실링 테이프 적용에 따른 시공조인트 균열 저항성 평가 (Evaluation of Crack Resistance of Cold Joint as Usage of Sealing Tape)

  • 이재준;이선행;김두병;이진욱
    • 한국도로학회논문집
    • /
    • 제20권3호
    • /
    • pp.1-9
    • /
    • 2018
  • PURPOSES : In order to evaluate a crack resistance at cold joint, sealing tape was adopted to apply at cold joint instead of typical tack coat material(RSC-4). The sealing tape was made by hot sealing material. The crack resistance as function of environmental and traffic loading was measured with visual observation. METHODS : In this study, the crack resistance was evaluated as function of environmental and traffic loading. The freeze-thaw method was adopted for environmental loading of asphalt pavement. condition. The damage of cold joint under freeze-thaw action is initiated by ice expansion load and accelerated by the interfacial damage between new and old asphalt pavement. The traffic loading was applied with wheel tracking machine on the cold joint area of the asphalt pavement for 3 hours at $25^{\circ}C$. The evaluation of crack resistance was measured with visual observation. The freeze-thaw results shows that the sealing tape was significantly increased the crack resistance based on. RESULTS : To estimate the crack resistance at cold joint area due to the environmental loading, the Freeze-thaw test was conducted by exposing the product to freezing temperature(approximately $-18^{\circ}C$) for 24 hours, and then allowing it to thaw at $60^{\circ}C$ for 24 hours. The tack coat material(RSC-4) was debonded after 21 cycles of the Freeze-thaw test. The first crack was observed after 14 freeze-thaw cycle with RSC-4 material. But, the sealing tape was not debonded after 24 cycle test. Also, the sealing tape shows the better performance of the crack resistance under the traffic loading with wheel track test. The crack was generated the under traffic loading with RSC-4(tack coating), however, the crack was not shown with sealing tape. It indicates that the sealing tape has a strong resistance of tensile stress due to traffic loading. CONCLUSIONS :Based on limited laboratory test result, a performance of crack resistance using the sealing tape is better than that of general tack coat material(RSC-4). It means that the sealing tape is possible to extend a pavement service life because the crack, one of the main pavement distresses, will be delayed.

Integrity Evaluation of Ice Plugged Pipes Applied on Short Jacket

  • Park, Yeong-Don;Son, Geum-Su
    • Nuclear Engineering and Technology
    • /
    • 제34권2호
    • /
    • pp.105-116
    • /
    • 2002
  • In special industrial fields such 3s nuclear power plants and chemical plants, it is often necessary to repair system components without plant shutdown or drainage of system having many piping structures which may have hazardous or expensive fluid. A temporary ice plugging method for blocking internal flow is considered as a useful method in that case. According to the pipe freezing guideline of the nuclear power plant, the length of a freezing jacket must be longer than twice of the pipe diameter. However, for applying the ice plugging to short pipes which do not have enough freezing length because of geometrical configuration, it is inevitable to use shorter jacket less than twice of the pipe diameter. In this study, the integrity evaluation for short pipes in the nuclear power plant Is conducted by an experiment and the finite element analysis. From the results, the ice plugging process in short pipes can be safely carried out without any plastic deformation and fracture.

결빙 관막음시 배관내 유체 결빙현상의 실험적 연구 (An Experimental Study for the Liquid Freezing Phenomena in a Pipe During Ice Plugging)

  • 박영돈;조현철;최병익;김귀순
    • 대한기계학회논문집B
    • /
    • 제25권3호
    • /
    • pp.366-372
    • /
    • 2001
  • The ice plugging process consists of placing liquid nitrogen around a pipe and removing heat until the water in the pipe freezes and provides a solid plug or seal against fluid movement. This technique enables us to repair or inspect a pipe system without shutdown of entire system. A set of test apparatus for investigation of the liquid freezing phenomena during ice plugging is prepared. This study shows the characteristics of the liquid freezing and the heat transfer with various pipe and freezing jacket conditions. And in case there is flow of the fluid inside the pipe, the flow rate which can be able to form the ice plug is identified with the effect of the pipe diameter and freezing jacket length on the plug formation. The permissible maximum flow rate for the complete plug formation is approximately proportional to the freezing jacket length at the same pipe diameter condition.

내한촉진제를 사용한 한중콘크리트의 실구조물 적용에 관한 연구 (Application of Cold Weather Concreting with Accelerator for Freeze Protection to Full Scale Structures)

  • 김영진;백태룡;이상수;원철;김동석
    • 콘크리트학회논문집
    • /
    • 제15권2호
    • /
    • pp.254-262
    • /
    • 2003
  • 본 연구는 내한촉진제를 사용한 한중콘크리트의 배합선정, 제조 생산, 타설 및 양생 등 실구조물에 대한 적용성에 관한 것이다. 내한촉진제의 사용량 및 물-시멘트비의 선정이 한중콘크리트의 초기동해방지 및 강도증진성상에 커다란 영향을 주기 때문에 배합설계단계에서 충분한 검토가 필요하다. 내한촉진제를 사용한 굳지 않은 콘크리트의 유동성상은 전반적으로 동일 물-시멘트비에서 유사한 결과를 나타나고 있었으며, 고성능감수제의 종류에 따른 경시변화 검토결과, 초기 플로우 및 유동성 손실이 적게 나타나는 폴리카르본산계 고성능감수제가 멜라민계 보다 우수한 것으로 판단된다. 강도관리용 공시체는 기존의 현장봉함 양생보다는 실구조물의 온도이력과 유사한 경향을 보이는 간이단열방법으로 양생하는 것이 유효할 것으로 판단된다. 로지스틱곡선을 이용하여 각 양생 방법별 내한촉진제를 사용한 한중콘크리트의 강도증진성상을 검토한 결과, 강도증진에 미치는 내한촉진제의 영향이 상온조건보다는 저온조건 하에서 효과가 높은 것으로 나타났다. 내한촉진제를 사용한 콘크리트는 평균 외기온 $-2^{\circ}C$(최저기온$-12^{\circ}C$)에서 간단한 비닐양생만으로 초기동해 방지를 위해 필요한 압축강도 $5N/{mm}^2$의 발현이 가능하였고 재령28일에 목표로 하는 소요강도를 만족시켰다.