Strength Property Improvement of OCC-based Paper by Chemical and Mechanical Treatments (II) (골판지 고지의 물리화학적 처리에 의한 강도향상(제2보))

  • Lee, Jong-Hoon;Seo, Yung B.;Jeon, Yang;Lee, Hak-Lae;Shin, Jong-Ho
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.32 no.2
    • /
    • pp.1-7
    • /
    • 2000
  • In the previous experiment, it was found that OCC pre-treatment with Hobart mixer at 20-25% consistency for 3 hrs or more followed by the application of the equal refining time, caused the increase of tensile strength, burst strength, compressive strength and tear resistance, compared to the no pre-treated. Four completely different fibers, which were Hw-BKP, Sw-BKP, White ledger, and OCC were selected for this experiment to investigate the effect of mechanical pre-treatment process on different fibers. From the experiment, it was found that the mechanical pre-treatment did not decrease fiber length at all, but decreased freeness, com-pared to the no pre-treated, when the same refining time was applied. WRVs of the pre-treated fibers were higher than the no pre-treated at the same freeness level. It was speculated that the mechanical pre-treatment induced only hydrophilic nature of fibers without damaging fiber length by delaminating fiber walls. The fiber surface area and the physical strength differences of handsheets will be discussed in the next publication.

  • PDF

Strength Property Improvement of OCC-based Paper by Chemical and Mechanical Treatments (III) - Handsheet physical properties - (골판지 고지의 물리화학적 처리에 의한 강도향상(제3보) - 수초지의 물리적 특성변화 -)

  • Lee, Jong-Hoon;Seo, Yung B.;Jeon, Yang;Lee, Hak-Lae;Shin, Jong-Ho
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.32 no.2
    • /
    • pp.8-15
    • /
    • 2000
  • This study is a continuation of the previous experimental analysis and is mostly focused on handsheet strength properties. Four completely different fibers, which were Hw-BKP, SW-BKP, White ledger, and OCC, were selected to investigate the effect of mechanical pre-treatment by Hobart mixer on handsheet strehgth properties. After equal time mechanical pre-treatment, the fibers were refined with laboratory valley beater for 10, 20 and 30 minutes, and handsheets were prepared from the fibers for physical strength comparison. Handsheets from SW-BKP and OCC showed 5-30% increase of breaking length, burst index, tear index, and compression index while handsheets from HW-BKP and White ledger no increase except tear index. In Hobart mixer pre-treatment, HW-BKP and White ledger fibers were easily attached to the wall of the mixer bowl and mechanical action was not effectively applied. The fiber length of Hw-BKP and White ledger were 0.837 mm and 1.591 mm, respectively, while SW-BKP and OCC were 2.744 mm and 2.033 mm, respectively, in weight weighted length. The effective mechanical pre-treatment seems to be related to the fiber length. Tear indexes of the pre-treated furnish were much higher than no pre-treatment at the same breaking length level.

  • PDF

Strength property improvement of OCC-based paper by chemical and mechanical treatments (2) (골판지 고지의 물리화학적 처리에 의한 강도향상 (제2보))

  • Lee, Jong-Hoon;Seo, Yung B.;Jeon, Yang;Lee, Hak-Lae;Shin, Jong-Ho
    • Proceedings of the Korea Technical Association of the Pulp and Paper Industry Conference
    • /
    • 2000.04a
    • /
    • pp.69-69
    • /
    • 2000
  • In the previous experiment, it was found that OCC pre-treatment with Hobat mixer at 20-25% consistency for 3 hrs or more followed by the application of the equal refining time, caused the increase of tensile strength, burst strength, compressive strength and tear resistance, compared to the no pre-treated. Four completely different fibers, which were Hw-BKP, Sw-BKP, White ledger, and OCC were selected for this experiment to investigate the effect of mechanical pre-treatment process on different fibers. From the experiment, it was found that the mechanical pre-treatment did not decrease fiber length at all, but decreased freeness, compared to the no pre-treated, when the same refining time was applied WRVs of the pre-treated fibers were higher than the no pre-treated at the same freeness level. It was speculated that the mechanical pre-treatment induced only hydrophilic nature of fibers without damaging fiber length by delaminating fiber walls. The fiber surface area and the physical strength differences of handsheets will be discussed in the next publication.

  • PDF

Strength property improvement of OCC-based paper by chemical and mechanical treatments (3 - handsheet physical properties) (골판지 고지의 물리화학적 처리에 의한 강도향상 (제3보 - 수초지의 물리적특성변화))

  • Lee, Jong-Hoon;Seo, Yung B.;Jeon, Yang;Lee, Hak-Lae;Shin, Jong-Ho
    • Proceedings of the Korea Technical Association of the Pulp and Paper Industry Conference
    • /
    • 2000.04a
    • /
    • pp.70-70
    • /
    • 2000
  • This study is a continuation of the previous experimental analysis and is mostly focused on handsheet strength properties. Four completely different fibers, which were Hw-BKP, Sw-BKP, white ledger, and OCC, were selected to investigate the effect of mechanical pre-treatment by Hobart mixer on handsheet strength properties. After equal time mechanical pre-treatment, the fibers were refined with laboratory valley beater for 10, 20 and 30 minutes, and handsheets were prepared from the fibers for physical strength comparison. Handsheets from SW-BKP and OCC showed 5-30% increase of breaking length, burst index, tear index, and compression index while handsheets from HW-BKP and white ledger no Increase except tear index. In Hobart mixer pre-treatment, HW-BKP and white ledger fibers were easily attached to the wall of the mixer bowl and mechanical action was not effectively applied. The fiber length of Hw-BKP and white ledger were 0.837mm and 1.591 mm, respectively, while SW-BKP and OCC were 2.744 mn and 2.033 mm, respectively, in weight weighted length. The effective mechanical pre-treatment seems to be related to the fiber length. Tear indexes of the pre-treated furnish were much higher than no pre-treatment at the same breaking length level.

  • PDF

Influence of Chemical and Mechanical Treatments of the Screened Short Fibers from OCC on Paper Properties -Strength Property Improvement of OCC-based Paper by Chemical and Mechanical Treatment (IV)- (골판지 고지섬유의 단섬유분의 물리화학적 처리에 관한 연구 -골판지 고지의 물리화학적 처리에 의한 강도향상 제4보-)

  • Lee, Jong-Hoon;Seo, Yung B.;Choi, Chan-Ho;Jeon, Yang
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.33 no.4
    • /
    • pp.7-14
    • /
    • 2001
  • Recycled fibers usually give slow drainage in the paper forming process, which limits the application of more refining to the recycled fibers for improving paper strength and formation. To use recycled fibers more effectively, especially OCC, developing very efficient handling technique of short fibers and fines is inevitable. We tried to make hard flocs of fractionated short fibers and fines, which were the main cause of slow drainage, by adding excessive amount of retention aid selectively on them. This technique was proved to increase drainage considerably, but to decrease strength properties, compared to the conventional technique of adding the same amount of polymers to the whole furnish in the lab test. The bonding capability of short fibers and fines in Korean OCC was very poor. Various chemical treatment on the short fibers and fines of the Korean OCC did not improve their bonding and optical properties. One of the reasons of no improvement in their properties was their high amount of ashes.

  • PDF

Effect of Different Conditions of Sodium Chloride Treatment on the Characteristics of Kenaf Fiber Bundles

  • Tamaryska, SETYAYUNITA;Ragil, WIDYORINI;Sri Nugroho, MARSOEM;Denny, IRAWATI
    • Journal of the Korean Wood Science and Technology
    • /
    • v.50 no.6
    • /
    • pp.392-403
    • /
    • 2022
  • Currently, composite board manufacturing using natural fibers has the potential to expand owing to environmental awareness. To produce a composite board, treatment is required to improve the mechanical and physical properties of the natural fibers. In this study, sodium chloride (NaCl) was used for the chemical treatment. However, studies on chemical treatments using NaCl are limited. This study aimed to investigate the characteristics of kenaf fibers after NaCl treatment. The NaCl treatment concentrations were 1, 3, and 5 wt.% at room temperature, with soaking durations of 1, 2, and 3 h. The tensile strength, strain, and Young's modulus were measured to evaluate the mechanical properties of the fibers. The fiber bundle diameter, weight change owing to treatment, and contact angle were determined to analyze the effect of NaCl treatment. The kenaf fiber bundle treated with 5 wt.% NaCl for 3 h exhibited the highest tensile strength, Young's modulus, reduction in fiber bundle diameter, weight change, and decrease in contact angle compared to those of untreated fiber bundles. The tensile properties of the fiber bundle exhibited a tendency to decrease with increasing fiber bundle diameter. Increasing the soaking duration from 1 to 2 h did not result in a significant decrease in the fiber bundle diameter or an increase in tensile strength. However, a further increase in the soaking duration from 2 to 3 h resulted in a considerable decrease in the fiber bundle diameter and an increase in the tensile strength.

Preference of Subterranean Termites among Community Timber Species in Bogor, Indonesia

  • Arinana, ARINANA;Mohamad M., RAHMAN;Rachel E.G., SILABAN;Setiawan Khoirul, HIMMI;Dodi, NANDIKA
    • Journal of the Korean Wood Science and Technology
    • /
    • v.50 no.6
    • /
    • pp.458-474
    • /
    • 2022
  • Many methods have been explored to increase the palatability of pine (Pinus merkusii), the most common wood used for termite baiting. However, because of the undersupply of pine in Indonesia, it is crucial to vary the wood species for termite baiting and look for potential alternatives. Furthermore, various studies have shown that baiting time influences the intensity and pattern of termite attacks. Therefore, the present research aimed to study the preferences of subterranean termites and find the ideal baiting time among community wood species from Bogor, West Java, as a baiting alternative to pine. The woods tested were Acacia mangium (acacia), Falcataria moluccana (sengon), Anthocephalus cadamba (jabon), Maesopsis eminii (manii), Swietenia mahagoni (mahogany), Hevea brasiliensis (rubberwood), and P. merkusii (pine). Field tests were carried out based on the American Society for Testing and Materials D 1758-06 at the Arboretum, Faculty of Forestry and Environment, IPB University, with a baiting time of one to six months. The results led to the identification of four species of termites, namely Microtermes sp., Macrotermes sp., Shedorhinotermes sp., and Capritermes sp.. The frequency of termite attacks on the test site reached 93.1%. Rubberwood was the most potential wood bait for subterranean termites, indicated by the highest average weight loss value (65.8%) with a shorter optimal baiting time (up to one month) than that of other tested woods.

Effect of Different Conditions of Sodium Chloride Treatment on the Characteristics of Kenaf Fiber-Epoxy Composite Board

  • SETYAYUNITA, Tamaryska;WIDYORINI, Ragil;MARSOEM, Sri Nugroho;IRAWATI, Denny
    • Journal of the Korean Wood Science and Technology
    • /
    • v.50 no.2
    • /
    • pp.93-103
    • /
    • 2022
  • Currently, biofibers are used as a reinforcement in polymer composites for structural elements and construction materials instead of the synthetic fibers which cause environmental problems and are expensive. One of the chemicals with a pH close to neutral that can be potentially used as a modified fiber material is sodium chloride (NaCl). Therefore, this study aims to investigate the characteristics of a composite board made from NaCl-treated kenaf fiber. A completely randomized design method was used with consideration of two factors: the content of NaCl in the treatment solution (1 wt%, 3 wt%, and 5 wt%) and the duration of immersion of fibers in the solution (1 h, 2 h, and 3 h). The NaCl treatment was conducted by soaking the fibers in the solution for different durations. The fibers were then rinsed with water until the pH of the water reached 7 and subsequently dried inside an oven at 80℃ for 6 h. Kenaf fiber and epoxy were mixed manually with the total loading of 20 wt% based on the dry weight of the fiber. Physical and mechanical properties of the fibers were then evaluated based on JIS A 5908 particleboard standards. The results showed that increasing NaCl content in the fiber treatment solution can increase the physical and mechanical properties of the composite board. The properties of fibers treated with 5 wt% NaCl for 3 h were superior with a modulus of elasticity of 2.085 GPa, modulus of rupture of 19.77 MPa, internal bonding of 1.8 MPa, thickness swelling of 3%, and water absorption of 10.9%. The contact angle of untreated kenaf fibers was 104°, which increased to 80° and 73° on treatment with 1 wt% and 5 wt% NaCl for 3 h, respectively.