가지주 장치 개발 (Development of a Temporary Pole Supporting System to Protect the Plastic Greenhouses from Heavy Snow Damage)

  • 남상운
    • 한국농공학회지
    • /
    • 제44권4호
    • /
    • pp.107-113
    • /
    • 2002
  • The pipe framed and arch shape plastic greenhouse, which is the most popular greenhouse in Korea, is relatively weak in snowdrift. Reinforcement of rigid frame or column is required to reduce the damage from heavy snow in this type. But additional rigid frames or columns decrease light transmissivity or workability, and increase construction cost. So it is desirable to prepare some temporary poles and to install them when the warning of heavy snow is announced. This study was carried out to develop the temporary pole supporting system using galvanized steel pipes for plastic housing and to evaluate the safe snow load on a temporary pole. A pipe connector, which is inserted in the top of pipe used in the temporary pole and supports the center purline, was designed and manufactured to be able to carry the upper loads safely. And a bearing plate was safely designed and manufactured in order to carry the loads acting on it to the ground. When temporary poles of ${\phi}$ 25 pipe are installed at 2.4m interval, it shows that the single span plastic greenhouses with 5~7 m width are able to support the additional snow depth of 13.9~25.3 cm beyond the snow load supported by main frame.

비금속관 설비관통부의 슬리브 종류에 따른 내화성능 비교 (Comparison of the Fire Resistance Performance of Firestop Systems on Non-Metallic Pipes, Based on the Type of Through-Penetration Sleeve Used)

  • 정아영;최홍범;박진오;이형도
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2023년도 봄 학술논문 발표대회
    • /
    • pp.301-302
    • /
    • 2023
  • In this study, we aimed to identify changes in fire resistance according to the type of sleeves used for pipe penetrations and to examine their accreditation of fire resistance performance and use them as basic data. The test results of fire resistance according to the type of sleeve used in non-metallic pipe facilities showed that the temperature on the support side was higher for sleeves with higher thermal conductivity. For the temperature on the surface of the pipes, in the case of galvanized steel plates, steel pipes, and structures without sleeves, the highest temperature was observed after the expansion of the firestop material for 46 to 53 minutes and then decreased. PVC sleeves showed a steady increase in temperature until 53 minutes, after which the temperature did not increase further. In addition, for non-metallic pipes, the effect of the type of sleeve on fire resistance is considered to be insignificant because the lower part (heating direction of the furnace) under the support structure is cut off to block the heat during the two-hour fire resistance test.

  • PDF

온실 환경 하에서 20년 경과된 농업용 강관의 부식 및 강도변화 (Corrosion and Strength Changes of Agricultural Steel Pipes Elapsed 20 Years under the Greenhouse Environment)

  • 남상운;류희룡;최만권;신현호
    • 생물환경조절학회지
    • /
    • 제29권2호
    • /
    • pp.196-201
    • /
    • 2020
  • 파이프 골조 온실의 내구성 증대를 위하여 4가지의 부식방지 처리를 한 파이프를 실험온실 내부에 설치하여 20년경과 후 표면부식 상태와 강도 변화 실험을 실시하였다. 대기 중에 노출된 지상부위에서 무처리 파이프는 강도가 1.3%정도 줄었지만 다른 처리와의 차이는 거의 없는 것으로 나타났다. 지하 매설부위에서 중방식 처리한 파이프의 강도는 0.6%정도 줄어 거의 변화가 없었으나 무처리는 15.7% 감소하는 것으로 나타났다. 그리고 방청 페인트나 아스팔트 도포는 4.2~4.4%정도 감소하는 것으로 나타났다. 지상부위는 모든 시료에서 심한 부식상태를 보이지 않았다. 중방식 처리는 변화가 없었고, 방청페인트 처리도 녹은 발견되지 않고 약간의 변색만 있었다. 아스팔트 도포는 검게 변색되고 약간의 녹이 발견되었으며, 무처리는 표면의 20~30%정도가 녹슨 것으로 나타났다. 지하 매설부위 무처리 파이프의 경우에는 전체가 완전히 녹슬어 있었고, 아스팔트 도포한 파이프도 표면의 80~90%가 녹슬어 있었다. 방청페인트 처리는 20~30%정도 녹슬어 있었고, 중방식 처리는 거의 변화가 없었다. 중방식 처리는 지하 매설부위에서도 확실한 부식 방지 효과를 보이는 것을 확인할 수 있었고, 방청페인트 처리도 어느 정도 부식 방지 효과를 나타내고 있으므로 현장에 적용할 수 있을 것으로 판단된다.

기초형식 및 지반조건에 따른 하우스파이프기초의 인발저항력 특성 (Characteristics of Uplift Capacity of House Pipe Foundation according to Foundation Types and Soil Conditions)

  • 송창섭;장웅희;최득호;김정철
    • 한국농공학회논문집
    • /
    • 제62권1호
    • /
    • pp.117-126
    • /
    • 2020
  • The area of facility horticulture in Korea is increasing rapidly, the single-span pipe house which uses galvanized steel pipe as the main rafters occupies 78.7% of the facility area. Lightweight structures such as the single-span pipe house are vulnerable to meteorological disasters such as strong winds, economic losses of the state, local governments and farmers are continuing as construction does not meet the design standards. In order to minimize economic losses in the horticultural specialty facilities sector, the Rural Development Administration has been operating the horticultural disaster resilient standard for horticultural specialty facilities since April 2007. The only standard for the pipe connector is the disaster resilient standard, there is no standard for the uplift capacity of the house pipe foundation and the research on it is also insufficient. The purpose of this study is to investigate the characteristics of uplift capacity according to the foundation type, compaction ratio and embedded depth through soil box test. The results of the maximum uplift capacity according to the type, compaction ratio and embedded depth can be used as the basic data for the basic design of the pipe house conforming to the disaster resilient standard. Due to the limitation of soil box test, it may be different from the behavior of pipe house installed on site. In the future, the field test and the actual pipe house should be made and supplemented by comparing this result with the field test values.

수돗물속 생물막 형성의 초기 세균 (Initial Bacterial Groups in the Development of Biofilm in Drinking Water)

  • 이동근
    • 한국환경보건학회지
    • /
    • 제33권5호
    • /
    • pp.428-433
    • /
    • 2007
  • To clarify the pioneer group in the development of biofilms in high chlorine residual water, a semi-pilot model system was operated and 16S rDNA V3 targeted PCR-DGGE was submitted. Biofilm formation occurred rapidly in the model of a drinking water distribution system. It reached $10^3\;CFU/cm^2$ or more on the surface of stainless steel, PVC, and galvanized iron in chlorinated (1.0 mg/l) water within a week. Within a week, uncultured Proteobacteria- and Bacillales group-like sequences were detected and Sphingomonas-like sequences were identified from all season and all pipe materials tested. Hence Sphingomonas species were regarded as the potential pioneer group in the development of biofilm in drinking water and this results would be useful for the prevention of biofilm formation and safety of drinking tap water.

플라스틱 온실용 아연도강관의 내식성 증대방법 (Experiment on the Improvement in Corrosion Resistance of Galvanized Steel Pipes for Plastic Greenhouse)

  • 남상운;노상목
    • 한국농공학회:학술대회논문집
    • /
    • 한국농공학회 2005년도 학술발표논문집
    • /
    • pp.175-180
    • /
    • 2005
  • Experiments on the improvement in durability of pipe framework for plastic greenhouse were carried out. Effect of protection treatment such as primer and paint coating for new pipes and old rusted ones were evaluated by change of rusty degree and yield strength. The experiments have been conducted during five years until now but it was too short to find the clear differences. However, there was a little improvement in durability of greenhouse pipes by painting after removal of rust. And also component and corrosion characteristics of pipes being used in greenhouses were analyzed, and several countermeasures for protection from corrosion were reviewed.

  • PDF

Effect of Distribution System Materials and Water Quality on Heterotrophic Plate Counts and Biofilm Proliferation

  • 장영철;정권
    • Journal of Microbiology and Biotechnology
    • /
    • 제14권6호
    • /
    • pp.1114-1119
    • /
    • 2004
  • The biofilms on pipe walls in water distribution systems are of interest since they can lead to chlorine demand, coliform growth, pipe corrosion, and water taste and odor problems. As such, the study described in this paper is part of an AWWARF and Tampa Bay Water tailored collaboration project to determine the effect of blending different source waters on the water quality in various distribution systems. The project was based on 18 independent pilot distribution systems (PDS), each being fed by a different water blend (7 finished waters blended in different proportions). The source waters compared were groundwater, surface water, and brackish water, which were treated in a variety of pilot distribution systems, including reverse osmosis (RO) (desalination), both membrane and chemical softening, and ozonation-biological activated carbon (BAC), resulting in a total of 7 different finished waters. The observations from this study consistently demonstrated that unlined ductile iron was more heavily colonized by a biomass than galvanized steel, lined ductile iron, and PVC (in that order) and that the fixed biomass accumulation was more influenced by the nature of the supporting material than by the water quality (including the secondary residual levels). However, although the bulk liquid water cultivable bacterial counts (i.e. heterotrophic plate counts or HPCs) did not increase with a greater biofilm accumulation, the results also suggested that high HPCs corresponded to a low disinfectant residual more than a high biofilm inventory. Furthermore, temperature was found to affect the biofilms, plus the AOC was important when the residual was between 0.6 and 2.0 mg $Cl_2/l$. An additional aspect of the current study was that the potential of the exoproteolytic activity (PEPA) technique was used along with a traditional so-called destructive technique in which the biofilm was scrapped off the coupon surface, resuspended, and cultivated on an R2A agar. Both techniques indicated similar trends and relative comparisons among the PDSs, yet the culturable biofilm values for the traditional method were several orders of magnitude lower than the PEPA values.

수돗물 수질에 따른 옥내급수관 부식에 미치는 영향분석 (The Corrosion Effect of the Water Pipelines in Buildings according to Drinking Water Quality)

  • 유순주;박수정;안경희;김현구;김창수;정일록;박영복
    • 한국물환경학회지
    • /
    • 제24권6호
    • /
    • pp.701-708
    • /
    • 2008
  • As a countermeasure for reduction of corrosion in the delivery and distribution pipes used for tap water, materials for the pipelines in-houses and the effect of water quality on corrosivity of water pipelines were investigated in the distribution system of Han river. As the corrosion index at 6 water purification facilities of Han river, average Langelier Saturation Index (LI) of raw and finished water were -1.0 and -1.4 respectively and average Larson Index (LR) were 9.5 and 9.9, respectively. And also corrosion potential showed corrosivity in finished water (-431~-462 mV) as well as raw water (-426~-447 mV). This results indicate that tap water quality of han river have corrosivity. To understand the corrosivity effect in pipe material used for premise distribution system, water quality of stagnant tap water and tap water were analyzed and the differences between them were calculated. The difference concentration of iron, copper and zinc were $12.9{\mu}g/L$, $31.0{\mu}g/L$ and $45.0{\mu}g/L$ respectively in galvanized steel pipe for use more than 15 years and showed highest concentration. As a result, the control to corrosivity in the water pipelines, corrosivity control treatment in the water purification system can be applied. In advance it is necessary to monitor corrosivity of water quality using corrosive index because corrosivity may differ from the seasonal and regional characteristics and water chemicals dosage. For the future the guideline for corrosion index have to be established.