레이저 위빙을 이용한 Al 6k21-T4 합금의 용접 강도 향상 (A Study to Improve Weld Strength of Al 6k21-T4 Alloy by using Laser Weaving Method)

  • 김병훈;강남현;박용호;안영남;김철희;김정한
    • Journal of Welding and Joining
    • /
    • 제27권4호
    • /
    • pp.49-53
    • /
    • 2009
  • For Al 6k21-T4 alloy, linear laser welding produced the lower shear-tensile strength than the base metal. This study improved the shear-tensile strength by using the weaving laser at the optimized welding condition, i.e., 2mm weaving width and 25Hz frequency. The large weaving width increased the weld width, therefore improving the joint strength. For the specimen of low strength, the porosity was distributed continuously along the intersection between the plates and fusion line. However, for the optimized welding condition, large oval-shaped porosities were located only in the advancing track of the concave part. Regardless of the welding condition, solidification cracking was initiated at the intersection and propagated through small porosities in the weld part. furthermore, the concave part had more significant porosity in the weld and HAZ, respectively than the convex part. The continuity of porosities played a key role to determine the strength. And, the weaving width was an important parameter to control the strength.

Pulsed Nd : YAG 레이저 조사와 불소 화합물 도포가 초기 우식 법랑질의 표면 경도에 미치는 영향 (Effects of Pulsed Nd:YAG Laser Irradiation and Fluoride Compound Application on Surface Hardness of Incipient Carious Lesion in Enamel of Bovine Teeth)

  • Jun-Bong Kwag;Woo-Cheon Kee
    • Journal of Oral Medicine and Pain
    • /
    • 제21권2호
    • /
    • pp.207-224
    • /
    • 1996
  • This study was designed to determine the most effective concentration of fluoride and energy density of laser irradiation for the anticarious effect. For this study surface hardness in enamel was measured before and after irradiation with pulsed Nd;YAG laser and the topical application of fluoride. Of the permanent mandibular anterior hovine teeth, healthy, carious free ones were used. Three hundred specimens were made. Specimens within 25~45 Vickers hardness numbers were assigned to 20 control and experimental stoops ; each containing 15 specimens. After forming artificial carious lesions, 10 J/$\textrm{cm}^2$, 20 J/$\textrm{cm}^2$, and 30 J/$\textrm{cm}^2$ energies were irradiated on the enamel surface of each experimental group. Also NaF, NH4F, Elmex gel(amine fluoride) and APF gel fluoride compounds were applied topically. Next, all the specimens were placed into the pH circulatory procedures for eight days. Vickers hardness numbers were measured using a microhardness tester. Surface changes of the enamel were observed using an scanning electron microscope. The comparative ana1ysis yielded the following results : 1. The reduction of surface hardness of the enamel surface was less in all groups with fluoride application than in the group without fluoride application. 2. The APF gel croup with 10 J/$\textrm{cm}^2$ irradiation showed the lowest reduction of surface hardness. 3. The reduction of surface hardness of the enamel surface in the group of laser irradiation without fluoride application not showed any significant difference according to the energy density of the laser. 4. Under the scanning electron microscope, in enamel irradiated with 10J/$\textrm{cm}^2$ showed appearance similar to acid etching surface. In enamel irradiated with 20 J/$\textrm{cm}^2$, line enamel crack was detected. In enamel irradiated with 30j/$\textrm{cm}^2$, severe enamel crack and fusion of enamel were detected. These results suggest that one could obtain the best anticariogenic effects without damage to teeth in the group of application of APF gel after laser irradiation with 10 J/$\textrm{cm}^2$.

  • PDF