• 제목/요약/키워드: Frost damage ar early age

검색결과 2건 처리시간 0.02초

단열양생재 변화 및 열선 전력용량 차이에 따른 슬래브 콘크리트의 온도이력 특성 (Characteristic of Temperature History of Slab concrete by the Change of Insulation Curing Material and Difference of Heated cable Power Capacity.)

  • 정은봉;안상구;정상현;고경택;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 춘계 학술논문 발표대회
    • /
    • pp.334-336
    • /
    • 2013
  • In this study, the temperature history was evaluated for the improved bubble sheets combining hot wires and PE films, which were developed under the extreme environmental condition of -10℃ and applied on the top surface of slab to prevent initial damage by freezing. Results can be summarized as follows. If improved bubble sheets combining hot wires with different capacity on double and quadruple bubble sheets are used, the temperature history for all materials decreased to 2~3℃ below zero but all test materials except Type 1 secured the accumulative temperature of 45° D·D at 7 days of material age, required for the prevention of initial freezing damage. This indicates the bubble sheets can prevent the initial damage by freezing.

  • PDF

-10℃ 조건에서의 열선 열용량 크기 변화에 따른 슬래브 콘크리트의 온도이력 특성 (Characteristics of Temperature History of Slab concrete by the Change of Hot wire Heat Capacity at -10℃)

  • 정은봉;안상구;정상현;고경택;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 춘계 학술논문 발표대회
    • /
    • pp.75-77
    • /
    • 2013
  • In this study, the characteristics of temperature history was evaluated for three hot wires with different capacity installed in slab concrete which are relatively thin. Results can be summarized as follows. First, for the case of material using 5W hot wire, all decreased to below zero at or around 24 hours. Similarly, the material using 20W hot wire decreased to 2℃ below zero at or around 80 hours but satisfied the accumulative temperature of 45° D·D at 7 days of material age. On the other hand, the case of 30W hot wire, the biggest capacity, showed the high temperature history of 5℃ in average at all areas except the corners. Thus, the target accumulative temperature was secured at or around the 3 days of material age. Considering the above, the initial damage by freezing can be prevented only if 20W or higher hot wires are used for the slabs at -10℃ of extremely low temperature environment.

  • PDF